GB/T 3531 06Ni9DR Steel Plate | 06Ni9DR -196°C Vessel Plate | GB/T 3531 Steel - SHH STEEL

GB/T 3531 06Ni9DR Steel Plate | 06Ni9DR -196°C Vessel Plate

GB/T 3531 06Ni9DR is 9 % nickel steel plate for cryogenic pressure vessels under GB/T 3531-2014. It is supplied quenched and tempered in 5–50 mm, with Charpy V-notch energy of 100 J minimum at -196°C and minimum yield of 560 MPa up to 30 mm. The grade moved to GB/T 713.4-2023 in the 2023 revision. SHH STEEL produces and exports 06Ni9DR plate to the 2014 edition when the project documents call for it.
Equivalent Grades:
Near: ASTM A553 Type I, ASTM A353, EN 10028-4 X8Ni9 / X7Ni9, JIS G3127 SL9N590. Successor: GB/T 713.4 06Ni9DR. None is automatic.
Heat Treatment
Quenched and tempered; ≤12 mm may be double normalized and tempered; tempering not below 540°C.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is GB/T 3531-2014 06Ni9DR steel plate?

GB/T 3531 06Ni9DR Steel Plate is a 9 % nickel steel plate (Ni 8.50–10.00 %) for welded vessels and tanks at cryogenic temperatures, ordered to GB/T 3531-2014. It was one of the three grades added in the 2014 edition and covers the lower end of the standard’s -196°C scope.

GB/T 3531-2014, Steel plates for low temperature pressure vessels, was issued on 24 June 2014 as GB 3531-2014 and implemented on 1 April 2015, replacing GB 3531-2008. It was later converted to a recommended national standard, which is why it is cited as GB/T 3531-2014. It covers plates 5 mm to 120 mm thick for pressure vessels working from -196°C to below -20°C. The edition was withdrawn on 1 March 2024 and replaced by GB/T 713.3-2023, with the nickel grades moved to GB/T 713.4-2023.

In the 2023 revision this designation moved into the nickel-steel book as GB/T 713.4 06Ni9DR. Order this page when the drawing or data sheet still names GB/T 3531-2014.

SHH STEEL produces and exports GB/T 3531-2014 06Ni9DR plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. This grade is listed in our GB/T 3531 range under Nuclear-Grade Steel Plates.

Material specification for GB/T 3531 06Ni9DR

The items below follow GB/T 3531-2014. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.

Parameter Detail
Standard GB/T 3531-2014, Steel plates for low temperature pressure vessels (issued as GB 3531-2014; replaced GB 3531-2008)
Edition status Withdrawn 1 March 2024. Replaced by GB/T 713.3-2023 for the low-alloy grades and GB/T 713.4-2023 for 08Ni3DR and 06Ni9DR. This page covers the 2014 edition only
Scope of the standard Plates 5 mm to 120 mm thick for low-temperature pressure vessels from -196°C to below -20°C
Grades in the 2014 edition 16MnDR, 15MnNiDR, 15MnNiNbDR, 09MnNiDR, 08Ni3DR, 06Ni9DR
Grade 06Ni9DR
Delivery condition (Table 2) Quenched and tempered (plate not thicker than 12 mm may be double normalized and tempered)
Impact requirement -196°C / 100 J for all tabulated thicknesses
Tempering Not lower than 540°C
Mechanical test frequency Each heat-treated plate
Thickness tabulated for this grade 5–50 mm (standard limits in Table 2, not a stock range)
Steelmaking Basic oxygen or electric furnace with secondary refining. Reduction ratio at least 3 from continuous-cast slab or ingot, at least 2 from electroslag remelted slab
Dimensions and tolerances GB/T 709-2006, thickness tolerance Class B; Class C or tighter tolerances by agreement
Ultrasonic testing Plate by plate for N or N+T plate over 20 mm and Q+T plate over 16 mm; method JB/T 4730.3, GB/T 2970 or GB/T 28297, class stated on the contract
Our supply We produce and export 06Ni9DR plate to GB/T 3531-2014 with the dimensions, tests and inspection document written on the enquiry

Chemical composition of GB/T 3531-2014 06Ni9DR

The heat analysis below is the 06Ni9DR row of GB/T 3531-2014 Table 1. Phosphorus and sulfur limits are the tightest in the standard.

Element Heat analysis, GB/T 3531-2014 Table 1 (wt. %)
Carbon (C) ≤0.08
Silicon (Si) 0.15–0.35
Manganese (Mn) 0.30–0.80
Nickel (Ni) 8.50–10.00
Vanadium (V) ≤0.01
Molybdenum (Mo) ≤0.10
Phosphorus (P) ≤0.008
Sulfur (S) ≤0.004

Notes to Table 1: as residual elements, Cr and Cu are each limited to 0.25 %; the supplier need not analyse them when it guarantees compliance. Product analysis tolerances follow GB/T 222, except that for 08Ni3DR and 06Ni9DR the permitted product-analysis excess is +0.003 % for phosphorus and +0.002 % for sulfur. Confirm residual limits on the mill test certificate.

