ISO 9329-4 X6CrNiMoTi17-12 Seamless Stainless Steel Tube
What is ISO 9329-4 X6CrNiMoTi17-12 Seamless Stainless Steel Tube
ISO 9329-4 covers seamless hot- and/or cold-finished austenitic tubes selected from ISO 1127 / ISO 4200 dimensions. Inside that standard, X6CrNiMoTi17-12 is filed as austenitic Ti-stabilised Mo 17-12-2. X6CrNiMoTi17-12 is the ISO 316Ti seamless pressure tube — Ti stabilisation plus Mo 2.00–2.50, with a hard 6 mm wall note on Table 3 tensile floors.
From billet through marking and crate protection, SHH STEEL can produce ISO 9329-4 X6CrNiMoTi17-12 for the sizes and tests on your RFQ. Application sketch: chemical plant welded Mo tubing, heat-exchanger interconnects, and chloride-lean process lines that specify titanium stabilisation with molybdenum. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Pair EN 10216-5 1.4571 and ASTM A312 aliases share chemistry families with X6CrNiMoTi17-12, yet hydrostatic, NDT, and delivery-condition text diverge. Document the medium, design temperature, and weld map beside the X6CrNiMoTi17-12 line item so sister-grade swaps stay engineering decisions. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Document test category (I or II), type of condition, and any optional elevated-temperature proof-stress or IGC requirements with the X6CrNiMoTi17-12 size list so quality planners book the correct benches before tube is cut to length. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Inside this ISO 9329-4 series, compare ISO 9329-4 X6CrNiMoNb17-12, ISO 9329-4 X5CrNiMo17-12, ISO 9329-4 X2CrNiMo17-12, ISO 9329-4 X6CrNiTi18-10. Hub: ISO 9329-4. Related pressure-tube page (not interchangeable by default): EN 10216-5 1.4571. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP316Ti.
When X6CrNiMoTi17-12 pipe sits beside plate on the same BOM, Stainless Steel Pipes and Tubes covers the tubular parent, Stainless Steel Sheets and Plates covers flats, and ASTM A240 UNS S31635 is the live plate chemistry match — do not merge MTCs. Confirm X6CrNiMoTi17-12 OD × wall and plate thickness on separate drawings.
Chemical Composition of ISO 9329-4 X6CrNiMoTi17-12
If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 1, SHH STEEL will confirm melt feasibility for X6CrNiMoTi17-12 before the order is acknowledged. Keep caution visible: Table 3 tensile values apply ONLY for wall ≤6 mm (note 11) — thicker walls need agreed properties; verify Ti ≥5×C on cast.
Heat identity for X6CrNiMoTi17-12 stays unbroken from melt through bundle tags; transition material from sequential strand casts must be positively separated per clause 5.1 practice. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
| Grade | C | Si | Mn | P | S | Cr | Mo | Ni | Ti |
|---|---|---|---|---|---|---|---|---|---|
| X6CrNiMoTi17-12 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 16.50–18.50 | 2.00–2.50 | 11.00–14.00 | ≥5×%C ≤0.80 |
Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.
Mechanical Properties of ISO 9329-4 X6CrNiMoTi17-12
Elevated-temperature Rp0.2 / Rp1.0 values live in Table 4 and are not normally verified unless the purchaser orders 9.4.2 testing for X6CrNiMoTi17-12. Ambient floors remain the Table 3 pair above. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Size practice for X6CrNiMoTi17-12 remains thin-to-medium wall ISO 1127 OD×wall — note 6 mm tensile limit on Table 3. Do not substitute sister-grade tensile floors onto this certificate without a written dual-product plan. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | Rp0.2 min (N/mm²) | Rp1.0 min (N/mm²) | Rm (N/mm²) | A long. min (%) | A trans. min (%) | KV long. min (J) | Solution treatment |
|---|---|---|---|---|---|---|---|
| X6CrNiMoTi17-12 | 210 | 245 | 510–710 | 40 | 35 | 85 | 1020–1120 °C |
Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X6CrNiMoTi17-12 (solution-treated; wall ≤50 mm unless noted). Table 3 tensile values ONLY for wall ≤6 mm (note 11); thicker walls by agreement. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: Yes — guideline limit ~400 °C / 100000 h.
