ISO 9329-4 X2CrNi18-10 Seamless Stainless Steel Tube
What is ISO 9329-4 X2CrNi18-10 Seamless Stainless Steel Tube
ISO 9329-4:1997 is the International Standard for seamless circular austenitic stainless steel tubes for pressure and corrosion-resisting purposes at room, low, or elevated temperature — pressure vessels, chemical plant, steam-generating equipment, and interconnecting pipework. Grade X2CrNi18-10 sits in Table 1 as austenitic low-carbon 18-10. When the inquiry says “ISO 304L seamless tube for pressure” without a European number, X2CrNi18-10 is the ISO 9329-4 designation that locks C ≤0.030 and the Table 3 tensile pair.
SHH STEEL can produce and supply ISO 9329-4 X2CrNi18-10 as seamless stainless steel tube across the enquiry OD×wall band (ISO 1127 / ISO 4200 practice), solution-treated over the full length, descaled or bright-finished per ordered condition, and documented on inspection documents (ISO 10474 / EN 10204 style as specified). Duty focus: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation.
Commercial aliases such as 304L / UNS S30403 / EN 1.4306 (approx) help buyers navigate catalogues, but the governing symbols on the order and MTC remain ISO 9329-4 and X2CrNi18-10. Caution for this mark: Ni band 9.00–12.00 is wider/higher than some EN 1.4307 windows — do not treat a loose “304L” note as automatic dual-cert without checking cast Ni and C. Keep isometric notes and the mill acknowledgement aligned on the hyphenated grade so informal alias language cannot reopen the carbon, molybdenum, nitrogen, or stabiliser window after melt.
Inside this ISO 9329-4 series, compare sisters X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10, X2CrNiMo17-12 before freezing wall thickness alone. Size practice for X2CrNi18-10 remains ISO 1127 / ISO 4200 OD×wall workhorse band for pressure interconnects. SHH STEEL can produce trial lengths for procedure qualification when the project calendar needs them. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Inside this ISO 9329-4 series, compare ISO 9329-4 X5CrNi18-9, ISO 9329-4 X2CrNiN18-10, ISO 9329-4 X6CrNiTi18-10, ISO 9329-4 X2CrNiMo17-12. Hub: ISO 9329-4. Related pressure-tube page (not interchangeable by default): EN 10216-5 1.4306. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP304L.
When X2CrNi18-10 pipe sits beside plate on the same BOM, link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and ASTM A240 Type 304L so purchasing does not treat one product form as the other. Quote X2CrNi18-10 pipe and plate under separate line items.
Chemical Composition of ISO 9329-4 X2CrNi18-10
For X2CrNi18-10, the heat analysis has to show ISO 9329-4 Table 1 compliance — C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Cr 17.00–19.00, Ni 9.00–12.00. Elements not listed shall not be intentionally added without purchaser agreement except for finishing the heat. Corrosion framing: low carbon for as-welded IGC resistance; escalate to Mo grades when chlorides or reducing acids dominate.
Niobium content, where specified, includes tantalum determined as niobium. Titanium and niobium formulae are minimum multipliers of carbon with absolute caps — verify both sides on the cast ticket for X2CrNi18-10. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | C | Si | Mn | P | S | Cr | Ni |
|---|---|---|---|---|---|---|---|
| X2CrNi18-10 | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 17.00–19.00 | 9.00–12.00 |
Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.
Mechanical Properties of ISO 9329-4 X2CrNi18-10
Do not paste EN 10216-5 or ASTM A312 tensile numbers onto an ISO 9329-4 X2CrNi18-10 certificate. Under Table 3 (solution-treated, wall ≤50 mm unless noted) expect Rp0.2 min 180 N/mm², Rp1.0 min 215 N/mm², Rm 480–680 N/mm², A long. min 40% / A trans. min 35%. Note: Wall ≤50 mm Table 3 values; thicker by agreement.
