ASME SA387 Grade 12 Class 2 (SA387 Gr 12 Cl 2) Steel Plate
What is ASME SA387 Grade 12 Class 2?
ASME SA387 Grade 12 Class 2 (SA387 Gr 12 Cl 2) alloy steel plates are a premium chrome-moly grade in the ASME SA387 specification. Unlike Class 1, which is normalized for moderate strength, Class 2 is quenched and tempered, providing higher tensile strength (515–690 MPa) and yield strength (minimum 345 MPa) with superior creep resistance.
The plates are manufactured using quenching and tempering heat treatment, which refines the microstructure for enhanced toughness and durability at elevated temperatures, making them ideal for boilers, pressure vessels, and petrochemical equipment under demanding high-heat conditions.
SHH STEEL supplies ASME SA387 Grade 12 Class 2 plates in a wide size range from 6mm to 100mm thickness, up to 4600mm width, and up to 12000mm length, meeting both ASME Section VIII pressure vessel code and customer-specific requirements.
Material Specification
As a production and export expert at SHH STEEL, we can confirm that ASME SA387 Grade 12 Class 2 alloy steel plates are governed by ASME SA-387/SA-387M, the standard for pressure vessel plates, alloy steel, chromium-molybdenum.
This specification outlines requirements for quenched and tempered plates for elevated temperature service, ensuring suitability for welded pressure vessels and boilers. SHH STEEL complies fully with this standard, providing plates in quenched and tempered conditions to optimize mechanical properties.
The specification supports thicknesses from 6mm to 100mm, widths up to 4600mm, and lengths to 12000mm, with custom dimensions available for vessel designs. Ultrasonic examination per ASME SA-578 Class 1 detects laminations, guaranteeing defect-free material, while dual certification with ASTM A387 Gr 12 Cl 2 or EN 10028-2 is offered for international compatibility.
This makes our ASME SA387 Gr 12 Cl 2 plates a reliable choice for global buyers, supported by mill test certificates for complete traceability.
| Specification Element | Requirement | SHH STEEL Compliance | Keywords |
| Primary Standard | ASME SA-387/SA-387M | ASME Section VIII | SA387 Gr 12 Cl 2 specification |
| Thickness Range | 6mm-100mm (custom) | Mill Test Certificate | SA387 Gr 12 Cl 2 dimensions |
| Width/Length | Up to 4600mm / 12000mm | Custom fabrication available | SA387 Gr 12 Cl 2 size options |
| Ultrasonic Testing | No laminations >0.25% thickness | Class 1 per ASME SA-578 | SA387 Gr 12 Cl 2 inspection |
| Heat Treatment | Quenched and tempered | 870-900°C quench, 620-650°C temper | SA387 Gr 12 Cl 2 heat treat |
Chemical Composition
At SHH STEEL, we ensure the chemical composition of ASME SA387 Grade 12 Class 2 is tightly controlled per ASME SA-387/SA-387M to guarantee elevated temperature stability and weldability.
The maximum carbon content is 0.20%, preventing brittleness, while manganese (0.30-0.60%) and silicon (0.15-0.40%) enhance strength and deoxidation. Phosphorus and sulfur are capped at 0.025% each to minimize cracking, chromium (0.80-1.25%) and molybdenum (0.15-0.30%) provide creep resistance.
Our testing per ASME SA-350 maintains a Carbon Equivalent (CE) ≤0.45 per AWS D1.1. Melt analysis (heat analysis) and product analysis differ slightly with tolerances. Melt analysis is stricter for ladle chemistry, while product analysis allows variation for finished plates.
This ensures consistency, making ASME SA387 Gr 12 Cl 2 plates a reliable choice for buyers searching for “ASME SA387 Gr 12 Cl 2 chemical composition.”
