ISO 9329-4 X2CrNiN18-10 Seamless Stainless Steel Tube
What is ISO 9329-4 X2CrNiN18-10 Seamless Stainless Steel Tube
Pressure packages that cite ISO 9329-4 expect seamless austenitic tube with Table 1 chemistry and Table 3 tensile floors, not an automatic ASTM A312 or EN 10216-5 certificate. X2CrNiN18-10 is the hyphenated steel name matching ISO’s spaced designation for this austenitic low-carbon N-strengthened 18-10 chemistry. X2CrNiN18-10 lifts Table 3 Rp0.2 to 270 N/mm² with intentional nitrogen — the ISO 304LN seamless pressure tube under 9329-4.
Mill path for X2CrNiN18-10: seamless hot and/or cold finish, Table 3 solution treatment, Table 1 heat analysis, Table 3 Rm/Rp/A pair, optional elevated proof stress, impact, hydro, NDT, and IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: pressure vessels and interconnects needing higher design proof stress than X2CrNi18-10 at similar corrosion family, cryogenic-capable austenitic tubing, and weight-sensitive pressure packages.
On the floor people say “304LN tube”; in QA they must not stop there. X2CrNiN18-10 under ISO 9329-4 carries specific Table 1 and Table 3 limits that a loose alias will not enforce. Design caution: N 0.12–0.22 is mandatory — residual nitrogen is not enough; Rp0.2 min 270 N/mm² is the design reason to pick this mark.
Use thread: pressure vessels and interconnects needing higher design proof stress than X2CrNi18-10 at similar corrosion family, cryogenic-capable austenitic tubing, and weight-sensitive pressure packages. Size and test clarity on the RFQ lets SHH STEEL lock the correct seamless pressure-tube scope for X2CrNiN18-10 before production starts. Size practice for X2CrNiN18-10 remains ISO 1127 OD×wall where thinner wall is justified by higher proof stress.
Inside this ISO 9329-4 series, compare ISO 9329-4 X2CrNi18-10, ISO 9329-4 X2CrNiMoN17-13, ISO 9329-4 X5CrNi18-9, ISO 9329-4 X2CrNiMo17-12. Hub: ISO 9329-4. Related pressure-tube page (not interchangeable by default): EN 10216-5 1.4311. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP304LN.
Chemical Composition of ISO 9329-4 X2CrNiN18-10
Table 1 cast windows for X2CrNiN18-10 lock C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Cr 17.00–19.00, Ni 8.50–11.50, N 0.12–0.22. Product analysis, when ordered, uses Table 2 permissible deviations — not a free rewrite of the grade. Role: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
ISO 9329-4 does not publish a separate “welding grade” sulphur tighten inside Table 1; if the order needs S ≤0.015 or similar for fabrication, write it as a purchaser agreement on X2CrNiN18-10. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | C | Si | Mn | P | S | Cr | Ni | N |
|---|---|---|---|---|---|---|---|---|
| X2CrNiN18-10 | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 17.00–19.00 | 8.50–11.50 | 0.12–0.22 |
Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.
Mechanical Properties of ISO 9329-4 X2CrNiN18-10
Room-temperature mechanical properties for X2CrNiN18-10 are measured at 23±5 °C and must meet Table 3. Summary: Rp0.2 min 270 N/mm², Rp1.0 min 305 N/mm², Rm 580–780 N/mm², A long. min 40% / A trans. min 35%. Duty: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Flattening and expansion technological tests follow Table 3 coefficients when required by the test category for X2CrNiN18-10. Wall >50 mm mechanical values are by agreement — do not assume thin-wall floors. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | Rp0.2 min (N/mm²) | Rp1.0 min (N/mm²) | Rm (N/mm²) | A long. min (%) | A trans. min (%) | KV long. min (J) | Solution treatment |
|---|---|---|---|---|---|---|---|
| X2CrNiN18-10 | 270 | 305 | 580–780 | 40 | 35 | 85 | 1000–1100 °C |
Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X2CrNiN18-10 (solution-treated; wall ≤50 mm unless noted). Nitrogen lifts proof stress vs X2CrNi18-10; wall ≤50 mm. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: Yes — guideline limit ~400 °C / 100000 h.
Seamless Tube Manufacture of ISO 9329-4 X2CrNiN18-10
SHH STEEL can produce X2CrNiN18-10 as seamless pressure tube to ISO 9329-4:1997, apply solution treatment over the full length, descale or bright-finish per the ordered surface condition, and cut to ISO 1127 lengths. Plain or bevelled ends follow the enquiry. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Solution treatment shall heat X2CrNiN18-10 tubes uniformly into the Table 3 band and cool rapidly. Hot-finished tubes pressed or extruded inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Cold finishing after hot work for X2CrNiN18-10 still ends in full-length heat treatment per 5.3 unless the hot-finish-in-band exception applies. Surface descaling follows the ordered condition symbol. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dimensions and Tolerances for ISO 9329-4 X2CrNiN18-10
Out-of-table OD×wall combinations for X2CrNiN18-10 are by agreement — still under the same steel grade symbol. Duty: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo. Cap/practice: ISO 1127 OD×wall where thinner wall is justified by higher proof stress. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Mass calculation for X2CrNiN18-10 follows the dimensional standard; do not invent a density override without a written agreement. Random vs exact length must appear on the PO. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Equivalent Grades for ISO 9329-4 X2CrNiN18-10
For X2CrNiN18-10, start with identity under ISO 9329-4 and only then walk commercial / UNS aliases. 304LN / UNS S30453 / EN 1.4311 (approx) is useful in body text; it is not the PO grade by itself. ASTM A312 / A213 related counterparts share a chemistry family at best — wall basis and NDT do not transfer by default.
