What is ASTM A517 Grade A Steel?
ASTM A517 Grade A is the other 32 mm grade in ASTM A517/A517M, sitting next to Grade B. The tensile table is the same 690 MPa class, but the alloy is not. Grade A uses a higher silicon band and a different chromium-molybdenum window, plus zirconium. If the drawing says Grade A, a Grade B heat is not a substitute. As Direct Mill Supply by SHH STEEL, the plate is produced to the ASTM product specification.
The same plate is written A517 Gr.A, A517GRA, A517 GR A, A517 Grade A, ASME SA517 Grade A, SA517 Gr.A, SA517GRA and A/SA517 Grade A. They all mean Grade A. ASTM A517/A517M is the product specification. ASME SA-517/SA-517M is the Code companion used with Section VIII.
ASTM A517 lists eight grades—A, B, E, F, H, P, Q and S. They share one mechanical table where thickness overlaps. They do not share alloy content or maximum thickness. Grade A and Grade B both stop at 32 mm (1.25 in.). Grade H and Grade S stop at 50 mm. Grade F stops at 65 mm. Grade P stops at 100 mm. Grade Q and Grade E stop at 150 mm.
The steel is killed and made to fine austenitic grain practice under ASTM A20 / ASME SA-20. Heat treatment is mandatory quench and temper: austenitize at not less than 900 °C, quench in water or oil, temper at not less than 620 °C. As-rolled or normalize-only plate is not A517GRA.
Do not mix this page with ASTM A516 or ASME SA516. Those are carbon vessel plates. ASTM A517 Grade A is a QT alloy plate. It is also not structural A514. A514 Grade A looks close on a strength sheet. A514 is a structural specification. A517 is a pressure-vessel specification with A20 general requirements and vessel testing.
For Code work the plate is dual-certified to ASME SA517 Grade A and used under ASME Section VIII. Certificates can be EN 10204 3.1 or EN 10204 3.2.
When a project is still choosing high-strength vessel plate, a China mill Agent path through SHH STEEL puts A517GRA next to ASME SA537, ASTM A537, ASME SA387 and ASTM A285, so the buyer can see whether they actually need 690 MPa QT or a lower-strength carbon / Cr-Mo route.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | ASTM A517 Grade A / A517 Gr.A / A517GRA | Confirmed |
| Product Specification | ASTM A517/A517M | Applied |
| Companion Spec | ASME SA517 Grade A / SA517GRA | Dual cert available |
| General Requirements | ASTM A20 / ASME SA-20 | Applied |
| Code Context | ASME Section VIII when dual certified | As specified |
| Product Form | Pressure vessel / boiler plate | Available |
| Steel Practice | Killed, fine austenitic grain | Confirmed |
| Heat Treatment | Quench and temper (mandatory) | Confirmed |
| Maximum Thickness (Grade A) | 32 mm (1.25 in.) | Per A517 |
| Typical Supply | 8 mm – 32 mm | By mill enquiry |
| Width / Length | Up to about 4000 mm / 12000 mm | Mill capability |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate belongs to the Pressure Vessel Steel Plates family. It is not a structural HSLA Steel Plates substitute and not a Carbon Steel Plates grade.
Chemical Composition
Chemistry for ASTM A517 Grade A is reported as heat analysis and, when specified, product analysis under ASTM A517/A517M. Grade A is a Cr-Mo alloy with a high silicon band. Silicon heat analysis is 0.40–0.80%, which is the easiest way to tell it from Grade B on a ladle report.
Heat Analysis — ASTM A517 Grade A / A517GRA
| Element | Heat Analysis (%) |
|---|---|
| Carbon (C) | 0.15 – 0.21 |
| Manganese (Mn) | 0.80 – 1.10 |
| Phosphorus (P), max | 0.025 |
| Sulfur (S), max | 0.025 |
| Silicon (Si) | 0.40 – 0.80 |
| Chromium (Cr) | 0.50 – 0.80 |
| Molybdenum (Mo) | 0.18 – 0.28 |
| Zirconium (Zr) | 0.05 – 0.15 |
| Boron (B), max | 0.0025 |
Product Analysis — A517 Gr.A / SA517 Grade A
| Element | Product Analysis (%) |
|---|---|
| Carbon (C) | 0.13 – 0.23 |
| Manganese (Mn) | 0.74 – 1.20 |
| Silicon (Si) | 0.34 – 0.86 |
| Chromium (Cr) | 0.46 – 0.84 |
| Molybdenum (Mo) | 0.16 – 0.30 |
| Zirconium (Zr) | 0.04 – 0.16 |
| P, S, B | Per A20 / order |
A Grade B heat cannot be recertified as Grade A. Silicon on Grade B is 0.15–0.35%. Nickel is not specified on Grade A. If the drawing says ASTM A517 Grade A, the ladle must sit in the Grade A table. SHH STEEL reports heat analysis on every certificate and adds product analysis when ASTM A20 or the vessel specification requires it.
