EN 10025-4 S460ML Steel Plate | S460ML Fine Grain Structural Steel
What is EN 10025-4 S460ML Steel Plate?
As a professional steel plate supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present EN 10025-4 S460ML Steel Plate (Material Number: 1.8838).
S460ML is a thermomechanically rolled (TMCP) weldable fine-grain structural steel under the European standard EN 10025-4. It provides a minimum yield strength of 460 MPa (for thickness ≤ 16 mm) and is impact tested at –50°C with a minimum energy of 27 J. This is one of the highest strength low-temperature grades in the EN 10025-4 series, combining high load-bearing capacity with excellent toughness in cold environments. SHH STEEL sources this material directly from leading Chinese steel mills, ensuring competitive mill-direct pricing, stable quality and reliable delivery.
We supply S460ML steel plate in thicknesses from 6 mm to 120 mm (thicker plates available on request), widths up to 3000–4000 mm, and lengths up to 12000–18000 mm. Custom cutting, shot blasting and priming services are available. All plates are delivered with full Mill Test Certificates (EN 10204 3.1).
Material Specification
EN 10025-4 S460ML steel plate is produced in accordance with EN 10025-4.
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Primary Standard | EN 10025-4 | Full compliance |
| Steel Grade | S460ML (1.8838) | Confirmed |
| Delivery Condition | Thermomechanically rolled (M) | Confirmed |
| Product Form | Steel Plate | Available |
| Thickness Range | 6 mm – 120 mm | Custom sizes available |
| Width / Length | Up to 3000–4000 mm / 12000–18000 mm | Custom cutting supported |
| Certification | EN 10204 3.1 / 3.2 | Available |
Chemical Composition
According to EN 10025-4, the chemical composition is specified for both ladle analysis (cast analysis) and product analysis.
Ladle Analysis (Cast Analysis)
| Element | Max. / Range (%) |
|---|---|
| Carbon (C) | ≤ 0.16 |
| Silicon (Si) | ≤ 0.60 |
| Manganese (Mn) | ≤ 1.70 |
| Phosphorus (P) | ≤ 0.025 |
| Sulfur (S) | ≤ 0.020 |
| Niobium (Nb) | ≤ 0.05 |
| Vanadium (V) | ≤ 0.12 |
| Aluminium (Al total) | ≥ 0.020 |
| Titanium (Ti) | ≤ 0.05 |
| Chromium (Cr) | ≤ 0.30 |
| Nickel (Ni) | ≤ 0.80 |
| Molybdenum (Mo) | ≤ 0.20 |
| Copper (Cu) | ≤ 0.55 |
| Nitrogen (N) | ≤ 0.025 |
Product Analysis
| Element | Max. / Range (%) |
|---|---|
| Carbon (C) | ≤ 0.18 |
| Silicon (Si) | ≤ 0.65 |
| Manganese (Mn) | ≤ 1.80 |
| Phosphorus (P) | ≤ 0.030 |
| Sulfur (S) | ≤ 0.025 |
| Niobium (Nb) | ≤ 0.06 |
| Vanadium (V) | ≤ 0.14 |
| Aluminium (Al total) | ≥ 0.015 |
| Titanium (Ti) | ≤ 0.06 |
| Chromium (Cr) | ≤ 0.35 |
| Nickel (Ni) | ≤ 0.85 |
| Molybdenum (Mo) | ≤ 0.23 |
| Copper (Cu) | ≤ 0.60 |
| Nitrogen (N) | ≤ 0.027 |
Note:
- The minimum Al content does not apply if sufficient other nitrogen-binding elements are present.
- Carbon Equivalent (CEV) is controlled to ensure good weldability.
