EN 10025-6 S460QL1 Steel Plate | S460QL1 QT High Structural Steel - SHH STEEL

EN 10025-6 S460QL1 Steel Plate | S460QL1 QT High Structural Steel

EN 10025-6 S460QL1 is a quenched and tempered high-strength structural steel plate with a minimum yield strength of 460 MPa and superior impact toughness at –60°C. It is designed for heavily loaded structures operating in extremely low-temperature environments. SHH STEEL supplies this grade as a China Mill-Direct Exporter with full mill certification and competitive pricing.
Equivalent Grades:
ASTM A514 Gr P (-60℃ CVN) / JIS SHT60 (L1 ref) / GB Q460CF-E / ISO E460QL1
Material Specification:
EN 10025-6 — Delivery: Quenched & Tempered (Q+T)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Tolerances
Weldability
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10025-6 S460QL1 Steel Plate?

SHH STEEL is a professional China Mill-Direct Exporter of high-strength structural steel plates. We are pleased to offer EN 10025-6 S460QL1 Steel Plate (Material Number 1.8916), a quenched and tempered grade engineered for the most demanding structural applications that require both high strength and exceptional low-temperature toughness.

S460QL1 belongs to the family of EN 10025-6 steel plate products covering high-yield-strength steels in the quenched and tempered condition. The “QL1” designation indicates the most stringent impact requirement within the S460 series, with testing performed at –60°C. This makes the grade particularly suitable for structures exposed to arctic or extremely cold service conditions. After quenching and tempering, the steel develops a fine-grained tempered microstructure that delivers a minimum yield strength of 460 MPa (up to 50 mm thickness) together with high Charpy-V toughness at very low temperature.

SHH STEEL supplies S460QL1 plates in thicknesses ranging from 6 mm to 150 mm, widths up to 3000–4000 mm and lengths up to 12000–18000 mm. Custom cutting, ultrasonic testing, surface treatment and third-party inspection services are available. Every plate is delivered with a full EN 10204 3.1 Mill Test Certificate, ensuring complete traceability from the producing mill.

Material Specification

Parameter Requirement / Availability
Governing Standard EN 10025-6
Steel Designation S460QL1 (1.8916)
Delivery Condition Quenched and Tempered (Q)
Product Form Flat steel plate
Thickness Range 6 mm – 150 mm (thicker plates on request)
Width / Length Up to 3000–4000 mm / 12000–18000 mm
Certification EN 10204 3.1 / 3.2
Additional Testing UT, Z-test, third-party inspection available

Chemical Composition

Chemical composition is controlled in accordance with EN 10025-6 for both ladle (heat) analysis and product analysis. The QL1 grade features tighter limits on phosphorus and sulphur to support superior low-temperature toughness.

Ladle Analysis (Cast Analysis)

Element Maximum (%)
Carbon (C) 0.20
Silicon (Si) 0.80
Manganese (Mn) 1.70
Phosphorus (P) 0.020
Sulfur (S) 0.010
Chromium (Cr) 1.50
Nickel (Ni) 2.00
Molybdenum (Mo) 0.70
Copper (Cu) 0.50
Niobium (Nb) 0.06
Vanadium (V) 0.12
Titanium (Ti) 0.05
Boron (B) 0.005
Nitrogen (N) 0.015

Product Analysis

Element Maximum (%)
Carbon (C) 0.22
Silicon (Si) 0.86
Manganese (Mn) 1.80
Phosphorus (P) 0.025
Sulfur (S) 0.012
Chromium (Cr) 1.60
Nickel (Ni) 2.10
Molybdenum (Mo) 0.74
Copper (Cu) 0.55
Niobium (Nb) 0.07
Vanadium (V) 0.14
Titanium (Ti) 0.06
Boron (B) 0.006
Nitrogen (N) 0.016

The restricted impurity levels and controlled alloying contribute to the excellent toughness performance at –60°C while maintaining acceptable weldability after quenching and tempering.

Mechanical Properties

Nominal Thickness (mm) Min. Yield Strength ReH Tensile Strength Rm Min. Elongation A Impact Energy (longitudinal)
≤ 50 460 MPa 550 – 720 MPa 17 % 30 J at –60 °C
50 < t ≤ 100 440 MPa 550 – 720 MPa 17 % 30 J at –60 °C
100 < t ≤ 150 400 MPa 500 – 670 MPa 17 % 30 J at –60 °C

Density is approximately 7.85 g/cm³. Transverse impact values are also specified in the standard and can be provided when required by the project.

