GOST 5520 20K Steel Plate | 20K Carbon Boiler & Pressure Vessel Plate

GOST 5520 20K (20К) steel plate is non-alloy carbon boiler steel for pressure-retaining fabrication under GOST 5520-2017. Table 1 covers 4–60 mm plate. Delivery condition and inspection category must be ordered together; they determine which tensile, impact and elevated-temperature tests apply. SHH STEEL produces and exports this grade to the specified 2017 edition requirements.
Equivalent Grades:
Related, not equivalent: GB/T 713 Q245R, EN 10028-2 P265GH. Engineer approval is required for substitution.
Heat Treatment
Delivery condition ordered under GOST 5520-2017 clause 7.1.5; not automatically normalized or QT.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GOST 5520-2017 20K steel plate?

GOST 5520 20K Steel Plate is supplied for welded boilers and pressure vessels under GOST 5520-2017, Rolled non-alloy and alloy steel plates for boilers and pressure vessels. Specifications. The standard is in force, implemented in Russia on 1 October 2018, and replaced GOST 5520-79. This page uses the 2017 edition and its corrected tables, not the withdrawn 1979 tables.

20K is a carbon boiler grade, not a structural grade carrying a similar number. Its 2017 yield minima are lower than those of 18K even though its carbon range is higher. Do not rank these grades by the leading number alone.

A complete enquiry identifies the grade, thickness, delivery condition, inspection category and ultrasonic class. A grade name alone does not promise every test in the standard. Category 1 is chemistry-only in the base category matrix; other categories add specific tensile, bend, impact or elevated-temperature requirements.

SHH STEEL supplies this plate within the GOST 5520 range under Boiler & Pressure Vessel Steel Plates. We review the ordered category and delivery condition before quoting production and export requirements.

Material specification for GOST 5520 20K

The following scope and ordering requirements come from the 2017 edition. The thickness range is a standard range, not a stock availability claim.

Parameter Detail
Standard GOST 5520-2017; in force; replaced GOST 5520-79
Grade 20K
2017 chemical classification Non-alloy (clause 7.1.1.1; Annex A)
Table 1 thickness 4–60 mm
Dimensions and tolerances GOST 19903; state dimensional accuracy and flatness on the order
Product form Hot-rolled plate; plate-mill production or coil rolled and cut into sheets
Permitted inspection categories (Table 5) 1–5, 10, 11, 16, 18–21, 23, 24
Delivery condition As ordered under clause 7.1.5; see Delivery Conditions below
Room-temperature tensile and KCU data Table 6, subject to the ordered category and thickness
V-notch impact data Table 8, subject to category; KCV in J/cm², not absorbed energy in J
Elevated-temperature yield Table 9 for categories 16–18, 23 and 24; test temperature stated in the order
Ultrasonic testing Each plate; class 1, 2 or 3 under GOST 22727, specified by the purchaser
Quality document GOST 7566 or the inspection-document reference cited by the standard; state required document type

Chemical composition of GOST 5520-2017 20K

The following ladle-analysis limits are the 20K row of GOST 5520-2017 Table 2. A maximum sign means an upper limit, not a target addition. Values are mass percent.

Element Ladle analysis, wt. %
C 0.16–0.24
Si 0.15–0.30
Mn 0.35–0.65
S ≤0.025
P ≤0.035
Cr ≤0.30
Ni ≤0.30
Cu ≤0.30
Mo ≤0.08
V ≤0.05

For plate over 20 mm, Table 2 note 1 permits the manganese upper limit to rise to 0.80 %.

Residual arsenic is limited to 0.08 %. Residual nitrogen is limited to 0.008 %, or 0.012 % for electric-furnace steel. Nitrogen up to 0.012 % is also permitted for other melting routes when the plate passes the required impact test after mechanical ageing, irrespective of the ordered category.

Table 2 permits niobium microalloying up to 0.05 %.

Product-analysis deviations are separately defined in Table 3; they must not be used to widen the ladle-analysis order limits. Elements not listed in Table 2 may not be deliberately added without agreement. Any supplementary chemistry requirement must be written on the order.

Mechanical properties and impact tests for GOST 5520 20K

The 20K data below are transcribed from GOST 5520-2017, not from GOST 19281 or a foreign vessel specification. Table 6 tensile tests are at room temperature, specified as 20°C with a +15/−10°C tolerance. The category matrix determines which characteristics are controlled.