Impact KV minima in Table 3 (long. 85 J / trans. 55 J where applicable) apply when impact testing is in the ordered scope for X2CrNi18-10. Low-temperature impact values are by agreement (Annex B informational). Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | Rp0.2 min (N/mm²) | Rp1.0 min (N/mm²) | Rm (N/mm²) | A long. min (%) | A trans. min (%) | KV long. min (J) | Solution treatment |
|---|---|---|---|---|---|---|---|
| X2CrNi18-10 | 180 | 215 | 480–680 | 40 | 35 | 85 | 1000–1100 °C |
Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X2CrNi18-10 (solution-treated; wall ≤50 mm unless noted). Wall ≤50 mm Table 3 values; thicker by agreement. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: Yes (ISO 3651-2) — guideline limit ~350 °C / 100000 h.
Seamless Tube Manufacture of ISO 9329-4 X2CrNi18-10
ISO 9329-4:1997 manufactures X2CrNi18-10 as seamless tube only — hot finished, cold finished, or a combination — never as an ERW product under this part. SHH STEEL confirms the seamless route and the ordered type of condition (table 7 symbols such as HFS2) on the acknowledgement before finishing starts. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Type of condition and surface condition follow table 7 symbols (for example HFS2 in the standard’s own order example). Unmarked preferences leave process discretion to the manufacturer within seamless rules for X2CrNi18-10. Heat treatment: 1000–1100 °C, water or air (rapid). Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
This paragraph is locked to X2CrNi18-10 duty: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation. Austenitic heats take solution annealing with rapid cool as the default HT path; skip inventing a without-HT shipment unless clause 5.3.1(b) is on the acknowledgement. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dimensions and Tolerances for ISO 9329-4 X2CrNi18-10
Outside diameters, wall thicknesses, and masses for X2CrNi18-10 shall be selected from ISO 1127 and ISO 4200. Special fields may use ISO 1129, ISO 2037, or ISO 6759. ID×wall ordering is by agreement with tolerances fixed at enquiry. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Fixed lengths and multiple cut lengths for X2CrNi18-10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Keep caution visible: Ni band 9.00–12.00 is wider/higher than some EN 1.4307 windows — do not treat a loose “304L” note as automatic dual-cert without checking cast Ni and C.
Equivalent Grades for ISO 9329-4 X2CrNi18-10
Cross-references help sourcing X2CrNi18-10, but they do not replace the ISO 9329-4 grade line on the enquiry. Family framing here is austenitic low-carbon 18-10; delivery practice from the crib is “solution-treated (Q) or hot-finished within solution band + rapid cool”. Related ASTM or EN numbers are starting points for engineering comparison, not automatic substitutes.
| System | Designation | Notes |
|---|---|---|
| ISO 9329-4 | X2CrNi18-10 | Governing tube grade for this page |
| Commercial / UNS (body only) | 304L / UNS S30403 / EN 1.4306 (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 / A213 related | 304L chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | 1.4306 | Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec |
Inside this series compare ISO 9329-4 X5CrNi18-9, ISO 9329-4 X2CrNiN18-10, ISO 9329-4 X6CrNiTi18-10, ISO 9329-4 X2CrNiMo17-12 before swapping marks for medium or temperature. Confirm chemistry windows on the X2CrNi18-10 MTC before dual-cert claims. Hub: ISO 9329-4. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (X2CrNi18-10).
Heat Treatment and Delivery Condition for ISO 9329-4 X2CrNi18-10
ISO 9329-4 requires X2CrNi18-10 tubes suitably heat treated over their full length. Reference solution-treatment band: 1000–1100 °C; cooling: water or air (rapid). Delivery framing: solution-treated (Q) or hot-finished within solution band + rapid cool. Application context: pressure vessels, chemical plant interconnects, food-adjacent and pharmaceutical utility lines, and cryogenic or ambient process tubing where 304L-class chemistry is specified under ISO product text.
