ASME SA789 UNS S83071 Super Duplex Stainless Steel Tube
What is ASME SA789 UNS S83071 Super Duplex Stainless Steel Tube
ASME SA-789 / SA-789M lists UNS S83071 as a high-chromium super duplex: chromium 29.0–31.0%, nickel 6.0–8.0%, molybdenum 3.0–4.0%, nitrogen 0.28–0.40%, copper 0.80% max, manganese 0.50–1.50%, carbon ≤0.030%. High Cr with solid Mo/N places estimated PREN deep in the super-duplex band, and Table 4 sets a high 120/98 ksi tensile pair.
SHH STEEL can produce and supply ASME SA789 UNS S83071 super duplex stainless steel tube in seamless and welded (no filler metal) forms, with EN 10204 3.1 MTCs reporting the high Cr/N chemistry, the 120/98 ksi tensile pair with 25% elongation, and Table 2 heat treatment at 1830–2100 °F with rapid water (or other) cooling. Dual marking is available when requested.
Compare SA789 S32750 for PREN ≥41 2507; SA789 S32707/SA789 S33207 for hyper duplex; SA789 S32205 for standard duplex. Plate: A240 / SA240. Hub: SA789/SA789M. Keep the ASME designation on Code purchase orders even when dual ASTM marking is also requested for documentation convenience.
Chemical Composition of SA789 S83071
Table 1 of ASME SA-789 fixes the heat analysis for S83071. Product analysis applies when Section 8 or the purchase order invokes it through A1016/A1016M, using A480/A480M tolerances. SHH STEEL reports actual ladle values on the EN 10204 3.1 MTC for every heat.
| Element | Heat analysis (ASME SA-789 Table 1) |
|---|---|
| Carbon (C) | 0.030 max |
| Manganese (Mn) | 0.50–1.50 |
| Phosphorus (P) | 0.030 max |
| Sulfur (S) | 0.020 max |
| Silicon (Si) | 0.50 max |
| Nickel (Ni) | 6.0–8.0 |
| Chromium (Cr) | 29.0–31.0 |
| Molybdenum (Mo) | 3.0–4.0 |
| Nitrogen (N) | 0.28–0.40 |
| Copper (Cu) | 0.80 max |
Mid-range PREN with Cr ≈30, Mo ≈3.5, N ≈0.34 gives PREN ≈ 47.0 — firmly super duplex, approaching hyper territory depending on exact ladle aims. SA-789 does not publish a PREN footnote for S83071. Copper is 0.80% max.
Mechanical Properties of SA789 S83071
Table 4 sets tensile and hardness requirements for S83071 after final heat treatment. Lot sampling follows Section 9. Mechanical properties do not apply below 1/8 in. [3.2 mm] OD or 0.015 in. [0.4 mm] wall.
| Property | Requirement (SA-789 Table 4) |
|---|---|
| Tensile strength, min | 120 ksi [830] MPa |
| Yield strength (0.2% offset), min | 98 ksi [680] MPa |
| Elongation in 2 in. or 50 mm, min | 25% |
| Hardness, max | 300 HBW / 32 HRC / 300 HV |
Table 4 requires tensile 120 ksi [830 MPa] min, yield 98 ksi [680 MPa] min, elongation 25% min, hardness max 300 HBW / 32 HRC / 300 HV. Yield is notably high versus S32750’s 80 ksi floor. Source: ASME BPVC.II.A-2023 SA-789 Table 4.
Seamless and Welded Tube
ASME SA-789 allows S83071 as seamless tube or as welded tube made with no filler metal. After welding, the finished tube is heat-treated under Table 2, and marking must state the manufacture route with average or minimum wall so receiving can match each length to the purchase order and MTC.
Seamless lots take flaring to at least 10% ID expansion on one end of one tube per lot. Welded lots take flange testing plus reverse flattening on each 1500 ft [450 m] of finished tubing. Tension and hardness apply to both routes. SHH STEEL produces both SA789 S83071 routes and records them on stencil and EN 10204 3.1 MTC.