Seamless Tube Manufacture of ISO 9329-4 X6CrNiMoTi17-12
ISO 9329-4:1997 manufactures X6CrNiMoTi17-12 as seamless tube only — hot finished, cold finished, or a combination — never as an ERW product under this part. SHH STEEL confirms the seamless route and the ordered type of condition (table 7 symbols such as HFS2) on the acknowledgement before finishing starts. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Manufacture stays seamless. Size: thin-to-medium wall ISO 1127 OD×wall — note 6 mm tensile limit on Table 3. Hydrostatic pressure class or NDT options for X6CrNiMoTi17-12 are frozen with the size list so quality planners book the correct benches before tube is cut to length. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Bevelled ends, special straightness, bar coding, and protective coating for X6CrNiMoTi17-12 are optional purchaser items under clause 4.2 — list them explicitly or expect mill defaults. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Dimensions and Tolerances for ISO 9329-4 X6CrNiMoTi17-12
Precision and tolerance class for X6CrNiMoTi17-12 follow the dimensional standard cited on the order (typically ISO 1127 series). Ambiguous “standard tube” language is clarified before rolling slots are booked. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
When ISO 2037 food-tube dimensions are mixed into an ISO 9329-4 X6CrNiMoTi17-12 enquiry, separate the dimensional reference from the pressure product standard so QA does not merge acceptance texts. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Equivalent Grades for ISO 9329-4 X6CrNiMoTi17-12
Cross-references help sourcing X6CrNiMoTi17-12, but they do not replace the ISO 9329-4 grade line on the enquiry. Family framing here is austenitic Ti-stabilised Mo 17-12-2; delivery practice from the crib is “solution-treated (Q) or hot-finished within solution band + rapid cool”. Related ASTM or EN numbers are starting points for engineering comparison, not automatic substitutes.
| System | Designation | Notes |
|---|---|---|
| ISO 9329-4 | X6CrNiMoTi17-12 | Governing tube grade for this page |
| Commercial / UNS (body only) | 316Ti / UNS S31635 / EN 1.4571 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 / A213 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | 1.4571 | Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec |
We deliberately avoid inventing a false one-to-one for every foreign system on X6CrNiMoTi17-12. Use ISO 9329-4 X6CrNiMoNb17-12, ISO 9329-4 X5CrNiMo17-12, ISO 9329-4 X2CrNiMo17-12, ISO 9329-4 X6CrNiTi18-10 for in-series alternatives, and keep ISO 9329-4 as the category landing page. Dual marking is a purchase-order option that still requires every limit that matters for X6CrNiMoTi17-12 to be verified on the heat.
Heat Treatment and Delivery Condition for ISO 9329-4 X6CrNiMoTi17-12
Party acceptance groups tubes by size, steel grade, and heat-treatment kind for X6CrNiMoTi17-12. Mixing differently treated lengths in one lot breaks batch rules. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Continuous-furnace practice for X6CrNiMoTi17-12 should hold near the upper end of 1020–1120 °C when the standard’s guidance notes apply; for subsequent fabricator HT, prefer the lower end of the band. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Corrosion Resistance of ISO 9329-4 X6CrNiMoTi17-12
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for X6CrNiMoTi17-12. Duty lock: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Pickled vs bright surfaces change initiation sites for X6CrNiMoTi17-12; state the finish beside the corrosion requirement so lab coupons match installed tube. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Applications of ISO 9329-4 X6CrNiMoTi17-12 Seamless Tube
Commissioning teams benefit when isometric revisions for X6CrNiMoTi17-12 link to the same mill certificates and test category stated on the acknowledgement. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Replace X6CrNiMoTi17-12 with a Mo or N sister when chloride or strength demand outgrows this chemistry — sisters X6CrNiMoNb17-12, X5CrNiMo17-12, X2CrNiMo17-12, X6CrNiTi18-10. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Weldability of ISO 9329-4 X6CrNiMoTi17-12
For corrosive as-welded duty on X6CrNiMoTi17-12, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable to this mark. Role: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Keep Table 3 tensile values apply ONLY for wall ≤6 mm (note 11) — thicker walls need agreed properties; verify Ti ≥5×C on cast visible when selecting fillers for X6CrNiMoTi17-12; boron- or nitrogen-bearing marks need matching intent in the weld metal. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Surface Finishes for ISO 9329-4 X6CrNiMoTi17-12
X6CrNiMoTi17-12 under ISO 9329-4 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (X6CrNiMoTi17-12).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Do not polish over unresolved defects on X6CrNiMoTi17-12; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but ISO 9329-4 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (X6CrNiMoTi17-12).
