ASTM A553 Type I 9% Nickel Steel Plate
What is ASTM A553 Type I steel plate?
ASTM A553 Type I is quenched and tempered 9% nickel alloy steel plate. The current ASTM publication, A553/A553M-22, lists Type I (9% nickel), Type II (8% nickel) and Type III (7% nickel). Type I is impact tested at −320 °F [−195 °C] unless another temperature is agreed. Thickness is limited only by the ability of the plate to meet the specified mechanical properties. SHH STEEL produces and exports ASTM A553 Type I plate to the edition and heat treatment named on the order.
Material specification for ASTM A553 Type I
Type identification from the ASTM A553/A553M-22 store scope, with table values cited as noted below.
| Parameter | Detail |
|---|---|
| Standard | ASTM A553/A553M-22, Standard Specification for Pressure Vessel Plates, Alloy Steel, Quenched and Tempered 7%, 8%, and 9% Nickel |
| Official split | Type I (nominal 9% nickel). The specification uses Type, not Grade or Class |
| Other types in the same specification | Type I = 9% nickel; Type II = 8% nickel; Type III = 7% nickel. This page specifies only Type I |
| Product form | Pressure-vessel steel plate, water quenched and tempered |
| General requirements | ASTM A20/A20M; A553/A553M prevails in a conflict |
| Steelmaking | Killed steel; fine austenitic grain size (ASTM store abstract and A553-17 / SA-553 text) |
| Chemical analysis | Table 1 for Type I from ASTM A553/A553M-17 as published in ASME BPVC.II.A-2023 SA-553/SA-553M; not presented as the A553/A553M-22 text |
| Delivery condition | Water quenched and tempered; QT marking, or QTT when the optional intermediate treatment is used |
| Thickness | ASTM A553/A553M-22 scope: limited only by the capacity of the material to meet the specified mechanical property requirements |
| Impact testing | Mandatory Charpy V-notch at −320 °F [−195 °C] unless another temperature is agreed; lateral expansion not less than 0.015 in. [0.381 mm] |
| Units | Inch-pound and SI values are separate standards; do not combine them |
| Magnetization | The material is susceptible to magnetization after heat treatment |
| Our supply | We produce and export ASTM A553 Type I plate to the ordered edition, heat treatment, dimensions and extra tests |
Types in ASTM A553/A553M-22:
| Type | Nominal nickel, % | Default impact test temperature |
|---|---|---|
| I | 9 | −320 °F [−195 °C] |
| II | 8 | −275 °F [−170 °C] |
| III | 7 | −320 °F [−195 °C] |
Chemical composition of ASTM A553 Type I
The current ASTM publication is A553/A553M-22. Its published scope lists three types — Type I (nominal 9% nickel), Type II (nominal 8% nickel) and Type III (nominal 7% nickel) — and requires impact testing at −320 °F [−195 °C] for Type I or Type III and at −275 °F [−170 °C] for Type II, unless another temperature is agreed. Maximum thickness is limited only by the capacity of the material to meet the specified mechanical property requirements.
The chemical composition, tensile values and heat-treatment temperatures below are those of ASTM A553/A553M-17, as published in ASME BPVC Section II, Part A, 2023 under SA-553/SA-553M (identical with A553/A553M-17). They are not presented as the A553/A553M-22 text.
Name the edition required on the purchase order: ASTM A553/A553M-22, ASME SA-553/SA-553M in the stated Section II year, or both when dual documents are required. We produce and export to the documents named on the order.
| Element | Type I heat analysis (wt. %) | Type I product analysis (wt. %) |
|---|---|---|
| Carbon (C), max | 0.13 | 0.13 |
| Manganese (Mn), max | 0.90 | 0.98 |
| Phosphorus (P), max | 0.015 | 0.015 |
| Sulfur (S), max | 0.015 | 0.015 |
| Silicon (Si) | 0.15–0.40 | 0.13–0.45 |
| Nickel (Ni) | 8.50–9.50 | 8.40–9.60 |
Carbon, phosphorus and sulfur limits apply to both heat and product analyses. Silicon may be less than the stated heat-analysis minimum of 0.15% if total aluminum is 0.030% or over, or if acid-soluble aluminum is 0.025% or over; the matching product-analysis note allows silicon below 0.13% on the same aluminum basis. Type III is a separate official type in the same table and is specified on its own product page.