Dimensions and Tolerances
Order ASME SA789 S83071 by OD × wall (average unless minimum is specified) and length in tube / BWG language, not B36.19 pipe schedules first. Table 5 sets OD-group tolerances; clause 12.2 covers thin-wall ovality.
| OD group (Table 5 summary) | OD tolerance | Avg / Min wall |
|---|---|---|
| Up to ½ in. excl. | ±0.005 in. [0.13 mm] | Avg ±15%; Min +30%/−0% |
| ½ to 1½ in. excl. | ±0.005 in. [0.13 mm] | Avg ±10%; Min +20%/−0% |
| 1½ to 3½ in. excl. | ±0.010 in. [0.25 mm] | Avg ±10%; Min +20%/−0% |
| 3½ to 5½ in. excl. | ±0.015 in. [0.38 mm] | Avg ±10%; Min +20%/−0% |
| 5½ to 8 in. incl. | ±0.030 in. [0.76 mm] | Avg ±10%; Min +20%/−0% |
Source: ASME BPVC.II.A-2023 SA-789 Table 5. SHH STEEL quotes average-versus-minimum wall explicitly on every S83071 enquiry. Write average or minimum wall on every line item so Table 5 percentage bands are unambiguous at receiving.
Equivalent Grades
ASME SA-789 UNS S83071 is the governing tubing designation for this article. Approximate wrought names are chemistry-family hints, not automatic Code substitutes on an SA-789 mill test certificate. Confirm the product standard and tensile row before accepting a commercial nickname on the certificate.
| Designation | Notes |
|---|---|
| ASME SA789 / SA789M UNS S83071 | Governing Code Book tubing designation |
| ASTM A789 / A789M UNS S83071 | Sister ASTM A789 S83071; dual-stencil on request |
| Related super duplex | SA789 S32750, SA789 S32707, SA789 S33207 |
| Standard duplex | SA789 S32205 |
| Plate / sheet | Related duplex plate under A240 / SA240 |
Spell the UNS number and ASME SA789 on the purchase order rather than relying on a shop nickname alone. Confirm the product standard and tensile row before accepting a commercial nickname on the certificate.
Heat Treatment and Delivery Condition
Table 2 requires S83071 solution treatment at 1830–2100 °F [1000–1150 °C] followed by rapid cooling in water or by other means. The 1830–2100 °F [1000–1150 °C] band with rapid cooling in water or by other means is a wide window suited to this high-alloy grade.
Seamless tubes may be quenched after hot forming when temperature is not below the minimum solution-treatment temperature. Skipping or under-cooling risks intermetallics and undermines corrosion performance. SHH STEEL delivers SA789 S83071 only heat-treated per Table 2, with the record on the MTC.
Corrosion Resistance
Estimated PREN near 47.0 supports aggressive chloride and seawater-leaning duty when this UNS is specified. Confirm whether the project requires a Code PREN footnote grade such as SA789 S32750 (PREN ≥41) or a hyper-class grade such as SA789 S32707.
High Cr/Mo/N need rapid cooling. Observe SA-789 embrittlement warnings and 475 °C / sigma practice notes. Materials review should precede any attempt to stretch this grade outside its PREN and temperature envelope.
Applications of SA789 S83071 Tube
S83071 tube is for high-chromium super duplex exchangers and high-yield process lines naming this UNS. Match fluid chemistry and temperature to the PREN estimate and Table 4 floors before freezing the bill of materials.
| Application area | Typical use | Selection note |
|---|---|---|
| Aggressive chloride HX | High-Cr super duplex | PREN estimate ~47 |
| High-yield process tubing | YS 98 ksi min | Compare S32750 |
| Offshore / specialty service | Beyond standard 2205 | Match exact UNS |
| Code pressure-boundary tube | SA-789 S83071 named | Keep ASME designation |
If PREN ≥41 footnote is mandatory, confirm whether SA789 S32750 is intended. For hyper duplex see SA789 S32707 or SA789 S33207. Match fluid chemistry and temperature to the PREN estimate and Table 4 floors before freezing the bill of materials.
Weldability
Welding high-Cr/Mo/N super duplex needs qualified procedures with strict heat-input and cooling control. Mill welded SA-789 product stays autogenous. Do not borrow 2205 PQRs for S83071 tube-to-tubesheet work.
