ISO 9329-4 X2CrNiMo17-13 Seamless Stainless Steel Tube

ISO 9329-4 X2CrNiMo17-13 seamless stainless steel tube (316L higher-Mo / EN 1.4435 (approx)), austenitic low-carbon higher-Mo 17-13-3, Table 1 heat analysis, Rp0.2 min 190 N/mm² / Rm 490–690 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.
Grade
X2CrNiMo17-13 (ISO 9329-4 Table 1 / 316L higher-Mo / EN 1.4435 (approx) — body alias)
Standard
ISO 9329-4:1997
Product form
Seamless stainless steel tube (hot and/or cold finished), delivery solution-treated (Q) or hot-finished within solution band + rapid cool
Size
OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759; ID×wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ISO 9329-4 X2CrNiMo17-13 Seamless Stainless Steel Tube

Pressure packages that cite ISO 9329-4 expect seamless austenitic tube with Table 1 chemistry and Table 3 tensile floors, not an automatic ASTM A312 or EN 10216-5 certificate. X2CrNiMo17-13 is the hyphenated steel name matching ISO’s spaced designation for this austenitic low-carbon higher-Mo 17-13-3 chemistry. Pick X2CrNiMo17-13 when the ISO PO explicitly wants the 2.5–3.0 Mo low-carbon window, not the 2.0–2.5 band of X2CrNiMo17-12.

Mill path for X2CrNiMo17-13: seamless hot and/or cold finish, Table 3 solution treatment, Table 1 heat analysis, Table 3 Rm/Rp/A pair, optional elevated proof stress, impact, hydro, NDT, and IGC when ordered. SHH STEEL can make and supply the grade to that stack. Typical use: chemical process tubing with elevated chloride risk, heat-exchanger interconnects, and pressure lines where EN 1.4435-class Mo is preferred over standard 2% Mo.

On the floor people say “316L higher-Mo tube”; in QA they must not stop there. X2CrNiMo17-13 under ISO 9329-4 carries specific Table 1 and Table 3 limits that a loose alias will not enforce. Design caution: Mo 2.50–3.00 and Ni 11.50–14.50 — do not dual-cert as plain 316L without checking both windows.

Use thread: chemical process tubing with elevated chloride risk, heat-exchanger interconnects, and pressure lines where EN 1.4435-class Mo is preferred over standard 2% Mo. Size and test clarity on the RFQ lets SHH STEEL lock the correct seamless pressure-tube scope for X2CrNiMo17-13 before production starts. Size practice for X2CrNiMo17-13 remains ISO 1127 OD×wall for higher-Mo low-carbon pressure tube.

Inside this ISO 9329-4 series, compare ISO 9329-4 X2CrNiMo17-12, ISO 9329-4 X5CrNiMo17-13, ISO 9329-4 X2CrNiMoN17-13, ISO 9329-4 X6CrNiMoTi17-12. Hub: ISO 9329-4. Related pressure-tube page (not interchangeable by default): EN 10216-5 1.4435. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP316L.

Chemical Composition of ISO 9329-4 X2CrNiMo17-13

Table 1 cast windows for X2CrNiMo17-13 lock C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.040, S ≤0.030, Cr 16.50–18.50, Mo 2.50–3.00, Ni 11.50–14.50. Product analysis, when ordered, uses Table 2 permissible deviations — not a free rewrite of the grade. Role: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

ISO 9329-4 does not publish a separate “welding grade” sulphur tighten inside Table 1; if the order needs S ≤0.015 or similar for fabrication, write it as a purchaser agreement on X2CrNiMo17-13. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Grade C Si Mn P S Cr Mo Ni
X2CrNiMo17-13 ≤0.030 ≤1.00 ≤2.00 ≤0.040 ≤0.030 16.50–18.50 2.50–3.00 11.50–14.50

Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.