| System | Designation | Notes |
|---|---|---|
| ISO 9329-4 | X2CrNiN18-10 | Governing tube grade for this page |
| Commercial / UNS (body only) | 304LN / UNS S30453 / EN 1.4311 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 / A213 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | 1.4311 | Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec |
Order discipline for X2CrNiN18-10 still points at ISO 9329-4, not the brochure alias. Neighbours ISO 9329-4 X2CrNi18-10, ISO 9329-4 X2CrNiMoN17-13, ISO 9329-4 X5CrNi18-9, ISO 9329-4 X2CrNiMo17-12 each carry their own mechanical table. Category hub: ISO 9329-4. Dual marking is a purchase-order option that still requires every limit that matters for X2CrNiN18-10 to be verified on the heat.
For X2CrNiN18-10 dual-form buying, link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and ASTM A240 UNS S30453 so purchasing does not treat one product form as the other. Do not stretch a X2CrNiN18-10 pipe certificate onto plate.
Heat Treatment and Delivery Condition for ISO 9329-4 X2CrNiN18-10
Recorded furnace charts for X2CrNiN18-10 should support the heat-treatment claim on the certificate, including quench or cool method where rapid cooling is required. Band note: 1000–1100 °C. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
IGC applicability for X2CrNiN18-10: Yes — guideline limit ~400 °C / 100000 h. Elevated-temperature grades marked N/A for IGC in Table 3 are not “exempt from corrosion engineering” — they are oriented to hot service acceptance paths. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Corrosion Resistance of ISO 9329-4 X2CrNiN18-10
ISO 9329-4 corrosion text focuses on intergranular corrosion (ISO 3651-1 / 3651-2) for X2CrNiN18-10. Other corrosion modes are outside the standard’s normative scope and must be engineered separately. Framing: low-C 18-10 plus nitrogen; corrosion similar to 304L family with higher strength — Mo still needed for chlorides. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Specific corrosion tests beyond IGC for X2CrNiN18-10 shall be agreed at enquiry with method and acceptance criteria written down — the standard will not invent them. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Applications of ISO 9329-4 X2CrNiN18-10 Seamless Tube
Typical duties for X2CrNiN18-10: pressure vessels and interconnects needing higher design proof stress than X2CrNi18-10 at similar corrosion family, cryogenic-capable austenitic tubing, and weight-sensitive pressure packages. Role: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo. Keep the as-built dossier repeating X2CrNiN18-10 beside heat numbers. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Cryogenic or elevated-temperature options for X2CrNiN18-10 need explicit impact or Table 4 proof-stress orders — ambient Table 3 alone does not prove those duties. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Weldability of ISO 9329-4 X2CrNiN18-10
Automatic mill welding is outside seamless ISO 9329-4; manual and automatic field welds must still respect X2CrNiN18-10 chemistry. Guidance: 308L / LN-aware practice; nitrogen loss in weld metal may need matching LN fillers. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Post-weld solution treatment of X2CrNiN18-10 should chase 1000–1100 °C when the corrosion file demands restored IGC resistance after heavy fabrication. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Surface Finishes for ISO 9329-4 X2CrNiN18-10
Iron-free handling after pickle matters for X2CrNiN18-10 — carbon-steel strapping stains show up later as rust blooms on finished tube. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Roughness or appearance callouts never waive the anneal or solution-anneal proof required by the product standard (X2CrNiN18-10).
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
When X2CrNiN18-10 ships, the finish route belongs on the quotation and the MTC. Passivation is not a substitute for solution anneal; packing must keep chloride films and carbon-steel marks off the finished OD/ID. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for X2CrNiN18-10.
