SA542 Type C Class 4 Q&T 3Cr-1Mo-V, TS 85–110 ksi, YS 55 ksi, SHH STEEL

ASME SA542 Type C Class 4 Steel Plate | SA542 Type C Cl.4 QT Cr-Mo-V Vessel Plate

ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M. Type C carries the vanadium band. Class 4 is 380 MPa yield and 585–760 MPa tensile, temper 650 °C. SHH STEEL is the supplier and exporter of SA542 Type C Cl.4, with 3.1 or 3.2 certificates.
Keywords
ASME SA542 Type C Class 4, ASME SA542 TYPE C CL.4, SA542 Type C Cl.4, SA542C CL4, SA-542 Type C Class 4, QT Cr-Mo-V vessel plate, 3Cr-1Mo-V QT plate, SA542 Type C Class 4 supplier
Equivalent Grades:
ASTM A542 Type C (3Cr-1Mo-V) / ASME SA542 Type C / JIS — / GB 12Cr3MoVTiB (near) / EN — — Material Specification: ASME SA-542 / ASTM A542 — Delivery: Quenched + Tempered (QT)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
QT Cr-Mo-V Vessel Service
Weldability
Heat Treatment
Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA542 Type C Class 4 Steel?

ASME SA542 Type C Class 4, also written ASME SA542 TYPE C CL.4, is quenched-and-tempered chromium-molybdenum-vanadium alloy plate under ASME SA-542/SA-542M. Type C is the 3Cr-1Mo-V line. Chromium heat is 2.75–3.25%. Molybdenum heat is 0.90–1.10%. Vanadium heat is 0.20–0.30%. Class 4 shares the 585–760 MPa tensile band with Class 4a, but yield is 380 MPa, not 415 MPa. Elongation is 20%. Temper floor for Type A, B and C Class 4 is 650 °C, not the 565 °C floor used on Class 1, 2 and 3, and not the 675 °C floor used on Class 4a. SHH STEEL is the supplier, exporter and distributor of this Type and Class. Plate is produced to ASME SA-542/SA-542M.

Buyers write ASME SA542 Type C Class 4, ASME SA542 TYPE C CL.4, SA542 Type C Class 4, SA542 Type C Cl.4, SA542C CL4, SA-542 Type C Class 4 and SA 542 Type C Cl 4. ASTM A542 Type C Class 4 is the companion product spec. A purchase order that only says “SA542 Type C” is incomplete. A purchase order that writes Class 4 when the drawing says Class 4a is the wrong yield and the wrong temper floor. A purchase order that says “SA542 Grade 21 Class 4” is mixing this book with SA387 Gr.21 Cl.2.

This page is not Type A or Type B. Those are 2.25Cr-1Mo without the Type C vanadium band. It is not Type D, which is 2.25Cr-1Mo-V. It is not Type E, which is 3Cr-1Mo-V but only Class 4 and 4a with a different residual and austenitizing practice. It is not SA832 21V or 23V; those are normalized-and-tempered. It is not SA517 Gr.A. It is not SA516 Gr.70. Minimum thickness in the specification is about 5 mm. Maximum thickness is limited by the ability of the heat to meet Class 4 after quench and temper.

Dual marking SA542 / A542 Type C Class 4 is available from SHH STEEL as mill supplier. Certificates can be EN 10204 3.1 or 3.2. Company scope: China steel Mill Agent-SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Type / Class ASME SA542 Type C Class 4 Confirmed
Product Specification ASME SA-542/SA-542M Applied
Companion Spec ASTM A542 Type C Class 4 Dual cert available
General Requirements ASME SA-20 / ASTM A20 Applied
Process Quenched and tempered Confirmed
Class 4 temper floor 650 °C min Applied
Alloy idea 3Cr-1Mo-V Confirmed
Sister N+T spec SA-832 / A832 Not this page
Supply role Supplier / exporter / distributor SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and next to the ASME SA387 family, not as a substitute. It does not sit with carbon steel plates or ASTM A36 steel plate.

SA-20 still governs marking, testing location, retests and repair rules.

Chemical Composition

ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 uses Type C chemistry. Class only changes strength and temper floor.

