ISO 9329-4 X6CrNiTi18-10 Seamless Stainless Steel Tube
What is ISO 9329-4 X6CrNiTi18-10 Seamless Stainless Steel Tube
ISO 9329-4:1997 is the International Standard for seamless circular austenitic stainless steel tubes for pressure and corrosion-resisting purposes at room, low, or elevated temperature — pressure vessels, chemical plant, steam-generating equipment, and interconnecting pipework. Grade X6CrNiTi18-10 sits in Table 1 as austenitic Ti-stabilised 18-10. X6CrNiTi18-10 is the ISO 9329-4 Ti-stabilised 18-10 pressure tube — use it when the corrosion file wants 321-class stabilisation under ISO product text.
SHH STEEL can produce and supply ISO 9329-4 X6CrNiTi18-10 as seamless stainless steel tube across the enquiry OD×wall band (ISO 1127 / ISO 4200 practice), solution-treated over the full length, descaled or bright-finished per ordered condition, and documented on inspection documents (ISO 10474 / EN 10204 style as specified). Duty focus: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service.
Commercial aliases such as 321 / UNS S32100 / EN 1.4541 (approx) help buyers navigate catalogues, but the governing symbols on the order and MTC remain ISO 9329-4 and X6CrNiTi18-10. Caution for this mark: Table 3 Rp0.2 min is 175 N/mm² — lower than X5CrNi18-9; do not assume 304 tensile floors on a 321-class ISO certificate. Keep isometric notes and the mill acknowledgement aligned on the hyphenated grade so informal alias language cannot reopen the carbon, molybdenum, nitrogen, or stabiliser window after melt.
Inside this ISO 9329-4 series, compare sisters X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9, X6CrNiMoTi17-12 before freezing wall thickness alone. Size practice for X6CrNiTi18-10 remains ISO 1127 / ISO 4200 OD×wall for Ti-stabilised pressure interconnects. SHH STEEL can produce trial lengths for procedure qualification when the project calendar needs them. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Inside this ISO 9329-4 series, compare ISO 9329-4 X7CrNiTi18-10, ISO 9329-4 X6CrNiNb18-11, ISO 9329-4 X5CrNi18-9, ISO 9329-4 X6CrNiMoTi17-12. Hub: ISO 9329-4. Related pressure-tube page (not interchangeable by default): EN 10216-5 1.4541. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP321.
Chemical Composition of ISO 9329-4 X6CrNiTi18-10
For X6CrNiTi18-10, the heat analysis has to show ISO 9329-4 Table 1 compliance — C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Cr 17.00–19.00, Ni 9.00–12.00, Ti ≥5×%C ≤0.80. Elements not listed shall not be intentionally added without purchaser agreement except for finishing the heat. Corrosion framing: titanium stabilisation for welded IGC; guideline IGC limit ~400 °C; Mo sisters when chlorides rise.
Niobium content, where specified, includes tantalum determined as niobium. Titanium and niobium formulae are minimum multipliers of carbon with absolute caps — verify both sides on the cast ticket for X6CrNiTi18-10. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | C | Si | Mn | P | S | Cr | Ni | Ti |
|---|---|---|---|---|---|---|---|---|
| X6CrNiTi18-10 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 17.00–19.00 | 9.00–12.00 | ≥5×%C ≤0.80 |
Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.
Mechanical Properties of ISO 9329-4 X6CrNiTi18-10
Do not paste EN 10216-5 or ASTM A312 tensile numbers onto an ISO 9329-4 X6CrNiTi18-10 certificate. Under Table 3 (solution-treated, wall ≤50 mm unless noted) expect Rp0.2 min 175 N/mm², Rp1.0 min 210 N/mm², Rm 490–690 N/mm², A long. min 40% / A trans. min 35%. Note: Wall ≤50 mm Table 3 values.
