GB/T 713.3 09MnNiDR Steel Plate | 09MnNiDR -70°C Vessel Plate
What is GB/T 713.3 09MnNiDR Steel?
GB/T 713.3 09MnNiDR, also written 09MnNiDR steel plate, GB/T 3531 09MnNiDR and 09MnNiDR -70°C vessel plate, is a Chinese nickel low-temperature pressure-vessel plate. Current product rules sit in GB/T 713.3-2023. That book replaces GB/T 3531-2014. Buyers still search GB/T 3531 and 09MnNiDR. The name itself is the search term: about 0.09% C, Mn, Ni, and DR for low-temperature vessel. Yield is 300 MPa at 6–16 mm. Tensile is 440–570 MPa. Delivery is normalizing or normalizing plus tempering. Impact is −70 °C, 60 J through 80 mm. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade.
A purchase order that only says “-70 °C vessel plate” is incomplete. Write GB/T 713.3 09MnNiDR. Do not ship 16MnDR against a 09MnNiDR drawing. 16MnDR is the −40 °C workhorse in the same book. Do not ship 08Ni3DR against a 09MnNiDR drawing. 08Ni3DR is 3.5Ni and now sits in GB/T 713.4-2023.
This page is not Q345R. It is not 15MnNiNbDR. It is not Q420DR / Q460DR. It is not 06Ni9DR.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | GB/T 713.3 09MnNiDR | Confirmed |
| Product Specification | GB/T 713.3-2023 (replaces GB/T 3531-2014) | Applied |
| Service idea | Low-temperature vessels, not lower than −70 °C | Confirmed |
| Steel type | Killed Mn-Ni low-temp vessel plate | Confirmed |
| Usual delivery | N or N+T | Confirmed |
| Yield idea | 300 MPa at 6–16 mm | Confirmed |
| Tensile | 440–570 MPa at 6–16 mm | Confirmed |
| Impact | −70 °C / 60 J (to 80 mm) | Confirmed |
| Thickness range | 6–120 mm | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | Americas, Europe, Middle East, Africa, Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. ASME comparisons belong on ASME SA203 and ASME SA662, not as automatic substitutes.
Chemical Composition
GB/T 713.3 09MnNiDR heat analysis follows GB/T 713.3 Table 1. Product analysis follows the permitted deviations in GB/T 713.1. Write “heat + product analysis” on the order if both are required.
Heat Analysis and Product Analysis — GB/T 713.3 09MnNiDR
| Element | Heat Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.12 | 0.14 |
| Silicon (Si) | 0.15 – 0.50 | 0.13 – 0.55 |
| Manganese (Mn) | 1.20 – 1.60 | 1.15 – 1.70 |
| Phosphorus (P), max | 0.015 | 0.020 |
| Sulfur (S), max | 0.005 | 0.008 |
| Nickel (Ni) | 0.30 – 0.80 | 0.28 – 0.85 |
| Molybdenum (Mo), max | 0.08 | 0.10 |
| Niobium (Nb), max | 0.040 | 0.050 |
| Nitrogen (N), max | 0.012 | 0.014 |
| Acid-soluble aluminum (Alt), min | 0.020 | 0.015 |
Nickel is required. Carbon is lower than on 16MnDR. Sulfur is tighter. That package is why 09MnNiDR holds −70 °C and 16MnDR does not. Do not treat 16MnDR chemistry as 09MnNiDR. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.
Mechanical Properties
Yield starts at 300 MPa at 6–16 mm and falls as thickness rises.
Tensile and Yield — GB/T 713.3 09MnNiDR
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) | Impact |
|---|---|---|---|
| 6 – 16 | 300 | 440 – 570 | −70 °C / 60 J |
| 16 – 36 | 280 | 430 – 560 | −70 °C / 60 J |
| 36 – 60 | 270 | 430 – 560 | −70 °C / 60 J |
| 60 – 80 | 260 | 420 – 550 | −70 °C / 60 J |
| 80 – 120 | 260 | 420 – 550 | −60 °C / 60 J |
| Density | 7.85 g/cm³ | 7.85 g/cm³ | — |
Elongation is commonly 23% min. Do not quote −70 °C on a 100 mm plate without checking the 80–120 mm column. That band drops to −60 °C unless the order names a tighter extra.
Do not treat 440–570 MPa tensile as permission to stamp SA203 Gr.A or SA662 Gr.C. SA-203 Grade A is 2.25Ni. 09MnNiDR nickel is only 0.30–0.80%.