Mechanical Properties
Mechanical properties of EN 10025-4 S460ML (longitudinal direction):
| Thickness (mm) | Yield Strength ReH (min) | Tensile Strength Rm | Elongation A (min) | Impact Energy KV (min) |
|---|---|---|---|---|
| ≤ 16 | 460 MPa | 540 – 720 MPa | 17% | 27 J at –50°C |
| > 16 ≤ 40 | 440 MPa | 540 – 720 MPa | 17% | 27 J at –50°C |
| > 40 ≤ 63 | 430 MPa | 530 – 710 MPa | 17% | 27 J at –50°C |
| > 63 ≤ 80 | 410 MPa | 510 – 690 MPa | 17% | 27 J at –50°C |
| > 80 ≤ 100 | 400 MPa | 500 – 680 MPa | 17% | 27 J at –50°C |
| > 100 ≤ 120 | 385 MPa | 490 – 660 MPa | 17% | 27 J at –50°C |
Density: 7.85 g/cm³
Delivery Conditions
SHH STEEL, as a China Mill-Direct Supplier, supplies EN 10025-4 S460ML steel plate in the thermomechanically rolled (M) condition.
Additional options:
- Shot blasting and shop primer
- Ultrasonic testing (EN 10160)
- Z-direction testing (Z15 / Z25 / Z35)
- Third-party inspection (SGS, BV, TUV, etc.)
Tolerances
Dimensional tolerances for S460ML steel plate follow EN 10029 (for plates).
- Thickness, width and length tolerances according to the ordered class.
- Flatness according to EN 10029.
- Edge conditions: Mill edge or cut edge (flame / plasma).
Tighter tolerances can be provided upon request.
Weldability
S460ML has moderate-to-good weldability for a high-strength thermomechanically rolled fine-grain steel. It can be welded by conventional methods (SMAW, GMAW, FCAW, SAW).
Recommended welding consumables:
| Welding Process | Recommended Consumables |
|---|---|
| SMAW (Stick) | E8018, E7018 |
| GMAW (MIG/MAG) | ER80S-D2, ER70S-6 |
| FCAW | E81T1, E71T-1 |
| SAW | EH14 / EM12K + suitable flux |
Preheating is generally required for thicker plates. Low-hydrogen consumables and strict control of heat input are strongly recommended, especially for low-temperature service.
Equivalent Material Grades
| Grade | Standard | Notes |
|---|---|---|
| S460ML | EN 10025-4 | — |
| 1.8838 | EN | Material number |
| Q460ML / Q460ME | GB/T 1591 | Closest Chinese equivalents |
| A572 Grade 65 / A633 (approx.) | ASTM | Similar strength / toughness concept |
| TStE 460 TM | DIN (old) | Former designation |
Applications
EN 10025-4 S460ML is used in structural applications requiring very high strength and excellent low-temperature toughness. Typical uses include:
| Application Area | Typical Components / Uses (Keywords) |
|---|---|
| Building Structures | Heavy beams, columns in cold regions – S460ML Structural Steel |
| Bridges | Bridge components – S460ML Bridge |
| Offshore & Marine | Heavy structural components – S460ML Offshore |
| Machinery | Heavy equipment frames – S460ML Machinery |
| Low-Temperature Construction | High-strength structures requiring –50°C toughness – S460ML Construction |
| General Fabrication | Critical high-strength fine-grain structures – S460ML Fabrication |
Why Choose SHH STEEL
SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level (primary) agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, stable and traceable quality, and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-4 S460ML Steel Plate.
Customers benefit from reliable supply, short lead times and cost-effective solutions for high-strength thermomechanically rolled fine-grain low-temperature structural steel projects worldwide. Our professional export team provides technical support and customized processing services to meet project requirements.
FAQ
-
What does the “ML” in S460ML mean?
- “M” indicates thermomechanically rolled condition, and “L” indicates impact tested at –50°C with a minimum of 27 J.
-
What is the difference between S460M and S460ML?
- Both are thermomechanically rolled. S460M is impact tested at –20°C (40 J), while S460ML is impact tested at –50°C (27 J), providing better low-temperature toughness.
-
What is the material number of S460ML?
- 1.8838
-
Is S460ML suitable for low-temperature high-strength applications?
- Yes. With a minimum yield strength of 460 MPa and guaranteed impact toughness at –50°C, S460ML is ideal for demanding structural applications in cold environments.
Conclusion
EN 10025-4 S460ML (1.8838) Steel Plate from SHH STEEL is a high-strength thermomechanically rolled fine-grain structural steel offering 460 MPa yield strength and excellent toughness at –50°C. As a China Mill-Direct Exporter, we provide competitive pricing, fast delivery and consistent quality backed by full mill certifications. Trust SHH STEEL for your S460ML fine grain structural steel plate requirements.