ASME SA516GR60 Carbon Steel Plates | SA516GR60 China steel mill-Direct Supply - SHH STEEL

ASME SA516 GRADE 60 | ASME SA516GR60 Carbon Steel Plates

ASME SA516 Grade 60 carbon steel plates are high-strength, ideal for pressure vessels and boilers. With 415-550 MPa tensile and 220 MPa yield, they suit 400°C, 300 bar use per ASME Section VIII, widely applied globally by SHH STEEL.
Specification:
ASME SA-516/SA-516M for pressure vessels and boilers
Dimensions:
5-500mm thick, 4600mm max wide, 12000mm max long
Hardness/Density:
ASME SA516 GR 60 Hardness 120-170 HB, Density 7.85g/cm³
Equivalent Material:
P295GH (EN10028-2), SPV315 (JISG3115), 16MnR/Q245R (GB/T713)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grade
Supplementary Requirements
Applications
Why Choose SHH STEEL
FAQ
Conclusion

General Description

As an expert at SHH STEEL, I’m pleased to detail our ASME SA516 Grade 60 Carbon Steel Plates, also known as ASME SA516GR60 or ASME SA516 GR 60. This grade is a versatile carbon steel designed for moderate and lower temperature pressure vessels, boilers, and storage tanks, providing a tensile strength of 415-550 MPa and a minimum yield strength of 220 MPa. It’s engineered for applications requiring good toughness and weldability under pressures up to 300 bar and temperatures up to 400°C, making it a staple in industries like oil & gas and power generation. SHH STEEL, a leading carbon steel exporter, supplies these plates in thicknesses from 5mm to 500mm, with widths up to 4600mm and lengths to 12000mm, offering flexibility for large-scale projects.

The normalized condition of ASME SA 516 GR 60 plates refines the grain structure, boosting ductility and impact resistance, which is vital for welded constructions in challenging environments. For buyers looking for ASME SA516 Gr.60 properties or equivalents, this grade offers cost-effectiveness and strict compliance with ASME Section VIII Division 1, the code for pressure-containing equipment. SHH STEEL’s ASME SA516 GR.60 plates are thoroughly tested for ultrasonic inspection and Charpy impact, delivering defect-free performance that meets global standards.

With a balanced carbon equivalent (CE ≤0.40 per AWS D1.1), these plates facilitate seamless welding, reducing the risk of hydrogen-induced cracking. The material’s ability to retain properties after heat treatment makes it ideal for multi-pass welding in vessel fabrication. SHH STEEL’s dedication to quality means every plate comes with mill test certificates, giving buyers confidence in critical applications like petrochemical storage and power boilers.

Material Specification

As an production expert at SHH STEEL, I can confirm that ASME SA516 Grade 60 carbon steel plates are governed by ASME SA-516/SA-516M, the ASME Boiler and Pressure Vessel Code Section II Part A adaptation of ASTM A516/A516M-17.

This specification outlines requirements for carbon steel plates for moderate and lower temperature service, ensuring suitability for welded pressure vessels and boilers.

SHH STEEL complies fully with this standard, providing plates in normalized or stress-relieved conditions to optimize mechanical properties. The specification supports thicknesses from 5mm to 500mm, widths up to 4600mm, and lengths to 12000mm, with custom dimensions available for large-diameter vessel designs.

Ultrasonic examination per ASME SA-20 or ASTM A435 Class 1 detects laminations, guaranteeing defect-free material, while dual certification with EN 10028-2 or GB/T 713 is offered for international compatibility. This makes our ASME SA516 GR 60 plates a reliable choice for global buyers, supported by mill test certificates for complete traceability.

Specification Element Requirement SHH STEEL Compliance Keywords
Primary Standard ASME SA-516/SA-516M ASME Section VIII SA516 Gr.60 specification
Thickness Range 5mm-500mm (custom) Mill Test Certificate SA516 Gr.60 dimensions
Width/Length Up to 4600mm / 12000mm Custom fabrication available SA516 Gr.60 size options
Ultrasonic Testing No laminations >0.25% thickness Class 1 per ASME SA-20 SA516 Gr.60 inspection
Heat Treatment Normalized or stress-relieved 900-950°C furnace control SA516 Gr.60 heat treat

Chemical Composition

At SHH STEEL, we ensure the chemical composition of ASME SA516 Grade 60 is tightly controlled per ASME SA-516/SA-516M to guarantee weldability and toughness. The maximum carbon content is 0.23%, preventing brittleness, while manganese (0.60-1.20%) boosts strength.

Phosphorus and sulfur are capped at 0.035% each to minimize cracking, and silicon (0.15-0.40%) supports deoxidation during steelmaking. Optional vanadium (≤0.02%) refines grains, improving low-temperature impact resistance.