Tighter phosphorus, sulfur or residuals are supplementary. Vacuum carbon deoxidation and other A20 chemistry items are available when written on the order.
Mechanical Properties
Where Grade A is permitted (32 mm and under), it uses the high line of the A517 tensile table.
Tensile Requirements — ASTM A517 Grade A per ASTM A517/A517M
| Property | ≤ 32 mm (1.25 in.), within Grade A limit |
|---|---|
| Tensile strength | 795 – 930 MPa (115 – 135 ksi) |
| Yield strength, min | 690 MPa (100 ksi) |
| Elongation in 50 mm, min | 16% |
| Reduction of area, rectangular, min | 35% |
| Reduction of area, round, min | 45% |
There is no 65 mm or 150 mm line on Grade A. The specification itself ends at 32 mm. A 40 mm inquiry is not Grade A.
Density is 7.85 g/cm³. Hardness after QT is typically in a high-strength vessel range; a special HBW window is a supplementary requirement.
ASTM A517 requires transverse Charpy V-notch testing with a minimum lateral expansion of 0.38 mm (0.015 in.) on each specimen. The test temperature is agreed between purchaser and manufacturer. Write the temperature on the PO.
Specimens follow ASTM A20. If simulated PWHT is specified, coupons from the same A517 Gr.A heat follow the vessel cycle before tensile and impact testing. On QT 690 MPa plate that request should be on the mill order whenever the shop will PWHT the vessel.
Material Comparison
| Grade | Alloy emphasis | Max thickness | Same strength table where allowed? |
|---|---|---|---|
| ASTM A517 Gr.A / ASME SA517 Gr.A | High-Si Cr-Mo-Zr | 32 mm | Yes |
| ASTM A517 Gr.B / ASME SA517 Gr.B | Cr-Mo-B-Ti, lower Si | 32 mm | Yes |
| ASTM A517 Gr.H / ASME SA517 Gr.H | Lower-Ni Cr-Mo | 50 mm | Yes |
| ASTM A517 Gr.F / ASME SA517 Gr.F | Ni-Cr-Mo-B | 65 mm | Yes |
| ASTM A517 Gr.Q / ASME SA517 Gr.Q | Ni-Cr-Mo-V | 150 mm | Yes |
| ASTM A537 Cl.2 / ASME SA537 Cl.2 | Carbon QT | By class | Lower strength |
| ASTM A514 Gr.A | Structural QT | Structural spec | Not a vessel spec |
| EN 10028-6 P690Q / P690QL | European QT vessel | By EN thickness | Project comparison only |
Order ASTM A517 Grade A when the drawing names Grade A and thickness is 32 mm or less. If thickness exceeds 32 mm, Grade A is not available under A517. Grade B is the other 32 mm option with a different silicon and microalloy route. SHH STEEL does not swap A for B on a Code vessel without a written revision.
HSLA Steel Plates and S690QL structural plate are not ASTM A517. If the equipment is Section VIII, stay on A517 / SA517.
High-Strength QT Vessel Service
ASTM A517 Grade A exists because some thin vessels need 690 MPa yield on the Grade A alloy route. The 32 mm ceiling is the specification limit, not a mill preference.
When dual certified to ASME SA517 Grade A, allowable stress comes from ASME Section II Part D, not from a mill flyer. Impact temperature is an order number.
Typical use is thinner high-pressure shells, modular equipment and other fusion-welded parts specified to A517 Grade A. It is not a cryogenic 3.5Ni or 9Ni grade, and it is not a creep-focused Cr-Mo grade such as A387.
Weldability
A517GRA is a high-strength QT alloy. Welding is not the same job as welding A516 Gr.70.
Procedures for Code work are qualified to ASME Section IX. Consumables should match the required joint strength and toughness, usually a high-strength low-hydrogen family selected for 690 MPa class steel. Hydrogen control, preheat and interpass still matter at 20–32 mm. High silicon and hardenability mean a cold, restrained start can crack.