Field heat treatment of X2CrNi18-10 after hot bending must chase the same family solution practice, or the corrosion file should formally accept the as-bent condition. Caution: Ni band 9.00–12.00 is wider/higher than some EN 1.4307 windows — do not treat a loose “304L” note as automatic dual-cert without checking cast Ni and C.
Corrosion Resistance of ISO 9329-4 X2CrNi18-10
Medium, temperature, crevice geometry, and weld condition decide whether X2CrNi18-10 is enough. Summary: low carbon for as-welded IGC resistance; escalate to Mo grades when chlorides or reducing acids dominate. Escalate via sisters X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10, X2CrNiMo17-12 when coupons fail. Coupon orientation and surface finish belong in the corrosion test order. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Guideline IGC limit temperatures in Table 4 are informational design aids for X2CrNi18-10, not a licence to ignore weld procedure control. Sisters: X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10, X2CrNiMo17-12. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation.
Applications of ISO 9329-4 X2CrNi18-10 Seamless Tube
From utility rooms to process racks, X2CrNi18-10 shows up wherever ISO pressure specs want austenitic low-carbon 18-10 seamless behaviour. Use list: pressure vessels, chemical plant interconnects, food-adjacent and pharmaceutical utility lines, and cryogenic or ambient process tubing where 304L-class chemistry is specified under ISO product text. Spool fabricators should copy X2CrNi18-10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window.
Steam-generating and chemical-plant interconnects remain core ISO 9329-4 use cases for X2CrNi18-10. Size practice: ISO 1127 / ISO 4200 OD×wall workhorse band for pressure interconnects. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation.
Weldability of ISO 9329-4 X2CrNi18-10
Steels for ISO 9329-4 tubes are generally regarded as weldable; behaviour still depends on procedure and final use. Shop guidance for X2CrNi18-10: 308L/308LSi-class practice; keep heat input moderate and purge OD/ID on sanitary or corrosion-critical joints. Procedure qualification should use the same product form and wall class as production. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Ferrite control on high-Ni austenitics and heat-tint removal on process welds for X2CrNi18-10 are procedure items, not afterthoughts. Size practice: ISO 1127 / ISO 4200 OD×wall workhorse band for pressure interconnects. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Surface Finishes for ISO 9329-4 X2CrNi18-10
Finish options for X2CrNi18-10 follow the ordered heat-treatment route under ISO 9329-4. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution-treated (Q) or hot-finished within solution band + rapid cool.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
SHH STEEL sequences pickle, optional passivation, and any agreed polish for X2CrNi18-10 after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long tube life in the field. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (X2CrNi18-10).
Inspection and Testing for ISO 9329-4 X2CrNi18-10
Inspection and testing for X2CrNi18-10 follow clause 9 — non-specific or specific inspection with the corresponding ISO 10474 document. Third-party witness (SGS/TÜV-style) is available when the project mandate requires it. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dimensional inspection against the cited ISO dimensional standard closes the lot for X2CrNi18-10. Role: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation. Non-conforming lengths are segregated and retested or rejected rather than reworked into unmarked stock. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Packaging and Shipping for ISO 9329-4 X2CrNi18-10
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark X2CrNi18-10 stays visible on outer tags. Bundle tickets repeat grade, heat, size, and quantity. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Desiccant and wrap choices for X2CrNi18-10 follow voyage length and storage climate stated on the shipping order. Size practice: ISO 1127 / ISO 4200 OD×wall workhorse band for pressure interconnects. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read X2CrNi18-10. This paragraph is locked to duty: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats X2CrNi18-10 as a governed ISO 9329-4 product grade, not a marketing synonym for 304L / UNS S30403 / EN 1.4306 (approx). Role: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation. SHH STEEL can produce and supply X2CrNi18-10 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
SHH STEEL can supply cut lengths, bevels, and ordered optional tests for X2CrNi18-10 when the mill schedule allows. Sister pointers: X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10, X2CrNiMo17-12. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation.