Mechanical Properties of ISO 9329-4 X2CrNiMo17-13

Room-temperature mechanical properties for X2CrNiMo17-13 are measured at 23±5 °C and must meet Table 3. Summary: Rp0.2 min 190 N/mm², Rp1.0 min 225 N/mm², Rm 490–690 N/mm², A long. min 40% / A trans. min 35%. Duty: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

Flattening and expansion technological tests follow Table 3 coefficients when required by the test category for X2CrNiMo17-13. Wall >50 mm mechanical values are by agreement — do not assume thin-wall floors. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Grade Rp0.2 min (N/mm²) Rp1.0 min (N/mm²) Rm (N/mm²) A long. min (%) A trans. min (%) KV long. min (J) Solution treatment
X2CrNiMo17-13 190 225 490–690 40 35 85 1020–1120 °C

Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X2CrNiMo17-13 (solution-treated; wall ≤50 mm unless noted). Wall ≤50 mm Table 3 values. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: Yes — guideline limit ~400 °C / 100000 h.

Seamless Tube Manufacture of ISO 9329-4 X2CrNiMo17-13

ISO 9329-4:1997 manufactures X2CrNiMo17-13 as seamless tube only — hot finished, cold finished, or a combination — never as an ERW product under this part. SHH STEEL confirms the seamless route and the ordered type of condition (table 7 symbols such as HFS2) on the acknowledgement before finishing starts. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Solution treatment shall heat X2CrNiMo17-13 tubes uniformly into the Table 3 band and cool rapidly. Hot-finished tubes pressed or extruded inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Cold finishing after hot work for X2CrNiMo17-13 still ends in full-length heat treatment per 5.3 unless the hot-finish-in-band exception applies. Surface descaling follows the ordered condition symbol. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Dimensions and Tolerances for ISO 9329-4 X2CrNiMo17-13

Out-of-table OD×wall combinations for X2CrNiMo17-13 are by agreement — still under the same steel grade symbol. Duty: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file. Cap/practice: ISO 1127 OD×wall for higher-Mo low-carbon pressure tube. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Mass calculation for X2CrNiMo17-13 follows the dimensional standard; do not invent a density override without a written agreement. Random vs exact length must appear on the PO. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Equivalent Grades for ISO 9329-4 X2CrNiMo17-13

Equivalence language around X2CrNiMo17-13 is often looser than a tube purchase order can afford. ISO 9329-4 X2CrNiMo17-13 governs this article; 316L higher-Mo / EN 1.4435 (approx) is body-only framing for catalogues and dual-cert talk, not a substitute mark on the MTC. Keep the ISO 9329-4 symbol unless a written dual-cert plan lists both standards with separate test scopes.

System Designation Notes
ISO 9329-4 X2CrNiMo17-13 Governing tube grade for this page
Commercial / UNS (body only) 316L higher-Mo / EN 1.4435 (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 / A213 related 316L chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other 1.4435 Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec

We deliberately avoid inventing a false one-to-one for every foreign system on X2CrNiMo17-13. Use ISO 9329-4 X2CrNiMo17-12, ISO 9329-4 X5CrNiMo17-13, ISO 9329-4 X2CrNiMoN17-13, ISO 9329-4 X6CrNiMoTi17-12 for in-series alternatives, and keep ISO 9329-4 as the category landing page. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (X2CrNiMo17-13).

Project teams specifying X2CrNiMo17-13 should the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as ASTM A240 Type 316L. Keep X2CrNiMo17-13 acceptance text on the governing pipe/tube standard.