Mechanical properties of GB/T 3531-2014 06Ni9DR

Table 2 of GB/T 3531-2014 tabulates 06Ni9DR in two bands up to 50 mm. The impact test is at -196°C with 100 J minimum, the highest energy requirement in the 2014 book.

Nominal thickness (mm) Tensile strength Rm (MPa) Yield strength ReL, min (MPa) Elongation A, min (%) Charpy V test temperature KV2, min (J) 180° bend, b = 2a
5–30 680–820 560 18 -196°C 100 D = 3a
>30–50 680–820 550 18 -196°C 100 D = 3a

Charpy V-notch energy is the mean of three specimens. One single value may fall below the Table 2 figure, but not below 70 % of it. Plates under 12 mm are tested with sub-size specimens: 10 × 7.5 × 55 mm for plate over 8 mm and under 12 mm, with results not less than 75 % of the Table 2 value, and 10 × 5 × 55 mm for 6–8 mm plate, with results not less than 50 %. Plate thinner than 6 mm is not impact tested. Higher impact energy than Table 2 may be agreed and written on the contract. Yield is ReL; where yielding is not distinct, Rp0.2 is measured instead. In the bend column, a is the specimen thickness and D the mandrel diameter; the bend test may be waived when the supplier guarantees it.

Delivery conditions for GB/T 3531 06Ni9DR

Table 2 lists 06Ni9DR as quenched and tempered. Plate not thicker than 12 mm may instead be delivered double normalized and tempered. The tempering temperature shall be not lower than 540°C.

Every heat-treated plate is mechanically tested. Quenched-and-tempered plate thicker than 16 mm is ultrasonically tested plate by plate.

Welding and thermal cutting

9 % nickel steel is normally welded with high-nickel alloy consumables chosen for cryogenic toughness. Weld-metal strength must be checked against the design, since it can be lower than the plate.

Residual magnetism is a known problem with 9 % nickel plate and causes arc blow; check and demagnetise before welding. Heat input, interpass control and any post-weld heat treatment are set by the qualified procedure and the vessel code.

Dimensions, tolerances and inspection

Dimensions, shape and permitted deviations follow GB/T 709-2006. Thickness tolerance is Class B unless the purchaser asks for Class C, and tighter tolerances may be agreed. Plates are invoiced on theoretical weight, calculated from the mean of the maximum and minimum permitted thickness.

Cracks, blisters, scabs, folds and inclusions are not permitted on the surface. They may be removed by dressing, provided the dressed depth does not exceed half the thickness tolerance and the minimum permitted thickness is kept. Dressed areas must be smooth.

Acceptance is by batch: one grade, one heat, one thickness and one heat-treatment condition, not more than 30 t per batch; a single plate heavier than 30 t is its own batch. Each batch receives one tensile test, one bend test and a set of three Charpy specimens; chemical analysis is one per heat. Each heat-treated plate is mechanically tested. Ultrasonic testing is plate by plate for quenched-and-tempered plate thicker than 16 mm.

Applications and specification limits

We produce and export 06Ni9DR for cryogenic vessels and tanks such as LNG storage inner tanks, liquid nitrogen and liquid oxygen equipment and other service designed around a -196°C impact class. The allowable minimum design temperature and design stress are set by the vessel or tank code.

The 2014 impact test is at -196°C. Some commercial tables quote a -165°C test for this grade; that is not the GB/T 3531-2014 requirement. Order the impact temperature in the standard, or a stricter one written on the contract.

Edition note. This page is the GB/T 3531-2014 product. Its 2023 successor coverage is GB/T 713.4 06Ni9DR in GB/T 713.4-2023, the separate nickel-steel book. The 2014 and 2023 books are not the same specification, and a certificate to one edition is not an automatic substitute for an order written to the other.

GB/T 3531-2014 is a low-temperature pressure vessel plate standard. On its own it does not impose nuclear-class requirements; where a nuclear or other special code applies, its supplementary requirements must be written on the order.

Compare GB/T 3531 06Ni9DR with other low-temperature plates

The comparison below places 06Ni9DR against the 3.5 % nickel grade of the 2014 book, its 2023 successor and the other 9 % nickel plates we publish. These grades are related, not interchangeable.

