ISO 9329-4 X7CrNiMo17-12 Seamless Stainless Steel Tube

ISO 9329-4 X7CrNiMo17-12 seamless stainless steel tube (316H-class / EN 1.4919-family (approx)), austenitic elevated-carbon Mo 17-12-2, Table 1 heat analysis, Rp0.2 min 205 N/mm² / Rm 510–710 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.
Grade
X7CrNiMo17-12 (ISO 9329-4 Table 1 / 316H-class / EN 1.4919-family (approx) — body alias)
Standard
ISO 9329-4:1997
Product form
Seamless stainless steel tube (hot and/or cold finished), delivery solution-treated (Q) or hot-finished within solution band + rapid cool
Size
OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759; ID×wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ISO 9329-4 X7CrNiMo17-12 Seamless Stainless Steel Tube

ISO 9329-4 covers seamless hot- and/or cold-finished austenitic tubes selected from ISO 1127 / ISO 4200 dimensions. Inside that standard, X7CrNiMo17-12 is filed as austenitic elevated-carbon Mo 17-12-2. X7CrNiMo17-12 locks carbon at 0.04–0.10 with Mo 2.00–2.50 — the ISO high-carbon 316-class pressure tube. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

From billet through marking and crate protection, SHH STEEL can produce ISO 9329-4 X7CrNiMo17-12 for the sizes and tests on your RFQ. Application sketch: high-temperature chemical and steam tubing where molybdenum and a carbon floor are both required. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Pair EN 10216-5 1.4919 and ASTM A312 aliases share chemistry families with X7CrNiMo17-12, yet hydrostatic, NDT, and delivery-condition text diverge. Document the medium, design temperature, and weld map beside the X7CrNiMo17-12 line item so sister-grade swaps stay engineering decisions. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Document test category (I or II), type of condition, and any optional elevated-temperature proof-stress or IGC requirements with the X7CrNiMo17-12 size list so quality planners book the correct benches before tube is cut to length. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Inside this ISO 9329-4 series, compare ISO 9329-4 X5CrNiMo17-12, ISO 9329-4 X7CrNiMoB17-12, ISO 9329-4 X7CrNi18-9, ISO 9329-4 X7CrNiTi18-10. Hub: ISO 9329-4. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP316H.

For X7CrNiMo17-12 dual-form buying, Stainless Steel Pipes and Tubes is the tubular parent and Stainless Steel Sheets and Plates is the flat parent; a same-chemistry plate product URL is not linked until it is live. Confirm X7CrNiMo17-12 OD × wall and plate thickness on separate drawings.

Chemical Composition of ISO 9329-4 X7CrNiMo17-12

If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 1, SHH STEEL will confirm melt feasibility for X7CrNiMo17-12 before the order is acknowledged. Keep caution visible: IGC N/A; not a drop-in for X2CrNiMo17-12 on aqueous as-welded chloride duty. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Heat identity for X7CrNiMo17-12 stays unbroken from melt through bundle tags; transition material from sequential strand casts must be positively separated per clause 5.1 practice. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Grade C Si Mn P S Cr Mo Ni
X7CrNiMo17-12 0.04–0.10 ≤1.00 ≤2.00 ≤0.040 ≤0.030 16.50–18.50 2.00–2.50 10.50–13.50

Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.

Mechanical Properties of ISO 9329-4 X7CrNiMo17-12

Elevated-temperature Rp0.2 / Rp1.0 values live in Table 4 and are not normally verified unless the purchaser orders 9.4.2 testing for X7CrNiMo17-12. Ambient floors remain the Table 3 pair above. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Size practice for X7CrNiMo17-12 remains ISO 1127 with Table 4 elevated proof-stress options. Do not substitute sister-grade tensile floors onto this certificate without a written dual-product plan. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Grade Rp0.2 min (N/mm²) Rp1.0 min (N/mm²) Rm (N/mm²) A long. min (%) A trans. min (%) KV long. min (J) Solution treatment
X7CrNiMo17-12 205 240 510–710 40 35 85 1050–1120 °C

Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X7CrNiMo17-12 (solution-treated; wall ≤50 mm unless noted). Wall ≤50 mm Table 3 values. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: N/A (elevated-temperature oriented).

Seamless Tube Manufacture of ISO 9329-4 X7CrNiMo17-12

For X7CrNiMo17-12, the mill path is pierce / extrude / cold-draw as agreed, then full-length solution treatment (Q) in the Table 3 temperature band — or hot finish inside that band with rapid cool when the purchaser allows clause 5.3.1(b). Order test category I or II with the size. Manufacture for X7CrNiMo17-12 stays seamless under ISO 9329-4 clause 5.2 — never ERW under this part.