Heat Analysis and Product Analysis — ASME SA542 Type C (typical Table 1 limits)

Element Heat Analysis (%) Product Analysis (%)
Carbon (C) 0.10 – 0.15 0.08 – 0.18
Manganese (Mn) 0.30 – 0.60 0.25 – 0.66
Phosphorus (P), max 0.025 0.025
Sulfur (S), max 0.025 0.025
Silicon (Si), max 0.10 0.13
Chromium (Cr) 2.75 – 3.25 2.63 – 3.37
Molybdenum (Mo) 0.90 – 1.10 0.85 – 1.15
Vanadium (V) 0.20 – 0.30 0.18 – 0.33
Titanium, boron, copper, nickel, niobium, calcium As Table 1 of the named edition As Table 1 of the named edition

Vanadium is not optional decoration. If V is missing, the plate is closer to SA387 Gr.21 Cl.2 than to SA542 Type C. Chromium at 2.00–2.50% is Type A, B or D, not Type C.

SHH STEEL reports heat analysis on every certificate, including Cr, Mo and V.

Mechanical Properties

Class 4 shares tensile with Class 4a. Yield is lower.

Tensile Requirements — ASME SA542 Type C Class 4

Property Requirement
Yield strength, min 380 MPa (55 ksi)
Tensile strength 585 – 760 MPa (85 – 110 ksi)
Elongation in 50 mm, min 20%
Density 7.85 g/cm³
Hardness Not a default substitute for tensile

Class 4a is 415 MPa yield, same tensile band, 18% elongation. Class 3 is 515 MPa yield and 655–795 MPa tensile. Class 1 is 585 / 725–860. Class 2 is 690 / 795–930. Do not stamp Class 4 as Class 4a because tensile matches.

Density is 7.85 g/cm³. Notch toughness is commonly added. Write the temperature, energy, location and orientation. Simulated PWHT is common.

Do not treat 380 MPa yield as permission to substitute A516 Grade 70, SA533 Type A Cl.1 or high strength low alloy plates.

Material Comparison

Grade Route Alloy / strength idea Swap?
SA542 Type C Class 1 QT 3Cr-1Mo-V 585 / 725–860 No
SA542 Type C Class 2 QT 3Cr-1Mo-V 690 / 795–930 No
SA542 Type C Class 3 QT 3Cr-1Mo-V 515 / 655–795 No
SA542 Type C Cl.4 QT 3Cr-1Mo-V 380 / 585–760, temper 650 °C This page
SA542 Type C Class 4a QT 3Cr-1Mo-V 415 / 585–760, temper 675 °C No
SA542 Type A / B Class 4 QT 2.25Cr-1Mo No Type C vanadium band No
SA542 Type E Class 4 QT 3Cr-1Mo-V Type E practice No
SA387 Gr.21 Cl.2 Cr-Mo family 3Cr-1Mo, not QT Type C No
SA832 21V / 23V N+T Cr-Mo-V Not QT Type C No

SA299 Gr.B, SA225 Gr.D, SA455 steel plate and SA285 Gr.C are also vessel plates. None of them is ASME SA542 TYPE C CL.4.

QT Cr-Mo-V Vessel Service

ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 is selected when the vessel wants quenched-and-tempered 3Cr-1Mo-V at the Class 4 line. Typical equipment is high-temperature welded pressure vessels and components written to SA-542 Type C Class 4. Allowable stress comes from ASME Section II Part D after the Code lists this Type and Class.

SHH STEEL supplies this plate as exporter and stockist. It is not nickel low-temp plate like SA203 Gr.D or SA203 Gr.E. It is not layered QT carbon like SA724. It is not SA302 Gr.C. Stainless inquiries belong on ASME SA240 or ASTM A240.

Do not form this plate as if it were as-rolled SA285 Gr.A. Quench-and-temper properties are the product. A later PWHT cycle has to be planned and, when required, simulated on coupons.

Weldability

SA542 Type C Cl.4 is killed, fine-grain 3Cr-1Mo-V at Class 4 strength. Welding is Code welding.

