EN 10028-4 X7Ni9 9% nickel cryogenic pressure vessel steel plate, −196 °C, 1.5663, SHH STEEL

EN 10028-4 X7Ni9 Steel Plate | X7Ni9 9Ni -196°C Vessel Plate supplier

EN 10028-4 X7Ni9 is European 9Ni cryogenic vessel plate, steel number 1.5663. Yield is 490 MPa class. Impact is −196 °C. SHH STEEL supplies X7Ni9 worldwide as a global steel mill sourcing partner.
Keywords
EN 10028-4 X7Ni9, X7Ni9, X7Ni9 steel plate, 1.5663, X7Ni9 9Ni, X7Ni9 -196°C, X7Ni9 LNG, X7Ni9 equivalent, X7Ni9 supplier
Equivalent Grades:
EN X7Ni9 / ASTM A553 Type I (improved) / ASME SA553 Type I / GB 06Ni9DR (premium) — Material Specification: EN 10028-4 — Delivery: Quenched + Tempered (QT) or Q+Q+T; -196℃ LNG, stricter inclusion control
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
9Ni -196°C Cryogenic Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10028-4 X7Ni9 Steel ?

X7Ni9 is the lower-carbon 9Ni sister in EN 10028-4. Buyers search EN 10028-4 X7Ni9, X7Ni9 steel plate, 1.5663, X7Ni9 9Ni -196°C vessel plate, X7Ni9 LNG and X7Ni9 supplier. Nickel is about 8.50–9.50%. Carbon is tighter than on X8Ni9. This page is not X8Ni9. X8Ni9 is steel number 1.5662. This page is not X10Ni9. This page is not 12Ni14. 12Ni14 is 3.5Ni. This page is not X12Ni5. X12Ni5 is 5Ni.

Yield is in the 490 MPa class after quench and temper. Tensile is 640–840 MPa. Steel number is 1.5663. Delivery is usually quenched and tempered (QT). Charpy is specified at −196 °C when the order follows this grade. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check the certificate against EN 10028-4, and ship it to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America.

Do not ship X8Ni9 against an X7Ni9 drawing and call 9Ni the same. Do not ship 06Ni9DR steel plate and call 9Ni automatic dual name unless both books are met. Dual marking is possible only when chemistry, tensile, impact temperature and delivery all fit.

Company scope: global exporter SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-4 X7Ni9 Confirmed
Steel number 1.5663 Confirmed
Product specification EN 10028-4 + EN 10028-1 Applied
Steel type 9Ni cryogenic vessel plate Confirmed
Usual delivery QT quenched and tempered Confirmed
Yield idea 490 MPa class Confirmed
Tensile 640–840 MPa Confirmed
Impact idea −196 °C Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates and nuclear-grade steel plates when the project file uses that path. Chinese 9Ni belongs on GB/T 713.4. 3.5Ni ASME comparisons belong on ASME SA-203.

Chemical Composition

Cast analysis follows EN 10028-4. Product analysis follows EN 10028-1 when ordered. People who search X7Ni9 chemical composition and 1.5663 chemistry want the tighter carbon band plus 9% nickel, not an X8Ni9 table copied across.

Cast Analysis and Product Analysis — EN 10028-4 X7Ni9 (1.5663)

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C), max 0.10 0.12
Silicon (Si), max 0.35 0.40
Manganese (Mn) 0.30 – 0.80 0.25 – 0.85
Phosphorus (P), max 0.015 0.020
Sulfur (S), max 0.010 0.013
Aluminum total (Al), min 0.020 0.015
Nitrogen (N), max 0.020 0.024
Nickel (Ni) 8.50 – 9.50 8.40 – 9.60
Chromium (Cr), max 0.25 0.30
Copper (Cu), max 0.30 0.35
Molybdenum (Mo), max 0.10 0.12
Vanadium (V), max 0.05 0.06

Nickel at 8.50–9.50% is the grade marker. The X7 name is there because carbon is held down for −196 °C toughness. This is still 9Ni, not 5Ni and not 3.5Ni. SHH STEEL prints heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search X7Ni9 mechanical properties, X7Ni9 yield strength and X7Ni9 -196°C. Strength comes from quench and temper.