SHH STEEL can discuss filler families; the fabricator owns WPS/PQR under the applicable Code. Procedure qualification on the actual UNS avoids ferrite and sigma surprises in the heat-affected zone.
Surface Finishes
Standard delivery for SA789 S83071 is heat-treated and descaled/pickled per Section 13, free of excessive mill scale. Bright anneal or Ra-controlled finishes are agreement items that must appear on the order.
SHH STEEL quotes special finishes against the written enquiry rather than assuming them with the grade stamp for S83071. Call any Ra or bright requirement out on the enquiry so mill routing can include it before the heat is reserved.
Inspection and Testing
Testing covers Table 1 chemistry, Table 4 tension and hardness, flare or flange tests by route, reverse flattening for welded tube, and hydro or NDE on each length using duplex hydrostatic factor 64000 (441.2). Manufacturer chooses hydro versus NDE unless the PO locks the method.
Marking shows seamless or welded and wall basis. SHH STEEL 3.1 MTCs tie heat, chemistry, mechanicals, heat treatment, and test method to each length for receiving clearance. Receiving teams should verify hydro-versus-NDE against the purchase order before releasing tube to fabrication.
Packaging and Shipping
S83071 tube ships from SHH STEEL in tagged bundles with end protection matched to length. Tags repeat ASME SA789, grade, route, OD × wall, heat number, and PO reference for export or domestic delivery.
Wrapped bundles or wooden cases are available for bright or small-bore material. Incoterms and MTC flow follow the order acknowledgment. Keep bundle tags legible after ocean transit so port and site receiving can proceed without remarking every length.
Why Choose SHH STEEL
SHH STEEL produces and supplies ASME SA789 UNS S83071 as manufactured high-chromium super-duplex Code Book tube, reporting chemistry and the 120/98 ksi tensile floors on the EN 10204 3.1 MTC.
If a different super or hyper duplex UNS is written, we clarify before producing. Dual marking is available on request. Honest sister-grade advice protects Code stamp integrity when a different UNS would fit the corrosion envelope better.
Supply Capability
SHH STEEL can produce and supply ASME SA789 UNS S83071 against the edition, route, and finish on your enquiry. Capability and Stock / Available sizes follow. Clear enquiry data on OD, wall, and route shortens quotation turnaround for export and domestic Code jobs.
| Item | SHH STEEL capability for S83071 |
|---|---|
| Standard | ASME SA789 / SA789M (dual A789 marking on request) |
| Grade | UNS S83071 |
| Manufacture | Seamless; welded with no filler metal |
| Size range (enquiry) | Common HX / general-service OD × wall (and BWG); other sizes by agreement |
| Wall basis | Average or minimum wall as ordered |
| Delivery condition | Heat-treated 1830–2100 °F [1000–1150 °C], rapid cooling in water or by other means |
| Testing | Heat analysis, tensile, hardness, flare/flange/reverse-flatten; hydro or NDE |
| Documents | EN 10204 3.1 MTC; third-party inspection on request |
Stock / Available sizes — Regular enquiry bands include OD about 12.7–50.8 mm with common BWG / metric walls; larger Table 5 groups by agreement. Cut lengths on request. Send OD × wall, route, and quantity — no invented tonnage lists.
List ASME SA789 UNS S83071, seamless or welded, OD × wall, wall basis, length, and quantity on the enquiry. Clear enquiry data on OD, wall, and route shortens quotation turnaround for export and domestic Code jobs.
FAQ
-
What tensile strength does SA789 S83071 require?
- Table 4 requires 120 ksi [830 MPa] minimum tensile strength, 98 ksi [680 MPa] minimum yield, 25% minimum elongation, and hardness max 300 HBW / 32 HRC / 300 HV after heat treatment. The 98 ksi yield floor is substantially higher than S32750’s 80 ksi — confirm the UNS on the datasheet.
-
What PREN should I expect from S83071?
- SA-789 does not publish a PREN footnote for S83071. Mid-range Cr ≈30, Mo ≈3.5, N ≈0.34 give PREN ≈ 47.0 using %Cr + 3.3×%Mo + 16×%N. That is an engineering estimate from stated chemistry — recalculate on actual ladle values when corrosion margin is tight.
