ASME SA302 Grade B Steel Plate | SA302 Gr.B Mn-Mo Vessel Plate
What is ASME SA302 Grade B Steel?
As a professional China mill-Direct Supply and ASME pressure-vessel plate exporter, SHH STEEL supplies ASME SA302 Grade B Steel Plate produced to ASME SA-302/SA-302M.
On drawings, MTCs and RFQs this grade is written many ways: ASME SA302 Grade B, SA302 Gr.B, SA302 Gr B, SA302GRB, SA302 GR B, SA-302 Grade B, SA-302 Gr.B, ASTM A302 Grade B, A302 Gr.B, A302GRB, Mn-Mo vessel plate, manganese molybdenum boiler plate and A/SA302 Grade B. All of these names refer to the same manganese-molybdenum alloy plate. ASME SA-302/SA-302M is the Boiler and Pressure Vessel Code companion to ASTM A302/A302M.
SA302 Gr.B is the workhorse grade in ASME SA-302. Grade A is the lower-strength Mn-Mo plate. Grade B raises manganese and strength. Grades C and D keep Grade B strength and add nickel. Minimum yield of Grade B is 345 MPa (50 ksi). Tensile strength is 550–690 MPa (80–100 ksi). Molybdenum heat analysis is 0.45–0.60%. Nickel is not specified for Grade B.
The plate is intended for welded boilers and other pressure vessels under ASME Section VIII. It is not a 2.25Ni / 3.5Ni low-temperature grade such as SA203, and it is not a Cr-Mo elevated-temperature grade such as ASME SA387 (SA-387). Compared with carbon vessel steels such as ASME SA516 (SA-516) and ASTM A516, Grade B adds molybdenum for higher allowable strength in boiler and vessel service.
General requirements follow ASME SA-20. Steel is killed and produced to fine-grain practice. Plates 50 mm and under are normally supplied as-rolled unless normalizing or stress relieving is ordered. Plates over 50 mm shall be normalized.
SHH STEEL supplies SA302 Gr.B as true China mill-Direct Supply. Dual marking ASME SA302 Grade B / ASTM A302 Grade B is available for equipment built to ASME Section VIII. Certificates can be EN 10204 3.1 or EN 10204 3.2.
If the project compares other coded vessel plates, SHH STEEL places SA302 Gr.B next to ASME SA537 (SA-537), ASTM A537, ASME SA515 (SA-515) and ASTM A285.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | ASME SA302 Grade B / SA302 Gr.B / SA302GRB | Confirmed |
| Product Specification | ASME SA-302/SA-302M | Applied |
| Companion Spec | ASTM A302 Grade B / A302 Gr.B | Dual cert available |
| General Requirements | ASME SA-20 / ASTM A20 | Applied |
| Code Context | ASME Section VIII | As specified |
| Product Form | Pressure vessel / boiler plate | Available |
| Alloy Type | Manganese-molybdenum (no specified Ni) | Confirmed |
| Delivery Condition | As-rolled ≤50 mm; normalized >50 mm | As specified |
| Typical Thickness | 6 mm – 150 mm | Heavier by enquiry |
| Width / Length | Up to about 4600 mm wide / 12000 mm long | Mill capability |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This product belongs to the Pressure Vessel Steel Plates family. It is a Mn-Mo coded vessel plate under ASME SA-302, not a structural Carbon Steel Plates grade.
Chemical Composition
SA302 Grade B chemistry under ASME SA-302/SA-302M is reported as heat analysis (ladle analysis) and, when specified, product analysis.
Heat Analysis (Ladle Analysis) — Grade B
| Element | Thickness / Basis | Heat Analysis (%) |
|---|---|---|
| Carbon (C), max | ≤ 25 mm (1 in.) | 0.20 |
| Carbon (C), max | > 25 mm to 50 mm (1–2 in.) | 0.23 |
| Carbon (C), max | > 50 mm (2 in.) | 0.25 |
| Manganese (Mn) | All | 1.15 – 1.50 |
| Phosphorus (P), max | All | 0.025 |
| Sulfur (S), max | All | 0.025 |
| Silicon (Si) | All | 0.15 – 0.40 |
| Molybdenum (Mo) | All | 0.45 – 0.60 |
| Nickel (Ni) | All | Not specified |
Product Analysis — Grade B
| Element | Thickness / Basis | Product Analysis (%) |
|---|---|---|
| Manganese (Mn) | All | 1.07 – 1.62 |
| Silicon (Si) | All | 0.13 – 0.45 |
| Molybdenum (Mo) | All | 0.41 – 0.64 |
| C, P, S | Product check per SA-20/SA-302 | Per order |
Grade B uses a higher manganese band than Grade A so the 345 MPa yield in ASME SA-302 can be met. Molybdenum stays 0.45–0.60% on heat analysis for all four grades. Nickel is the separator: Grade B has no Ni requirement; Grade C adds 0.40–0.70% Ni; Grade D adds 0.70–1.00% Ni. Tighter residuals or carbon equivalent limits are supplementary requirements.