Heat Treatment and Delivery Condition for ISO 9329-4 X2CrNiMo17-13

Recorded furnace charts for X2CrNiMo17-13 should support the heat-treatment claim on the certificate, including quench or cool method where rapid cooling is required. Band note: 1020–1120 °C. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

IGC applicability for X2CrNiMo17-13: Yes — guideline limit ~400 °C / 100000 h. Elevated-temperature grades marked N/A for IGC in Table 3 are not “exempt from corrosion engineering” — they are oriented to hot service acceptance paths. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Corrosion Resistance of ISO 9329-4 X2CrNiMo17-13

ISO 9329-4 corrosion text focuses on intergranular corrosion (ISO 3651-1 / 3651-2) for X2CrNiMo17-13. Other corrosion modes are outside the standard’s normative scope and must be engineered separately. Framing: higher Mo lifts PREN vs X2CrNiMo17-12; still austenitic — severe seawater crevices may need duplex or super-austenitic. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Specific corrosion tests beyond IGC for X2CrNiMo17-13 shall be agreed at enquiry with method and acceptance criteria written down — the standard will not invent them. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

Applications of ISO 9329-4 X2CrNiMo17-13 Seamless Tube

Typical duties for X2CrNiMo17-13: chemical process tubing with elevated chloride risk, heat-exchanger interconnects, and pressure lines where EN 1.4435-class Mo is preferred over standard 2% Mo. Role: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file. Keep the as-built dossier repeating X2CrNiMo17-13 beside heat numbers.

Cryogenic or elevated-temperature options for X2CrNiMo17-13 need explicit impact or Table 4 proof-stress orders — ambient Table 3 alone does not prove those duties. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

Weldability of ISO 9329-4 X2CrNiMo17-13

Automatic mill welding is outside seamless ISO 9329-4; manual and automatic field welds must still respect X2CrNiMo17-13 chemistry. Guidance: 316L / 1.4435-class fillers matching Mo; control ferrite and heat tint on process welds. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Post-weld solution treatment of X2CrNiMo17-13 should chase 1020–1120 °C when the corrosion file demands restored IGC resistance after heavy fabrication. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

Surface Finishes for ISO 9329-4 X2CrNiMo17-13

X2CrNiMo17-13 under ISO 9329-4 typically ships solution annealed and pickled so scale and heat tint are removed before installation. Bright anneal covers appearance orders; special roughness is by agreement. Role: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (X2CrNiMo17-13).

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Bright or polished callouts for X2CrNiMo17-13 never waive heat-treatment proof. After finishing, keep iron-free handling through storage and shipment so ISO 9329-4 tube does not leave the yard with free-iron blooms. Ambiguous finish wording is rewritten into measurable OD/ID scope before the finishing bay is booked for X2CrNiMo17-13.

Inspection and Testing for ISO 9329-4 X2CrNiMo17-13

Sampling plans for X2CrNiMo17-13 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Caution: Mo 2.50–3.00 and Ni 11.50–14.50 — do not dual-cert as plain 316L without checking both windows. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Weld-shop note tied to X2CrNiMo17-13: 316L / 1.4435-class fillers matching Mo; control ferrite and heat tint on process welds. Mill tests do not replace fabricator WPS qualification. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Packaging and Shipping for ISO 9329-4 X2CrNiMo17-13

Container loading plans should keep heavy walls from crushing thin-wall X2CrNiMo17-13 layers. Corrosion framing: higher Mo lifts PREN vs X2CrNiMo17-12; still austenitic — severe seawater crevices may need duplex or super-austenitic. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Mixed-grade bundles are forbidden when X2CrNiMo17-13 shares a crate with a different Table 1 steel — heat identity must remain auditable at receipt. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

Claims handling for X2CrNiMo17-13 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

Why Choose SHH STEEL

SHH STEEL can make X2CrNiMo17-13 to the written scope: Table 1 chemistry, Table 3 tensile, ordered condition symbol, and test category. Use: chemical process tubing with elevated chloride risk, heat-exchanger interconnects, and pressure lines where EN 1.4435-class Mo is preferred over standard 2% Mo. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Dual-cert discussions for X2CrNiMo17-13 start with a chemistry and test matrix — not with a promise that “304/316 equivalent” clears ASTM by default. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