-
How does S83071 compare with S32750?
- Both are super duplex. S83071 runs higher chromium (29–31%) and a 120/98 ksi tensile/yield pair with 25% elongation and no PREN footnote; SA789 S32750 has PREN ≥41 footnote, Cr 24–26%, and 116/80 ksi with 15% elongation. Match the UNS and footnotes on the purchase order.
-
Is ASME SA-789 the same as ASTM A789?
- No. SA-789 / SA-789M is the ASME Section II Part A Code Book adoption of duplex tubing; A789 / A789M is the ASTM product specification. The 2023 BPVC text matches A789/A789M-18 on the grade tables, but the standards remain independent. Dual-mark only when the purchase order asks for both names on stencil and MTC.
-
Does this grade include seamless and welded tube?
- Yes. SA-789 covers both manufacture routes for S83071, and welded tube is made with no filler metal in the longitudinal seam. Flaring applies to seamless lots; flange testing and reverse flattening apply to welded lots. SHH STEEL produces both routes and marks them on tube and certificate.
-
Can SHH STEEL produce SA789 S83071?
- Yes. SHH STEEL can produce and supply ASME SA789 UNS S83071 seamless and welded tube against the ordered edition, with Table 2 heat treatment, Section 9 testing, and EN 10204 3.1 documentation. Production capability is part of the offer, not trader-only brokering.
-
What heat treatment applies under SA789?
- Table 2 requires S83071 solution treatment at 1830–2100 °F [1000–1150 °C] followed by rapid cooling in water or by other means. Seamless tubes may be quenched after hot forming when temperature stays at or above the minimum solution-treatment temperature. Proper quench practice limits intermetallics and supports corrosion performance for this grade.
-
What PREN estimate follows from Table 1 chemistry?
- Unless a grade-specific footnote applies, SA-789 does not publish a PREN minimum for S83071. Using PREN = %Cr + 3.3×%Mo + 16×%N on mid-range Table 1 aims gives roughly PREN ≈ 47.0. That is an engineering estimate from stated chemistry, not a Code acceptance number; recalculate on actual ladle values when margin is tight.
-
What sizes can SHH STEEL supply?
- Common heat-exchanger OD × wall bands around 12.7–50.8 mm with usual BWG or metric walls are regularly quoted, and larger Table 5 OD groups are available by agreement. Average or minimum wall, cut lengths, and U-bends are enquiry items. Send OD, wall, length, quantity, and seamless or welded preference without relying on published fictitious stock tonnages.
-
What tests does each tube length receive?
- Each finished length receives hydrostatic or nondestructive electric testing, at the manufacturer’s option unless the purchase order fixes the method. Lot-basis tension, hardness, and flaring or flange tests also apply, and welded tube takes reverse flattening on a length basis. Name hydro-versus-NDE preference on the PO when one method must be locked in.
-
Does elevated-temperature service need extra caution?
- Yes. SA-789 notes embrittlement risk after prolonged elevated-temperature exposure, and duplex metallurgy flags 475 °C ferrite embrittlement plus sigma-phase risk from slow cooling after hot work or welding. Keep continuous-service temperature and fabrication heat practice inside the limits your materials engineer and Code design allow for S83071.
-
Where do I send an enquiry for this grade?
- Send size, quantity, seamless or welded preference, wall basis, and document needs through your SHH STEEL sales channel for a formal quotation. The conclusion of this page lists the steelspecs.com contact email for technical follow-up on ASME SA789 UNS S83071, including dual-marking or third-party inspection requests.
Conclusion
ASME SA789 UNS S83071 is supplied by SHH STEEL as seamless and welded (no filler metal) super duplex tubing under the Section II Part A Code Book product standard, heat-treated per Table 2, tested per Section 9, and certified on EN 10204 3.1 MTCs. Confirm OD × wall, wall basis, manufacture route, and any dual SA-789/A789 marking on the purchase order so stencil and certificate match the datasheet. For technical follow-up, contact admin@steelspecs.com.