| Element | Melt Analysis (%) | Product Analysis (%) | Standard Limit | Test Method | Role | Keywords |
| Carbon (C) | 0.05-0.20 | 0.04-0.21 | 0.20 max | ASME SA-350 | Strength without brittleness | SA387 Gr 12 Cl 2 carbon |
| Manganese (Mn) | 0.30-0.60 | 0.27-0.66 | 0.30-0.60 | ASME SA-350 | Toughness, hardenability | SA387 Gr 12 Cl 2 manganese |
| Phosphorus (P) | ≤0.025 | ≤0.025 | 0.025 max | ASME SA-350 | Reduces brittleness | SA387 Gr 12 Cl 2 phosphorus |
| Sulfur (S) | ≤0.025 | ≤0.025 | 0.025 max | ASME SA-350 | Improves weldability | SA387 Gr 12 Cl 2 sulfur |
| Silicon (Si) | 0.15-0.40 | 0.13-0.45 | 0.15-0.40 | ASME SA-350 | Deoxidation, fluidity | SA387 Gr 12 Cl 2 silicon |
| Chromium (Cr) | 0.80-1.25 | 0.75-1.31 | 0.80-1.25 | ASME SA-350 | Corrosion resistance | SA387 Gr 12 Cl 2 chromium |
| Molybdenum (Mo) | 0.15-0.30 | 0.13-0.33 | 0.15-0.30 | ASME SA-350 | Creep resistance | SA387 Gr 12 Cl 2 molybdenum |
Mechanical Properties
As a production and export expert at SHH STEEL, we can assure you that ASME SA387 Grade 12 Class 2 pressure vessel steel plates deliver strong mechanical properties, tested per ASME SA-370 for tensile/yield, ASME SA-23 for impact, and ASME SA-466 for fatigue.
With a minimum yield strength of 345 MPa and tensile range of 485-620 MPa, these plates support high load-bearing capacity, while 19% elongation ensures ductility for forming. The impact energy of 27J typical prevents brittle failure, and the modulus of elasticity (200 GPa) provides structural stability.
The fatigue limit (230 MPa est.) varies with surface finish, optimized by our grinding process. This makes ASME SA387 Gr 12 Cl 2 plates a reliable choice for buyers searching for “ASME SA387 Gr 12 Cl 2 mechanical properties.”
| Property | Value | Test Method | Temperature (°C) | Thickness Effect | Keywords |
| Tensile Strength | 485-620 MPa | ASME SA-370 | Ambient | -5% >100mm | SA387 Gr 12 Cl 2 tensile |
| Yield Strength | 345 MPa (min) | ASME SA-370 | Ambient | Stable to 100mm | SA387 Gr 12 Cl 2 yield |
| Elongation | 19% (min) | ASME SA-370 | Ambient | 17-21% (6-25mm) | SA387 Gr 12 Cl 2 elongation |
| Impact Energy | 27J typical | ASME SA-23 | Ambient | All thicknesses | SA387 Gr 12 Cl 2 impact |
| Modulus of Elasticity | 200 GPa | ASME SA-111 | Ambient | Constant | SA387 Gr 12 Cl 2 modulus |
| Fatigue Limit | 230 MPa (est.) | ASME SA-466 | Ambient | Varies with surface | SA387 Gr 12 Cl 2 fatigue |
Heat Treatment
SHH STEEL provides ASME SA387 Gr 12 Cl 2 plates in quenched and tempered condition as standard, quenched at 870-900°C and tempered at 620-650°C to achieve higher strength and toughness for elevated temperature applications.
| Factor | Value/Condition | Standard | Recommended | Keywords |
| Heat Treatment | Quench 870-900°C, Temper 620-650°C | ASME SA387 | Q&T standard | SA387 Gr 12 Cl 2 heat treat |
Delivery
Plates are delivered with normalized options for flexibility, including heat numbers for traceability. Our global shipping ensures timely delivery, with 3-7 days to Asia for standard orders.
| Factor | Value/Condition | Standard | Recommended | Keywords |
| Delivery Condition | Quenched & Tempered | ASME SA-20 | Transit 3-7 days Asia | SA387 Gr 12 Cl 2 delivery |
Tolerances
We maintain strict tolerances per ASME SA-20: thickness ±1.5mm for <40mm and ±2.0mm for thicker up to 100mm; width/length ±10mm (or ±5mm custom); flatness 3mm per meter. EN 10029 Class B available for European compatibility.
| Factor | Value/Condition | Standard | Recommended | Keywords |
| Thickness Tolerance (<40mm) | ±1.5mm | ASME SA-20 | 6-40mm | SA387 Gr 12 Cl 2 tolerance |
| Flatness | 3mm per meter | ASME SA-20 | All | SA387 Gr 12 Cl 2 flatness |
Weldability
ASME SA387 Gr 12 Cl 2 is highly weldable with low CE ≤0.45 per AWS D1.1. SHH STEEL recommends preheating at 150-200°C for thicknesses over 25mm to prevent hydrogen-induced cracking, with post-weld heat treatment (PWHT) at 620-650°C for stress relief. Supported processes include GTAW, SMAW, and GMAW with E7018 filler (AWS A5.1), achieving 90-95% joint efficiency per ASME Section IX. Low sulfur (≤0.025%) reduces hot shortness, and 19% elongation ensures ductility. Testing includes bend tests (ASTM E190) for 3t radius and ultrasonic for weld integrity per ASTM A435.