Material Type Delivery Key requirement Substitution limit
GB/T 3531 06Ni9DR (this plate) 9 % Ni Q+T (≤12 mm: double N + T) Yield 560 MPa min at 5–30 mm; Rm 680–820 MPa; -196°C / 100 J; to 50 mm 2014 edition only
GB/T 3531 08Ni3DR 3.5 % Ni N, N+T or Q+T -100°C / 60 J Not for -196°C service
GB/T 713.4 06Ni9DR 9 % Ni (2023 edition) See that page 2023 tables; see that page Successor coverage, not the same specification
GB/T 713.4 06Ni7DR 7 % Ni (2023 edition) See that page 2023 tables New 2023 grade, not in GB/T 3531-2014
ASTM A353 9% Nickel 9 % Ni ASTM plate Double normalized and tempered Per ASTM A353 Different heat treatment
ASTM A553 Type I 9 % Ni ASTM plate Quenched and tempered Per ASTM A553 Different strength and impact rules

Equivalent and related grades by country

The grades below are near equivalents in the 9 % nickel family, not certified equivalents. Check heat treatment, strength, impact rules and thickness limits against the project specification.

Country / region Standard Grade Similarity and key differences Caveat
China GB/T 3531-2014 06Ni9DR This product —
China GB/T 713.4-2023 GB/T 713.4 06Ni9DR Same designation in the 2023 nickel-steel book Different edition; not automatic
United States ASTM A553 / ASME SA553 ASTM A553 Type I, ASME SA553 Type I Quenched-and-tempered 9 % nickel plate Different strength and impact rules
United States ASTM A353 / ASME SA353 ASTM A353 9% Nickel, ASME SA353 9% Nickel Double normalized and tempered 9 % nickel plate Different heat treatment
Europe EN 10028-4 EN 10028-4 X8Ni9, EN 10028-4 X7Ni9 9 % nickel plate for cryogenic vessels Different heat-treatment and impact rules
Japan JIS G3127 JIS G3127 SL9N520, JIS G3127 SL9N590 9 % nickel low-temperature plate Different strength classes

Why choose SHH STEEL for GB/T 3531 06Ni9DR

  • SHH STEEL produces and exports GB/T 3531-2014 06Ni9DR plate as a producer, exporter and mill agent
  • We quote to the edition written on your order and keep GB/T 3531-2014 values separate from GB/T 713.3 or GB/T 713.4 values
  • We quote the -196°C / 100 J requirement of the 2014 edition and do not substitute a -165°C test
  • We review impact temperature, ultrasonic class and any simulated PWHT before quoting, not after rolling
  • We match the inspection document to what the purchase order requires

How to enquire for GB/T 3531 06Ni9DR plate

Item What to specify
Standard and grade GB/T 3531-2014 06Ni9DR; state the edition year rather than only GB/T 3531
Delivery condition Quenched and tempered; double normalized and tempered only for plate not thicker than 12 mm if agreed
Dimensions Thickness, width and length; we confirm production and export feasibility against the enquiry
Impact testing Table 2 temperature and energy, or a higher agreed energy; state specimen orientation if the project specifies it
Ultrasonic testing JB/T 4730.3, GB/T 2970 or GB/T 28297, with the acceptance class
Supplementary tests Simulated post-weld heat treatment, through-thickness or product analysis only when written on the order
Documentation Inspection document type required by the project, for example EN 10204 3.1 or 3.2
Other editions If GB/T 713.3-2023 or GB/T 713.4-2023 must also be met, say so on the enquiry; we review both editions before quoting

FAQ

What impact temperature does GB/T 3531-2014 06Ni9DR meet?
Table 2 requires 100 J minimum at -196°C for thicknesses from 5 mm to 50 mm. Tables quoting -165°C do not reflect the 2014 requirement.
How is 06Ni9DR heat treated?
Quenched and tempered, with tempering not lower than 540°C. Plate not thicker than 12 mm may be delivered double normalized and tempered.
What is the yield strength of 06Ni9DR?
Minimum yield is 560 MPa for 5–30 mm and 550 MPa over 30–50 mm, with tensile strength 680–820 MPa and elongation of at least 18 %.
Is 06Ni9DR the same as ASTM A553 Type I?
No. Both are quenched-and-tempered 9 % nickel steels, but strength, impact and testing rules differ. Treat them as related grades and check the project specification.
What should a quotation enquiry include?
GB/T 3531-2014, grade 06Ni9DR, delivery condition, thickness by width by length, quantity, impact and ultrasonic requirements, any residual magnetism limit, and the inspection document.

Request a quotation

Contact SHH STEEL for a quotation for GB/T 3531-2014 06Ni9DR low-temperature pressure vessel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.

State the delivery condition, the Charpy test temperature and energy if they differ from Table 2, the ultrasonic testing standard and class, any simulated post-weld heat treatment, and the inspection document required by the project.

If you are considering ASTM A553 Type I, ASTM A353 or the GB/T 713.4-2023 version of 06Ni9DR, send the project specification. We will review the differences rather than assume the grades or editions are interchangeable.

For a detailed quotation, email your material specification, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X