ASTM A517 Grade F Steel Plate | A517 Gr.F QT High Strength Vessel Plate
What is ASTM A517 Grade F Steel?
ASTM A517 Grade F is the workhorse grade in ASTM A517/A517M. When a vessel shop asks for 690 MPa QT plate without going beyond 65 mm, this is usually the grade on the drawing. As a China mill Agent, SHH STEEL supplies it to the ASTM product specification.
The same plate is written A517 Gr.F, A517GRF, A517 GR F, A517 Grade F, ASME SA517 Grade F, SA517 Gr.F, SA517GRF and A/SA517 Grade F. They all mean Grade F. ASTM A517/A517M is the product specification. ASME SA-517/SA-517M is the Code companion used with Section VIII.
ASTM A517 lists eight grades—A, B, E, F, H, P, Q and S. They share one mechanical table where thickness overlaps. They do not share alloy content or maximum thickness. Grade F may be furnished up to 65 mm (2.50 in.). If the course is 80 mm, Grade F is the wrong specification; Grade Q or Grade E is the thick option.
The steel is killed and made to fine austenitic grain practice under ASTM A20 / ASME SA-20. Heat treatment is mandatory quench and temper: austenitize at not less than 900 °C, quench in water or oil, temper at not less than 620 °C. As-rolled or normalize-only plate is not A517GRF.
Do not mix this page with ASTM A516 or ASME SA516. Those are carbon vessel plates. ASTM A517 Grade F is a QT alloy plate. It is also not structural A514. A514 is a structural specification. A517 is a pressure-vessel specification with A20 general requirements and vessel testing.
For Code work the plate is dual-certified to ASME SA517 Grade F and used under ASME Section VIII. Certificates can be EN 10204 3.1 or EN 10204 3.2.
When a project is still choosing high-strength vessel plate, a China mill Distributor path through SHH STEEL puts A517GRF next to ASME SA537, ASTM A537, ASME SA387 and ASTM A285, so the buyer can see whether they actually need 690 MPa QT or a lower-strength carbon / Cr-Mo route.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | ASTM A517 Grade F / A517 Gr.F / A517GRF | Confirmed |
| Product Specification | ASTM A517/A517M | Applied |
| Companion Spec | ASME SA517 Grade F / SA517GRF | Dual cert available |
| General Requirements | ASTM A20 / ASME SA-20 | Applied |
| Code Context | ASME Section VIII when dual certified | As specified |
| Product Form | Pressure vessel / boiler plate | Available |
| Steel Practice | Killed, fine austenitic grain | Confirmed |
| Heat Treatment | Quench and temper (mandatory) | Confirmed |
| Maximum Thickness (Grade F) | 65 mm (2.50 in.) | Per A517 |
| Typical Supply | 8 mm – 65 mm | By mill enquiry |
| Width / Length | Up to about 4000 mm / 12000 mm | Mill capability |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate belongs to the Pressure Vessel Steel Plates family. It is not a structural HSLA Steel Plates substitute and not a Carbon Steel Plates grade.
Chemical Composition
Chemistry for ASTM A517 Grade F is reported as heat analysis and, when specified, product analysis under ASTM A517/A517M. Grade F is a Ni-Cr-Mo-B alloy. Nickel is lower than Grade Q. That is one reason Grade F is widely used inside its 65 mm ceiling.
Heat Analysis — ASTM A517 Grade F / A517GRF
| Element | Heat Analysis (%) |
|---|---|
| Carbon (C) | 0.10 – 0.20 |
| Manganese (Mn) | 0.60 – 1.00 |
| Phosphorus (P), max | 0.025 |
| Sulfur (S), max | 0.025 |
| Silicon (Si) | 0.15 – 0.35 |
| Nickel (Ni) | 0.70 – 1.00 |
| Chromium (Cr) | 0.40 – 0.65 |
| Molybdenum (Mo) | 0.40 – 0.60 |
| Vanadium (V) | 0.03 – 0.08 |
| Boron (B) | 0.0005 – 0.005 |
| Copper (Cu) | 0.15 – 0.50 |
Product Analysis — A517 Gr.F / SA517 Grade F
| Element | Product Analysis (%) |
|---|---|
| Carbon (C) | 0.08 – 0.22 |
| Manganese (Mn) | 0.55 – 1.10 |
| Silicon (Si) | 0.13 – 0.37 |
| Nickel (Ni) | 0.67 – 1.03 |
| Chromium (Cr) | 0.36 – 0.69 |
| Molybdenum (Mo) | 0.36 – 0.64 |
| Vanadium (V) | 0.02 – 0.09 |
| Copper (Cu) | 0.12 – 0.53 |
| P, S, B | Per A20 / order |
A Grade Q heat cannot be recertified as Grade F. Nickel and chromium bands are different, and Grade Q exists because thickness goes beyond 65 mm. If the drawing says ASTM A517 Grade F, the ladle must sit in the Grade F table. SHH STEEL reports heat analysis on every certificate and adds product analysis when ASTM A20 or the vessel specification requires it.