Thickness (mm) Yield, min (MPa) Tensile (MPa) Elongation, min (%) KCU at room temperature (J/cm²) KCU at −40°C (J/cm²) KCU at −70°C (J/cm²) KCU after mechanical ageing at room temperature (J/cm²)
4 to <5 245 400–510 25 – – – –
5–20 245 400–510 25 59 – – 29**
>20–40 235 400–510 24 54 – – 24**
>40–60 225 400–510 23 49 – – 24**

Table 6 symbols: “+” means testing for statistical data with results recorded, not a numerical acceptance minimum; “−” means the characteristic is not specified or controlled. “**” values are used only by agreement and must be written on the order. Repeated thickness rows with a “**” tensile band represent alternatives, not cumulative limits.

Clause 7.1.6.2 permits elongation adjustments below 8 mm and above 20 mm: a reduction of 1 percentage point per millimetre below 8 mm, or 0.25 percentage point per millimetre above 20 mm, with the latter reduction capped at 2 points relative to Table 6. Apply the clause to the ordered thickness; the table above retains the printed values.

For the five carbon K grades, clause 7.1.6.2 also permits the upper tensile limit to be increased by 29 MPa relative to Table 6. This permission is separate from the printed base range.

V-notch impact, Table 8. KCV is impact toughness per ligament area in J/cm². It is not an absorbed-energy value in joules, and KCU and KCV are not interchangeable.

Thickness (mm) KCV +20°C (J/cm²) KCV 0°C (J/cm²) KCV −20°C (J/cm²) KCV −40°C (J/cm²)
5–60 39 29 20* –

Table 8 applies through the ordered V-notch categories (19–22 and 24), restricted to categories permitted for the grade in Table 5. “+” is statistical-only; “−” is not specified. A single asterisk is retained from the source, whose note gives a historical non-rejection period ending on 1 January 2022. Do not treat starred values as an unconditional exemption from present acceptance requirements.

Impact testing at room and subzero temperatures is required for plate 12 mm and thicker when the category requires it; below 12 mm it is by purchaser request. For the carbon and Mn-Si grades, aged-impact testing is specified from 7 mm; below 7 mm it is on request with results recorded but not used for rejection. Specimen selection follows clause 9.8: full-size types from 10 mm and reduced-size types from 5 to under 10 mm, with the stated thickness-tolerance exceptions. One impact specimen may be 4.9 J/cm² below the table value. These are not permission to omit the ordered tests.

Elevated-temperature yield, Table 9. The temperature is a test condition, not a maximum service temperature or an allowable design stress.

Requirement 200°C 250°C 300°C 320°C 350°C 400°C 450°C 500°C
Base requirements 216 196 176 – 157 137 118 –

All Table 9 numbers are minimum yield strength in MPa. “*” in this table has a different meaning from Tables 6 and 8: the starred value and its test require agreement and inclusion on the order. “−” means no requirement at that temperature. No interpolation or allowable-stress calculation is supplied.

180° bend, Table 7: 4–30 mm: d = 1.5a; over 30–60 mm: d = 2.5a. Here d is mandrel diameter and a is specimen thickness. No tears, cracks or laminations are permitted at the bend.

Delivery conditions for GOST 5520 20K

Clause 7.1.5 supplies plate in the condition stated in the order. The standard lists normalizing, normalizing plus tempering, quenching plus tempering, tempering and annealing, including applicable processing from rolling heat; controlled rolling with or without accelerated cooling; controlled rolling followed by high tempering; and hot-rolled delivery without heat treatment.

This list does not mean that every 20K enquiry should default to one treatment. Select the condition with the vessel designer and mill to meet the ordered category. If the condition is not stated, the manufacturer determines it and records it in the quality document. Category 1 is hot-rolled in the base matrix; heat-treated or thermomechanically processed category 1 plate is an agreement option under clause 7.2.6.

The standard does not prescribe one universal normalizing, tempering or welding temperature for this grade on this page. Request the actual heat-treatment regime when the fabrication code requires it; clause 8.3 allows agreed reporting of that information. Fabrication heat treatments and simulated post-weld heat-treatment tests must be discussed before supply.

Weldability and fabrication heat treatment

GOST 5520-2017 clause 7.1.7 states that weldability is ensured by chemical composition and manufacturing technology. This is not a qualified welding procedure for 20K. Welding consumables, preheat, interpass temperature, heat input and any post-weld heat treatment must follow the qualified procedure and the pressure-equipment design requirements.

Thickness, restraint, hydrogen level and the actual heat chemistry influence cracking risk. Matching a nominal carbon or manganese level is not enough to approve a procedure or substitute another steel.

