Product Showcase
ASME SA 789/SA 789M Stainless Steel Products
SHH STEEL offers ASME SA789/SA789M-compliant 304/316 stainless steel tubes. ASME SA789/SA789M specifies seamless and welded duplex stainless steel tubes for high-corrosion and high-strength environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASME SA789 UNS S32750 Super Duplex Stainless Steel Tube
ASME SA789 UNS S32750 super duplex stainless steel tube (seamless and welded, no filler metal) — 2507-type — with Cr 24.0–26.0%, Ni 6.0–8.0%, Mo 3.0–5.0%, N 0.24–0.32% (PREN ≥41 footnote), tensile floor 116 ksi [800 MPa], yield 80 ksi [550 MPa], elong 15% min, hardness max 300 HBW / 32 HRC, solution treated 1880–2060 °F [1025–1125 °C]. SHH STEEL produces and supplies SA789 S32750 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32707 Super Duplex Stainless Steel Tube
ASME SA789 UNS S32707 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 26.0–29.0%, Ni 5.5–9.5%, Mo 4.0–5.0%, N 0.30–0.50%, Co 0.5–2.0%, tensile floor 133 ksi [920 MPa], yield 101 ksi [700 MPa], hardness max 318 HBW / 34 HRC, solution treated 1975–2050 °F [1080–1120 °C]. SHH STEEL produces and supplies SA789 S32707 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32550 Super Duplex Stainless Steel Tube
ASME SA789 UNS S32550 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 24.0–27.0%, Ni 4.5–6.5%, Mo 2.9–3.9%, N 0.10–0.25%, Cu 1.50–2.50%, tensile floor 110 ksi [760 MPa], yield 80 ksi [550 MPa], elong 15% min, hardness max 297 HBW / 31 HRC, solution treated 1900 °F [1040 °C] min. SHH STEEL produces and supplies SA789 S32550 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32520 Super Duplex Stainless Steel Tube
ASME SA789 UNS S32520 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 23.0–25.0%, Ni 5.5–8.0%, Mo 3.0–5.0%, N 0.20–0.35%, Cu 0.50–3.00%, tensile floor 112 ksi [770 MPa], yield 80 ksi [550 MPa], hardness max 310 HBW / 32 HRC, solution treated 1975–2050 °F [1080–1120 °C]. SHH STEEL produces and supplies SA789 S32520 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32506 Duplex Stainless Steel Tube
ASME SA789 UNS S32506 duplex stainless steel tube (seamless and welded, no filler metal) with Cr 24.0–26.0%, Ni 5.5–7.2%, Mo 3.0–3.5%, N 0.08–0.20%, W 0.05–0.30%, tensile floor 90 ksi [620 MPa], yield 65 ksi [450 MPa], elong 18% min, hardness max 302 HBW / 32 HRC, solution treated 1870–2050 °F [1020–1120 °C]. SHH STEEL produces and supplies SA789 S32506 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32304 Lean Duplex Stainless Steel Tube
ASME SA789 UNS S32304 lean duplex stainless steel tube (seamless and welded, no filler metal) — 2304-type — with Cr 21.5–24.5%, Ni 3.0–5.5%, Mo 0.05–0.60%, N 0.05–0.20% and Cu 0.05–0.60%, OD-dependent tensile floors, hardness per Table 4, solution treated 1700–1920 °F [925–1050 °C]. SHH STEEL produces and supplies SA789 S32304 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32205 Duplex Stainless Steel Tube
ASME SA789 UNS S32205 duplex stainless steel tube (seamless and welded, no filler metal) — the modern 2205 row — with Cr 22.0–23.0%, Ni 4.5–6.5%, Mo 3.0–3.5% and N 0.14–0.20%, tensile floor 95 ksi [655 MPa], yield 70 ksi [485 MPa], hardness max 290 HBW / 30 HRC, solution treated 1870–2010 °F [1020–1100 °C]. SHH STEEL produces and supplies SA789 S32205 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32202 Lean Duplex Stainless Steel Tube
ASME SA789 UNS S32202 lean duplex stainless steel tube (seamless and welded, no filler metal) with Cr 21.5–24.0%, Ni 1.00–2.80%, Mo 0.45 max, N 0.18–0.26%, tensile floor 94 ksi [650 MPa], yield 65 ksi [450 MPa], hardness max 290 HBW / 30 HRC, solution treated 1870–1975 °F [1020–1080 °C]. SHH STEEL produces and supplies SA789 S32202 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32101 Lean Duplex Stainless Steel Tube
ASME SA789 UNS S32101 lean duplex stainless steel tube (seamless and welded, no filler metal) with Cr 21.0–22.0%, Ni 1.35–1.70%, Mn 4.0–6.0%, Mo 0.10–0.80% and N 0.20–0.25%, wall-dependent tensile (101/77 ksi ≤0.187 in. wall; 94/65 ksi above), hardness max 290 HBW / 30 HRC, solution treated at 1870 °F [1020 °C] min. SHH STEEL produces and supplies SA789 S32101 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32003 Lean Duplex Stainless Steel Tube
ASME SA789 UNS S32003 lean duplex stainless steel tube (seamless and welded, no filler metal) with Cr 19.5–22.5%, Ni 3.0–4.0%, Mo 1.50–2.00% and N 0.14–0.20%, wall-dependent tensile floors (100/70 ksi ≤0.187 in. wall; 95/65 ksi above), hardness max 290 HBW / 30 HRC, solution treated 1850–2050 °F [1010–1120 °C]. SHH STEEL produces and supplies SA789 S32003 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S32001 Lean Duplex Stainless Steel Tube
ASME SA789 UNS S32001 lean duplex stainless steel tube (seamless and welded, no filler metal) with Cr 19.5–21.5%, Ni 1.0–3.0%, Mn 4.00–6.00%, Mo 0.60 max and N 0.05–0.17%, tensile floor 90 ksi [620 MPa], yield 65 ksi [450 MPa], hardness max 290 HBW / 30 HRC, solution treated 1800–1950 °F [982–1066 °C]. SHH STEEL produces and supplies SA789 S32001 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More -
ASME SA789 UNS S31803 Duplex Stainless Steel Tube
ASME SA789 UNS S31803 duplex stainless steel tube (seamless and welded, no filler metal) with Cr 21.0–23.0%, Ni 4.5–6.5%, Mo 2.5–3.5% and N 0.08–0.20%, tensile floor 90 ksi [620 MPa], yield 65 ksi [450 MPa], hardness max 290 HBW / 30 HRC, solution treated 1870–2010 °F [1020–1100 °C]. SHH STEEL produces and supplies SA789 S31803 tube with EN 10204 3.1 MTC under ASME Section II Part A.View More
ASME SA 789/SA 789M Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.
Stainless Steel Pipes and Tubes
X