Material Comparison
| Grade | Book | Service idea | Swap? |
|---|---|---|---|
| GB/T 713.3 16MnDR | −40 °C Mn | 315 / 490–620 | No |
| GB/T 713.3 09MnNiDR | −70 °C Mn-Ni | 300 / 440–570 | This page |
| GB/T 713.3 15MnNiNbDR | −50 °C Ni-Nb | Different temp | No |
| GB/T 713.3 13MnNiDR | Ni sister | Different strength | No |
| GB/T 713.4 08Ni3DR | 3.5Ni cryogenic | Different book | No |
| SA203 Gr.A | 2.25Ni ASME | Higher Ni | No |
Equivalent Material Grades
These names are project-comparison grades. They are not automatic substitutes.
| Designation | Standard / region | Notes |
|---|---|---|
| GB/T 713.3 09MnNiDR | GB/T 713.3-2023 | Name on this page |
| GB/T 3531-2014 09MnNiDR | Replaced book | Same commercial name |
| 11MnNi5-3 | EN 10028-4 | Closest EN comparison |
| 13MnNi6-3 | EN 10028-4 | Related EN Ni grade |
| 16MnDR | GB/T 713.3 | −40 °C sister |
| 15MnNiNbDR | GB/T 713.3 | −50 °C Ni-Nb sister |
| 13MnNiDR | GB/T 713.3 | Ni sister |
| 11MnNiMoDR | GB/T 713.3 | Ni-Mo sister |
| SA203 Gr.A | SA-203 | 2.25Ni, not 0.3–0.8Ni |
| SA203 Gr.D | SA-203 | 3.5Ni |
| SA662 Gr.C | SA-662 | Low-temp carbon comparison |
| SA516 Gr.70 | SA-516 | Carbon vessel, no Ni |
| P355NL1 | EN 10028-3 | Fine-grain, usually no required Ni |
| ASTM A36 steel plate | A36 | Structural, not vessel |
ASME SA515 is not 09MnNiDR.
−70 °C Pressure-Vessel Service
GB/T 713.3 09MnNiDR is selected for ethylene-related equipment, cold-region tanks, separators and other pressure equipment that name the Chinese −70 °C Mn-Ni vessel book. Nickel at 0.30–0.80% is the reason this grade holds lower temperature than 16MnDR. It is not 3.5Ni or 9Ni plate. Those grades now sit in GB/T 713.4.
It is not automatically an ASME Section VIII plate. If the vessel is ASME, the drawing should name SA203 Gr.A, SA203 Gr.D or SA662 Gr.C with the impact extras written.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia. It is not QT Ni-Cr-Mo like SA543 Type B Cl.1. Stainless inquiries belong on ASME SA240 or ASTM A240.
Weldability
09MnNiDR is killed Mn-Ni low-temperature vessel plate. Welding is production welding, and Code welding when the equipment is a vessel.
Qualify procedures to the applicable code. For ASME work that happens to use a dual-named plate, use ASME Section IX. Consumables should match the 440–570 MPa tensile band and the −70 °C toughness target, not a 16MnDR-only procedure and not a 3.5Ni SA203 Gr.D procedure. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized or normalized-and-tempered GB/T 713.3 09MnNiDR. As-rolled shipment is not the default.
If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the Cr-Mo 650 °C / 680 °C temper route used on 15CrMoR or 12Cr2Mo1R. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.
The certificate lists GB/T 713.3 09MnNiDR; heat number; heat analysis; product analysis when ordered; tensile results to the correct thickness column; N or N+T; impact at −70 °C or −60 °C by thickness. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for 09MnNiDR -70°C vessel plate:
- Thickness: commonly 6 mm – 120 mm
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
- Cut-to-length plates and nest sizes inside those limits
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.
Tolerances
Dimensional limits follow GB/T 713.1 and the mill rolling standard named on the order. Do not apply ASTM A36/A36M structural tolerances to a Chinese vessel plate without writing them. UT to GB/T 2970, JB/T 4730 / NB/T 47013.3, EN 10160 or ASTM A435 / A577 / A578 is added when the order names it.
Supplementary Requirements
Most export GB/T 713.3 09MnNiDR orders add extras. SHH STEEL does not assume them.
Charpy details. Temperature, energy, location and orientation. GB default is −70 °C / 60 J to 80 mm, −60 °C above 80 mm.
Product analysis. Add this when the destination file wants finished-plate chemistry.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. UT per the named method.
Z-direction. Z15 / Z25 / Z35 when the drawing names it.
HIC / NACE / SSC. Only when written.
Third-party. EN 10204 3.2, with inspectors arranged for US, Mexican, European, Middle East, Japanese or Korean documentation packages.