Preheat depends on thickness, restraint, hydrogen and the qualified WPS. After welding, many shops want to PWHT. On QT plate that decision has to be engineered. A shop cycle that is too hot or too long can drop yield below the A517 table. Simulated PWHT of mill coupons should be on the purchase order whenever the vessel specification includes PWHT.
Do not copy an A516 or Grade B procedure onto ASTM A517 Grade A without review. Procedure review can go through steel welding services. The fabricator owns the qualified WPS.
Heat Treatment
Heat treatment of ASTM A517 Grade A follows ASTM A517/A517M:
- Heat to not less than 900 °C (1650 °F)
- Quench in water or oil
- Temper at not less than 620 °C (1150 °F)
That sequence is the product. As-rolled plate is not A517 Grade A. Normalized-only plate is not A517 Grade A.
Holding time follows mill practice and ASTM A20 thickness rules. If the purchaser fixes a tempering band or a maximum tempering temperature because later PWHT is planned, those limits go on the mill instruction and onto the certificate.
SHH STEEL reports the actual heat-treatment condition on the MTC for every A517 Gr.A plate
Delivery Condition
Delivery condition for this grade is quenched and tempered. That is the only standard condition.
The certificate lists ASTM A517 Grade A and, when dual certified, ASME SA517 Grade A; heat number; heat analysis; product analysis when ordered; tensile results; reduction of area; Charpy lateral expansion and test temperature; heat-treatment temperatures; and supplementary tests.
Surface is vessel-plate quality. Shot blasting and shop primer are available. Decorative 2B or BA finishes are not used on QT vessel plate.
Certificates may be EN 10204 3.1 or EN 10204 3.2. BV, LR, DNV, TUV, SGS or the buyer’s agency can witness quench, temper, mechanical tests and documents when the order says so.
Dimensions
Usual supply range from SHH STEEL for A517 Gr.A QT high strength vessel plate:
- Thickness: 8 mm – 32 mm (Grade A maximum in ASTM A517 is 32 mm)
- Width: up to about 4000 mm
- Length: up to about 12000 mm
If the inquiry is 40 mm, say so immediately. That thickness is outside Grade A. Cut-to-length shells and nest sizes are available inside the 32 mm limit.
Tolerances
Dimensional limits follow ASTM A20 / ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances. QT plate can move during quench; extra-flatness is a negotiated item.
Ultrasonic testing to A435 or A578 is commonly added. Finished sizes go through steel cutting services. Thermal cutting of 690 MPa QT plate needs preheat and edge control.
Supplementary Requirements
Most ASTM A517 Grade A orders add tests beyond the base tensile table. Thin plate does not remove those extras when the vessel specification includes PWHT or a stated impact temperature. SHH STEEL does not assume them. They run only when they are written on the purchase order.
Simulated PWHT. Same-heat coupons follow the vessel cycle: heating rate, soak temperature, hold time and cooling path as stated by the fabricator. Tensile and Charpy are then run on those coupons, not only on the as-QT plate. On 690 MPa QT plate this is the test that prevents a shop surprise. If the vessel specification includes PWHT and simulated PWHT is omitted from the mill order, the plate can still meet ASTM A517 as delivered and miss the after-PWHT numbers the shop needs.
Charpy details. The base specification requires transverse Charpy V-notch lateral expansion of 0.38 mm (0.015 in.) on each specimen. The test temperature is agreed. Purchasers commonly add an energy minimum in joules, a colder temperature than the mill default, and a retest rule. Write those items on the RFQ. Do not assume −18 °C or −40 °C.
NDE. Ultrasonic testing to ASTM A435, A577 or A578 with purchaser acceptance levels. Edge magnetic-particle or liquid-penetrant examination after cutting is added when nozzles or strained joints are cut from the plate.
Hardness survey. Surface HBW or HV after QT, and again after simulated PWHT when that cycle is specified. A hardness window is not a default in ASTM A517. It is a supplementary limit used to control weldability and to confirm the temper.
Restricted chemistry. Tighter phosphorus and sulfur, residual limits, or vacuum carbon deoxidation per ASTM A20 supplementary requirements. High silicon on Grade A already changes weld practice versus Grade B. Restricted P and S help toughness when the datasheet asks for them.
HIC / NACE. Hydrogen-induced cracking tests to NACE TM0284, or sour-service chemistry to NACE MR0175 / ISO 15156, only when the datasheet cites those documents. Grade A is not automatically sour-service plate. Do not print “NACE” on a certificate unless the tests and chemistry were actually ordered.