Where the design needs weld or HAZ toughness at a particular temperature, specify it in the procedure qualification. Base-plate KCU or KCV results do not demonstrate the toughness of a completed weld.

Dimensions, surface quality and inspection

Dimensions, thickness deviations and flatness follow GOST 19903. State plate size, manufacturing accuracy and flatness in the enquiry rather than treating the full Table 1 scope as a warehouse size list.

The standard prohibits cracks, rolled-in surface defects and laminations. Grinding or dressing must not take the plate below its permitted minimum thickness. Surface repair by welding is allowed only within clause 7.1.2.3 limits, with its inspection, thermal-treatment and reporting requirements; specify any project restriction on repair welding at enquiry stage.

Every plate is checked for dimensions, surface and edge quality, and ultrasonically examined. GOST 22727 continuity class 1, 2 or 3 is chosen on the order; there is no single universal class for every GOST 5520 grade. Mechanical specimens are transverse to rolling under clause 9.5 unless longitudinal testing is requested with the permitted acceptance adjustment.

Batch acceptance follows GOST 7566 and clauses 8–9. The quality document records the inspection category, delivery condition, test results and internal-defect examination; additional tests and any repair-weld information are reported where applicable. Heat/plate identification must remain traceable through cutting and shipment.

Applications and service limits of 20K

20K plate is specified for welded boiler drums, pressure-vessel shells, heads and other pressure-retaining fabrications where the design specifies a carbon boiler steel. Suitability for a particular temperature, pressure and wall thickness is established by the design code and ordered tests, not by a generic boiler-plate label.

Room-temperature tensile tests and elevated-temperature yield tests do not themselves establish creep life or an allowable operating temperature. Those limits belong in the engineering design and project material specification.

Edition note. Order GOST 5520-2017 explicitly. GOST 5520-79 is the replaced edition; an older designation or catalogue table is not proof that the current category, chemistry and testing requirements have been met.

Related standard ranges include GB/T 713, EN 10028-2 and ASTM A516. These are routes for a design review, not substitute certificates.

Compare GOST 5520 20K with related boiler grades

The other twelve grades in the GOST 5520 range are linked below so a buyer can compare the specified product, not just its name. They are related, not equivalent. Thickness and category entries are from GOST 5520-2017 Tables 1 and 5.

Material Type / purpose Table 1 thickness Permitted categories Substitution limit
GOST 5520 20K (this plate) non-alloy carbon boiler steel 4–60 mm 1–5, 10, 11, 16, 18–21, 23, 24 2017 edition; select delivery condition and category
GOST 5520 15K Steel Plate non-alloy carbon boiler steel 4–60 mm 1–4, 10, 16, 18–21, 23, 24 Related within GOST 5520; different grade requirements
GOST 5520 16K Steel Plate non-alloy carbon boiler steel 4–60 mm 1–4, 10, 16, 18–21, 23, 24 Related within GOST 5520; different grade requirements
GOST 5520 18K Steel Plate non-alloy carbon boiler steel 4–60 mm 1–4, 10, 16, 18–21, 23, 24 Related within GOST 5520; different grade requirements
GOST 5520 22K Steel Plate non-alloy carbon boiler steel 4–120 mm 1–4, 10, 16, 18–21, 23, 24 Related within GOST 5520; different grade requirements
GOST 5520 16GS Steel Plate manganese-silicon boiler and vessel steel, classified as non-alloy in the 2017 edition 4–160 mm 1–24 Related within GOST 5520; different grade requirements
GOST 5520 17GS Steel Plate manganese-silicon boiler and vessel steel, classified as non-alloy in the 2017 edition 4–50 mm 1–6, 10–12, 16, 18–24 Related within GOST 5520; different grade requirements
GOST 5520 17G1S Steel Plate manganese-silicon boiler and vessel steel, classified as non-alloy in the 2017 edition 4–50 mm 1–6, 10–12, 16, 18–24 Related within GOST 5520; different grade requirements
GOST 5520 09G2S Steel Plate low-carbon manganese-silicon alloy boiler and vessel steel 4–160 mm 1–24 Related within GOST 5520; different grade requirements
GOST 5520 10G2S1 Steel Plate low-carbon manganese-silicon alloy boiler and vessel steel 4–160 mm 1–24 Related within GOST 5520; different grade requirements
GOST 5520 10Kh2M Steel Plate chromium-molybdenum alloy boiler and vessel steel 8–50 mm 2–3, 16, 18–20, 23, 24 Related within GOST 5520; different grade requirements
GOST 5520 12KhM Steel Plate chromium-molybdenum alloy boiler and vessel steel 4–160 mm 2–3, 16, 18–20, 23, 24 Related within GOST 5520; different grade requirements
GOST 5520 12Kh1MF Steel Plate chromium-molybdenum-vanadium alloy boiler and vessel steel 4–50 mm 2–3, 16, 18–20, 23, 24 Related within GOST 5520; different grade requirements

Equivalent grades and related products — not equivalent

No formal equivalence has been verified for the products below. They are related, not equivalent, and are linked for a purchasing/design comparison only. A cross-reference chart cannot replace review of the two complete specifications.