Applications
| Industry | Typical components |
|---|---|
| −70 °C vessels | GB/T 713.3 09MnNiDR shells |
| Ethylene and cold-region tanks | 09MnNiDR courses |
| Separators and drums | 09MnNiDR plate from SHH STEEL |
| Fabrication | 09MnNiDR cut to nest sizes |
Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to:
- North America: USA, Mexico
- South America: Argentina, Peru and other South American ports
- Central America: El Salvador
- Europe: Spain, Netherlands, Germany and surrounding ports
- Middle East: UAE, Saudi Arabia and nearby Gulf ports
- Africa: South Africa
- South / Southeast Asia: India, Thailand, Singapore, Vietnam, Philippines
- East Asia: Japan, Korea
Typical trade terms on this grade: FOB Shanghai, CIF Singapore, CIF Antwerp, CIF Manzanillo, plus Houston, Rotterdam, Jebel Ali, Callao, Buenos Aires, Barcelona, Durban, Laem Chabang, Ho Chi Minh, Manila, Mumbai, Yokohama and Busan.
Typical lead time for GB/T 713.3 09MnNiDR:
- Ex-stock: about 5–7 days
- Mill rolling, standard N or N+T: about 45 days
- Simulated PWHT, 3.2 or extra NDE: about 2 months
Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading. Packing is seaworthy, with edge protection and marking in English as specified on the order.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS / GB steel to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia. On GB/T 713.3 09MnNiDR that means mill pricing, 09MnNiDR chemistry reported as heat analysis and as product analysis when ordered, recorded N or N+T, tensile results to the correct thickness column, −70 °C impact, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. 09MnNiDR is not 16MnDR. 09MnNiDR is not 15MnNiNbDR. 09MnNiDR is not 08Ni3DR. 09MnNiDR is not SA203 Gr.A. If the drawing names −40 °C only, we will not force 09MnNiDR. If the drawing names 3.5Ni, we will not ship 09MnNiDR and call it close.
Company scope: global steel mill sourcing partner – SHH STEEL.
FAQ
-
What is 09MnNiDR steel plate?
- 09MnNiDR is a GB/T 713.3 Mn-Ni low-temperature pressure-vessel plate. Yield is 300 MPa at 6–16 mm and tensile is 440–570 MPa. Impact is −70 °C / 60 J through 80 mm. Delivery is N or N+T. SHH STEEL supplies this plate as a global steel mill sourcing partner.
-
Does GB/T 713.3 replace GB/T 3531 for 09MnNiDR?
- Yes. GB/T 713.3-2023 replaces GB/T 3531-2014. The commercial name 09MnNiDR is unchanged.
-
What is the equivalent of 09MnNiDR?
- The closest EN comparison is 11MnNi5-3. ASME comparisons are often SA662 or SA203 Grade A, but nickel content is not the same. Dual marking is possible only when both books are fully met.
-
How is 09MnNiDR different from 16MnDR?
- 16MnDR is −40 °C without required nickel. 09MnNiDR requires 0.30–0.80% Ni and holds −70 °C.
-
How is 09MnNiDR different from 08Ni3DR?
- 08Ni3DR is 3.5Ni and now sits in GB/T 713.4. 09MnNiDR is 0.30–0.80% Ni in GB/T 713.3.
-
Can SHH STEEL ship 09MnNiDR to Mexico, South America or Southeast Asia?
- Yes. SHH STEEL has supplied plates to Mexico, Argentina, El Salvador, Peru, Spain, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea, as well as the USA, Europe and the Middle East.
-
What is the delivery time for 09MnNiDR?
- Ex-stock about 5–7 days. Standard N or N+T mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
Conclusion
GB/T 713.3 09MnNiDR Steel Plate is Chinese −70 °C Mn-Ni pressure-vessel plate at the 300 MPa yield step, 440–570 MPa tensile at 6–16 mm, N or N+T delivery. Whether the inquiry says GB/T 713.3 09MnNiDR, GB/T 3531 09MnNiDR or 09MnNiDR -70°C Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 09MnNiDR chemistry, heat and product analysis when ordered, recorded N or N+T, −70 °C impact, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies GB/T 713.3 09MnNiDR -70°C Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Singapore / Antwerp / Manzanillo.
Contact SHH STEEL for mill rolling, stock inquiry, N or N+T, 3.2 inspection or a quotation.
GB/T 713.3 09MnNiDR Steel Plate, GB/T 3531 09MnNiDR, 09MnNiDR -70°C vessel plate, 09MnNiDR supplier, global steel mill sourcing partner SHH STEEL