Manufacture stays seamless. Size: ISO 1127 with Table 4 elevated proof-stress options. Hydrostatic pressure class or NDT options for X7CrNiMo17-12 are frozen with the size list so quality planners book the correct benches before tube is cut to length. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Bevelled ends, special straightness, bar coding, and protective coating for X7CrNiMo17-12 are optional purchaser items under clause 4.2 — list them explicitly or expect mill defaults. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Dimensions and Tolerances for ISO 9329-4 X7CrNiMo17-12

Precision and tolerance class for X7CrNiMo17-12 follow the dimensional standard cited on the order (typically ISO 1127 series). Ambiguous “standard tube” language is clarified before rolling slots are booked. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

When ISO 2037 food-tube dimensions are mixed into an ISO 9329-4 X7CrNiMo17-12 enquiry, separate the dimensional reference from the pressure product standard so QA does not merge acceptance texts. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Equivalent Grades for ISO 9329-4 X7CrNiMo17-12

Equivalence language around X7CrNiMo17-12 is often looser than a tube purchase order can afford. ISO 9329-4 X7CrNiMo17-12 governs this article; 316H-class / EN 1.4919-family (approx) is body-only framing for catalogues and dual-cert talk, not a substitute mark on the MTC. Keep the ISO 9329-4 symbol unless a written dual-cert plan lists both standards with separate test scopes.

System Designation Notes
ISO 9329-4 X7CrNiMo17-12 Governing tube grade for this page
Commercial / UNS (body only) 316H-class / EN 1.4919-family (approx) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 / A213 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other 1.4919 Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec

We deliberately avoid inventing a false one-to-one for every foreign system on X7CrNiMo17-12. Use ISO 9329-4 X5CrNiMo17-12, ISO 9329-4 X7CrNiMoB17-12, ISO 9329-4 X7CrNi18-9, ISO 9329-4 X7CrNiTi18-10 for in-series alternatives, and keep ISO 9329-4 as the category landing page. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (X7CrNiMo17-12).

Heat Treatment and Delivery Condition for ISO 9329-4 X7CrNiMo17-12

Party acceptance groups tubes by size, steel grade, and heat-treatment kind for X7CrNiMo17-12. Mixing differently treated lengths in one lot breaks batch rules. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Continuous-furnace practice for X7CrNiMo17-12 should hold near the upper end of 1050–1120 °C when the standard’s guidance notes apply; for subsequent fabricator HT, prefer the lower end of the band. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Corrosion Resistance of ISO 9329-4 X7CrNiMo17-12

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for X7CrNiMo17-12. Duty lock: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Pickled vs bright surfaces change initiation sites for X7CrNiMo17-12; state the finish beside the corrosion requirement so lab coupons match installed tube. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Applications of ISO 9329-4 X7CrNiMo17-12 Seamless Tube

Commissioning teams benefit when isometric revisions for X7CrNiMo17-12 link to the same mill certificates and test category stated on the acknowledgement. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Replace X7CrNiMo17-12 with a Mo or N sister when chloride or strength demand outgrows this chemistry — sisters X5CrNiMo17-12, X7CrNiMoB17-12, X7CrNi18-9, X7CrNiTi18-10. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Weldability of ISO 9329-4 X7CrNiMo17-12

For corrosive as-welded duty on X7CrNiMo17-12, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable to this mark. Role: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Keep IGC N/A; not a drop-in for X2CrNiMo17-12 on aqueous as-welded chloride duty visible when selecting fillers for X7CrNiMo17-12; boron- or nitrogen-bearing marks need matching intent in the weld metal. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Surface Finishes for ISO 9329-4 X7CrNiMo17-12

Surface supply for X7CrNiMo17-12 should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless tube, so finish is part of performance, not only appearance. Ambiguous “bright tube” language is clarified before finishing slots are booked.

Finish Typical supply Order note
Solution annealed and pickled Standard tube mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Passivation restores the chromium-rich film after pickling or light fabrication on X7CrNiMo17-12; it does not replace the heat treatment that sets mechanical properties under ISO 9329-4. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.