Inspection and Testing for ISO 9329-4 X6CrNiMoTi17-12
Test category I vs II for X6CrNiMoTi17-12 changes the intensity of testing — freeze it on the order example style used in the standard (grade – condition – category – document). Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Documents for X6CrNiMoTi17-12 cite the actual tests performed. An MTC that only lists chemistry is incomplete against a specific-inspection order. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Packaging and Shipping for ISO 9329-4 X6CrNiMoTi17-12
Protective coating per clause 11 for X6CrNiMoTi17-12 is agreed when open storage or salt air exposure is expected before installation. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Packing list line items for X6CrNiMoTi17-12 must match stencil text; alias-only labels are a common customs and QA failure mode. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
SHH STEEL can supply export packing for X6CrNiMoTi17-12 sized to the container plan on the shipping order when the mill schedule allows. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Why Choose SHH STEEL
Ask for a written acknowledgement that names X6CrNiMoTi17-12, dimensional standard, condition symbol, and test category before melt. SHH STEEL can produce to that acknowledgement. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
Repeat orders for X6CrNiMoTi17-12 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Supply Capability
Documents available for X6CrNiMoTi17-12: ISO 10474 / EN 10204 style as ordered, with heat analysis and Table 3 tensile as baseline specific-inspection content. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service.
| Item | Capability |
|---|---|
| Standard | ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes |
| Grade | X6CrNiMoTi17-12 (Table 1; alias 316Ti / UNS S31635 / EN 1.4571 (approx)) |
| Product form | Seamless tube only — hot and/or cold finished before heat treatment |
| Delivery condition | solution-treated (Q) or hot-finished within solution band + rapid cool |
| Documents | ISO 10474 / EN 10204 3.1 style as ordered |
| Typical size practice | OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759 |
| Condition symbols | Table 7 (e.g. HFS2) as ordered |
| Tests | Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered |
Stock / Available sizes
Stock / Available sizes map for X6CrNiMoTi17-12 is refreshed on enquiry. Role: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service. Optional hydro, UT, IGC, and elevated proof tests are booked with the size list, not as afterthoughts. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
SHH STEEL can make X6CrNiMoTi17-12 to ISO 9329-4 with the hyphenated grade frozen on tags and certificates so spaced ISO designations and commercial aliases cannot drift apart in receiving inspection. Keep ISO 9329-4 and X6CrNiMoTi17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
FAQ
-
What is ISO 9329-4 X6CrNiMoTi17-12 seamless stainless steel tube used for?
- ISO 9329-4 X6CrNiMoTi17-12 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — chemical plant welded Mo tubing, heat-exchanger interconnects, and chloride-lean process lines that specify titanium stabilisation with molybdenum. Role summary: Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
-
Is ISO 9329-4 X6CrNiMoTi17-12 seamless only, or does it cover welded tube?
- Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X6CrNiMoTi17-12 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
-
What heat treatment does X6CrNiMoTi17-12 require under ISO 9329-4?
- Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X6CrNiMoTi17-12: 1020–1120 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
-
How does X6CrNiMoTi17-12 compare with sister grades X6CrNiMoNb17-12, X5CrNiMo17-12, X2CrNiMo17-12?
- X6CrNiMoTi17-12 is filed as austenitic Ti-stabilised Mo 17-12-2. Typical sisters on the same RFQ are X6CrNiMoNb17-12, X5CrNiMo17-12, X2CrNiMo17-12. Design caution: Table 3 tensile values apply ONLY for wall ≤6 mm (note 11) — thicker walls need agreed properties; verify Ti ≥5×C on cast Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
-
What tests appear on the mill certificate for X6CrNiMoTi17-12?
- Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
-
Is 316Ti / UNS S31635 / EN 1.4571 (approx) the same as ordering X6CrNiMoTi17-12?
- No. 316Ti / UNS S31635 / EN 1.4571 (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X6CrNiMoTi17-12 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for ISO 9329-4 X6CrNiMoTi17-12?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X6CrNiMoTi17-12 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: thin-to-medium wall ISO 1127 OD×wall — note 6 mm tensile limit on Table 3. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should X6CrNiMoTi17-12 be welded on site?
- Shop guidance: 316Ti / 1.4571-class practice; confirm Ti formula after multipass welds. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: Table 3 tensile values apply ONLY for wall ≤6 mm (note 11) — thicker walls need agreed properties; verify Ti ≥5×C on cast
-
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X6CrNiMoTi17-12?
- Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic Ti-stabilised Mo 17-12-2 practice can defend for the temperature and stress state. Caution for this mark: Table 3 tensile values apply ONLY for wall ≤6 mm (note 11) — thicker walls need agreed properties; verify Ti ≥5×C on cast Sister pointers: X6CrNiMoNb17-12, X5CrNiMo17-12, X2CrNiMo17-12. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify ISO 9329-4 X6CrNiMoTi17-12 with ASTM A312 or EN 10216-5?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X6CrNiMoTi17-12 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What is the difference between hyphenated X6CrNiMoTi17-12 and the spaced ISO designation?
- They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X6CrNiMoTi17-12 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.
Conclusion
ISO 9329-4 X6CrNiMoTi17-12 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — Ti-stabilised Mo 17-12-2 austenitic pressure tube — ISO 316Ti-class mark for welded Mo-bearing corrosion service. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X6CrNiMoNb17-12, X5CrNiMo17-12, X2CrNiMo17-12. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.