SHH STEEL reports ladle analysis on every certificate. Product analysis is added when ASME SA-20 product analysis or the vessel specification requires it.
Mechanical Properties
Tensile Requirements — ASME SA302 Grade B per ASME SA-302/SA-302M
| Property | Requirement |
|---|---|
| Tensile strength | 550 – 690 MPa (80 – 100 ksi) |
| Yield strength, min (0.2%) | 345 MPa (50 ksi) |
| Elongation in 200 mm (8 in.), min | 15% |
| Elongation in 50 mm (2 in.), min | 18% |
These limits apply to SA302 Gr.B at both thin and thick sizes. Density is 7.85 g/cm³. Hardness after the agreed heat treatment is typically in the 160–200 HB range unless a special window is ordered.
Compared with SA302 Grade A, Grade B gives 35 MPa more yield and a higher tensile band. Compared with Grades C and D, strength is the same; only nickel changes. Specimens are prepared under ASME SA-20. If simulated PWHT is specified, coupons are heat-treated to the vessel cycle before testing.
Material Comparison
| Grade | Alloy type | Ni (heat) | Yield min | Tensile | Typical use |
|---|---|---|---|---|---|
| SA302 Gr.A | Mn-Mo | Not specified | 310 MPa | 515–655 MPa | Lower-strength Mn-Mo |
| SA302 Gr.B | Mn-Mo | Not specified | 345 MPa | 550–690 MPa | Workhorse Mn-Mo vessel plate |
| SA302 Gr.C | Mn-Mo-Ni | 0.40–0.70% | 345 MPa | 550–690 MPa | Same strength, added Ni |
| SA302 Gr.D | Mn-Mo-Ni | 0.70–1.00% | 345 MPa | 550–690 MPa | Same strength, higher Ni |
Order SA302 Gr.B / SA302GRB when the ASME SA-302 drawing needs Mn-Mo plate at 345 MPa yield and nickel is not required. If the same strength is needed with nickel for toughness, use Grade C or Grade D. If 310 MPa yield is enough, Grade A is sufficient. Carbon QT options include ASME SA537 and ASTM A537. HSLA Steel Plates are not a coded substitute for ASME SA-302.
Elevated-Temperature and Vessel Service
SA302 Grade B is specified for welded boilers and pressure vessels, not for cryogenic 3.5Ni or 9% Ni service. Molybdenum in ASME SA-302/SA-302M supports strength in boiler and process equipment covered by ASME Section VIII. Allowable stress at temperature is taken from the applicable ASME Section II Part D table for SA-302 Grade B, not from a commercial datasheet.
Impact temperature, orientation and energy minimums are agreed on the order. They are not automatic on Grade B. When the vessel specification sets Charpy values, SHH STEEL produces SA302 Gr.B Mn-Mo vessel plate with those sets and lists the results on the 3.1 or 3.2 certificate.
Weldability
SA302 Grade B under ASME SA-302 is a welded boiler and pressure-vessel plate. Mn-Mo steel is welded with low-hydrogen procedures qualified to ASME Section IX.
Consumables are selected to match molybdenum and the required joint strength and toughness. Preheat depends on thickness, hydrogen control and restraint. When ASME Section VIII requires PWHT, the shop cycle is commonly in the 595–650°C range for this alloy family. If properties after that cycle are needed, simulated PWHT of mill coupons should be ordered before shipment.
SHH STEEL recommends a qualified WPS/PQR for each thickness break and can support procedure review through steel welding services. Do not assume an SA516 procedure is automatically valid for SA302 Gr.B.
Heat Treatment
Heat treatment of SA302 Grade B follows ASME SA-302/SA-302M:
- Plates 50 mm (2 in.) and under are normally supplied in the as-rolled condition. They may be ordered normalized, stress relieved, or both.
- Plates over 50 mm (2 in.) shall be normalized.
Normalizing is heating into the austenite range followed by air cooling. Stress relieving, when ordered, is a separate lower-temperature hold to reduce residual stress. Quench-and-temper practice used for SA533 / SA537 Class 2 must not be applied to Grade B unless the order is changed to a QT specification.