Tensile and Yield — EN 10028-4 X7Ni9

Thickness (mm) Yield min (MPa) Tensile (MPa)
≤ 30 490 640 – 840
30 – 50 480 640 – 840
50 – 80 470 620 – 820
Density 7.85 g/cm³ 7.85 g/cm³

Elongation is typically 18% min on thinner plate. Charpy for this grade is −196 °C. Energy is commonly 70 J average when the LNG file names that value, or 27 J when the order follows the base book. Location and orientation must be written. Do not assume an X8Ni9 certificate covers X7Ni9.

Do not quote 490 MPa yield on a plate that was only normalized. Do not treat −196 °C as permission to stamp 06Ni9DR steel plate without checking both books.

Material Comparison

Grade Book What buyers search Swap?
EN 10028-4 X8Ni9 EN 10028-4 X8Ni9 steel plate No auto swap
EN 10028-4 X7Ni9 EN 10028-4 X7Ni9 steel plate This page
EN 10028-4 X10Ni9 EN 10028-4 X10Ni9 No auto swap
EN 10028-4 X12Ni5 EN 10028-4 X12Ni5 5Ni No
EN 10028-4 12Ni14 EN 10028-4 12Ni14 3.5Ni No
06Ni9DR steel plate GB/T 713.4 06Ni9DR No auto swap
07Ni5DR steel plate GB/T 713.4 07Ni5DR No
08Ni3DR steel plate GB/T 713.4 08Ni3DR No
SA203 Grade E SA-203 SA203 Gr.E No

Equivalent Material Grades

Designation Standard / region Notes
EN 10028-4 X7Ni9 / 1.5663 EN 10028-4 Name on this page
X8Ni9 / 1.5662 EN 10028-4 Sister 9Ni name
X10Ni9 / 1.5665 EN 10028-4 Sister 9Ni name
06Ni9DR steel plate GB/T 713.4 Chinese 9Ni −196 °C
06Ni7DR steel plate GB/T 713.4 7Ni
07Ni5DR steel plate GB/T 713.4 5Ni
08Ni3DR steel plate GB/T 713.4 3.5Ni
ASTM A353 / ASME SA-353 A353 / SA-353 9Ni double-normalized talk
ASTM A553 Type I / SA-553 A553 / SA-553 9Ni QT talk

9Ni -196°C Cryogenic Service

Buyers pick X7Ni9 when a PED / LNG file names this exact 9Ni designation. Search phrases such as X7Ni9 LNG, X7Ni9 -196°C and 1.5663 steel plate all point here.

It is not a substitute for 08Ni3DR steel plate. That grade is 3.5Ni. It is not a substitute for 07Ni5DR steel plate. That grade is 5Ni. It is not a substitute for Q400GMDR steel plate. That grade is high-Mn cryogenic plate, not 9Ni.

An ASME file should name A353 / SA-353 or A553 Type I / SA-553. Dual marking is possible only when both books are met. SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

X7Ni9 is 9Ni cryogenic vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is an LNG tank or cryogenic vessel.

Qualify to the applicable code. Consumables must match 9Ni practice and keep toughness at −196 °C. A 3.5Ni procedure written for SA203 Grade D is the previous family. A 5Ni procedure written for X12Ni5 is the previous family. An X8Ni9 procedure is a sister procedure, not an automatic cover. A carbon procedure written for SA516 Grade 70 is not valid. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is quenched and tempered EN 10028-4 X7Ni9 (QT). Double-normalize routes exist on related ASME 9Ni books. Write the route on the order.

If the tank will see a heat cycle, say so. Many 9Ni tanks limit conventional carbon-steel PWHT. Impact after any simulated cycle must be named. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists EN 10028-4 X7Ni9; 1.5663; heat number; cast analysis including nickel; product analysis when ordered; tensile to the correct thickness column; QT; Charpy at −196 °C when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for X7Ni9 9Ni -196°C vessel plate:

  • Thickness: commonly 6 mm – 80 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Sister 9Ni is X8Ni9. 5Ni plate is X12Ni5 / 07Ni5DR steel plate. 3.5Ni plate is 12Ni14 / 08Ni3DR steel plate. Chinese 9Ni is 06Ni9DR steel plate.