Country / region Standard Grade / product Relationship Caveat
China GB/T 713 GB/T 713 Q245R Steel Plate Related boiler/vessel plate family; not equivalent Verify chemistry, thickness, delivery, impact, elevated-temperature tests and design-code approval
Europe EN 10028-2 EN 10028-2 P265GH Steel Plate Related boiler/vessel plate family; not equivalent Verify chemistry, thickness, delivery, impact, elevated-temperature tests and design-code approval

A similar tensile class or intended use does not establish equal impact testing, delivery condition or elevated-temperature acceptance. Confirm the project design-code route and all supplementary requirements before substitution.

Why choose SHH STEEL for 20K plate

  • SHH STEEL produces and exports 20K boiler and pressure-vessel plate to the ordered specification
  • We check the 4–60 mm Table 1 scope and ordered category rather than quote one generic 4–160 mm range for every grade
  • The quotation separates delivery condition, ultrasonic class and category-specific testing
  • We keep GOST 5520-2017 data separate from the replaced edition and from foreign and structural standards
  • We review traceability, inspection documents, cutting and export requirements before confirming the order

How to enquire for GOST 5520 20K plate

Send the drawing or material schedule with the following details. Production feasibility, dimensions, documentation and delivery are confirmed against the enquiry.

Item What to specify
Edition and grade GOST 5520-2017 20K; no assumed dual certification
Dimensions and quantity Thickness, width, length and tonnage; Table 1 range 4–60 mm
Delivery condition State the required processing condition under clause 7.1.5
Inspection category Choose from 1–5, 10, 11, 16, 18–21, 23, 24 under Table 5; do not leave the required tests implicit
Impact tests KCU and/or KCV; test temperature, thickness applicability, mechanical ageing and any agreed minima
Elevated-temperature yield Test temperature for the applicable category; identify any agreed Table 9 starred values
Ultrasonic examination GOST 22727 class 1, 2 or 3 as ordered; any supplementary acceptance criteria
Fabrication and documentation PWHT or simulated PWHT requirements, repair-weld restrictions, quality-document type and traceability
Supplementary scope If ordering outside the Table 1 grade thickness range, invoke clause 7.2.5 and agree mechanical and bend requirements; do not extrapolate the tables

FAQ

Is GOST 5520-2017 current for 20K?
Yes. The 2017 standard is in force and replaced GOST 5520-79. In Russia it was implemented on 1 October 2018. State the 2017 edition and the required category on the order.
What thickness range does GOST 5520 specify for 20K?
Table 1 gives 4–60 mm. This is the grade-specific standard scope, not a stock promise. A different thickness within the overall standard scope needs agreement under clause 7.2.5, including mechanical and bend requirements.
Is every 20K plate normalized?
No. Clause 7.1.5 allows several delivery routes. The ordered condition and category govern supply; if the condition is omitted, the manufacturer determines it and records it in the quality document. Do not assume normalized or QT delivery from the grade name.
Does 20K always have a guaranteed subzero Charpy value?
No. Impact testing depends on the ordered category, thickness, notch type and temperature. KCU and KCV are reported as J/cm² in this standard, not simply absorbed energy in J. Statistical-only entries are not numerical acceptance minima.
What should a quotation enquiry include?
GOST 5520-2017 20K, plate dimensions and quantity, delivery condition, inspection category, impact and elevated-temperature test requirements, ultrasonic class, fabrication heat-treatment requirements and the inspection document.

Request a quotation for GOST 5520 20K plate

Contact SHH STEEL for a quotation for GOST 5520-2017 20K boiler and pressure-vessel plate. Send thickness, width, length, quantity, destination and the project material specification.

Specify the delivery condition and inspection category, required KCU/KCV temperatures and acceptance criteria, any elevated-temperature yield test, and the GOST 22727 ultrasonic class. Include PWHT or simulated PWHT, supplementary testing and the quality-document requirement.

If a related grade or another standard is being considered, send the design requirements for review. We do not assume interchangeability or dual certification from a grade comparison alone.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X