Tensile and impact requirements for ASTM A553 Type I
The current ASTM publication is A553/A553M-22. Its published scope lists three types — Type I (nominal 9% nickel), Type II (nominal 8% nickel) and Type III (nominal 7% nickel) — and requires impact testing at −320 °F [−195 °C] for Type I or Type III and at −275 °F [−170 °C] for Type II, unless another temperature is agreed. Maximum thickness is limited only by the capacity of the material to meet the specified mechanical property requirements.
The chemical composition, tensile values and heat-treatment temperatures below are those of ASTM A553/A553M-17, as published in ASME BPVC Section II, Part A, 2023 under SA-553/SA-553M (identical with A553/A553M-17). They are not presented as the A553/A553M-22 text.
Name the edition required on the purchase order: ASTM A553/A553M-22, ASME SA-553/SA-553M in the stated Section II year, or both when dual documents are required. We produce and export to the documents named on the order.
Table 2 tensile requirements in the A553/A553M-17 / SA-553 2023 text are the same for the types covered by that table.
| Property | Requirement (A553/A553M-17 as in SA-553, 2023) |
|---|---|
| Tensile strength | 100–120 ksi [690–825 MPa] |
| Yield strength (0.2% offset), min | 85 ksi [585 MPa] |
| Elongation in 2 in. [50 mm], min | 20.0% (see A20/A20M for elongation adjustment) |
| Impact test method | Charpy V-notch to A20/A20M |
| Specimen orientation | Longitudinal axis of the specimen transverse to the final rolling direction |
| Default test temperature for this type | −320 °F [−195 °C], unless otherwise agreed |
| Mandatory acceptance | Each specimen: lateral expansion opposite the notch not less than 0.015 in. [0.381 mm] |
Optional S55 and S56 energy-absorption requirements apply only when ordered. They are not the default mandatory impact criterion.
Heat treatment for ASTM A553 Type I
Plates are supplied in the water-quenched and tempered condition. Shell plates and other parts heated for forming shall be heat treated after forming to the same procedure.
- Hardening: heat to a suitable temperature in the range 1475–1700 °F [800–925 °C], hold long enough to obtain a uniform temperature through the thickness, and quench in water (the detailed hardening clause also says quench in a liquid medium).
- Tempering 1050–1175 °F [565–635 °C] for Type I: hold at least 30 min/in. [1.2 min/mm] of thickness and not less than 15 min, then cool in air or quench at a rate not less than 300 °F/h [165 °C/h].
Before tempering, plates may receive an optional intermediate heat treatment (1165–1290 °F [630–700 °C] for Type I), held at least 15 min, then cooled as specified by thickness in the standard. When that optional treatment is used, plates are marked QTT instead of QT. The intermediate treatment may be performed at the manufacturer option or specified by the purchaser. This page does not offer heat-treatment or fabrication services.
The heat-treatment temperatures above are those of ASTM A553/A553M-17 as published in ASME BPVC.II.A-2023 SA-553/SA-553M. They are not presented as the A553/A553M-22 text.
Water quenched and tempered: heat 1475–1700 °F [800–925 °C] and water quench; temper 1050–1175 °F [565–635 °C] for Type I and Type II, hold at least 30 min/in. [1.2 min/mm] and not less than 15 min, then air cool or quench at not less than 300 °F/h [165 °C/h]. Optional intermediate treatment is marked QTT. Temperatures are those of ASTM A553/A553M-17 as published in ASME BPVC.II.A-2023 SA-553/SA-553M; they are not presented as the A553/A553M-22 text.
Welding and handling notes
ASTM A553 covers plates intended for the fabrication of welded pressure vessels. Welding procedures and any post-weld heat treatment belong to the project specification and the fabricator. This page does not offer fabrication or procedure qualification.
