ISO 9329-4 X7CrNiTi18-10 Seamless Stainless Steel Tube
What is ISO 9329-4 X7CrNiTi18-10 Seamless Stainless Steel Tube
When the approved vendor list prints ISO 9329-4, the steel grade has to be one of the seventeen Table 1 austenitics. X7CrNiTi18-10 is the full product grade for this austenitic elevated-carbon Ti-stabilised 18-10 seamless pressure tube. X7CrNiTi18-10 is the ISO high-carbon Ti-stabilised sister — carbon intentional for hot duty, titanium still required on the cast.
SHH STEEL can supply X7CrNiTi18-10 seamless tube with plain or bevelled ends, standard or exact lengths, and ISO 10474 3.1.B / EN 10204 3.1 style certificates when specified. Role on the line: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Sister grades often compared on the same RFQ include X6CrNiTi18-10, X7CrNiNb18-11, X7CrNi18-9, X7CrNiMo17-12. Pick the sister when carbon, Mo, N, or stabiliser intent changes — not when purchasing wants a cheaper synonym. Corrosion framing beside X7CrNiTi18-10: Ti stabilisation plus elevated carbon for hot oxidation/strength balance; aqueous IGC not Table 3 path. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Delivery condition for X7CrNiTi18-10 is solution-treated (Q) or hot-finished within solution band + rapid cool. Solution-treatment band: 1050–1120 °C with water or air (rapid). Do not invent a non-heat-treated shipment unless clause 5.3.1(b) hot-finish-in-band is explicitly agreed. Keep IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties visible on the enquiry checklist.
Inside this ISO 9329-4 series, compare ISO 9329-4 X6CrNiTi18-10, ISO 9329-4 X7CrNiNb18-11, ISO 9329-4 X7CrNi18-9, ISO 9329-4 X7CrNiMo17-12. Hub: ISO 9329-4. ASTM/ASME related pipe pages (not interchangeable by default): ASTM A312 TP321H.
On X7CrNiTi18-10 packages that also list flats, use Stainless Steel Pipes and Tubes for pipes/tubes and Stainless Steel Sheets and Plates for sheets/plates without inventing a plate SKU here. Quote X7CrNiTi18-10 pipe and plate under separate line items.
Chemical Composition of ISO 9329-4 X7CrNiTi18-10
Where Mo, Ti, Nb, N, or B appear for X7CrNiTi18-10, they are intentional levers, not optional marketing. Confirm them line-by-line on the MTC. Alias reminder: 321H-class / EN 1.4541-H family (approx) is body text only. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dual-cert plans that also cite EN 10216-5 1.4541 or ASTM A312 must satisfy each standard’s chemistry on its own terms for X7CrNiTi18-10 — overlapping aliases are not automatic clearance. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | C | Si | Mn | P | S | Cr | Ni | Ti |
|---|---|---|---|---|---|---|---|---|
| X7CrNiTi18-10 | 0.04–0.10 | ≤1.00 | ≤2.00 | ≤0.040 | ≤0.030 | 17.00–19.00 | 9.00–12.00 | ≥5×%C ≤0.80 |
Heat analysis windows from ISO 9329-4:1997 Table 1 (cross-checked GOST ISO 9329-4-2013). Product analysis uses Table 2 deviations when ordered. Nb includes Ta determined as Nb where applicable.
Mechanical Properties of ISO 9329-4 X7CrNiTi18-10
When comparing X7CrNiTi18-10 to a commercial 321H-class catalogue sheet, expect different Rm bands and elongation orientation rules. ISO reports longitudinal and transverse A minima separately. Caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Heat-treatment guidance: solution treat at 1050–1120 °C, cool water or air (rapid). If post-delivery HT differs from Table 3, agree additional sample tests at enquiry for X7CrNiTi18-10. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Grade | Rp0.2 min (N/mm²) | Rp1.0 min (N/mm²) | Rm (N/mm²) | A long. min (%) | A trans. min (%) | KV long. min (J) | Solution treatment |
|---|---|---|---|---|---|---|---|
| X7CrNiTi18-10 | 175 | 210 | 490–690 | 40 | 35 | 85 | 1050–1120 °C |
Ambient values from ISO 9329-4 Table 3 via GOST ISO 9329-4-2013 adoption for X7CrNiTi18-10 (solution-treated; wall ≤50 mm unless noted). Wall ≤50 mm Table 3 values. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool. Cooling: water or air (rapid). IGC: N/A (elevated-temperature oriented).