Qualify procedures to ASME Section IX. Use consumables written for 3Cr-1Mo-V QT at 585–760 MPa tensile, not a Class 1 procedure copied down and not an unreviewed SA387 Gr.12 Cl.2 procedure. Vanadium belongs in the WPS review. Hydrogen control, preheat, interpass and PWHT follow the qualified procedure and the vessel specification.

The fabricator owns the WPS. SHH STEEL as supplier can share mill heat data for review.

Heat Treatment

Plates shall be austenitized, quenched in a suitable liquid medium, then tempered. For Type A, B and C Class 4, the minimum tempering temperature is 650 °C (1200 °F). Soak is not less than 1.2 min/mm of thickness and not less than ½ hour. Class 1, 2 and 3 use 565 °C. Class 4a uses 675 °C. Do not temper Class 4 at the Class 1 floor and stamp Class 4.

If the vessel will see a long PWHT, test coupons shall follow a simulated cycle. This is not the SA832 N+T route and not the SA537 Cl.1 heat-treated carbon route. SHH STEEL as mill exporter prints QT, Type C, Class 4, austenitizing and tempering temperatures on the certificate when the mill record carries them.

Delivery Condition

Usual delivery from SHH STEEL as supplier and distributor is quenched-and-tempered ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 plate.

The certificate lists ASME SA542 Type C Class 4 and, when dual certified, ASTM A542 Type C Class 4; heat number; heat analysis including Cr, Mo and V; product analysis when ordered; tensile results to the Class 4 table; QT statement with the 650 °C floor; impact and simulated PWHT when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for SA542 Type C Cl.4 QT Cr-Mo-V vessel plate:

  • Thickness: commonly 8 mm – 150 mm, minimum about 5 mm, limited by the ability of the heat to meet Class 4 after QT
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length shells, heads and nest sizes inside those limits

Structural sizes belong on EN 10025-2 or JIS G3106. Weathering plate belongs on EN 10025-5 or Corten A/B. Fine-grain structural belongs on EN 10025-3 or EN 10025-4. QT structural belongs on EN 10025-6.

Tolerances

Dimensional limits follow ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances. UT to A435 / A577 / A578 is commonly added on reactor plate.

Supplementary Requirements

STEEL as supplier does not assume them.

Charpy details. Temperature, energy, location and orientation.

Simulated PWHT. Same-heat coupons follow the vessel cycle.

NDE. UT to A435 / A577 / A578.

Hydrogen-service extras. When the vessel specification names them.

Third-party. EN 10204 3.2.

Equivalent Material Grades

Designation Standard Notes
ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 ASME SA-542/SA-542M Code name on this page
ASTM A542 Type C Class 4 ASTM A542/A542M Companion spec
SA542 Type C Class 4a SA-542 Higher yield, higher temper floor
SA542 Type E Class 4 SA-542 Related 3Cr-1Mo-V
SA387 Gr.21 Cl.2 SA-387 3Cr-1Mo, not QT Type C
SA832 21V / 23V SA-832 N+T Cr-Mo-V
ASME SA387 SA-387 Related Cr-Mo family

DIN 17100, ASTM A516, ASME SA515 and ASTM A285 are not SA542 Type C Class 4.

Applications

Industry Typical components
High-temperature vessels ASME SA542 Type C Class 4 shells and ASME SA542 TYPE C CL.4 heads
QT 3Cr-1Mo-V equipment SA542 Type C Cl.4 courses
Dual-certified export SA542 / A542 Type C Class 4 plate from SHH STEEL
Fabrication SA542 Type C Cl.4 cut to nest sizes

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering inquiries belong on weathering steel plates. Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless.

Other vessel comparisons: SA203 Gr.B, SA302 Gr.A, A516 Grade 70, SA533 Type C Cl.2, SA517 Gr.P, SA387 Gr.11 Cl.2.

Why Choose SHH STEEL

SHH STEEL is the supplier, exporter, distributor and stockist of ASME SA-542/SA-542M plate. On ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 that means mill pricing, dual SA542/A542 marking, Type C chemistry with Cr-Mo-V reported, recorded quench and temper at the Class 4 floor of 650 °C, tensile results at 380 MPa yield and 585–760 MPa tensile, 3.1 as standard and 3.2 when specified.