Inspection and Testing for ISO 9329-4 X2CrNiN18-10
Sampling plans for X2CrNiN18-10 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Caution: N 0.12–0.22 is mandatory — residual nitrogen is not enough; Rp0.2 min 270 N/mm² is the design reason to pick this mark. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Weld-shop note tied to X2CrNiN18-10: 308L / LN-aware practice; nitrogen loss in weld metal may need matching LN fillers. Mill tests do not replace fabricator WPS qualification. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Packaging and Shipping for ISO 9329-4 X2CrNiN18-10
Container loading plans should keep heavy walls from crushing thin-wall X2CrNiN18-10 layers. Corrosion framing: low-C 18-10 plus nitrogen; corrosion similar to 304L family with higher strength — Mo still needed for chlorides. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Mixed-grade bundles are forbidden when X2CrNiN18-10 shares a crate with a different Table 1 steel — heat identity must remain auditable at receipt. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Claims handling for X2CrNiN18-10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Why Choose SHH STEEL
SHH STEEL can make X2CrNiN18-10 to the written scope: Table 1 chemistry, Table 3 tensile, ordered condition symbol, and test category. Use: pressure vessels and interconnects needing higher design proof stress than X2CrNi18-10 at similar corrosion family, cryogenic-capable austenitic tubing, and weight-sensitive pressure packages. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dual-cert discussions for X2CrNiN18-10 start with a chemistry and test matrix — not with a promise that “304/316 equivalent” clears ASTM by default. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
Supply Capability
SHH STEEL can produce ISO 9329-4 X2CrNiN18-10 in enquiry-oriented OD × wall bands under ISO 1127 / ISO 4200 practice. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Duty: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Item | Capability |
|---|---|
| Standard | ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes |
| Grade | X2CrNiN18-10 (Table 1; alias 304LN / UNS S30453 / EN 1.4311 (approx)) |
| Product form | Seamless tube only — hot and/or cold finished before heat treatment |
| Delivery condition | solution-treated (Q) or hot-finished within solution band + rapid cool |
| Documents | ISO 10474 / EN 10204 3.1 style as ordered |
| Typical size practice | OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759 |
| Condition symbols | Table 7 (e.g. HFS2) as ordered |
| Tests | Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered |
Stock / Available sizes
Stock / Available sizes for X2CrNiN18-10: enquire OD × wall × length × condition symbol. Size practice: ISO 1127 OD×wall where thinner wall is justified by higher proof stress. SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Export packing, third-party inspection, and dual-language MTCs for X2CrNiN18-10 are available when stated on the order. Sisters often quoted alongside: X2CrNi18-10, X2CrNiMoN17-13, X5CrNi18-9, X2CrNiMo17-12. Keep ISO 9329-4 and X2CrNiN18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo.
FAQ
-
What is ISO 9329-4 X2CrNiN18-10 seamless stainless steel tube used for?
- ISO 9329-4 X2CrNiN18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — pressure vessels and interconnects needing higher design proof stress than X2CrNi18-10 at similar corrosion family, cryogenic-capable austenitic tubing, and weight-sensitive pressure packages. Role summary: low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
-
Is ISO 9329-4 X2CrNiN18-10 seamless only, or does it cover welded tube?
- Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X2CrNiN18-10 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
-
What heat treatment does X2CrNiN18-10 require under ISO 9329-4?
- Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X2CrNiN18-10: 1000–1100 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
-
How does X2CrNiN18-10 compare with sister grades X2CrNi18-10, X2CrNiMoN17-13, X5CrNi18-9?
- X2CrNiN18-10 is filed as austenitic low-carbon N-strengthened 18-10. Typical sisters on the same RFQ are X2CrNi18-10, X2CrNiMoN17-13, X5CrNi18-9. Design caution: N 0.12–0.22 is mandatory — residual nitrogen is not enough; Rp0.2 min 270 N/mm² is the design reason to pick this mark Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
-
What tests appear on the mill certificate for X2CrNiN18-10?
- Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
-
Is 304LN / UNS S30453 / EN 1.4311 (approx) the same as ordering X2CrNiN18-10?
- No. 304LN / UNS S30453 / EN 1.4311 (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X2CrNiN18-10 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for ISO 9329-4 X2CrNiN18-10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X2CrNiN18-10 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: ISO 1127 OD×wall where thinner wall is justified by higher proof stress. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should X2CrNiN18-10 be welded on site?
- Shop guidance: 308L / LN-aware practice; nitrogen loss in weld metal may need matching LN fillers. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: N 0.12–0.22 is mandatory — residual nitrogen is not enough; Rp0.2 min 270 N/mm² is the design reason to pick this mark
-
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X2CrNiN18-10?
- Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic low-carbon N-strengthened 18-10 practice can defend for the temperature and stress state. Caution for this mark: N 0.12–0.22 is mandatory — residual nitrogen is not enough; Rp0.2 min 270 N/mm² is the design reason to pick this mark Sister pointers: X2CrNi18-10, X2CrNiMoN17-13, X5CrNi18-9. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify ISO 9329-4 X2CrNiN18-10 with ASTM A312 or EN 10216-5?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X2CrNiN18-10 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What is the difference between hyphenated X2CrNiN18-10 and the spaced ISO designation?
- They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X2CrNiN18-10 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.
Conclusion
ISO 9329-4 X2CrNiN18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — low-carbon nitrogen-strengthened 18-10 austenitic pressure tube — ISO 304LN-class for higher proof stress without Mo. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X2CrNi18-10, X2CrNiMoN17-13, X5CrNi18-9. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.