Our testing per ASME SA-350 maintains a Carbon Equivalent (CE) ≤0.40 per AWS D1.1, making ASME SA516 GR 60 plates a reliable choice for buyers searching for “ASME SA516 GR 60 chemical composition.”

Element Content (%) Standard Limit Test Method Role Keywords
Carbon (C) ≤0.23 0.23 max ASME SA-350 Strength without brittleness SA516 Gr.60 carbon
Manganese (Mn) 0.60-1.20 0.60-1.20 ASME SA-350 Toughness, hardenability SA516 Gr.60 manganese
Phosphorus (P) ≤0.035 0.035 max ASME SA-350 Reduces brittleness SA516 Gr.60 phosphorus
Sulfur (S) ≤0.035 0.035 max ASME SA-350 Improves weldability SA516 Gr.60 sulfur
Silicon (Si) 0.15-0.40 0.15-0.40 ASME SA-350 Deoxidation, fluidity SA516 Gr.60 silicon
Vanadium (V) ≤0.02 0.02 max ASME SA-350 Grain refinement SA516 Gr.60 vanadium

Mechanical Properties

Mechanical Properties

As an expert at SHH STEEL, I can assure you that ASME SA516 Grade 60 carbon steel plates deliver strong mechanical properties, tested per ASME SA-8 for tensile/yield, ASME SA-23 for impact, and ASME SA-466 for fatigue. With a minimum yield strength of 220 MPa and tensile range of 415-550 MPa, these plates support high load-bearing capacity, while 21% elongation ensures ductility for forming.

The impact energy of 27J at -20°C prevents brittle failure, and the modulus of elasticity (200 GPa per ASME SA-111) provides structural stability. The fatigue limit (230 MPa est. per ASME SA-466) varies with surface finish, optimized by our grinding process.

This makes ASME SA516 GR.60 plates a reliable choice for buyers searching for “ASME SA516 GR 60 mechanical properties.”

Property Value Test Method Temperature (°C) Thickness Effect Keywords
Tensile Strength 415-550 MPa ASME SA-8 Ambient -5% >100mm SA516 Gr.60 tensile
Yield Strength 220 MPa (min) ASME SA-8 Ambient Stable to 200mm SA516 Gr.60 yield
Elongation 21% (min) ASME SA-8 Ambient 18-22% (5-25mm) SA516 Gr.60 elongation
Impact Energy 27J @ -20°C (min) ASME SA-23 -20 27J all thicknesses SA516 Gr.60 impact
Modulus of Elasticity 200 GPa ASME SA-111 Ambient Constant SA516 Gr.60 modulus
Fatigue Limit 230 MPa (est.) ASME SA-466 Ambient Varies with surface SA516 Gr.60 fatigue

Delivery Conditions

SHH STEEL ensures ASME SA516 GR 60 carbon steel plates are delivered in optimal conditions to suit pressure vessel needs. We offer as-rolled, normalized (900-950°C), or stress-relieved (620-650°C) options per ASME SA-20, with quenched and tempered conditions available for enhanced toughness.

Normalized plates refine grain structure for improved impact resistance, ideal for boilers up to 350°C. Stress-relieved reduce residual stresses for welded structures, while quenched and tempered (870-900°C quench, 650°C temper) suits wear applications. Heat numbers provide traceability, and our global transit time, especially 3-7 days to Asia, ensures timely delivery.

Condition Temperature (°C) Duration (hours/inch) Standard Keywords
As-Rolled Ambient N/A ASME SA-20 SA516 Gr.60 delivery
Normalized 900-950 1 ASME SA-20 SA516 Gr.60 normalized
Stress-Relieved 620-650 1 ASME SA-20 SA516 Gr.60 stress relief
Quenched & Tempered Quench 870-900, Temper 650 0.5-1 ASME SA-20 SA516 Gr.60 tempered
Transit Time (Asia) 3-7 days N/A ISO 9001 SA516 Gr.60 shipping

Tolerances

Precision is paramount for ASME SA516 GR 60 carbon steel plates, and SHH STEEL maintains strict tolerances per ASME SA-6 to ensure seamless fabrication. Thickness tolerance is ±1.5mm for plates under 40mm and ±2.0mm for thicker sections up to 200mm (custom 300mm). Width and length tolerances are ±10mm standard, with ±5mm for precision orders up to 4600mm width and 12000mm length. Surface flatness is 3mm per meter, per ASME SA-6, preventing warping during welding or heat treatment. For European projects, EN 10029 Class B tolerances are offered, enhancing compatibility.

