Carbon Steel Plates

Product Showcase

ASME SA542/SA542M Carbon Steel Plates

SHH STEEL supplies ASME SA542 / ASTM A542 quenched-and-tempered chromium-molybdenum and chromium-molybdenum-vanadium alloy steel plates as China steel mill-Direct Supply. Available in Types A, B, C, D and E with multiple strength classes for welded pressure vessels and heavy-wall high-temperature equipment. Competitive mill price, cut-to-size service, fast delivery and full MTCs.

ASME SA542 Type E Class 4 Q&T 3Cr-1Mo-V plate, TS 85–110 ksi, YS 55 ksi,

ASME SA542 Type E Class 4 Steel Plate | SA542 Type E Cl.4 QT Cr-Mo-V Vessel Plate

ASME SA542 Type E Class 4 / ASME SA542 TYPE E CL.4 is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M. Type E uses the 1010 °C austenitize floor. Class 4 is 380 MPa yield and 585–760 MPa tensile, temper 650 °C. SHH STEEL is the supplier and exporter of SA542 Type E Cl.4, with 3.1 or 3.2 certificates.
View More
ASME SA542 Type D Class 4a Q&T 2.25Cr-1Mo-V vessel plate, YS 60 ksi, SHH STEEL

ASME SA542 Type D Class 4a Steel Plate | SA542 Type D Cl.4a QT Cr-Mo-V Vessel Plate

ASME SA542 Type D Class 4a / ASME SA542 TYPE D CL.4A is quenched-and-tempered 2.25Cr-1Mo-V plate under ASME SA-542/SA-542M. Type D carries the vanadium band on the 2.25Cr line. Class 4a is 415 MPa yield and 585–760 MPa tensile, temper 675 °C. SHH STEEL is the supplier and exporter of SA542 Type D Cl.4a, with 3.1 or 3.2 certificates.
View More
SA542 Type C Class 4a Q&T 3Cr-1Mo-V, TS 85–110 ksi, YS 60 ksi, SHH STEEL

ASME SA542 Type C Class 4a Steel Plate | SA542 Type C Cl.4a QT Cr-Mo-V Vessel Plate

ASME SA542 Type C Class 4a / ASME SA542 TYPE C CL.4A is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M. Type C carries the vanadium band. Class 4a is 415 MPa yield and 585–760 MPa tensile, temper 675 °C. SHH STEEL is the supplier and exporter of SA542 Type C Cl.4a, with 3.1 or 3.2 certificates.
View More
SA542 Type C Class 4 Q&T 3Cr-1Mo-V, TS 85–110 ksi, YS 55 ksi, SHH STEEL

ASME SA542 Type C Class 4 Steel Plate | SA542 Type C Cl.4 QT Cr-Mo-V Vessel Plate

ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M. Type C carries the vanadium band. Class 4 is 380 MPa yield and 585–760 MPa tensile, temper 650 °C. SHH STEEL is the supplier and exporter of SA542 Type C Cl.4, with 3.1 or 3.2 certificates.
View More
SA542 Type C Class 3 Q&T 3Cr-1Mo-V, TS 95–115 ksi, YS 75 ksi, SHH STEEL

ASME SA542 Type C Class 3 Steel Plate | SA542 Type C Cl.3 QT Cr-Mo-V Vessel Plate

ASME SA542 Type C Class 3 / ASME SA542 TYPE C CL.3 is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M. Type C carries the vanadium band. Class 3 is 515 MPa yield and 655–795 MPa tensile. SHH STEEL is the supplier and exporter of SA542 Type C Cl.3, with 3.1 or 3.2 certificates.
View More
SA542 Type C Class 2 Q&T 3Cr-1Mo-V, TS 115–135 ksi, YS 100 ksi, SHH STEEL

ASME SA542 Type C Class 2 Steel Plate | SA542 Type C Cl.2 QT Cr-Mo-V Vessel Plate

ASME SA542 Type C Class 2 / ASME SA542 TYPE C CL.2 is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M. Type C carries the vanadium band. Class 2 is 690 MPa yield and 795–930 MPa tensile. SHH STEEL is the supplier and exporter of SA542 Type C Cl.2, with 3.1 or 3.2 certificates.
View More
ASME SA542 Type C Class 1 Q&T 3Cr-1Mo-V vessel plate, TS 105–125 ksi, SHH STEEL