The specification warns that the material is susceptible to magnetization and that magnets should be avoided in handling after heat treatment if residual magnetism would be detrimental.
General requirements, marking and dimensions
Material supplied to ASTM A553/A553M shall conform to ASTM A20/A20M except where A553/A553M prevails. Dimensional tolerances are those of the ordered A20/A20M edition and the mill documents, not a stock list. In the A553-17 / SA-553 text, each plate is marked QT, or QTT when the optional intermediate heat treatment is used, in addition to A20/A20M marking. Plates shall be descaled by the producer after heat treatment.
Applications and specification limits
We produce and export this plate for projects that specify ASTM A553/A553M Type I. The specification is written for welded pressure vessels in the water-quenched and tempered condition. This page does not treat Type I, Type II and Type III as interchangeable.
Compare ASTM A553 Type I with related nickel steel plates
Type is the official ASTM split in A553/A553M. Type I is nominal 9% nickel and Type II is nominal 8% nickel. They share one tensile table in the A553-17 / SA-553 text but not the same nickel window or default impact temperature. European X8Ni9 is a 9% nickel grade; it is not an 8% nickel name.
| Material | Alloy / type | Delivery condition | Mechanical requirements | Typical service | Substitution limit |
|---|---|---|---|---|---|
| ASTM A553 Type I (this plate) | Official Type I, nominal 9% nickel; not a Grade or Class | Water quenched and tempered; optional intermediate treatment marked QTT | Tensile 100–120 ksi [690–825 MPa]; yield 85 ksi [585 MPa] min; impact −320 °F [−195 °C]; lateral expansion not less than 0.015 in. [0.381 mm] | Welded pressure vessels specified to A553 Type I | Do not substitute Type II (8% nickel, different impact temperature) or double-normalized A353 without a project review |
| ASTM A353 9% nickel steel plate | 9% nickel plate with no Type split | Double-normalized and tempered | Same tensile range; yield 75 ksi [515 MPa] min; same default −320 °F [−195 °C] impact temperature and 0.015 in. lateral-expansion floor | Orders written to A353 rather than A553 | Related nickel level, different heat treatment and a lower specified minimum yield. Not an automatic Type I substitute |
| ASTM A553 Type II (related type in the same specification) | Official Type II, nominal 8% nickel | Water quenched and tempered; same tempering range as Type I | Same tensile and yield table in the A553-17 / SA-553 text; default impact −275 °F [−170 °C] | Orders written to Type II | Different nickel window and different default impact temperature. Not Type I |
| EN 10028-4 X8Ni9 | European 9% nickel grade, steel number 1.5662 | Usually quenched and tempered on our X8Ni9 page | From our live X8Ni9 page: steel number 1.5662; nickel about 8.50–9.50% (the 8 in X8Ni9 is not 8% nickel); delivery usually quenched and tempered; yield in the 490 MPa class after QT; tensile 640–840 MPa; Charpy specified at −196 °C when the order follows that grade. | EN 10028-4 9Ni vessel plate | Near equivalent only. X8Ni9 is 9% nickel, which is why it is compared with Type I, not Type II |
| EN 10028-4 X7Ni9 | European 9% nickel sister grade, steel number 1.5663 | Usually quenched and tempered on our X7Ni9 page | From our live X7Ni9 page: steel number 1.5663; nickel about 8.50–9.50%; tighter carbon band than X8Ni9; usually QT; yield in the 490 MPa class after QT; tensile 640–840 MPa. | EN 10028-4 9Ni vessel plate | Near equivalent only |
| GB/T 713.4-2023 06Ni9DR | Chinese 9% nickel low-temperature vessel plate | Quenched and tempered or double-quenched and tempered on our 06Ni9DR page | From our live 06Ni9DR page: current rules in GB/T 713.4-2023 (this name left GB/T 24510-2017 and GB/T 3531-2014); nickel 8.50–10.00%; yield 560 MPa at 5–30 mm; tensile 680–820 MPa; delivery quenched and tempered or double-quenched and tempered; impact −196 °C; lateral expansion not less than 0.64 mm. | GB/T 713.4-2023 9Ni vessel plate | Near equivalent only. Yield, nickel window and impact acceptance differ |
Related published ranges: EN 10028-4 and GB/T 713.4-2023.