Tolerance Type Value (mm) Standard Applicable Thickness (mm) Keywords
Thickness (<40mm) ±1.5 ASME SA-6 5-40 SA516 Gr.60 tolerance
Thickness (>40mm) ±2.0 ASME SA-6 40-200 SA516 Gr.60 thickness tol
Width ±10 (standard), ±5 (custom) ASME SA-6, EN 10029 All SA516 Gr.60 width tol
Length ±10 (standard), ±5 (custom) ASME SA-6, EN 10029 All SA516 Gr.60 length tol
Flatness 3mm per meter ASME SA-6 All SA516 Gr.60 flatness spec

Weldability

ASME SA516 GR 60 carbon steel plates are highly weldable due to low carbon (≤0.23%) and CE ≤0.40 per AWS D1.1. SHH STEEL recommends preheating at 150-200°C for thicknesses over 25mm to prevent hydrogen-induced cracking, with post-weld heat treatment (PWHT) at 620-650°C for stress relief. Supported processes include GTAW, SMAW, and GMAW with E7018 filler (AWS A5.1), achieving 90-95% joint efficiency per ASME Section IX. Low sulfur (≤0.035%) reduces hot shortness, and 21% elongation ensures ductility. Testing includes bend tests (ASTM E190) for 3t radius and ultrasonic for weld integrity per ASME SA-435.

Weldability Factor Value/Condition Standard Recommended Process Keywords
Carbon Equivalent (CE) ≤0.40 AWS D1.1 GTAW, SMAW SA516 Gr.60 weldability
Preheating (°C) 150-200 (>25mm) ASME Section IX GMAW SA516 Gr.60 welding
PWHT (°C) 620-650 ASME SA-20 All SA516 Gr.60 heat treat
Filler Metal E7018 AWS A5.1 SMAW SA516 Gr.60 welding rod
Bend Test Radius (mm) 3t (t=thickness) ASTM E190 All SA516 Gr.60 bend test

Equivalent Material Grade

Global equivalents for ASME SA516 Gr.60 facilitate international projects, offering similar tensile and yield properties for pressure vessel use. For example, P295GH (EN 10028-2) is a European equivalent with 410-570 MPa tensile and 295 MPa yield, suitable for boilers in EU regulations. SPV315 (JIS G3115) serves Japanese applications with 450-570 MPa tensile and 315 MPa yield, ideal for high-toughness vessels. 16MnR/Q245R (GB/T 713) is the Chinese standard equivalent, providing 400-540 MPa tensile and 245 MPa yield for cost-effective pressure equipment in Asian markets. These equivalents ensure cross-compatibility, allowing buyers to substitute ASME SA516 GR 60 plates seamlessly in global supply chains.

Grade Standard Tensile (MPa) Yield (MPa) Elongation (%) Impact (J @ -20°C) Keywords
SA516 Gr.60 ASME SA-516/SA-516M 415-550 220 21 27 SA516 Gr.60 equivalent
P295GH EN 10028-2 410-570 295 22 27 SA516 Gr.60 EN grade
SPV315 JIS G3115 450-570 315 19 27 SA516 Gr.60 JIS grade
16MnR/Q245R GB/T 713 400-540 245 21 27 SA516 Gr.60 GB grade
A537 Cl.1 ASTM A537 485-620 345 18 41 SA516 Gr.60 alternative
A285 Gr.C ASTM A285 310-450 205 26 N/A SA516 Gr.60 low-cost alt

Supplementary Requirements

Supplementary requirements for ASME SA516 GR 60 carbon steel plates enhance performance for specialized applications, offering buyers tailored options. These include ultrasonic testing (Class 1 per ASME SA-435 for no laminations >0.25% thickness), Charpy impact at -50°C (27J min per ASME SA-20 for cold service), and heat analysis per heat number (ASME SA-350 for traceability). Product analysis allows ±0.02% tolerance on elements, while shot blasting to Sa 2.5 (50-100μm profile per ISO 8501-1) is available for surface preparation. SHH STEEL provides these to meet stringent needs, as buyers search for “SA516 Gr.60 supplementary requirements.”

Requirement Detail Standard Test Frequency Applicable Thickness (mm) Keywords
Ultrasonic Testing Class 1, no laminations ASME SA-435 Full plate 5-500 SA516 Gr.60 ultrasonic
Charpy Impact -50°C, 27J min ASME SA-20 Per heat 5-500 SA516 Gr.60 cold impact
Heat Analysis Per heat number ASME SA-350 Each batch All SA516 Gr.60 analysis
Product Analysis ±0.02% tolerance ASME SA-350 Sample per lot All SA516 Gr.60 product test
Shot Blasting Sa 2.5, 50-100μm profile ISO 8501-1 On request 5-100 SA516 Gr.60 blasting

Applications

ASME SA516 GR 60 carbon steel plates are versatile for moderate-pressure and temperature environments, with excellent strength and toughness.