Supply Capability

SHH STEEL can produce ISO 9329-4 X2CrNiMo17-13 in enquiry-oriented OD × wall bands under ISO 1127 / ISO 4200 practice. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Duty: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Item Capability
Standard ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes
Grade X2CrNiMo17-13 (Table 1; alias 316L higher-Mo / EN 1.4435 (approx))
Product form Seamless tube only — hot and/or cold finished before heat treatment
Delivery condition solution-treated (Q) or hot-finished within solution band + rapid cool
Documents ISO 10474 / EN 10204 3.1 style as ordered
Typical size practice OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759
Condition symbols Table 7 (e.g. HFS2) as ordered
Tests Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered

Stock / Available sizes

Stock / Available sizes for X2CrNiMo17-13: enquire OD × wall × length × condition symbol. Size practice: ISO 1127 OD×wall for higher-Mo low-carbon pressure tube. SHH STEEL can produce trial lengths for procedure qualification before bulk release when the project calendar needs it. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Export packing, third-party inspection, and dual-language MTCs for X2CrNiMo17-13 are available when stated on the order. Sisters often quoted alongside: X2CrNiMo17-12, X5CrNiMo17-13, X2CrNiMoN17-13, X6CrNiMoTi17-12. Keep ISO 9329-4 and X2CrNiMo17-13 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file.

FAQ

What is ISO 9329-4 X2CrNiMo17-13 seamless stainless steel tube used for?
ISO 9329-4 X2CrNiMo17-13 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — chemical process tubing with elevated chloride risk, heat-exchanger interconnects, and pressure lines where EN 1.4435-class Mo is preferred over standard 2% Mo. Role summary: low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
Is ISO 9329-4 X2CrNiMo17-13 seamless only, or does it cover welded tube?
Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X2CrNiMo17-13 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
What heat treatment does X2CrNiMo17-13 require under ISO 9329-4?
Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X2CrNiMo17-13: 1020–1120 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
How does X2CrNiMo17-13 compare with sister grades X2CrNiMo17-12, X5CrNiMo17-13, X2CrNiMoN17-13?
X2CrNiMo17-13 is filed as austenitic low-carbon higher-Mo 17-13-3. Typical sisters on the same RFQ are X2CrNiMo17-12, X5CrNiMo17-13, X2CrNiMoN17-13. Design caution: Mo 2.50–3.00 and Ni 11.50–14.50 — do not dual-cert as plain 316L without checking both windows Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
What tests appear on the mill certificate for X2CrNiMo17-13?
Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
Is 316L higher-Mo / EN 1.4435 (approx) the same as ordering X2CrNiMo17-13?
No. 316L higher-Mo / EN 1.4435 (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X2CrNiMo17-13 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for ISO 9329-4 X2CrNiMo17-13?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X2CrNiMo17-13 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: ISO 1127 OD×wall for higher-Mo low-carbon pressure tube. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should X2CrNiMo17-13 be welded on site?
Shop guidance: 316L / 1.4435-class fillers matching Mo; control ferrite and heat tint on process welds. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: Mo 2.50–3.00 and Ni 11.50–14.50 — do not dual-cert as plain 316L without checking both windows
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X2CrNiMo17-13?
Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic low-carbon higher-Mo 17-13-3 practice can defend for the temperature and stress state. Caution for this mark: Mo 2.50–3.00 and Ni 11.50–14.50 — do not dual-cert as plain 316L without checking both windows Sister pointers: X2CrNiMo17-12, X5CrNiMo17-13, X2CrNiMoN17-13. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify ISO 9329-4 X2CrNiMo17-13 with ASTM A312 or EN 10216-5?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X2CrNiMo17-13 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
What is the difference between hyphenated X2CrNiMo17-13 and the spaced ISO designation?
They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X2CrNiMo17-13 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.

Conclusion

ISO 9329-4 X2CrNiMo17-13 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — low-carbon higher-Mo 17-13-3 austenitic pressure tube when 2.5–3.0% Mo is written into the chloride file. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X2CrNiMo17-12, X5CrNiMo17-13, X2CrNiMoN17-13. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X