SHH STEEL offers ASTM A517/A517M-compliant Grade A/F/P quenched and tempered alloy steel plates. ASTM A517/A517M specifies high-strength steels for pressure vessels and fabrication. Impact-tough, certified quality, competitive prices, customizable. Trust SHH STEEL!

ASTM A517 Grade S Steel Plate | A517 Gr.S QT High Strength Vessel Plate - SHH STEEL

ASTM A517 Grade S Steel Plate | A517 Gr.S QT High Strength Vessel Plate

ASTM A517 Grade S is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa, tensile 795–930 MPa, max thickness 50 mm. China Mill Direct Exporter SHH STEEL supplies A517 Gr.S / SA517 Gr.S with 3.1 or 3.2 certificates.
View More
ASTM A517 Grade H Steel Plate | A517 Gr.H QT High Strength Vessel Plate - SHH STEEL

ASTM A517 Grade H Steel Plate | A517 Gr.H QT High Strength Vessel Plate

ASTM A517 Grade H is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa, tensile 795–930 MPa, max thickness 50 mm. China mill Agent SHH STEEL supplies A517 Gr.H / SA517 Gr.H with 3.1 or 3.2 certificates.
View More
ASTM A517 Grade A Steel Plate | A517 Gr.A QT High Strength Vessel Plate - SHH STEEL

ASTM A517 Grade A Steel Plate | A517 Gr.A QT High Strength Vessel Plate

ASTM A517 Grade A is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa, tensile 795–930 MPa, max thickness 32 mm. China mill Distributor SHH STEEL supplies A517 Gr.A / SA517 Gr.A with 3.1 or 3.2 certificates
View More
ASTM A517 Grade P Steel Plate | A517 Gr.P QT High Strength Vessel Plate - SHH STEEL

ASTM A517 Grade P Steel Plate | A517 Gr.P QT High Strength Vessel Plate

ASTM A517 Grade P is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa to 65 mm, 620 MPa to 100 mm. Direct Mill Supply by SHH STEEL for A517 Gr.P / SA517 Gr.P with 3.1 or 3.2 certificates
View More
ASTM A517 Grade E Steel Plate | A517 Gr.E QT High Strength Vessel Plate - SHH STEEL

ASTM A517 Grade E Steel Plate | A517 Gr.E QT High Strength Vessel Plate

ASTM A517 Grade E is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa to 65 mm, 620 MPa to 150 mm. China Mill Direct Exporter SHH STEEL supplies A517 Gr.E / SA517 Gr.E with 3.1 or 3.2 certificates.
View More
ASTM A517 Grade B Steel Plate | A517 Gr.B QT High Strength Vessel Plate - SHH STEEL

ASTM A517 Grade B Steel Plate | A517 Gr.B QT High Strength Vessel Plate

ASTM A517 Grade B is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa, tensile 795–930 MPa, max thickness 32 mm. China mill Agent SHH STEEL supplies A517 Gr.B / SA517 Gr.B with 3.1 or 3.2 certificates.
View More
ASTM A517 Grade F Steel Plate | A517 Gr.F QT High Strength Vessel Plate - SHH STEEL

ASTM A517 Grade F Steel Plate | A517 Gr.F QT High Strength Vessel Plate

ASTM A517 Grade F is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa, tensile 795–930 MPa, max thickness 65 mm. Direct Mill Supply by SHH STEEL for A517 Gr.F / SA517 Gr.F with 3.1 or 3.2 certificates.
View More
ASTM A517 Grade Q Steel Plate | A517 Gr.Q QT High Strength Vessel Plate - SHH STEE

ASTM A517 Grade Q Steel Plate | A517 Gr.Q QT High Strength Vessel Plate

ASTM A517 Grade Q is a quenched-and-tempered high-strength alloy vessel plate under ASTM A517/A517M. Yield 690 MPa to 65 mm, 620 MPa to 150 mm. China Mill Direct Exporter SHH STEEL supplies A517 Gr.Q / SA517 Gr.Q with 3.1 or 3.2 certificates.
View More
Boiler & Pressure Vessel Steel Plates Supplier | SHH STEEL – A516, A537, A285, P355GH

Boiler & Pressure Vessel Steel Plates

SHH STEEL, a trusted Pressure Vessel Steel Plates exporter, produces and exports pressure vessel steel plates for boilers, tanks, and petrochemical applications. Our plates, like ASTM A516 Grade 70, offer high tensile strength and toughness, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for boiler steel plates and custom high-pressure solutions.

Boiler & Pressure Vessel Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *



    X