We keep Type and Class on the order. Type C is not Type A, Type B, Type D or Type E. Class 4 is not Class 4a. SA542 Type C is not SA387 Gr.21 Cl.2. SA542 is not SA516 Gr.55. SA542 Type C Cl.4 is not SA533 Type C Cl.1. If the drawing names Class 4a, we will not ship Class 4. If the drawing names N+T Cr-Mo-V, we point the inquiry to SA832.

Company scope: China steel Mill Agent-SHH STEEL.

FAQ

What names are used for ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4?
Buyers write ASME SA542 Type C Class 4, ASME SA542 TYPE C CL.4, SA542 Type C Class 4, SA542 Type C Cl.4, SA542C CL4, SA-542 Type C Class 4 and SA 542 Type C Cl 4. SHH STEEL as supplier prints the wording on the purchase order.
Is ASME SA542 Type C Class 4 the same as ASTM A542 Type C Class 4?
Chemistry and tensile limits match. ASME SA-542 is the Code version. ASTM A542 is the product spec. As exporter and mill distributor, SHH STEEL dual-certifies both names when the vessel must be stamped.
What is the yield strength of SA542 Type C Cl.4?
380 MPa minimum. Tensile is 585–760 MPa. Elongation is 20% in 50 mm.
How is ASME SA542 TYPE C CL.4 different from Class 4a?
ame tensile band. Class 4 yield is 380 MPa and temper floor is 650 °C. Class 4a yield is 415 MPa and temper floor is 675 °C.
How is ASME SA542 Type C Class 4 different from Type A Class 4?
Same Class 4 tensile table. Type C is 3Cr-1Mo-V. Type A is 2.25Cr-1Mo without that vanadium band.
How is ASME SA542 Type C Class 4 different from Class 1, 2 and 3?
Class 4 is 380 / 585–760. Class 3 is 515 / 655–795. Class 1 is 585 / 725–860. Class 2 is 690 / 795–930. Temper floors also change.
s SA542 Type C Class 4 the same as SA832 21V or SA387 Grade 21?
No. SA832 21V is N+T Cr-Mo-V. SA387 Grade 21 is 3Cr-1Mo in the SA387 family. SA542 Type C Class 4 is QT 3Cr-1Mo-V at Class 4 strength.
Who supplies ASME SA542 Type C Class 4?
SHH STEEL is the supplier, exporter, distributor and stockist.
Can welding of SA542 Type C Cl.4 be qualified to ASME Section IX?
Yes. Use a WPS written for QT 3Cr-1Mo-V at Class 4 strength. The fabricator owns the procedure.
Can SHH STEEL issue EN 10204 3.2 for ASME SA542 Type C Class 4?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.

Conclusion

ASME SA542 Type C Class 4 Steel Plate, also searched as ASME SA542 TYPE C CL.4, is quenched-and-tempered 3Cr-1Mo-V plate under ASME SA-542/SA-542M, with 380 MPa yield and a 650 °C temper floor. Whether the inquiry says ASME SA542 Type C Class 4, ASME SA542 TYPE C CL.4, SA542 Type C Cl.4 or SA542C CL4, SHH STEEL as supplier, exporter, distributor and stockist supplies plate with Type C chemistry, recorded QT delivery, and EN 10204 3.1 or 3.2 certification.

SHH STEEL is the China mill vendor of ASME SA542 Type C Class 4 / ASME SA542 TYPE C CL.4 QT Cr-Mo-V Vessel Plate for ASME Section VIII work that actually names this Type and Class.

Contact SHH STEEL for mill rolling, stock inquiry, dual SA542/A542 marking, simulated PWHT testing, 3.2 inspection or a quotation.

ASME SA542 Type C Class 4 Steel Plate, ASME SA542 TYPE C CL.4, SA542 Type C Cl.4, SA542C CL4, SA-542 Type C Class 4, QT Cr-Mo-V vessel plate, SHH STEEL supplier exporter distributor stockist

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X