Delivery Conditions

All S460QL1 plates are supplied in the quenched and tempered condition as required by EN 10025-6. The quenching and tempering heat treatment is carefully controlled to achieve the required combination of high strength and exceptional low-temperature toughness.

Additional processing options available from SHH STEEL:

  • Shot blasting and shop primer application
  • Ultrasonic testing in accordance with EN 10160
  • Through-thickness (Z-direction) testing to Z15, Z25 or Z35
  • Independent third-party inspection (SGS, BV, TUV, Lloyd’s Register, etc.)
  • Precision cutting (flame, plasma or water-jet)

Tolerances

Dimensional tolerances are in accordance with EN 10029. Customers may select the required class for thickness, width, length and flatness. Both mill edges and cut edges (flame or plasma) can be supplied according to project requirements. Tighter tolerances are available by special agreement.

Weldability

S460QL1 is a high-strength quenched and tempered steel. Successful welding requires careful attention to preheating, heat input and the selection of low-hydrogen consumables in order to preserve toughness in the heat-affected zone, especially for low-temperature service.

Recommended welding consumables:

Welding Process Suggested Consumables
SMAW (Stick) E8018-G, E7018, E8018-C3
GMAW / MAG ER80S-G, ER70S-6, ER80S-Ni1
FCAW E81T1-Ni1, E71T-1, E81T1-K2
SAW Matching high-strength wire and flux combinations

Preheating is normally required for thicker plates. Interpass temperature should be strictly controlled, and post-weld heat treatment may be considered for critical applications operating at very low temperatures.

Equivalent Material Grades

Grade Standard Remarks
S460QL1 EN 10025-6 Primary designation
1.8916 EN Material number
Q460F GB/T 1591 Closest Chinese equivalent
Selected A514 / A517 grades ASTM Similar quenched & tempered concept
TStE 460 V Former DIN Historical related grade

Applications

Application Area Typical Components / Keywords
Heavy Construction Crane booms, heavy frames, high-load columns – S460QL1 Structural Steel
Bridge Engineering Main girders, support structures in cold regions – S460QL1 Bridge
Mining & Earthmoving Equipment Chassis, boom structures – S460QL1 Mining
Offshore & Arctic Structures Platform components, lifting equipment – S460QL1 Offshore
Extreme Low-Temperature Service Structures requiring –60°C toughness – S460QL1 Low Temperature
Energy & Power Wind turbine components, heavy fabrications – S460QL1 Energy
General Heavy Fabrication Critical high-strength welded assemblies – S460QL1 Fabrication

Why Choose SHH STEEL

SHH STEEL is a China Mill-Direct Exporter. We maintain long-term strategic cooperation with major Chinese steel mills and act as a first-level agent. This direct supply model allows us to offer competitive mill-direct pricing, shorter lead times, consistent quality and full Mill Test Certificates (EN 10204 3.1 / 3.2) for EN 10025-6 S460QL1 Steel Plate.

Our experienced export and technical teams provide support on material selection, welding procedures, cutting and processing. Customers benefit from reliable supply and professional service for high-strength quenched and tempered steel projects requiring superior low-temperature performance.

FAQ

What does “QL1” mean in S460QL1?
“Q” indicates the quenched and tempered condition, while “L1” means the steel meets the highest impact energy requirements at –60°C within the S460 series.
What is the difference between S460QL and S460QL1?
Both grades have the same strength level. S460QL is impact tested at –40°C, whereas S460QL1 is tested at –60°C and is intended for more severe low-temperature service.
What is the material number of S460QL1?
1.8916
Can SHH STEEL supply S460QL1 with Z-direction testing?
Yes. Z15, Z25 and Z35 testing can be arranged according to project requirements.

Conclusion

EN 10025-6 S460QL1 (1.8916) quenched and tempered steel plate from SHH STEEL combines high yield strength of 460 MPa with outstanding toughness at –60°C. As a China Mill-Direct Exporter, we provide competitive pricing, reliable quality and full technical support. Contact SHH STEEL today for stock availability, pricing or processing services.

EN 10025-6 S460QL1 Steel Plate, S460QL1 steel plate, S460QL1 QT, EN 10025 S460QL1, S460QL1 equivalent, S460QL1 supplier, 1.8916

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X