Product Showcase
ASME SA 789/SA 789M Stainless Steel Products
SHH STEEL offers ASME SA789/SA789M-compliant 304/316 stainless steel tubes. ASME SA789/SA789M specifies seamless and welded duplex stainless steel tubes for high-corrosion and high-strength environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASME SA789 UNS S31500 Duplex Stainless Steel Tube
ASME SA789 UNS S31500 duplex stainless steel tube (seamless and welded, no filler metal) with Cr 18.0–19.0%, Ni 4.3–5.2%, Mo 2.50–3.00%, Si 1.40–2.00% and N 0.05–0.10%, tensile floor 92 ksi [630 MPa], yield 64 ksi [440 MPa], hardness max 290 HBW / 30 HRC, solution treated 1800–1900 °F [980–1040 °C]. SHH STEEL produces and supplies SA789 S31500 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S31260 Duplex Stainless Steel Tube
ASME SA789 UNS S31260 duplex stainless steel tube (seamless and welded, no filler metal) with Cr 24.0–26.0%, Ni 5.5–7.5%, Mo 2.5–3.5%, N 0.10–0.30%, Cu 0.20–0.80% and W 0.10–0.50%, tensile floor 100 ksi [690 MPa], yield 65 ksi [450 MPa], hardness max 290 HBW / 30 HRC, solution treated 1870–2010 °F [1020–1100 °C]. SHH STEEL produces and supplies SA789 S31260 tube with EN 10204 3.1 MTC for general corrosion and chloride SCC service under ASME Section II Part A.View More -
ASME SA789 UNS S31200 Duplex Stainless Steel Tube
ASME SA789 UNS S31200 duplex stainless steel tube (seamless and welded, no filler metal) with Cr 24.0–26.0%, Ni 5.5–6.5%, Mo 1.20–2.00% and N 0.14–0.20%, tensile floor 100 ksi [690 MPa], yield 65 ksi [450 MPa], hardness max 280 HBW / 29 HRC, solution treated 1920–2010 °F [1050–1100 °C] then water-quenched. SHH STEEL produces and supplies SA789 S31200 tube with EN 10204 3.1 MTC for general corrosion and chloride SCC service under ASME Section II Part A.View More
ASME SA 789/SA 789M Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.
Stainless Steel Pipes and Tubes
X