Tighter phosphorus, sulfur or residuals are supplementary. Vacuum carbon deoxidation and other A20 chemistry items are available when written on the order.
Mechanical Properties
Where Grade F is permitted (65 mm and under), it uses the high line of the A517 tensile table.
Tensile Requirements — ASTM A517 Grade F per ASTM A517/A517M
| Property | ≤ 65 mm (2.50 in.) |
|---|---|
| Tensile strength | 795 – 930 MPa (115 – 135 ksi) |
| Yield strength, min | 690 MPa (100 ksi) |
| Elongation in 50 mm, min | 16% |
| Reduction of area, rectangular, min | 35% |
| Reduction of area, round, min | 45% |
There is no 150 mm line on Grade F. If the plate is thicker than 65 mm, the specification itself does not cover it. That is the whole point of moving to Grade Q or Grade E.
Density is 7.85 g/cm³. Hardness after QT is typically in a high-strength vessel range; a special HBW window is a supplementary requirement.
ASTM A517 requires transverse Charpy V-notch testing with a minimum lateral expansion of 0.38 mm (0.015 in.) on each specimen. The test temperature is agreed between purchaser and manufacturer. Do not assume −20 °C or −46 °C unless the purchase order says so.
Specimens follow ASTM A20. If simulated PWHT is specified, coupons from the same A517 Gr.F heat follow the vessel cycle before tensile and impact testing. On QT 690 MPa plate that request should be on the mill order whenever the shop will PWHT the vessel.
Material Comparison
| Grade | Alloy emphasis | Max thickness | Same strength table where allowed? |
|---|---|---|---|
| A517 Gr.A / B | Cr-Mo family | 32 mm | Yes |
| A517 Gr.F | Ni-Cr-Mo-B | 65 mm | Yes |
| A517 Gr.P | Higher Ni-Cr-Mo | 100 mm | Yes |
| A517 Gr.Q | Ni-Cr-Mo-V | 150 mm | Yes |
| A517 Gr.E | High Cr-Mo | 150 mm | Yes |
| A537 Cl.2 | Carbon QT | By class | Lower strength |
| A514 | Structural QT | Structural spec | Not a vessel spec |
Order ASTM A517 Grade F when the drawing names Grade F and thickness is 65 mm or less. If thickness exceeds 65 mm, Grade F is not available under A517. If the plate is only 20 mm and the drawing allows Grade B, Grade B may be the lower-alloy option at the same tensile table. SHH STEEL does not swap grades on a Code vessel without a written revision.
HSLA Steel Plates and S690QL structural plate are not ASTM A517. If the equipment is Section VIII, stay on A517 / SA517.
High-Strength QT Vessel Service
ASTM A517 Grade F exists because some vessels cannot be designed in A516 or A537 without excessive thickness, but the wall is still inside 65 mm. The 690 MPa yield line cuts thickness. The 65 mm ceiling is the specification limit, not a mill preference.
When dual certified to ASME SA517 Grade F, allowable stress comes from ASME Section II Part D, not from a mill flyer. Impact temperature is an order number.
Typical use is high-pressure process vessels, heat-exchange shells that need QT strength, modular and transportable pressure equipment, and other fusion-welded parts specified to A517 Grade F. It is not a cryogenic 3.5Ni or 9Ni grade, and it is not a creep-focused Cr-Mo grade such as A387.
Weldability
A517GRF is a high-strength QT alloy. Welding is not the same job as welding A516 Gr.70.
Procedures for Code work are qualified to ASME Section IX. Consumables should match the required joint strength and toughness, usually a high-strength low-hydrogen family selected for 690 MPa class steel. Hydrogen control, preheat and interpass are mandatory. Grade F has enough hardenability that a cold start on a restrained joint will crack.