Z-direction. ASTM A770 or quality classes Z15 / Z25 / Z35 when the joint is strained. On 32 mm plate this is less common than on Grade Q, but it is still an order item when written.
Third-party witnessing. Quench, temper, mechanical tests, UT and document review can be witnessed by BV, LR, DNV, TUV, SGS or the buyer’s appointed agency. Output can be EN 10204 3.2. EN 10204 3.1 remains the standard mill certificate when no witness is named.
These tests run through steel testing service. If an item is not on the purchase order, it is not assumed, not tested and not printed as if it were.
Equivalent Material Grades
These names are used for project comparison. They are not automatic substitutes. Chemistry, thickness limit, heat treatment, impact rule and Code marking still have to match the drawing.
| Designation | Standard | Region / notes |
|---|---|---|
| ASTM A517 Grade A / A517 Gr.A / A517GRA | ASTM A517/A517M | Product name on this page |
| ASME SA517 Grade A / SA517 Gr.A / SA517GRA | ASME SA-517/SA-517M | Identical Code companion for Section VIII |
| ASTM A517 Grade B / ASME SA517 Grade B | A517 / SA-517 | Same 32 mm ceiling, lower Si, different microalloy |
| ASTM A514 Grade A | ASTM A514/A514M | Structural QT cousin; not a vessel spec |
| EN 10028-6 P690Q | EN 10028-6 | European QT pressure-vessel plate, quality Q |
| EN 10028-6 P690QL | EN 10028-6 | Same family with specified low-temperature impact |
| EN 10028-6 P690QL1 | EN 10028-6 | Colder impact quality in the P690 line |
| EN 10025-6 S690QL | EN 10025-6 | Structural QT; not A517 vessel plate |
| DIN 17102 StE 690 / TStE 690 (historical) | DIN 17102 (withdrawn into EN) | Old German high-yield QT designation |
| SEW 088 related 690 QT | SEW | German mill comparison only |
| ISO 9328-4 P690Q / P690QL | ISO 9328 | ISO pressure-vessel QT comparison |
| JIS G3128 SHY685 | JIS G3128 | Japanese high-yield QT steel; project comparison |
| JIS G3115 SPV490 | JIS G3115 | Japanese PV plate, lower strength than A517 Gr.A |
| JIS G3106 SM570 | JIS G3106 | Welded structural; not QT 690 vessel plate |
| GB/T 16270 Q690E / Q690D | GB/T 16270 | Chinese high-strength QT structural comparison |
| GB 19189 WDB620 / WDB690 related | GB 19189 | Chinese high-strength QT vessel-related comparison |
For stamping a Section VIII vessel, write dual A517 / SA517 Grade A. Do not stamp EN P690QL, JIS SHY685 or A514 Grade A unless that specification is actually ordered and tested. Nearby vessel pages: ASTM A537, ASME SA537, ASTM A516, ASME SA516.
Applications
ASTM A517 Grade A / A517 Gr.A is selected when a Section VIII or equivalent vessel needs QT alloy strength on the Grade A chemistry and thickness stays at or below 32 mm.
| Industry | Typical components |
|---|---|
| High-pressure vessels | ASTM A517 Grade A shells and A517GRA heads |
| Petrochemical | A517 Grade A thin high-pressure drums |
| Energy and process | ASTM A517 Grade A QT high strength vessel plate |
| Modular equipment | A517 Gr.A courses inside 32 mm |
| Dual-certified export | A517 / SA517 Gr.A plate |
| Fabrication | A517GRA cut to nest sizes |
Related pages: petrochemical industry, energy industry, steel cutting services, steel welding services, steel testing service, worldwide shipping service.
Why Choose SHH STEEL
SHH STEEL works as a China Mill Direct Exporter for plates to ASTM A517/A517M. On ASTM A517 Grade A that is not a slogan. It is the supply route: the plate is rolled and quench-tempered at a producing mill, marked to the ordered specification, and exported with the tests the vessel shop wrote on the purchase order.
For this grade that means mill pricing instead of mixed-yard stock of unknown heats. Dual A517 / SA517 Grade A marking is available when the vessel must be stamped to ASME Section VIII. Heat analysis is reported on every certificate. Product analysis is added when ASTM A20 or the buyer asks for it. The 0.40–0.80% silicon band and the zirconium range are checked against Grade A, not against Grade B.
