EN 10028-2 P265GH high-temperature pressure vessel steel plate, steel number 1.0425, normalized C-Mn plate, SHH STEEL

EN 10028-2 P265GH Steel Plate | P265GH High Temp Vessel Plate

EN 10028-2 P265GH is European non-alloy high-temperature vessel plate, steel number 1.0425. Yield is 265 MPa at ≤16 mm. Tensile is 410–530 MPa. SHH STEEL supplies P265GH worldwide as a global steel mill sourcing partner. FOB Shanghai / CIF Rotterdam / Houston / Jebel Ali.
Keywords
EN 10028-2 P265GH, P265GH, P265GH steel plate, 1.0425, P265GH high temp vessel plate, P265GH equivalent, P265GH supplier
Equivalent Grades
EN 1.0425 / ASTM A515 Gr 60 / JIS SB450 / GB Q245R — Material Specification: EN 10028-2 — Delivery: Normalized (N) or As-rolled (AR, ≤30mm)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
High-Temperature Pressure-Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10028-2 P265GH Steel?

P265GH is the workhorse carbon grade in EN 10028-2. Buyers search EN 10028-2 P265GH, P265GH high temp vessel plate, 1.0425 and P265GH steel plate. GH means elevated-temperature properties. This page is not EN 10028-3 fine-grain low-temperature plate and not EN 10028-4 nickel plate.

Yield is 265 MPa at ≤16 mm. Tensile is 410–530 MPa. Steel number is 1.0425. Delivery is usually normalized (+N). SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade.

Do not ship Q345R steel plate against a P265GH drawing without checking both books. Q345R is stronger. The closer Chinese carbon vessel name is often Q245R steel plate. Do not ship SA516 Grade 70 carbon steel plates and call 70 the same as P265GH. SA-516 Grade 70 sits nearer P355GH. A closer ASME carbon comparison is often SA516 Grade 60 carbon steel plates or SA285 Grade C steel plate. Dual marking is possible only when chemistry, tensile, impact and delivery all fit.

Company scope: global steel mill sourcing partner – SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-2 P265GH Confirmed
Steel number 1.0425 Confirmed
Product specification EN 10028-2 + EN 10028-1 Applied
Steel type Non-alloy quality steel, elevated temperature Confirmed
Usual delivery +N normalized Confirmed
Yield idea 265 MPa at ≤16 mm Confirmed
Tensile 410–530 MPa at ≤16 mm Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Markets Americas, Europe, Middle East, Africa, Asia FOB / CIF as ordered
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and carbon steel plates. ASME carbon comparisons belong on ASME SA516 and ASME SA515.

Chemical Composition

Cast analysis follows EN 10028-2 Table 1. Product analysis follows EN 10028-1 when ordered.

Cast Analysis and Product Analysis — EN 10028-2 P265GH (1.0425)

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C), max 0.20 0.22
Silicon (Si), max 0.40 0.45
Manganese (Mn) 0.80 – 1.40 0.75 – 1.50
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.010 0.013
Aluminum total (Al), min 0.020 0.015
Nitrogen (N), max 0.012 0.014
Chromium (Cr), max 0.30 0.35
Copper (Cu), max 0.30 0.35
Molybdenum (Mo), max 0.08 0.10
Niobium (Nb), max 0.020 0.025
Nickel (Ni), max 0.30 0.35
Titanium (Ti), max 0.03 0.04
Vanadium (V), max 0.02 0.03

P265GH is killed carbon steel with a modest manganese band. It is not Cr-Mo plate and not 9Ni plate. SHH STEEL reports cast analysis on every certificate and product analysis when the order names it. Density is 7.85 g/cm³.

Mechanical Properties

Room-temperature values below are the usual ≤16 mm column. Yield falls as thickness rises. Use the thickness column on the mill certificate.

Tensile and Yield — EN 10028-2 P265GH

Thickness (mm) Yield min (MPa) Tensile (MPa)
≤ 16 265 410 – 530
16 – 40 255 410 – 530
40 – 60 245 410 – 530
60 – 100 215 400 – 530
100 – 150 200 380 – 510
Density 7.85 g/cm³ 7.85 g/cm³

Elongation is typically 22% min on thinner plate. Impact at 0 °C, 27 J, is the usual option when the order names it. Elevated-temperature proof strength is part of EN 10028-2. Ask for Table 5 values when the vessel calculation uses design temperature, not only room-temperature yield.

Do not quote 265 MPa yield on a 80 mm plate. Do not treat 410–530 MPa tensile as permission to stamp SA516 Grade 70 carbon steel plates or Q345R steel plate.

Material Comparison

Grade Book Service idea Swap?
EN 10028-2 P265GH EN 10028-2 High-temp carbon, 265 MPa This page
EN 10028-2 P235GH EN 10028-2 One step below No
EN 10028-2 P355GH EN 10028-2 One step above No
Q245R steel plate GB/T 713.2 Closest Chinese carbon No auto swap
Q345R steel plate GB/T 713.2 Stronger Chinese carbon No
SA516 Grade 60 carbon steel plates SA-516 Closest ASME carbon No auto swap
SA516 Grade 70 carbon steel plates SA-516 Stronger ASME carbon No
SPV315 steel plate JIS G3115 Japanese vessel No
StE255 steel plate DIN 17102 Fine grain, different book No

Equivalent Material Grades

Comparison names help a buyer search. They do not authorize substitution.