Equivalent and related grades by country
Near equivalents only. Type II in particular has no live European 8% nickel counterpart on this site; X8Ni9 must not be read as 8% nickel.
| Country / region | Standard | Grade or designation | Similarity and key differences | Substitution caveat |
|---|---|---|---|---|
| United States | ASTM A553/A553M-22 | Type I (nominal 9% nickel) | This plate. Quenched and tempered 9% nickel. Numerical chemistry and tensile tables on this page are from ASTM A553/A553M-17 as published in ASME BPVC.II.A-2023 SA-553/SA-553M. The current ASTM publication is A553/A553M-22; name the edition on the order. | This product |
| United States | ASME SA-553/SA-553M | Type I | BPVC.II.A-2023 marks SA-553/SA-553M identical with ASTM A553/A553M-17, not with A553/A553M-22. | Not an automatic dual stamp. |
| United States | ASTM A353/A353M-17(2022) | 9% nickel plate | Double-normalized and tempered 9% nickel; lower specified minimum yield (75 ksi vs 85 ksi). | Related, not interchangeable. |
| Europe | EN 10028-4 | X8Ni9 / X7Ni9 / X10Ni9 | 9% nickel European grades; usually QT on our live pages. | Near only. X8Ni9 is 9% nickel, not 8% nickel. |
| China | GB/T 713.4-2023 | 06Ni9DR | From our live 06Ni9DR page: current rules in GB/T 713.4-2023 (this name left GB/T 24510-2017 and GB/T 3531-2014); nickel 8.50–10.00%; yield 560 MPa at 5–30 mm; tensile 680–820 MPa; delivery quenched and tempered or double-quenched and tempered; impact −196 °C; lateral expansion not less than 0.64 mm. | Near only. |
| Japan | JIS G3127 | 9% nickel plate (SL9N590 cited on our 06Ni9DR page) | Japanese nickel steel plate specification. Complete official grade list not restated here. | Near only. No live JIS G3127 product page yet. |
Why choose SHH STEEL for ASTM A553 Type I
- We produce and export ASTM A553 Type I 9% nickel steel plate
- We review the enquiry for the named standard edition, type or designation, heat treatment, dimensions and any extra tests
- We keep ASTM and ASME orders distinct unless the purchase order requires dual documentation and both texts can be met
- We keep A353 double-normalizing distinct from A553 quenching and tempering, and Type I distinct from Type II
- We match the inspection document to what the purchase order requires
How to enquire for ASTM A553 Type I plate
| Item | What to specify |
|---|---|
| Standard and type | ASTM A553 Type I (name the Type) and the ASTM edition required; the current ASTM publication is A553/A553M-22 |
| Heat treatment | Water quenched and tempered; say if QTT (optional intermediate treatment) is required |
| Dimensions | Required thickness, width and length |
| Chemistry | Heat and product analysis for Type I; name the ASTM edition required on the order |
| Mechanical tests | Tension to Table 2 of the ordered edition; Charpy V-notch at −320 °F [−195 °C] unless otherwise agreed |
| Other tests | S55/S56 or NDE only when written on the order |
| Documentation | State the inspection document type required by the project |
| Code documents | If ASME SA-553 Type I documents are also required, say so explicitly and name the Section II edition |
Thickness, width and length are taken from the enquiry. This page does not list stock sizes, mill capacity or fabrication services.
Request a quotation
Contact SHH STEEL for a quotation for ASTM A553 Type I 9% nickel steel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
Specify ASTM A553 Type I, the ASTM edition required (the current publication is A553/A553M-22), and water-quenched and tempered delivery. If QTT marking, a non-default impact temperature, S55/S56, ultrasonic examination or ASME SA-553 Type I documents are required, include those acceptance criteria.
If you are considering a related European, Chinese or Japanese nickel steel grade as an alternative, send the applicable standard and project specification with your enquiry. We will review the differences in chemistry, heat treatment, impact rules and documentation rather than assume that related grades are interchangeable.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com