Heat treatment is recorded. Austenitizing temperature, quench medium when the mill records it, and tempering temperature go on the MTC. Charpy lateral expansion is run at the temperature agreed on the order. If the RFQ adds energy minima, those extras are scheduled with the mill, not promised after the plate has already been cut.
EN 10204 3.1 is standard. EN 10204 3.2 is arranged when a third party is named. Simulated PWHT, UT, hardness, Z-direction and restricted chemistry are treated as order items, not as brochure defaults. That is the difference between selling “A517 Grade A” as a name and supplying A517GRA as a Code plate.
We also keep the order on the right grade. Grade A is not Grade B. Grade A is not Grade F. Grade A is not A514. Grade A is not EN 10028-6 P690QL unless that specification is actually ordered. If the thickness is 40 mm, we will say so before anyone tries to buy Grade A.
Cutting, welding procedure review and testing can be coordinated through the service pages already linked above. Export packing and documents go through worldwide shipping service. Company scope: China steel Mill Agent-SHH STEEL.
FAQ
-
What names are used for ASTM A517 Grade A?
- Buyers write A517 Gr.A, A517GRA, A517 GR A, A517 Grade A, ASME SA517 Grade A and SA517GRA. They all mean Grade A in ASTM A517/A517M. SHH STEEL prints the wording on the purchase order.
-
Is ASTM A517 Grade A the same as ASME SA517 Grade A / SA517GRA?
- Chemistry and tensile limits match. ASTM A517 is the product spec. ASME SA-517 is the Code version used with ASME Section VIII. As China mill-Direct Supply, SHH STEEL dual-certifies A517 Gr.A / SA517 Gr.A when the vessel must be stamped.
-
What is the yield strength of A517 Gr.A?
- 690 MPa minimum through 32 mm. Tensile is 795–930 MPa. Grade A is not furnished above 32 mm under ASTM A517.
-
Why specify Grade A instead of Grade B?
- Strength and thickness limit are the same. Silicon, chromium, molybdenum and zirconium bands are not. Grade A silicon is 0.40–0.80%. Grade B silicon is 0.15–0.35%. Follow the grade on the drawing.
-
Can EN 10028-6 P690QL or JIS G3128 SHY685 replace ASTM A517 Grade A?
- Not automatically. Those grades are comparison names. Chemistry, thickness limit, impact rule and Code marking must match the drawing. SHH STEEL dual-certs A517/SA517 Grade A for Section VIII work.
-
Is A517GRA the same as A514 Grade A or S690QL?
- No. A514 Grade A and EN 10025-6 S690QL are structural specifications. ASTM A517 Grade A is a pressure-vessel plate under A517 and A20.
-
What heat treatment does ASTM A517 Grade A require?
- Quench and temper. Austenitize at not less than 900 °C, quench in water or oil, temper at not less than 620 °C. As-rolled or normalize-only delivery is not this grade.
-
Can welding of A517 Gr.A be qualified to ASME Section IX?
- Yes, when the plate is used on an ASME vessel. Use a high-strength low-hydrogen WPS written for this alloy and thickness. The fabricator owns the procedure.
-
Can SHH STEEL issue EN 10204 3.2 on ASTM A517 Grade A?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 or another third-party witness is arranged when it is written on the order.
-
What is the density of A517 Gr.A plate?
- 7.85 g/cm³. SHH STEEL uses this value for shipping-weight estimates on ASTM A517/A517M plate.
Conclusion
ASTM A517 Grade A Steel Plate is the high-silicon Cr-Mo, quenched-and-tempered high-strength vessel grade in ASTM A517/A517M, limited to 32 mm. Whether the inquiry says A517 Gr.A, A517GRA, A517 Grade A or ASME SA517 Grade A, SHH STEEL supplies plate with heat and product analysis, recorded QT, the 690 MPa tensile line, agreed Charpy testing, optional simulated PWHT, and EN 10204 3.1 or 3.2 certification.
As a China mill Distributor, SHH STEEL provides ASTM A517 Grade A / A517 Gr.A QT High Strength Vessel Plate for boiler and ASME Section VIII work.
Contact SHH STEEL for mill rolling, QT, dual A517/SA517 marking, 3.2 inspection or a quotation.
ASTM A517 Grade A Steel Plate, A517 Gr.A, A517GRA, ASTM A517, ASME SA517 Grade A, EN 10028-6 P690Q, JIS G3128 SHY685, QT high strength vessel plate, A517 Grade A supplier, Direct Mill Supply by SHH STEEL