If the specification fixes a normalizing temperature band or holding time per thickness under ASME SA-20, SHH STEEL writes those parameters into the mill instruction and reports them on the certificate.
Delivery Condition
SHH STEEL delivers ASME SA302 Grade B / SA302 Gr.B as follows:
- ≤ 50 mm: as-rolled as standard, or normalized / stress relieved when ordered
-
50 mm: normalized as required by ASME SA-302
The certificate lists SA302 Gr.B and, when dual certified, A302 Gr.B; heat number; heat analysis; product analysis when ordered; tensile results; heat-treatment condition; agreed Charpy values; and supplementary tests. Plates are industrial vessel plate: heat-treated as required, then pickled or shot-blasted as agreed.
Decorative finishes such as 2B, BA or No.4 are not used. Surface condition is vessel-plate quality for welding, NDE and coating. Heat number and grade marking support ASME Section VIII traceability.
Certificates may be EN 10204 3.1 or EN 10204 3.2. Third-party stamps (BV, LR, DNV, TUV, SGS or the purchaser’s agency) are arranged when written on the order.
Dimensions
Typical supply range from SHH STEEL for SA302 Gr.B Mn-Mo vessel plate:
- Thickness: 6 mm – 150 mm (heavier by mill enquiry)
- Width: up to about 4600 mm
- Length: up to about 12000 mm
Because heat treatment changes at 50 mm in ASME SA-302, the purchase order should state the ordered thickness and the required condition. Cut-to-length shells, heads and nest sizes are available.
Tolerances
Dimensional tolerances follow ASME SA-20 / ASTM A20 for pressure-vessel plates.
Thickness, width, length, flatness and camber are vessel-plate tolerances, not strip tolerances. Restricted thickness or extra-flatness can be accepted when the vessel drawing requires it. Ultrasonic testing to A435 or A578 is added when specified. Cutting to finished sizes is available through steel cutting services.
Supplementary Requirements
ASME Section VIII specifications often add tests beyond the base SA-302 Grade B table. SHH STEEL treats the following as supplementary requirements.
Simulated PWHT. Coupons from the same heat and thickness receive the vessel PWHT cycle. Tensile and Charpy tests are run on those coupons.
Nondestructive examination. UT to A435, A577 or A578 with purchaser acceptance levels. Edge MT/PT after cutting if required.
Impact testing. Test temperature, specimen size, orientation and minimum average/single values as written on the RFQ.
Special hardness. HBW or HV window after the agreed heat treatment or after simulated PWHT.
Restricted chemistry. Tighter C, P, S, residuals or carbon equivalent on heat and product analysis per ASME SA-302 / SA-20.
HIC testing. NACE TM0284 with purchaser solution and CLR/CTR/CSR limits. Not automatic on SA302 Gr.B.
NACE / sour-service notes. Review against NACE MR0175 / ISO 15156 or MR0103 only when the datasheet cites the clause.
Z-direction testing. ASTM A770 or purchaser Z15/Z25/Z35 for thick nozzles and restrained joints.
Third-party witnessing. Witness of heat treatment, mechanical tests, UT and documents. Output can be EN 10204 3.2.
Supplementary tests go through steel testing service and appear line by line on the certificate. Items not on the purchase order are not assumed.
Equivalent Material Grades
| Designation | Standard / Region | Notes |
|---|---|---|
| ASME SA302 Grade B / SA302 Gr.B / SA302GRB | ASME SA-302/SA-302M | Code name on this page |
| ASTM A302 Grade B / A302 Gr.B / A302GRB | ASTM A302/A302M | Companion material spec |
| Mn-Mo vessel plate | Commercial | Alloy-content search name |
| GB/T 713 15CrMoR related | GB | Closest Chinese Mo vessel |
| EN 10028 13CrMo4-5 / 16Mo3 related | EN | Project-specific comparison |
| JIS related Mo boiler plate | JIS | Project-specific dual cert |
For ASME stamping, the purchase order should say ASME SA302 Grade B to ASME SA-302/SA-302M, or dual SA302 / A302 Grade B. Nearby carbon vessel grades include ASME SA516, ASTM A516, ASME SA515 and ASTM A285.