Application Temperature (°C) Pressure (bar) Thickness (mm) Standard Compliance Keywords
Pressure Vessels Up to 400 300 20-100 ASME Section VIII SA516 Gr.60 vessels
Boilers Up to 350 200 10-50 ASME Section I SA516 Gr.60 boilers
Storage Tanks Up to 200 50 5-30 API 650 SA516 Gr.60 tanks
Oil & Gas Equipment Up to 300 250 30-120 NACE MR0175 SA516 Gr.60 oil equip
Heat Exchangers Up to 250 150 10-40 TEMA Standards SA516 Gr.60 heat exchange

Details: Pressure vessels benefit from 415-550 MPa tensile at 400°C, while boilers handle 350°C with 21% elongation for forming. Storage tanks use 5-30mm plates for 50 bar, and oil & gas equipment leverages 30-120mm for 250 bar with NACE compliance. Heat exchangers utilize 10-40mm plates for 150 bar at 250°C, per TEMA standards for efficient heat transfer.

Why Choose SHH STEEL

SHH STEEL offers ASME and ASTM-certified SA516 Gr.60 plates, with custom thicknesses up to 300mm and heat treatments tailored to your project. Our 15-year track record includes zero defect deliveries to 50+ countries, backed by SGS verification and mill test certificates.

Advantage Benefit Keywords
Expert Certification ASME Section VIII compliant SA516 Gr.60 certified
Custom Fabrication Up to 300mm thickness SA516 Gr.60 custom
Proven Reliability 50+ countries, zero rejects SA516 Gr.60 trusted supplier

FAQ

What is ASME SA516 Grade 60 used for?
ASME SA516 Grade 60 is widely used for pressure vessels, boilers, and storage tanks in oil & gas and power generation. It handles moderate temperatures up to 400°C and pressures to 300 bar, with 415-550 MPa tensile strength ensuring reliability. SHH STEEL supplies these for welded constructions per ASME Section VIII Division 1.
What is the difference between SA516 Gr.60 and SA516 Gr.70?
SA516 Gr.60 has tensile 415-550 MPa and yield 220 MPa, while Gr.70 offers 485-620 MPa and 260 MPa. Gr.60 is cost-effective for moderate stresses, with 21% elongation for forming, whereas Gr.70 suits higher pressure (500 bar). SHH STEEL recommends Gr.60 for standard applications; see our ASTM A 516 Gr 70 page for comparison.
What is the chemical composition of SA516 Gr.60?
The composition includes C ≤0.23%, Mn 0.60-1.20%, P ≤0.035%, S ≤0.035%, Si 0.15-0.40%, tested per ASME SA-350. This low-carbon formula ensures excellent weldability with CE ≤0.40 (AWS D1.1). SHH STEEL provides MTCs with full analysis for traceability.
Is ASME SA516 Gr.60 weldable?
Yes, SA516 Gr.60 is highly weldable with low carbon (≤0.23%) and preheating at 150-200°C for >25mm thicknesses. Use E7018 filler (AWS A5.1) for 90% joint efficiency per ASME Section IX. PWHT at 620-650°C reduces stress, validated by bend tests per ASTM E190.
What is the density of SA516 Gr.60?
The density is 7.85 g/cm³, standard for carbon steel, aiding weight calculations in vessel design. Hardness is 120-170 HB (ASME SA-18), balancing wear resistance for high-pressure use.
What is the equivalent of SA516 Gr.60 in EN standards?
The closest EN equivalent is P295GH (EN 10028-2), with 410-570 MPa tensile and 295 MPa yield, suitable for EU boilers. SHH STEEL provides dual-certified plates for seamless transitions.
What is the difference between SA516 Gr.60 and SA516 Gr.65?
SA516 Gr.65 has higher tensile (450-585 MPa) and yield (240 MPa) than Gr.60’s 415-550 MPa and 220 MPa. Gr.65 suits higher pressure (500 bar), while Gr.60 is for moderate use. Visit our ASTM A 516 Gr 65 page.
What is the difference between SA516 Gr.60 and SA516 Gr.55?
SA516 Gr.60 offers higher tensile (415-550 MPa vs. 380-515 MPa) and yield (220 MPa vs. 205 MPa) than Gr.55. Gr.60 handles moderate pressure better. Check our ASTM A 516 Gr 55 page.

Conclusion

SHH STEEL’s ASME SA516 Gr.60 Carbon Steel Plates provide unmatched strength and reliability for pressure vessels and boilers. With precise tolerances, superior weldability, and global equivalents, we offer customized solutions. Trust SHH STEEL for your steel needs—explore our ASTM A 516 Gr 60 page for more details.

For more other grade, please check in the following: ASME SA 516/SA 516M, ASME SA 516 GR 70, ASME SA 516 GR 65, ASME SA 516 GR 60 and ASME SA 516 gr 55 Steel Plate Grade.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X