ASME SA542 Type C Class 1 Steel Plate | SA542 Type C Cl.1 QT Cr-Mo-V Vessel Plate

ASME SA542 Type C Class 1 / ASME SA542 TYPE C CL.1 is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M. Type C carries the vanadium band. Class 1 is 585 MPa yield and 725–860 MPa tensile. SHH STEEL is the supplier and exporter of SA542 Type C Cl.1, with 3.1 or 3.2 certificates.
View More
SA542 Type A Class 4a Q&T 2.25Cr-1Mo, TS 85–110 ksi, YS 60 ksi, SHH STEEL

ASME SA542 Type A Class 4a Steel Plate | SA542 Type A Cl.4a QT Cr-Mo Vessel Plate

ASME SA542 Type A Class 4a / ASME SA542 TYPE A CL.4A is quenched-and-tempered 2.25Cr-1Mo plate under ASME SA-542/SA-542M. Type A is the standard residual line. Class 4a is 415 MPa yield and 585–760 MPa tensile, temper 675 °C. SHH STEEL is the supplier and exporter of SA542 Type A Cl.4a, with 3.1 or 3.2 certificates.
View More
SA542 Type A Class 4 Q&T 2.25Cr-1Mo, TS 85–110 ksi, YS 55 ksi, SHH STEEL

ASME SA542 Type A Class 4 Steel Plate | SA542 Type A Cl.4 QT Cr-Mo Vessel Plate

ASME SA542 Type A Class 4 / ASME SA542 TYPE A CL.4 is quenched-and-tempered 2.25Cr-1Mo plate under ASME SA-542/SA-542M. Type A is the standard residual line. Class 4 is 380 MPa yield and 585–760 MPa tensile, temper 650 °C. SHH STEEL is the supplier and exporter of SA542 Type A Cl.4, with 3.1 or 3.2 certificates.
View More
SA542 Type A Class 3 Q&T 2.25Cr-1Mo, TS 95–115 ksi, YS 75 ksi, SHH STEEL

ASME SA542 Type A Class 3 Steel Plate | SA542 Type A Cl.3 QT Cr-Mo Vessel Plate

ASME SA542 Type A Class 3 / ASME SA542 TYPE A CL.3 is quenched-and-tempered 2.25Cr-1Mo plate under ASME SA-542/SA-542M. Type A is the standard residual line. Class 3 is 515 MPa yield and 655–795 MPa tensile. SHH STEEL is the supplier and exporter of SA542 Type A Cl.3, with 3.1 or 3.2 certificates.
View More
SA542 Type A Class 2 Q&T 2.25Cr-1Mo, TS 115–135 ksi, YS 100 ksi, SHH STEEL

ASME SA542 Type A Class 2 Steel Plate | SA542 Type A Cl.2 QT Cr-Mo Vessel Plate

ASME SA542 Type A Class 2 / ASME SA542 TYPE A CL.2 is quenched-and-tempered 2.25Cr-1Mo plate under ASME SA-542/SA-542M. Type A is the standard residual line. Class 2 is 690 MPa yield and 795–930 MPa tensile. SHH STEEL is the supplier and exporter of SA542 Type A Cl.2, with 3.1 or 3.2 certificates.
View More
ASME SA542 Type A Class 1 Q&T 2.25Cr-1Mo vessel plate, TS 105–125 ksi, SHH STEEL

ASME SA542 Type A Class 1 Steel Plate | SA542 Type A Cl.1 QT Cr-Mo Vessel Plate

ASME SA542 Type A Class 1 / ASME SA542 TYPE A CL.1 is quenched-and-tempered 2.25Cr-1Mo plate under ASME SA-542/SA-542M. Type A is the standard residual line. Class 1 is 585 MPa yield and 725–860 MPa tensile. SHH STEEL is the supplier and exporter of SA542 Type A Cl.1, with 3.1 or 3.2 certificates.
View More

Nuclear-Grade Steel Plates

SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.

Nuclear-Grade Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X