Applications
ASME SA302 Grade B / SA302 Gr.B is selected for ASME Section VIII boilers and vessels that need Mn-Mo strength at 345 MPa yield. Typical applications of ASME SA302 Grade B Steel Plate include:
| Industry / Sector | Typical Components (with keywords) |
|---|---|
| Boilers & Steam Drums | SA302 Gr.B boiler plate and SA302GRB Mn-Mo vessel plate |
| ASME Section VIII Vessels | ASME SA302 Grade B shells, heads and welded pressure parts |
| Oil, Gas & Petrochemical | SA-302 Grade B reactors, separators and process vessels |
| Energy & Power | SA302 Grade B heat-exchange shells and power-plant vessels |
| Dual-Certified Export Jobs | SA302 / A302 Gr.B plate to ASME SA-302 and ASTM A302 |
| Heavy Vessel Fabrication | SA302 Gr B plate cut to nest sizes |
SHH STEEL supplies SA302 Gr.B with full heat traceability. Related industry pages include petrochemical industry and energy industry. Supporting services include steel cutting services, steel welding services, steel testing service and worldwide shipping service.
Why Choose SHH STEEL
SHH STEEL is a China mill-Direct Supply for plates to ASME SA-302/SA-302M. For SA302 Grade B we offer:
- China mill-Direct Supply pricing on SA302 Gr.B / A302 Gr.B
- Dual ASME SA302 / ASTM A302 marking
- Heat analysis and product analysis per ASME SA-20 / SA-302
- EN 10204 3.1 standard; EN 10204 3.2 or nominated third-party inspection on request
- As-rolled or normalized delivery per thickness rule
- Supplementary PWHT simulation, UT, HIC, NACE review and Z-direction testing
- Cutting to shell and head nest sizes
- Technical support to separate Grade B from A/C/D and from SA516 / SA387 / SA537
- Export packing through worldwide shipping service
For company scope and other vessel grades, visit China steel Mill Agent-SHH STEEL.
FAQ
-
What other names are used for ASME SA302 Grade B?
- We also write SA302 Gr.B, SA302GRB, SA-302 Grade B, ASTM A302 Grade B, A302GRB and Mn-Mo vessel plate. They all mean the manganese-molybdenum Grade B plate in ASME SA-302/SA-302M. SHH STEEL prints the exact name required on the purchase order.
-
Is SA302 Grade B the same as A302 Grade B?
- They are companion specifications. ASME SA-302 is the Code version used with ASME Section VIII; ASTM A302 is the ASTM product spec. Chemistry and tensile limits match. SHH STEEL dual-certifies when the vessel must be Code-stamped.
-
Does SA302 Gr.B contain nickel?
- No. Grade B in ASME SA-302 has no nickel requirement. Grade C adds 0.40–0.70% Ni and Grade D adds 0.70–1.00% Ni, at the same 345 MPa yield.
-
What is the difference between SA302 Grade A and Grade B?
- Both are Mn-Mo plates with no specified nickel. Grade B requires 345 MPa yield and 550–690 MPa tensile. Grade A requires 310 MPa yield and 515–655 MPa tensile. Grade B also uses a higher manganese band.
-
Must SA302 Grade B be normalized?
- Plates over 50 mm shall be normalized per ASME SA-302. Plates 50 mm and under are normally as-rolled unless the purchaser orders normalizing or stress relieving.
-
Can welding be qualified to ASME Section IX?
- Yes. SA302 Gr.B is a welded boiler and vessel plate. Procedures should be qualified to ASME Section IX with low-hydrogen consumables matched to the Mn-Mo chemistry. The fabricator owns the qualified WPS.
-
Can SHH STEEL issue EN 10204 3.2?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 or another third-party witness is arranged when it is written on the order.
-
What is the density of SA302 Gr.B?
- 7.85 g/cm³. SHH STEEL uses this value for shipping-weight estimates on ASME SA-302 plate.
Conclusion
ASME SA302 Grade B Steel Plate is the manganese-molybdenum, 345 MPa yield vessel grade in ASME SA-302/SA-302M. Whether the inquiry says SA302 Gr.B, SA302GRB, SA-302 Grade B or Mn-Mo vessel plate, SHH STEEL supplies plate with heat and product analysis, thickness-correct heat treatment, optional supplementary tests, and EN 10204 3.1 or 3.2 certification.
As a professional China mill-Direct Supply, SHH STEEL provides ASME SA302 Grade B / SA302 Gr.B Mn-Mo Vessel Plate with full traceability for ASME Section VIII fabrication.
Contact SHH STEEL today for stock, normalizing, dual SA302/A302 marking to ASME SA-302, 3.2 inspection or a quotation.
ASME SA302 Grade B Steel Plate, SA302 Gr.B, SA302GRB, SA-302 Grade B, ASME SA-302, ASTM A302 Grade B, Mn-Mo vessel plate, SA302 Grade B supplier, China mill-Direct Supply