Preheat depends on thickness, restraint, hydrogen and the qualified WPS. After welding, many shops want to PWHT. On QT plate that decision has to be engineered. A shop cycle that is too hot or too long can drop yield below the A517 table. Simulated PWHT of mill coupons should be on the purchase order whenever the vessel specification includes PWHT.
Do not copy an A516 or A537 procedure onto ASTM A517 Grade F. Do not assume a Grade Q WPS is automatically valid if nickel matching or thickness changes. Procedure review can go through steel welding services. The fabricator owns the qualified WPS.
Heat Treatment
Heat treatment of ASTM A517 Grade F follows ASTM A517/A517M:
- Heat to not less than 900 °C (1650 °F)
- Quench in water or oil
- Temper at not less than 620 °C (1150 °F)
That sequence is the product. As-rolled plate is not A517 Grade F. Normalized-only plate is not A517 Grade F.
Holding time follows mill practice and ASTM A20 thickness rules. If the purchaser fixes a tempering band or a maximum tempering temperature because later PWHT is planned, those limits go on the mill instruction and onto the certificate.
SHH STEEL reports the actual heat-treatment condition on the MTC for every A517 Gr.F plate.
Delivery Condition
Delivery condition for this grade is quenched and tempered. That is the only standard condition.
The certificate lists ASTM A517 Grade F and, when dual certified, ASME SA517 Grade F; heat number; heat analysis; product analysis when ordered; tensile results; reduction of area; Charpy lateral expansion and test temperature; heat-treatment temperatures; and supplementary tests.
Surface is vessel-plate quality. Shot blasting and shop primer are available. Decorative 2B or BA finishes are not used on QT vessel plate.
Certificates may be EN 10204 3.1 or EN 10204 3.2. BV, LR, DNV, TUV, SGS or the buyer’s agency can witness quench, temper, mechanical tests and documents when the order says so.
Dimensions
Usual supply range from SHH STEEL for A517 Gr.F QT high strength vessel plate:
- Thickness: 8 mm – 65 mm (Grade F maximum in ASTM A517 is 65 mm)
- Width: up to about 4000 mm
- Length: up to about 12000 mm
If the inquiry is 70 mm, say so immediately. That thickness is outside Grade F. Cut-to-length shells and nest sizes are available inside the 65 mm limit.
Tolerances
Dimensional limits follow ASTM A20 / ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances. QT plate can move during quench; extra-flatness is a negotiated item.
Ultrasonic testing to A435 or A578 is commonly added. Finished sizes go through steel cutting services. Thermal cutting of 690 MPa QT plate needs preheat and edge control.
Supplementary Requirements
Most ASTM A517 Grade F orders add tests beyond the base table.
Simulated PWHT. Same-heat coupons follow the vessel cycle. Tensile and Charpy are run after that cycle.
Charpy details. Base spec is lateral expansion 0.38 mm, temperature agreed. Purchasers often add energy minima and a stated test temperature.
NDE. UT to A435 / A577 / A578; edge MT/PT after cutting.
Hardness survey. Surface or through-thickness HBW/HV after QT or after simulated PWHT.
Restricted chemistry. Tighter P, S, residuals or vacuum treatment per A20.
HIC / NACE. Only when the datasheet cites TM0284 or MR0175 / ISO 15156. Grade F is not automatically sour-service plate.
Z-direction. A770 or Z15/Z25/Z35 for nozzles and strained joints.
Third-party. Witness of quench, temper, testing and documents. Output can be EN 10204 3.2.
These tests run through steel testing service. If it is not on the purchase order, it is not assumed.
Equivalent Material Grades
| Designation | Standard | Notes |
|---|---|---|
| ASTM A517 Grade F / A517 Gr.F / A517GRF | ASTM A517/A517M | Product name on this page |
| ASME SA517 Grade F / SA517GRF | ASME SA-517/SA-517M | Code companion |
| A517 / SA517 QT 690 vessel plate | Commercial | Strength search name |
| EN 10028-6 P690Q / P690QL related | EN | Project-specific comparison only |
| GB high-strength QT vessel related | GB | Project-specific dual cert |
For stamping, write dual A517 / SA517 Grade F. Nearby vessel pages: ASTM A537, ASME SA537, ASTM A516, ASME SA516.