Impact KV minima in Table 3 (long. 85 J / trans. 55 J where applicable) apply when impact testing is in the ordered scope for X6CrNiTi18-10. Low-temperature impact values are by agreement (Annex B informational). Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | Rp0.2 min (N/mm²) | Rp1.0 min (N/mm²) | Rm (N/mm²) | A long. min (%) | A trans. min (%) | KV long. min (J) | Solution treatment |
|---|---|---|---|---|---|---|---|
| X6CrNiTi18-10 | 175 | 210 | 490–690 | 40 | 35 | 85 | 1020–1120 °C |
Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X6CrNiTi18-10 (solution-treated; wall ≤50 mm unless noted). Wall ≤50 mm Table 3 values. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: Yes — guideline limit ~400 °C / 100000 h.
Seamless Tube Manufacture of ISO 9329-4 X6CrNiTi18-10
Seamless is mandatory wording for X6CrNiTi18-10: clause 5.2 requires a seamless process; hot-finished and cold-finished refer to the condition before heat treatment under 5.3. SHH STEEL will not quietly substitute a welded ISO 9330-6 tube under an ISO 9329-4 purchase order. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Type of condition and surface condition follow table 7 symbols (for example HFS2 in the standard’s own order example). Unmarked preferences leave process discretion to the manufacturer within seamless rules for X6CrNiTi18-10. Heat treatment: 1020–1120 °C, water or air (rapid). Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
This paragraph is locked to X6CrNiTi18-10 duty: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service. Austenitic heats take solution annealing with rapid cool as the default HT path; skip inventing a without-HT shipment unless clause 5.3.1(b) is on the acknowledgement. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dimensions and Tolerances for ISO 9329-4 X6CrNiTi18-10
Outside diameters, wall thicknesses, and masses for X6CrNiTi18-10 shall be selected from ISO 1127 and ISO 4200. Special fields may use ISO 1129, ISO 2037, or ISO 6759. ID×wall ordering is by agreement with tolerances fixed at enquiry. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Fixed lengths and multiple cut lengths for X6CrNiTi18-10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep caution visible: Table 3 Rp0.2 min is 175 N/mm² — lower than X5CrNi18-9; do not assume 304 tensile floors on a 321-class ISO certificate. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Equivalent Grades for ISO 9329-4 X6CrNiTi18-10
Under ISO 9329-4, X6CrNiTi18-10 is the governing seamless stainless steel tube for pressure purposes designation on this page. Commercial shorthand such as 321 / UNS S32100 / EN 1.4541 (approx) helps dual-cert conversations in the body text, but the purchase order and mill test certificate still have to carry the ISO 9329-4 X6CrNiTi18-10 line. ASTM A312 / A213 related pages that share chemistry remain different product standards with their own wall bases, tensile tables, and test rules.
| System | Designation | Notes |
|---|---|---|
| ISO 9329-4 | X6CrNiTi18-10 | Governing tube grade for this page |
| Commercial / UNS (body only) | 321 / UNS S32100 / EN 1.4541 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 / A213 related | 321 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | 1.4541 | Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec |
When the service outgrows X6CrNiTi18-10, move to a sister rather than stretching the alias: ISO 9329-4 X7CrNiTi18-10, ISO 9329-4 X6CrNiNb18-11, ISO 9329-4 X5CrNi18-9, ISO 9329-4 X6CrNiMoTi17-12. Apps context: chemical and petrochemical welded interconnects, heat-exchanger tubing packages, and process lines that specify titanium stabilisation instead of low carbon alone. Full list under ISO 9329-4. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (X6CrNiTi18-10).
On X6CrNiTi18-10 packages that also list flats, open Stainless Steel Pipes and Tubes for pipes/tubes and Stainless Steel Sheets and Plates for sheets/plates, then use ASTM A240 Type 321 only when the flat form is required. Confirm X6CrNiTi18-10 OD × wall and plate thickness on separate drawings.
Heat Treatment and Delivery Condition for ISO 9329-4 X6CrNiTi18-10
ISO 9329-4 requires X6CrNiTi18-10 tubes suitably heat treated over their full length. Reference solution-treatment band: 1020–1120 °C; cooling: water or air (rapid). Delivery framing: solution-treated (Q) or hot-finished within solution band + rapid cool. Application context: chemical and petrochemical welded interconnects, heat-exchanger tubing packages, and process lines that specify titanium stabilisation instead of low carbon alone.
Field heat treatment of X6CrNiTi18-10 after hot bending must chase the same family solution practice, or the corrosion file should formally accept the as-bent condition. Caution: Table 3 Rp0.2 min is 175 N/mm² — lower than X5CrNi18-9; do not assume 304 tensile floors on a 321-class ISO certificate. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Corrosion Resistance of ISO 9329-4 X6CrNiTi18-10
Medium, temperature, crevice geometry, and weld condition decide whether X6CrNiTi18-10 is enough. Summary: titanium stabilisation for welded IGC; guideline IGC limit ~400 °C; Mo sisters when chlorides rise. Escalate via sisters X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9, X6CrNiMoTi17-12 when coupons fail. Coupon orientation and surface finish belong in the corrosion test order. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Guideline IGC limit temperatures in Table 4 are informational design aids for X6CrNiTi18-10, not a licence to ignore weld procedure control. Sisters: X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9, X6CrNiMoTi17-12. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service.
Applications of ISO 9329-4 X6CrNiTi18-10 Seamless Tube
From utility rooms to process racks, X6CrNiTi18-10 shows up wherever ISO pressure specs want austenitic Ti-stabilised 18-10 seamless behaviour. Use list: chemical and petrochemical welded interconnects, heat-exchanger tubing packages, and process lines that specify titanium stabilisation instead of low carbon alone. Spool fabricators should copy X6CrNiTi18-10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window.
Steam-generating and chemical-plant interconnects remain core ISO 9329-4 use cases for X6CrNiTi18-10. Size practice: ISO 1127 / ISO 4200 OD×wall for Ti-stabilised pressure interconnects. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service.
Weldability of ISO 9329-4 X6CrNiTi18-10
Steels for ISO 9329-4 tubes are generally regarded as weldable; behaviour still depends on procedure and final use. Shop guidance for X6CrNiTi18-10: 321/321H-class practice; verify Ti ≥5×C ≤0.80 on the cast analysis. Procedure qualification should use the same product form and wall class as production. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Ferrite control on high-Ni austenitics and heat-tint removal on process welds for X6CrNiTi18-10 are procedure items, not afterthoughts. Size practice: ISO 1127 / ISO 4200 OD×wall for Ti-stabilised pressure interconnects. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Surface Finishes for ISO 9329-4 X6CrNiTi18-10
Finish options for X6CrNiTi18-10 follow the ordered heat-treatment route under ISO 9329-4. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution-treated (Q) or hot-finished within solution band + rapid cool.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
OD stencil ink on X6CrNiTi18-10 should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows. Close bundles only after free-iron and burn marks are cleared. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for X6CrNiTi18-10.
Inspection and Testing for ISO 9329-4 X6CrNiTi18-10
Inspection and testing for X6CrNiTi18-10 follow clause 9 — non-specific or specific inspection with the corresponding ISO 10474 document. Third-party witness (SGS/TÜV-style) is available when the project mandate requires it. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dimensional inspection against the cited ISO dimensional standard closes the lot for X6CrNiTi18-10. Role: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service. Non-conforming lengths are segregated and retested or rejected rather than reworked into unmarked stock. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Packaging and Shipping for ISO 9329-4 X6CrNiTi18-10
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark X6CrNiTi18-10 stays visible on outer tags. Bundle tickets repeat grade, heat, size, and quantity. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Desiccant and wrap choices for X6CrNiTi18-10 follow voyage length and storage climate stated on the shipping order. Size practice: ISO 1127 / ISO 4200 OD×wall for Ti-stabilised pressure interconnects. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read X6CrNiTi18-10. This paragraph is locked to duty: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats X6CrNiTi18-10 as a governed ISO 9329-4 product grade, not a marketing synonym for 321 / UNS S32100 / EN 1.4541 (approx). Role: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service. SHH STEEL can produce and supply X6CrNiTi18-10 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL can supply cut lengths, bevels, and ordered optional tests for X6CrNiTi18-10 when the mill schedule allows. Sister pointers: X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9, X6CrNiMoTi17-12. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service.