| Weldability Factor | Value/Condition | Standard | Recommended Process | Keywords |
| Carbon Equivalent (CE) | ≤0.45 | AWS D1.1 | GTAW, SMAW | SA387 Gr 12 Cl 2 weldability |
| Preheating (°C) | 150-200 (>25mm) | ASME Section IX | GMAW | SA387 Gr 12 Cl 2 welding |
| PWHT (°C) | 620-650 | ASME SA-20 | All | SA387 Gr 12 Cl 2 heat treat |
| Filler Metal | E7018 | AWS A5.1 | SMAW | SA387 Gr 12 Cl 2 welding rod |
| Bend Test Radius (mm) | 3t (t=thickness) | ASTM E190 | All | SA387 Gr 12 Cl 2 bend test |
Equivalent Grades
Global equivalents for ASME SA387 Gr 12 Cl 2 facilitate international projects, offering similar tensile and yield properties for pressure vessel use. For example, 10CrMo9-10 (EN 10028-2) is a European equivalent with 480-630 MPa tensile and 280 MPa yield, suitable for EU boilers. STBA24 (JIS G4109) serves Japanese applications with 480-630 MPa tensile and 280 MPa yield, ideal for high-strength vessels. 10CrMo910 (GB/T 713) is the Chinese standard equivalent, providing 480-630 MPa tensile and 280 MPa yield for cost-effective high-temperature equipment in Asian markets. These equivalents ensure cross-compatibility, allowing buyers to substitute ASME SA387 Gr 12 Cl 2 plates seamlessly in global supply chains.
| Grade | Standard | Tensile (MPa) | Yield (MPa) | Elongation (%) | Impact (J @ -20°C) | Keywords |
| SA387 Gr 12 Cl 2 | ASME SA-387/SA-387M | 515-690 | 345 | 19 | 27 | SA387 Gr 12 Cl 2 equivalent |
| 10CrMo9-10 | EN 10028-2 | 480-630 | 280 | 20 | 27 | SA387 Gr 12 Cl 2 EN grade |
| STBA24 | JIS G4109 | 480-630 | 280 | 20 | 27 | SA387 Gr 12 Cl 2 JIS grade |
| 10CrMo910 | GB/T 713 | 480-630 | 280 | 19 | 27 | SA387 Gr 12 Cl 2 GB grade |
| A387 Gr.12 Cl.2 | ASTM A387 | 515-690 | 345 | 19 | 34 | SA387 Gr 12 Cl 2 alternative |
| A516 Gr.60 | ASTM A516 | 415-550 | 220 | 21 | 27 | SA387 Gr 12 Cl 2 similar alt |
Supplementary Requirements
Supplementary requirements for ASME SA387 Gr 12 Cl 2 pressure vessel steel plates enhance performance for specialized applications. They offer buyers tailored options.
These include ultrasonic testing (Class 1 per ASTM A435 for no laminations >0.25% thickness). Charpy impact at -50°C (27J min per ASTM A20 for cold service) is another. Heat analysis per heat number (ASTM E350 for traceability) ensures quality. Product analysis allows ±0.02% tolerance on elements. Shot blasting to Sa 2.5 (50-100μm profile per ISO 8501-1) is available for surface preparation.
SHH STEEL provides these to meet stringent needs. Buyers search for “SA387 Gr 12 Cl 2 supplementary requirements.”
| Requirement | Detail | Standard | Test Frequency | Applicable Thickness (mm) | Keywords |
| Ultrasonic Testing | Class 1, no laminations | ASTM A435 | Full plate | 6-100 | SA387 Gr 12 Cl 2 ultrasonic |
| Charpy Impact | -50°C, 27J min | ASTM A20 | Per heat | 6-100 | SA387 Gr 12 Cl 2 cold impact |
| Heat Analysis | Per heat number | ASTM E350 | Each batch | All | SA387 Gr 12 Cl 2 analysis |
| Product Analysis | ±0.02% tolerance | ASTM E350 | Sample per lot | All | SA387 Gr 12 Cl 2 product test |
| Shot Blasting | Sa 2.5, 50-100μm profile | ISO 8501-1 | On request | 6-50 | SA387 Gr 12 Cl 2 blasting |
Applications
ASME SA387 Gr 12 Cl 2 pressure vessel steel plates are versatile for elevated-temperature and pressure environments. They have good toughness and formability.