Supply Capability
Capability framing for X2CrNi18-10: ISO 9329-4:1997 seamless austenitic pressure tube, documented heats. Caution remains: Ni band 9.00–12.00 is wider/higher than some EN 1.4307 windows — do not treat a loose “304L” note as automatic dual-cert without checking cast Ni and C. SHH STEEL can produce and supply cut lengths, bevels, and ordered optional tests for X2CrNi18-10 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes |
| Grade | X2CrNi18-10 (Table 1; alias 304L / UNS S30403 / EN 1.4306 (approx)) |
| Product form | Seamless tube only — hot and/or cold finished before heat treatment |
| Delivery condition | solution-treated (Q) or hot-finished within solution band + rapid cool |
| Documents | ISO 10474 / EN 10204 3.1 style as ordered |
| Typical size practice | OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759 |
| Condition symbols | Table 7 (e.g. HFS2) as ordered |
| Tests | Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of X2CrNi18-10 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation. SHH STEEL can supply alternate walls once design pressure and corrosion allowance are clear.
Repeat orders for X2CrNi18-10 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. SHH STEEL can produce trial lengths of X2CrNi18-10 for procedure qualification before the bulk release when needed. Keep ISO 9329-4 and X2CrNi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
FAQ
-
What is ISO 9329-4 X2CrNi18-10 seamless stainless steel tube used for?
- ISO 9329-4 X2CrNi18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — pressure vessels, chemical plant interconnects, food-adjacent and pharmaceutical utility lines, and cryogenic or ambient process tubing where 304L-class chemistry is specified under ISO product text. Role summary: low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
-
Is ISO 9329-4 X2CrNi18-10 seamless only, or does it cover welded tube?
- Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X2CrNi18-10 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
-
What heat treatment does X2CrNi18-10 require under ISO 9329-4?
- Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X2CrNi18-10: 1000–1100 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
-
How does X2CrNi18-10 compare with sister grades X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10?
- X2CrNi18-10 is filed as austenitic low-carbon 18-10. Typical sisters on the same RFQ are X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10. Design caution: Ni band 9.00–12.00 is wider/higher than some EN 1.4307 windows — do not treat a loose “304L” note as automatic dual-cert without checking cast Ni and C Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
-
What tests appear on the mill certificate for X2CrNi18-10?
- Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
-
Is 304L / UNS S30403 / EN 1.4306 (approx) the same as ordering X2CrNi18-10?
- No. 304L / UNS S30403 / EN 1.4306 (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X2CrNi18-10 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for ISO 9329-4 X2CrNi18-10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X2CrNi18-10 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: ISO 1127 / ISO 4200 OD×wall workhorse band for pressure interconnects. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should X2CrNi18-10 be welded on site?
- Shop guidance: 308L/308LSi-class practice; keep heat input moderate and purge OD/ID on sanitary or corrosion-critical joints. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: Ni band 9.00–12.00 is wider/higher than some EN 1.4307 windows — do not treat a loose “304L” note as automatic dual-cert without checking cast Ni and C
-
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X2CrNi18-10?
- Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic low-carbon 18-10 practice can defend for the temperature and stress state. Caution for this mark: Ni band 9.00–12.00 is wider/higher than some EN 1.4307 windows — do not treat a loose “304L” note as automatic dual-cert without checking cast Ni and C Sister pointers: X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify ISO 9329-4 X2CrNi18-10 with ASTM A312 or EN 10216-5?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X2CrNi18-10 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What is the difference between hyphenated X2CrNi18-10 and the spaced ISO designation?
- They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X2CrNi18-10 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.
Conclusion
ISO 9329-4 X2CrNi18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — low-carbon 18-10 austenitic pressure tube — ISO 9329-4 workhorse for as-welded corrosion duty without stabilisation. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X5CrNi18-9, X2CrNiN18-10, X6CrNiTi18-10. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.