Applications
ASTM A517 Grade F / A517 Gr.F is selected when a Section VIII or equivalent vessel needs QT alloy strength and thickness stays at or below 65 mm.
| Industry | Typical components |
|---|---|
| High-pressure vessels | ASTM A517 Grade F shells and A517GRF heads |
| Petrochemical | A517 Grade F reactors and high-pressure drums |
| Energy and process | ASTM A517 Grade F QT high strength vessel plate |
| Modular / transportable equipment | A517 Gr.F courses inside 65 mm |
| Dual-certified export | A517 / SA517 Gr.F plate |
| Heavy fabrication | A517GRF cut to nest sizes |
Related pages: petrochemical industry, energy industry, steel cutting services, steel welding services, steel testing service, worldwide shipping service.
Why Choose SHH STEEL
SHH STEEL works as a China Mill Direct Exporter for plates to ASTM A517/A517M. On ASTM A517 Grade F that means mill pricing, dual A517/SA517 marking, heat and product analysis, mandatory QT with recorded temperatures, Charpy lateral expansion at the agreed temperature, 3.1 as standard and 3.2 when specified, and the extra tests a 690 MPa vessel shop actually writes on the PO.
We also keep the order on the right grade. Grade F is not Grade Q. Grade F is not A537 Class 2. Grade F is not A514. If the thickness is 80 mm, we will say so before anyone tries to buy Grade F. Export packing goes through worldwide shipping service. Company scope: China steel Mill Agent-SHH STEEL.
FAQ
-
What names are used for ASTM A517 Grade F?
- Buyers write A517 Gr.F, A517GRF, A517 GR F, A517 Grade F, ASME SA517 Grade F and SA517GRF. They all mean Grade F in ASTM A517/A517M. SHH STEEL prints the wording on the purchase order.
-
Is ASTM A517 Grade F the same as ASME SA517 Grade F / SA517GRF?
- Chemistry and tensile limits match. ASTM A517 is the product spec. ASME SA-517 is the Code version used with ASME Section VIII. As China mill-Direct Supply, SHH STEEL dual-certifies A517 Gr.F / SA517 Gr.F when the vessel must be stamped.
-
What is the yield strength of A517 Gr.F?
- 690 MPa minimum through 65 mm. Tensile is 795–930 MPa. Grade F is not furnished above 65 mm under ASTM A517.
-
Why specify Grade F instead of Grade Q or Grade B?
- Strength is the same where thickness overlaps. Grade B stops at 32 mm. Grade F stops at 65 mm. Grade Q goes to 150 mm. Alloy content is also different. Follow the grade and thickness on the drawing.
-
Is A517GRF the same as A514 or S690QL?
- No. Those are structural specifications. ASTM A517 Grade F is a pressure-vessel plate under A517 and A20. Do not substitute structural QT plate on a Section VIII vessel.
-
What heat treatment does ASTM A517 Grade F require?
- Quench and temper. Austenitize at not less than 900 °C, quench in water or oil, temper at not less than 620 °C. As-rolled or normalize-only delivery is not this grade.
-
Can welding of A517 Gr.F be qualified to ASME Section IX?
- Yes, when the plate is used on an ASME vessel. Use a high-strength low-hydrogen WPS written for this alloy and thickness. The fabricator owns the procedure.
-
Can SHH STEEL issue EN 10204 3.2 on ASTM A517 Grade F?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 or another third-party witness is arranged when it is written on the order.
-
What is the density of A517 Gr.F plate?
- 7.85 g/cm³. SHH STEEL uses this value for shipping-weight estimates on ASTM A517/A517M plate.
Conclusion
ASTM A517 Grade F Steel Plate is the Ni-Cr-Mo-B, quenched-and-tempered high-strength vessel grade in ASTM A517/A517M, limited to 65 mm. Whether the inquiry says A517 Gr.F, A517GRF, A517 Grade F or ASME SA517 Grade F, SHH STEEL supplies plate with heat and product analysis, recorded QT, the 690 MPa tensile line, agreed Charpy testing, optional simulated PWHT, and EN 10204 3.1 or 3.2 certification.
As Direct Mill Supply by SHH STEEL, we provide ASTM A517 Grade F / A517 Gr.F QT High Strength Vessel Plate for boiler and ASME Section VIII work.
Contact SHH STEEL for mill rolling, QT, dual A517/SA517 marking, 3.2 inspection or a quotation.
ASTM A517 Grade F Steel Plate, A517 Gr.F, A517GRF, ASTM A517, ASME SA517 Grade F, QT high strength vessel plate, A517 Grade F supplier, China mill Agent