Designation Standard / region Notes
EN 10028-2 P265GH / 1.0425 EN 10028-2 Name on this page
P235GH / 1.0345 EN 10028-2 Lower yield sister
P295GH / 1.0481 EN 10028-2 Mid sister
P355GH / 1.0473 EN 10028-2 Higher yield sister
Q245R steel plate GB/T 713.2 Chinese carbon comparison
Q370R steel plate GB/T 713.2 Stronger Chinese vessel
SA515 Grade 60 steel plate SA-515 High-temp carbon comparison
SA516 Grade 60 carbon steel plates SA-516 Low-temp carbon comparison
ASTM A516 Grade 60 A516 ASTM twin of SA-516 60
SA285 Grade C steel plate SA-285 Intermediate tensile carbon
SPV235 steel plate JIS G3115 Japanese vessel
StE285 steel plate DIN 17102 Fine-grain comparison
ASTM A36 steel plate A36 Structural, not vessel

High-Temperature Pressure-Vessel Service

Buyers pick P265GH for boilers, drums, heat-exchanger shells and PED vessels that name EN 10028-2 carbon plate. It is the default European carbon grade when the drawing does not need P355GH strength and does not need Cr-Mo.

It is not a substitute for 16MnDR steel plate. That grade is GB/T 713.3 −40 °C plate. It is not a substitute for 06Ni9DR steel plate. That grade is 9Ni −196 °C plate.

An ASME file should name the SA/ASTM grade on ASTM A516 or ASME SA285 and then write extras. Dual marking is possible only when both books are met.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

P265GH is killed carbon vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.

Qualify to the applicable code. ASME dual-name work uses ASME Section IX. Consumables must match the 410–530 MPa tensile band. A Q345R steel plate procedure is not automatically valid. A Cr-Mo procedure written for 15CrMoR steel plate is the wrong family. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized EN 10028-2 P265GH (+N). As-rolled is not the default for pressure work.

If the vessel will see PWHT, say so. Test coupons then follow a simulated cycle. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists EN 10028-2 P265GH; 1.0425; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; +N; impact when ordered; elevated-temperature values when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for P265GH high temp vessel plate:

  • Thickness: commonly 6 mm – 150 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Ship plate inquiries belong on shipbuilding steel plates. Structural plate belongs on structural steel plates or EN 10025-2. Stainless inquiries belong on stainless steel products.

Tolerances

Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another tolerance table. Do not apply ASTM A36/A36M structural tolerances to a PED vessel plate without writing them.

Supplementary Requirements

Charpy details. Temperature, energy, location and orientation. 0 °C / 27 J is common, not assumed.

Product analysis. Add this when the destination file wants finished-plate chemistry.

Elevated-temperature proof strength. Add this when the calculation uses design temperature.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. EN 10160 or the named UT class.

Third-party. EN 10204 3.2 when written.

Applications

Industry Typical components
PED boilers and drums EN 10028-2 P265GH shells
Heat-exchanger shells P265GH courses
High-temp carbon vessels P265GH plate from SHH STEEL
Dual-certified export P265GH / SA516 Grade 60 carbon steel plates when both books fit

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical trade terms on this grade: FOB Shanghai, CIF Rotterdam, CIF Houston, CIF Jebel Ali, plus Antwerp, Hamburg, Barcelona, Singapore and Busan.

Typical lead time:

  • Ex-stock: about 5–7 days
  • Mill rolling, standard +N: about 45 days
  • Simulated PWHT, 3.2 or extra NDE: about 2 months

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). On EN 10028-2 P265GH that means mill pricing, 1.0425 chemistry reported as cast analysis and as product analysis when ordered, recorded +N, tensile results to the correct thickness column, 3.1 as standard and 3.2 when specified.

We keep the grade on the order. P265GH is not P355GH. P265GH is not Q345R steel plate. P265GH is not SA516 Grade 70 carbon steel plates. If the drawing says P355GH, we will not ship P265GH and call carbon close.

Company scope: global steel mill sourcing partner – SHH STEEL.

FAQ

What is P265GH steel plate?
P265GH is an EN 10028-2 non-alloy high-temperature pressure-vessel plate, steel number 1.0425. Yield is 265 MPa at ≤16 mm and tensile is 410–530 MPa. Delivery is usually normalized. SHH STEEL supplies this plate as a global steel mill sourcing partner.
What is the equivalent of P265GH?
Related comparisons are Q245R, SA-516 Grade 60 and SA-285 Grade C. Dual marking is possible only when both books are fully met.
How is P265GH different from P355GH?
P355GH yield is 355 MPa at ≤16 mm. P265GH yield is 265 MPa. Tensile bands are not the same.
How is P265GH different from Q345R?
Q345R is GB/T 713.2 at a higher yield. P265GH is EN 10028-2 at 265 MPa. Chemistry, impact and elevated-temperature tables are not the same.
Can SHH STEEL ship P265GH to the Netherlands, the USA or the UAE?
Yes. SHH STEEL has supplied plates to Europe, the USA, the Middle East, Asia, Africa and South America.
What is the delivery time for P265GH?
Ex-stock about 5–7 days. Standard +N mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.

Conclusion

EN 10028-2 P265GH Steel Plate is European non-alloy high-temperature pressure-vessel plate, steel number 1.0425, at the 265 MPa yield step and 410–530 MPa tensile at ≤16 mm, usually normalized. Whether the inquiry says EN 10028-2 P265GH, 1.0425 or P265GH High Temp Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with P265GH chemistry, heat and product analysis when ordered, recorded +N, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10028-2 P265GH High Temp Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Rotterdam / Houston / Jebel Ali.

Contact SHH STEEL for mill rolling, stock inquiry, +N, 3.2 inspection or a quotation.

EN 10028-2 P265GH Steel Plate, P265GH high temp vessel plate, 1.0425, P265GH supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *