ISO 9329-4 X6CrNiNb18-11 Seamless Stainless Steel Tube

ISO 9329-4 X6CrNiNb18-11 seamless stainless steel tube (347 / UNS S34700 / EN 1.4550 (approx)), austenitic Nb-stabilised 18-11, Table 1 heat analysis, Rp0.2 min 205 N/mm² / Rm 510–740 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.
Grade
X6CrNiNb18-11 (ISO 9329-4 Table 1 / 347 / UNS S34700 / EN 1.4550 (approx) — body alias)
Standard
ISO 9329-4:1997
Product form
Seamless stainless steel tube (hot and/or cold finished), delivery solution-treated (Q) or hot-finished within solution band + rapid cool
Size
OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759; ID×wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ISO 9329-4 X6CrNiNb18-11 Seamless Stainless Steel Tube

Pressure packages that cite ISO 9329-4 expect seamless austenitic tube with Table 1 chemistry and Table 3 tensile floors, not an automatic ASTM A312 or EN 10216-5 certificate. X6CrNiNb18-11 is the hyphenated steel name matching ISO’s spaced designation for this austenitic Nb-stabilised 18-11 chemistry. Order example in ISO 9329-4 itself uses X 6 CrNiNb 18 11 — this is the Nb-stabilised workhorse when the PO wants 347-class seamless pressure tube under ISO text.

Mill path for X6CrNiNb18-11: seamless hot and/or cold finish, Table 3 solution treatment, Table 1 heat analysis, Table 3 Rm/Rp/A pair, optional elevated proof stress, impact, hydro, NDT, and IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: chemical plant welded spools, heat-exchanger connecting tube, and process lines where 347-class stabilisation is written into the corrosion specification.

On the floor people say “347 tube”; in QA they must not stop there. X6CrNiNb18-11 under ISO 9329-4 carries specific Table 1 and Table 3 limits that a loose alias will not enforce. Design caution: Nb must meet ≥10×%C and ≤1.00 on the cast — a bare “347” alias will not enforce the ISO Nb formula.

Use thread: chemical plant welded spools, heat-exchanger connecting tube, and process lines where 347-class stabilisation is written into the corrosion specification. Size and test clarity on the RFQ lets SHH STEEL lock the correct seamless pressure-tube scope for X6CrNiNb18-11 before production starts. Size practice for X6CrNiNb18-11 remains ISO 1127 OD×wall typical of stabilised austenitic pressure interconnects.

Inside this ISO 9329-4 series, compare ISO 9329-4 X7CrNiNb18-11, ISO 9329-4 X6CrNiTi18-10, ISO 9329-4 X5CrNi18-9, ISO 9329-4 X6CrNiMoNb17-12. Hub: ISO 9329-4. Related pressure-tube page (not interchangeable by default): EN 10216-5 1.4550. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP347.

X6CrNiNb18-11 sourcing notes should keep forms separate: tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is ASTM A240 Type 347. Confirm X6CrNiNb18-11 OD × wall and plate thickness on separate drawings.

Chemical Composition of ISO 9329-4 X6CrNiNb18-11

Table 1 cast windows for X6CrNiNb18-11 lock C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Cr 17.00–19.00, Ni 9.00–13.00, Nb ≥10×%C ≤1.00. Product analysis, when ordered, uses Table 2 permissible deviations — not a free rewrite of the grade. Role: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

ISO 9329-4 does not publish a separate “welding grade” sulphur tighten inside Table 1; if the order needs S ≤0.015 or similar for fabrication, write it as a purchaser agreement on X6CrNiNb18-11. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Grade C Si Mn P S Cr Ni Nb
X6CrNiNb18-11 ≤0.08 ≤1.00 ≤2.00 ≤0.040 ≤0.030 17.00–19.00 9.00–13.00 ≥10×%C ≤1.00

Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.

Mechanical Properties of ISO 9329-4 X6CrNiNb18-11

Room-temperature mechanical properties for X6CrNiNb18-11 are measured at 23±5 °C and must meet Table 3. Summary: Rp0.2 min 205 N/mm², Rp1.0 min 240 N/mm², Rm 510–740 N/mm², A long. min 40% / A trans. min 35%. Duty: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

Flattening and expansion technological tests follow Table 3 coefficients when required by the test category for X6CrNiNb18-11. Wall >50 mm mechanical values are by agreement — do not assume thin-wall floors. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Grade Rp0.2 min (N/mm²) Rp1.0 min (N/mm²) Rm (N/mm²) A long. min (%) A trans. min (%) KV long. min (J) Solution treatment
X6CrNiNb18-11 205 240 510–740 40 35 85 1020–1120 °C

Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X6CrNiNb18-11 (solution-treated; wall ≤50 mm unless noted). Nb includes Ta determined as Nb; wall ≤50 mm. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: Yes — guideline limit ~400 °C / 100000 h.

Seamless Tube Manufacture of ISO 9329-4 X6CrNiNb18-11

SHH STEEL can produce X6CrNiNb18-11 as seamless pressure tube to ISO 9329-4:1997, apply solution treatment over the full length, descale or bright-finish per the ordered surface condition, and cut to ISO 1127 lengths. Plain or bevelled ends follow the enquiry. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Solution treatment shall heat X6CrNiNb18-11 tubes uniformly into the Table 3 band and cool rapidly. Hot-finished tubes pressed or extruded inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Cold finishing after hot work for X6CrNiNb18-11 still ends in full-length heat treatment per 5.3 unless the hot-finish-in-band exception applies. Surface descaling follows the ordered condition symbol. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Dimensions and Tolerances for ISO 9329-4 X6CrNiNb18-11

Out-of-table OD×wall combinations for X6CrNiNb18-11 are by agreement — still under the same steel grade symbol. Duty: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties. Cap/practice: ISO 1127 OD×wall typical of stabilised austenitic pressure interconnects. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Mass calculation for X6CrNiNb18-11 follows the dimensional standard; do not invent a density override without a written agreement. Random vs exact length must appear on the PO. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Equivalent Grades for ISO 9329-4 X6CrNiNb18-11

X6CrNiNb18-11 is the ISO 9329-4 designation for this seamless stainless steel tube for pressure purposes. Alias 347 / UNS S34700 / EN 1.4550 (approx) appears only as a cross-walk. When a dual-cert path is required, list both ISO 9329-4 X6CrNiNb18-11 and the foreign mark with separate scopes instead of assuming one chemistry line clears both files.

System Designation Notes
ISO 9329-4 X6CrNiNb18-11 Governing tube grade for this page
Commercial / UNS (body only) 347 / UNS S34700 / EN 1.4550 (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 / A213 related 347 chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other 1.4550 Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec

When the service outgrows X6CrNiNb18-11, move to a sister rather than stretching the alias: ISO 9329-4 X7CrNiNb18-11, ISO 9329-4 X6CrNiTi18-10, ISO 9329-4 X5CrNi18-9, ISO 9329-4 X6CrNiMoNb17-12. Apps context: chemical plant welded spools, heat-exchanger connecting tube, and process lines where 347-class stabilisation is written into the corrosion specification. Full list under ISO 9329-4. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (X6CrNiNb18-11).

Heat Treatment and Delivery Condition for ISO 9329-4 X6CrNiNb18-11

Recorded furnace charts for X6CrNiNb18-11 should support the heat-treatment claim on the certificate, including quench or cool method where rapid cooling is required. Band note: 1020–1120 °C. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

IGC applicability for X6CrNiNb18-11: Yes — guideline limit ~400 °C / 100000 h. Elevated-temperature grades marked N/A for IGC in Table 3 are not “exempt from corrosion engineering” — they are oriented to hot service acceptance paths. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Corrosion Resistance of ISO 9329-4 X6CrNiNb18-11

ISO 9329-4 corrosion text focuses on intergranular corrosion (ISO 3651-1 / 3651-2) for X6CrNiNb18-11. Other corrosion modes are outside the standard’s normative scope and must be engineered separately. Framing: niobium ties carbon for welded IGC resistance; guideline IGC limit temperature ~400 °C per Table 4 family data. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Specific corrosion tests beyond IGC for X6CrNiNb18-11 shall be agreed at enquiry with method and acceptance criteria written down — the standard will not invent them. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

Applications of ISO 9329-4 X6CrNiNb18-11 Seamless Tube

Typical duties for X6CrNiNb18-11: chemical plant welded spools, heat-exchanger connecting tube, and process lines where 347-class stabilisation is written into the corrosion specification. Role: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties. Keep the as-built dossier repeating X6CrNiNb18-11 beside heat numbers. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Cryogenic or elevated-temperature options for X6CrNiNb18-11 need explicit impact or Table 4 proof-stress orders — ambient Table 3 alone does not prove those duties. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

Weldability of ISO 9329-4 X6CrNiNb18-11

Automatic mill welding is outside seamless ISO 9329-4; manual and automatic field welds must still respect X6CrNiNb18-11 chemistry. Guidance: 347/347L-class practice; verify Nb ≥10×C on the MTC before releasing as-welded corrosive duty. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Post-weld solution treatment of X6CrNiNb18-11 should chase 1020–1120 °C when the corrosion file demands restored IGC resistance after heavy fabrication. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

Surface Finishes for ISO 9329-4 X6CrNiNb18-11

Welded or heavily formed X6CrNiNb18-11 may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to ISO 9329-4 seamless stainless steel tube for pressure purposes. Caution: Nb must meet ≥10×%C and ≤1. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for X6CrNiNb18-11.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

OD stencil ink on X6CrNiNb18-11 should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows: Nb must meet ≥10×%C and ≤1. Close bundles only after free-iron and burn marks are cleared. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for X6CrNiNb18-11.

Inspection and Testing for ISO 9329-4 X6CrNiNb18-11

Sampling plans for X6CrNiNb18-11 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Caution: Nb must meet ≥10×%C and ≤1.00 on the cast — a bare “347” alias will not enforce the ISO Nb formula. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Weld-shop note tied to X6CrNiNb18-11: 347/347L-class practice; verify Nb ≥10×C on the MTC before releasing as-welded corrosive duty. Mill tests do not replace fabricator WPS qualification. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Packaging and Shipping for ISO 9329-4 X6CrNiNb18-11

Container loading plans should keep heavy walls from crushing thin-wall X6CrNiNb18-11 layers. Corrosion framing: niobium ties carbon for welded IGC resistance; guideline IGC limit temperature ~400 °C per Table 4 family data. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Mixed-grade bundles are forbidden when X6CrNiNb18-11 shares a crate with a different Table 1 steel — heat identity must remain auditable at receipt. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

Claims handling for X6CrNiNb18-11 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

Why Choose SHH STEEL

SHH STEEL can make X6CrNiNb18-11 to the written scope: Table 1 chemistry, Table 3 tensile, ordered condition symbol, and test category. Use: chemical plant welded spools, heat-exchanger connecting tube, and process lines where 347-class stabilisation is written into the corrosion specification. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Dual-cert discussions for X6CrNiNb18-11 start with a chemistry and test matrix — not with a promise that “304/316 equivalent” clears ASTM by default. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

Supply Capability

SHH STEEL can produce ISO 9329-4 X6CrNiNb18-11 in enquiry-oriented OD × wall bands under ISO 1127 / ISO 4200 practice. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Duty: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Item Capability
Standard ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes
Grade X6CrNiNb18-11 (Table 1; alias 347 / UNS S34700 / EN 1.4550 (approx))
Product form Seamless tube only — hot and/or cold finished before heat treatment
Delivery condition solution-treated (Q) or hot-finished within solution band + rapid cool
Documents ISO 10474 / EN 10204 3.1 style as ordered
Typical size practice OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759
Condition symbols Table 7 (e.g. HFS2) as ordered
Tests Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered

Stock / Available sizes

Stock / Available sizes for X6CrNiNb18-11: enquire OD × wall × length × condition symbol. Size practice: ISO 1127 OD×wall typical of stabilised austenitic pressure interconnects. SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Export packing, third-party inspection, and dual-language MTCs for X6CrNiNb18-11 are available when stated on the order. Sisters often quoted alongside: X7CrNiNb18-11, X6CrNiTi18-10, X5CrNi18-9, X6CrNiMoNb17-12. Keep ISO 9329-4 and X6CrNiNb18-11 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties.

FAQ

What is ISO 9329-4 X6CrNiNb18-11 seamless stainless steel tube used for?
ISO 9329-4 X6CrNiNb18-11 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — chemical plant welded spools, heat-exchanger connecting tube, and process lines where 347-class stabilisation is written into the corrosion specification. Role summary: Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
Is ISO 9329-4 X6CrNiNb18-11 seamless only, or does it cover welded tube?
Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X6CrNiNb18-11 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
What heat treatment does X6CrNiNb18-11 require under ISO 9329-4?
Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X6CrNiNb18-11: 1020–1120 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
How does X6CrNiNb18-11 compare with sister grades X7CrNiNb18-11, X6CrNiTi18-10, X5CrNi18-9?
X6CrNiNb18-11 is filed as austenitic Nb-stabilised 18-11. Typical sisters on the same RFQ are X7CrNiNb18-11, X6CrNiTi18-10, X5CrNi18-9. Design caution: Nb must meet ≥10×%C and ≤1.00 on the cast — a bare “347” alias will not enforce the ISO Nb formula Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
What tests appear on the mill certificate for X6CrNiNb18-11?
Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
Is 347 / UNS S34700 / EN 1.4550 (approx) the same as ordering X6CrNiNb18-11?
No. 347 / UNS S34700 / EN 1.4550 (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X6CrNiNb18-11 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for ISO 9329-4 X6CrNiNb18-11?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X6CrNiNb18-11 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: ISO 1127 OD×wall typical of stabilised austenitic pressure interconnects. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should X6CrNiNb18-11 be welded on site?
Shop guidance: 347/347L-class practice; verify Nb ≥10×C on the MTC before releasing as-welded corrosive duty. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: Nb must meet ≥10×%C and ≤1.00 on the cast — a bare “347” alias will not enforce the ISO Nb formula
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X6CrNiNb18-11?
Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic Nb-stabilised 18-11 practice can defend for the temperature and stress state. Caution for this mark: Nb must meet ≥10×%C and ≤1.00 on the cast — a bare “347” alias will not enforce the ISO Nb formula Sister pointers: X7CrNiNb18-11, X6CrNiTi18-10, X5CrNi18-9. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify ISO 9329-4 X6CrNiNb18-11 with ASTM A312 or EN 10216-5?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X6CrNiNb18-11 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
What is the difference between hyphenated X6CrNiNb18-11 and the spaced ISO designation?
They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X6CrNiNb18-11 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.

Conclusion

ISO 9329-4 X6CrNiNb18-11 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — Nb-stabilised 18-11 austenitic pressure tube for welded IGC resistance without mandatory post-weld anneal in many duties. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X7CrNiNb18-11, X6CrNiTi18-10, X5CrNi18-9. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X