Seamless Tube Manufacture of ISO 9329-4 X7CrNiTi18-10
For X7CrNiTi18-10, the mill path is pierce / extrude / cold-draw as agreed, then full-length solution treatment (Q) in the Table 3 temperature band — or hot finish inside that band with rapid cool when the purchaser allows clause 5.3.1(b). Order test category I or II with the size. Manufacture for X7CrNiTi18-10 stays seamless under ISO 9329-4 clause 5.2 — never ERW under this part.
Test category I or II changes sampling density and NDT scope for X7CrNiTi18-10 — freeze the category with the size list. Hydraulic or other leak-tightness tests run when ordered under 9.5. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
SHH STEEL can produce X7CrNiTi18-10 on pierce-and-draw or extrusion-capable routes within the ordered OD×wall; out-of-ISO-1127 combinations need a written dimensional agreement on the same grade symbol. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dimensions and Tolerances for ISO 9329-4 X7CrNiTi18-10
Special tolerances on OD and wall (tables 5 and 6) apply only when ordered for X7CrNiTi18-10. Exact lengths greater than 12 m need an agreed length tolerance under 7.3.2. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Straightness special requirements for X7CrNiTi18-10 are optional under 4.2 — default mill straightness applies unless stated. Size practice remains pressure OD×wall with elevated-temperature proof options from Table 4. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Equivalent Grades for ISO 9329-4 X7CrNiTi18-10
Cross-references help sourcing X7CrNiTi18-10, but they do not replace the ISO 9329-4 grade line on the enquiry. Family framing here is austenitic elevated-carbon Ti-stabilised 18-10; delivery practice from the crib is “solution-treated (Q) or hot-finished within solution band + rapid cool”. Related ASTM or EN numbers are starting points for engineering comparison, not automatic substitutes.
| System | Designation | Notes |
|---|---|---|
| ISO 9329-4 | X7CrNiTi18-10 | Governing tube grade for this page |
| Commercial / UNS (body only) | 321H-class / EN 1.4541-H family (approx) | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 / A213 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | 1.4541 | Approximate EN steel number — starting point for comparison only; order EN product under the EN tube/pipe spec |
We deliberately avoid inventing a false one-to-one for every foreign system on X7CrNiTi18-10. Use ISO 9329-4 X6CrNiTi18-10, ISO 9329-4 X7CrNiNb18-11, ISO 9329-4 X7CrNi18-9, ISO 9329-4 X7CrNiMo17-12 for in-series alternatives, and keep ISO 9329-4 as the category landing page. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (X7CrNiTi18-10).
Heat Treatment and Delivery Condition for ISO 9329-4 X7CrNiTi18-10
If hot finishing of X7CrNiTi18-10 stays inside the solution band and cools rapidly, a separate furnace solution cycle may be omitted under clause 5.3.1(b) when agreed — mechanical and corrosion requirements still apply. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
When post-delivery HT differs from Table 3 for X7CrNiTi18-10, agree additional mechanical tests on specially treated samples at enquiry (clause 6.2.1 note). Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
Corrosion Resistance of ISO 9329-4 X7CrNiTi18-10
IGC status for X7CrNiTi18-10: N/A (elevated-temperature oriented). If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice rather than relying on wall thickness alone. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Mo-bearing and N-bearing sisters raise pitting resistance vs plain 18-10; duplex is still outside ISO 9329-4’s austenitic Table 1 set. Caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Applications of ISO 9329-4 X7CrNiTi18-10 Seamless Tube
If the only reason for X7CrNiTi18-10 is “we always used 321H-class,” reopen the corrosion and temperature file before repeating the order. Caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Food-adjacent duties using X7CrNiTi18-10 still need finish and iron-control language beyond the pressure product standard. Caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Weldability of ISO 9329-4 X7CrNiTi18-10
Consumable lot control and shielding-gas notes for X7CrNiTi18-10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Dissimilar welds from X7CrNiTi18-10 to carbon steel need qualified buttering/transition procedures — ISO 9329-4 weldability text does not replace a WPS. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
Surface Finishes for ISO 9329-4 X7CrNiTi18-10
Iron-free handling after pickle matters for X7CrNiTi18-10 — carbon-steel strapping stains show up later as rust blooms on finished tube. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for X7CrNiTi18-10.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard tube mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Reject grinding burns, embedded free iron, and unrepaired undercut on X7CrNiTi18-10 before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under ISO 9329-4 for this austenitic elevated-carbon Ti-stabilised 18-10 mark. Final visual release still rejects grinding burns, embedded free iron, and unrepaired weld undercut before bundles are closed (X7CrNiTi18-10).