Inspection and Testing for ISO 9329-4 X7CrNiMo17-12

Test category I vs II for X7CrNiMo17-12 changes the intensity of testing — freeze it on the order example style used in the standard (grade – condition – category – document). Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Documents for X7CrNiMo17-12 cite the actual tests performed. An MTC that only lists chemistry is incomplete against a specific-inspection order. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Packaging and Shipping for ISO 9329-4 X7CrNiMo17-12

Protective coating per clause 11 for X7CrNiMo17-12 is agreed when open storage or salt air exposure is expected before installation. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Packing list line items for X7CrNiMo17-12 must match stencil text; alias-only labels are a common customs and QA failure mode. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

SHH STEEL can supply export packing for X7CrNiMo17-12 sized to the container plan on the shipping order when the mill schedule allows. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Why Choose SHH STEEL

Ask for a written acknowledgement that names X7CrNiMo17-12, dimensional standard, condition symbol, and test category before melt. SHH STEEL can produce to that acknowledgement. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Repeat orders for X7CrNiMo17-12 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

Supply Capability

Documents available for X7CrNiMo17-12: ISO 10474 / EN 10204 style as ordered, with heat analysis and Table 3 tensile as baseline specific-inspection content. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service.

Item Capability
Standard ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes
Grade X7CrNiMo17-12 (Table 1; alias 316H-class / EN 1.4919-family (approx))
Product form Seamless tube only — hot and/or cold finished before heat treatment
Delivery condition solution-treated (Q) or hot-finished within solution band + rapid cool
Documents ISO 10474 / EN 10204 3.1 style as ordered
Typical size practice OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759
Condition symbols Table 7 (e.g. HFS2) as ordered
Tests Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered

Stock / Available sizes

Stock / Available sizes map for X7CrNiMo17-12 is refreshed on enquiry. Role: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service. Optional hydro, UT, IGC, and elevated proof tests are booked with the size list, not as afterthoughts. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

SHH STEEL can make X7CrNiMo17-12 to ISO 9329-4 with the hyphenated grade frozen on tags and certificates so spaced ISO designations and commercial aliases cannot drift apart in receiving inspection. Keep ISO 9329-4 and X7CrNiMo17-12 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.

FAQ

What is ISO 9329-4 X7CrNiMo17-12 seamless stainless steel tube used for?
ISO 9329-4 X7CrNiMo17-12 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — high-temperature chemical and steam tubing where molybdenum and a carbon floor are both required. Role summary: elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
Is ISO 9329-4 X7CrNiMo17-12 seamless only, or does it cover welded tube?
Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X7CrNiMo17-12 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
What heat treatment does X7CrNiMo17-12 require under ISO 9329-4?
Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X7CrNiMo17-12: 1050–1120 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
How does X7CrNiMo17-12 compare with sister grades X5CrNiMo17-12, X7CrNiMoB17-12, X7CrNi18-9?
X7CrNiMo17-12 is filed as austenitic elevated-carbon Mo 17-12-2. Typical sisters on the same RFQ are X5CrNiMo17-12, X7CrNiMoB17-12, X7CrNi18-9. Design caution: IGC N/A; not a drop-in for X2CrNiMo17-12 on aqueous as-welded chloride duty Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
What tests appear on the mill certificate for X7CrNiMo17-12?
Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
Is 316H-class / EN 1.4919-family (approx) the same as ordering X7CrNiMo17-12?
No. 316H-class / EN 1.4919-family (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X7CrNiMo17-12 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for ISO 9329-4 X7CrNiMo17-12?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X7CrNiMo17-12 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: ISO 1127 with Table 4 elevated proof-stress options. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should X7CrNiMo17-12 be welded on site?
Shop guidance: 316H-class fillers; post-weld solution treatment if returning to aqueous corrosion duty. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: IGC N/A; not a drop-in for X2CrNiMo17-12 on aqueous as-welded chloride duty
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X7CrNiMo17-12?
Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic elevated-carbon Mo 17-12-2 practice can defend for the temperature and stress state. Caution for this mark: IGC N/A; not a drop-in for X2CrNiMo17-12 on aqueous as-welded chloride duty Sister pointers: X5CrNiMo17-12, X7CrNiMoB17-12, X7CrNi18-9. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify ISO 9329-4 X7CrNiMo17-12 with ASTM A312 or EN 10216-5?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X7CrNiMo17-12 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
What is the difference between hyphenated X7CrNiMo17-12 and the spaced ISO designation?
They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X7CrNiMo17-12 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.

Conclusion

ISO 9329-4 X7CrNiMo17-12 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — elevated-carbon Mo 17-12-2 austenitic pressure tube for hot Mo-bearing service. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X5CrNiMo17-12, X7CrNiMoB17-12, X7CrNi18-9. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X