| Application | Temperature (°C) | Pressure (bar) | Thickness (mm) | Standard Compliance | Keywords |
| Pressure Vessels | Up to 550 | 400 | 20-100 | ASME Section VIII | SA387 Gr 12 Cl 2 vessels |
| Boilers | Up to 550 | 300 | 10-50 | ASME Section I | SA387 Gr 12 Cl 2 boilers |
| Heat Exchangers | Up to 500 | 200 | 6-30 | TEMA Standards | SA387 Gr 12 Cl 2 heat exchange |
| Storage Tanks | Up to 450 | 150 | 30-80 | API 650 | SA387 Gr 12 Cl 2 tanks |
| Steam Drums | Up to 550 | 350 | 20-60 | ASME Section VIII | SA387 Gr 12 Cl 2 steam drums |
Details: Pressure vessels benefit from 515-690 MPa tensile at 550°C. Boilers handle 550°C with 19% elongation for forming. Heat exchangers use 6-30mm plates for 200 bar at 500°C. Storage tanks leverage 30-80mm for 150 bar at 450°C per API 650. Steam drums utilize 20-60mm plates for 350 bar at 550°C, per ASME Section VIII for efficient steam generation.
Why Choose SHH STEEL
SHH STEEL offers ASME and ASTM-certified SA387 Gr 12 Cl 2 plates. We provide custom thicknesses up to 300mm. Heat treatments are tailored to your project. Our 15-year track record includes zero defect deliveries to 50+ countries. This is backed by SGS verification and mill test certificates.
| Advantage | Benefit | Keywords |
| Expert Certification | ASME Section VIII compliant | SA387 Gr 12 Cl 2 certified |
| Custom Fabrication | Up to 300mm thickness | SA387 Gr 12 Cl 2 custom |
| Proven Reliability | 50+ countries, zero rejects | SA387 Gr 12 Cl 2 trusted supplier |
FAQ
-
What is ASME SA387 Grade 12 Class 2 used for?
- ASME SA387 Grade 12 Class 2 is widely used for high-temperature pressure vessels, boilers, and heat exchangers in power generation and petrochemical industries. It handles temperatures up to 550°C and pressures to 400 bar, with 515-690 MPa tensile strength ensuring reliability. SHH STEEL supplies these for welded constructions per ASME Section VIII Division 1.
-
What is the difference between SA387 Gr 12 Cl 1 and SA387 Gr 12 Cl 2?
- SA387 Gr 12 Cl 1 is normalized with 275 MPa yield for standard service, while Gr 12 Cl 2 is quenched and tempered with 345 MPa yield for higher strength. SHH STEEL recommends Gr 12 Cl 1 for moderate loads.
-
What is the chemical composition of SA387 Gr 12 Cl 2?
- The composition includes C 0.05-0.17%, Mn 0.40-0.65%, P ≤0.025%, S ≤0.025%, Si 0.50-0.80%, Cr 1.00-1.50%, Mo 0.45-0.65%, tested per ASME SA-350. This alloyed formula ensures creep resistance with CE ≤0.45 (AWS D1.1). SHH STEEL provides MTCs with full analysis for traceability.
-
Is SA387 Gr 12 Cl 2 weldable?
- Yes, SA387 Gr 12 Cl 2 is highly weldable with low carbon (0.05-0.20%) and preheating at 150-200°C for >25mm thicknesses. Use E7018 filler (AWS A5.1) for 90% joint efficiency per ASME Section IX. PWHT at 620-650°C reduces stress, validated by bend tests per ASTM E190.
-
What is the density of SA387 Gr 12 Cl 2?
- The density is 7.85 g/cm³, standard for alloy steel, aiding weight calculations in vessel design. Hardness is 163-235 HB (ASME SA-18), balancing wear resistance for high-temperature use.
-
What is the equivalent of ASME SA387 Gr 12 Cl 2 in EN standards?
- The closest EN equivalent is 10CrMo9-10 (EN 10028-2), with 480-630 MPa tensile and 280 MPa yield, suitable for EU boilers. SHH STEEL provides dual-certified plates for seamless transitions.
-
What is the maximum thickness for SA387 Gr 12 Cl 2?
- Standard thickness is 100mm, with custom options up to 300mm available. Quenched and tempered at 620-650°C per ASME SA-20, these plates are ideal for high-temperature vessels, with ultrasonic testing per ASME SA-578 ensuring no laminations for structural integrity.
Conclusion
SHH STEEL’s ASME SA387 Gr 12 Cl 2 Pressure Vessel Steel Plates provide unmatched strength and reliability for high-temperature pressure vessels and boilers. With precise tolerances, superior weldability, and global equivalents, we offer customized solutions. Trust SHH STEEL for your steel needs.