Inspection and Testing for ISO 9329-4 X7CrNiTi18-10
Base acceptance tracks ISO 9329-4 for X7CrNiTi18-10: heat analysis, tensile, technological tests per category, and every optional hydro, NDT, impact, elevated proof, or IGC test actually ordered. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Marking per clause 10 for X7CrNiTi18-10 shall include ISO 9329-4 and the steel grade; specific marking and bar coding are optional purchaser items. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
Packaging and Shipping for ISO 9329-4 X7CrNiTi18-10
End caps and bore protection for X7CrNiTi18-10 follow the cleanliness class on the shipping order, not a one-size export habit. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
Wooden cradles and steel strapping for X7CrNiTi18-10 should avoid carbon-steel rub that embeds free iron into austenitic surfaces. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
Inland trucking of X7CrNiTi18-10 still needs weather protection when open-bed haulage is used; austenitic surfaces stain from road salt as readily as from seawater splash. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
Why Choose SHH STEEL
Response time stays short because common X7CrNiTi18-10 enquiry sizes and document packs are already exercised on prior ISO-spec orders. Caution locked: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties. SHH STEEL can produce and supply X7CrNiTi18-10 to the OD × wall, seamless route, and test scope on your RFQ.
Engineering support on medium selection for X7CrNiTi18-10 stays qualitative and standard-tied; SHH STEEL will not invent PREN marketing digits. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
Supply Capability
Stock conversation for X7CrNiTi18-10 is always RFQ-led — published ranges are capability envelopes, not frozen tonnage. Size hint: pressure OD×wall with elevated-temperature proof options from Table 4. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
| Item | Capability |
|---|---|
| Standard | ISO 9329-4:1997 seamless austenitic stainless steel tubes for pressure purposes |
| Grade | X7CrNiTi18-10 (Table 1; alias 321H-class / EN 1.4541-H family (approx)) |
| Product form | Seamless tube only — hot and/or cold finished before heat treatment |
| Delivery condition | solution-treated (Q) or hot-finished within solution band + rapid cool |
| Documents | ISO 10474 / EN 10204 3.1 style as ordered |
| Typical size practice | OD × wall from ISO 1127 / ISO 4200; special fields ISO 1129 / 2037 / 6759 |
| Condition symbols | Table 7 (e.g. HFS2) as ordered |
| Tests | Tensile per category; hydro / NDT / impact / elevated proof / IGC when ordered |
Stock / Available sizes
Stock / Available sizes — SHH STEEL can supply X7CrNiTi18-10 across common ISO 1127 diameters used in pressure interconnects; exotic ID×wall combinations need agreement. Caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias.
Lead time for X7CrNiTi18-10 depends on OD×wall, test category, and whether elevated-temperature or impact options are ordered — send the full matrix with the first RFQ. Keep ISO 9329-4 and X7CrNiTi18-10 frozen on the acknowledgement so Table 1 cast windows and Table 3 tensile floors cannot drift under a commercial alias. Role reminder for this mark: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon.
FAQ
-
What is ISO 9329-4 X7CrNiTi18-10 seamless stainless steel tube used for?
- ISO 9329-4 X7CrNiTi18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — high-temperature process and steam interconnects where 321H-class chemistry is preferred over plain X7CrNi18-9. Role summary: elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon. It is an ISO product standard grade (Table 1 chemistry / Table 3 tensile), not an automatic ASTM A312 or EN 10216-5 certificate.
-
Is ISO 9329-4 X7CrNiTi18-10 seamless only, or does it cover welded tube?
- Seamless only under ISO 9329-4. Longitudinally welded austenitic pressure tubes belong under ISO 9330-6, not this part. SHH STEEL can produce and supply the seamless route for X7CrNiTi18-10 when the mill can meet the ordered size and tests. Do not mix 9329-4 and 9330-6 certificates.