Supply Capability
Capability framing for X6CrNiTi18-10: ISO 9329-4:1997 seamless austenitic pressure tube, documented heats. Caution remains: Table 3 Rp0.2 min is 175 N/mm² — lower than X5CrNi18-9; do not assume 304 tensile floors on a 321-class ISO certificate. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for X6CrNiTi18-10 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes |
| Grade | X6CrNiTi18-10 (Table 1; alias 321 / UNS S32100 / EN 1.4541 (approx)) |
| Product form | Seamless tube only — hot and/or cold finished before heat treatment |
| Delivery condition | solution-treated (Q) or hot-finished within solution band + rapid cool |
| Documents | ISO 10474 / EN 10204 3.1 style as ordered |
| Typical size practice | OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759 |
| Condition symbols | Table 7 (e.g. HFS2) as ordered |
| Tests | Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of X6CrNiTi18-10 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service. SHH STEEL can supply alternate walls once design pressure and corrosion allowance are clear.
Repeat orders for X6CrNiTi18-10 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. SHH STEEL can produce trial lengths of X6CrNiTi18-10 for procedure qualification before the bulk release when needed. Keep ISO 9329-4 and X6CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
FAQ
-
What is ISO 9329-4 X6CrNiTi18-10 seamless stainless steel tube used for?
- ISO 9329-4 X6CrNiTi18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — chemical and petrochemical welded interconnects, heat-exchanger tubing packages, and process lines that specify titanium stabilisation instead of low carbon alone. Role summary: Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
-
Is ISO 9329-4 X6CrNiTi18-10 seamless only, or does it cover welded tube?
- Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X6CrNiTi18-10 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
-
What heat treatment does X6CrNiTi18-10 require under ISO 9329-4?
- Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X6CrNiTi18-10: 1020–1120 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
-
How does X6CrNiTi18-10 compare with sister grades X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9?
- X6CrNiTi18-10 is filed as austenitic Ti-stabilised 18-10. Typical sisters on the same RFQ are X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9. Design caution: Table 3 Rp0.2 min is 175 N/mm² — lower than X5CrNi18-9; do not assume 304 tensile floors on a 321-class ISO certificate Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
-
What tests appear on the mill certificate for X6CrNiTi18-10?
- Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
-
Is 321 / UNS S32100 / EN 1.4541 (approx) the same as ordering X6CrNiTi18-10?
- No. 321 / UNS S32100 / EN 1.4541 (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X6CrNiTi18-10 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for ISO 9329-4 X6CrNiTi18-10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X6CrNiTi18-10 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: ISO 1127 / ISO 4200 OD×wall for Ti-stabilised pressure interconnects. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should X6CrNiTi18-10 be welded on site?
- Shop guidance: 321/321H-class practice; verify Ti ≥5×C ≤0.80 on the cast analysis. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: Table 3 Rp0.2 min is 175 N/mm² — lower than X5CrNi18-9; do not assume 304 tensile floors on a 321-class ISO certificate
-
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X6CrNiTi18-10?
- Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic Ti-stabilised 18-10 practice can defend for the temperature and stress state. Caution for this mark: Table 3 Rp0.2 min is 175 N/mm² — lower than X5CrNi18-9; do not assume 304 tensile floors on a 321-class ISO certificate Sister pointers: X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify ISO 9329-4 X6CrNiTi18-10 with ASTM A312 or EN 10216-5?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X6CrNiTi18-10 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What is the difference between hyphenated X6CrNiTi18-10 and the spaced ISO designation?
- They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X6CrNiTi18-10 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.
Conclusion
ISO 9329-4 X6CrNiTi18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — Ti-stabilised 18-10 austenitic pressure tube — ISO 321-class mark for welded corrosion service. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X7CrNiTi18-10, X6CrNiNb18-11, X5CrNi18-9. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.