-
What heat treatment does X7CrNiTi18-10 require under ISO 9329-4?
- Tubes shall be suitably heat treated over their full length. Reference solution-treatment band for X7CrNiTi18-10: 1050–1120 °C, with rapid cool (water or air). Hot-finished tubes made inside that band and cooled rapidly may omit a separate furnace cycle when clause 5.3.1(b) is agreed. Delivery: solution-treated (Q) or hot-finished within solution band + rapid cool.
-
How does X7CrNiTi18-10 compare with sister grades X6CrNiTi18-10, X7CrNiNb18-11, X7CrNi18-9?
- X7CrNiTi18-10 is filed as austenitic elevated-carbon Ti-stabilised 18-10. Typical sisters on the same RFQ are X6CrNiTi18-10, X7CrNiNb18-11, X7CrNi18-9. Design caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties Pick the sister when carbon, Mo, N, or stabiliser intent changes rather than stretching wall alone.
-
What tests appear on the mill certificate for X7CrNiTi18-10?
- Expect Table 1 heat analysis, room-temperature tensile results (Table 3 Rp0.2 / Rp1.0 / Rm / A), dimensions, and every optional hydro, NDT, impact, elevated proof, flattening/expansion, or IGC test actually ordered. Documents follow ISO 10474 or EN 10204 3.1 style when specified. Test category I or II must be stated on the order.
-
Is 321H-class / EN 1.4541-H family (approx) the same as ordering X7CrNiTi18-10?
- No. 321H-class / EN 1.4541-H family (approx) is a commercial cross-walk for body text. The purchase order should lock ISO 9329-4 and X7CrNiTi18-10 so cast limits, Table 3 tensile floors, and delivery condition are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for ISO 9329-4 X7CrNiTi18-10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for X7CrNiTi18-10 within ISO 1127 / ISO 4200 practice (special fields ISO 1129 / 2037 / 6759 when applicable). Size context: pressure OD×wall with elevated-temperature proof options from Table 4. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should X7CrNiTi18-10 be welded on site?
- Shop guidance: 321H-class fillers; confirm Ti formula after elevated heat input. Mill heat treatment of seamless tube does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, nitrogen, or anneal practice as applicable. Caution: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties
-
When should I choose a Mo-bearing, N-bearing, or duplex grade instead of X7CrNiTi18-10?
- Move when chloride pitting, crevice attack, or strength demand exceeds what austenitic elevated-carbon Ti-stabilised 18-10 practice can defend for the temperature and stress state. Caution for this mark: IGC N/A; carbon floor 0.04–0.10 — not interchangeable with X6CrNiTi18-10 on aqueous as-welded IGC duties Sister pointers: X6CrNiTi18-10, X7CrNiNb18-11, X7CrNi18-9. Duplex is outside ISO 9329-4 Table 1. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify ISO 9329-4 X7CrNiTi18-10 with ASTM A312 or EN 10216-5?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites ISO 9329-4 X7CrNiTi18-10 does not clear ASTM A312 or EN 10216-5 acceptance by default. State both standards, sizes, and test scopes before melt.
-
What is the difference between hyphenated X7CrNiTi18-10 and the spaced ISO designation?
- They are the same steel grade. ISO text prints spaced forms (for example X 2 CrNi 18 10); steelspecs titles use hyphenated X7CrNiTi18-10 for readability per Jack’s confirmed list. Certificates may show either typography — chemistry and mechanical floors stay Table 1 / Table 3. SHH STEEL can produce and supply either marking style when the PO freezes it.
Conclusion
ISO 9329-4 X7CrNiTi18-10 is seamless austenitic stainless steel tube for pressure and corrosion-resisting service — elevated-carbon Ti-stabilised 18-10 austenitic pressure tube for hot service with titanium still locking carbon. SHH STEEL can produce and supply it in the seamless route with the solution treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include X6CrNiTi18-10, X7CrNiNb18-11, X7CrNi18-9. Related ASTM A312 and EN 10216-5 pages share chemistry families but not ISO acceptance text. Email admin@steelspecs.com with OD × wall, condition symbol, test category, and medium notes to start the quote.