Tolerances

Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another table. Class A is the usual default. If the calculation used minimum thickness after corrosion, write the allowed minus. Do not apply ASTM A36 structural tolerances to a PED −196 °C 9Ni plate without writing them. When dual-named against 06Ni9DR or A553 Type I, write which thickness table governs.

Supplementary Requirements

Charpy details. Write −196 °C, joules, location and orientation. LNG files often want 70 J, not only 27 J.

Impact after simulated heat treatment. When the tank procedure uses a cycle.

Product analysis. Especially nickel, carbon, P, S and Al.

NDE. EN 10160 or ASTM A435 / A578 as named. LNG tanks often add tighter UT.

Third-party. EN 10204 3.2 when written.

Applications

Industry Typical components
LNG inner tanks EN 10028-4 X7Ni9 shells at −196 °C
Liquid nitrogen / ethylene cryogenic vessels X7Ni9 courses
Dual-certified export X7Ni9 / 06Ni9DR steel plate when both books fit
Comparison vs X8Ni9 X7Ni9 when the drawing names 1.5663

X7Ni9 is the plate for a PED / LNG file that names this exact 9Ni designation. It is the wrong plate for a −40 °C carbon tank. That work is P355NL1. It is the wrong plate for 3.5Ni at −100 °C. That work is 12Ni14.

Supply Capability

SHH STEEL sources EN 10028-4 X7Ni9 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or QT route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, thicker by mill agreement.

Processing: CNC or flame cutting, bevel, flattening, UT to EN 10160 or the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard QT about 45–60 days; simulated heat treatment / 3.2 about 2 months.

Company scope: worldwide delivery SHH STEEL.

Why Choose SHH STEEL

Experience on this grade is simple: X7Ni9 and −196 °C must both be on the certificate. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices X7Ni9 from first-line mills, reports 1.5663 chemistry including nickel, records QT, prints Charpy at −196 °C when ordered, and issues 3.1 as standard or 3.2 when specified.

We keep the grade on the order. X7Ni9 is not X8Ni9. X7Ni9 is not X10Ni9. X7Ni9 is not 12Ni14. X7Ni9 is not Q345R steel plate. If the drawing says X8Ni9, we will not ship X7Ni9 and call 9Ni close.

Company scope: global exporter SHH STEEL.

FAQ

What is X7Ni9 steel plate?
X7Ni9 is an EN 10028-4 9Ni cryogenic pressure-vessel plate, steel number 1.5663. Yield is in the 490 MPa class after QT and tensile is 640–840 MPa. Impact is typically −196 °C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
What is the equivalent of X7Ni9?
Related comparisons are 06Ni9DR, ASTM A353 / SA-353 and ASTM A553 Type I / SA-553. Dual marking is possible only when both books are fully met.
How is X7Ni9 different from X8Ni9?
Both are 9Ni QT plate at −196 °C. X7Ni9 is steel number 1.5663. X8Ni9 is 1.5662. Carbon and exact book limits differ. Do not swap the names without checking the drawing.
How is X7Ni9 different from X10Ni9?
X10Ni9 is another 9Ni sister. Keep the designation that the PED file names.
How is X7Ni9 different from 12Ni14 and X12Ni5?
2Ni14 is 3.5Ni at about −100 °C. X12Ni5 is 5Ni at about −120 °C. X7Ni9 is 9Ni at −196 °C.
Is X7Ni9 used for LNG tanks?
Yes, when the file names X7Ni9. Many LNG files use X8Ni9 or 06Ni9DR instead. SHH STEEL ships the name that is written.
Can SHH STEEL ship X7Ni9 to the USA, Europe or the Middle East?
Ex-stock about 5–7 days when plate is in yard. Standard QT mill rolling about 45–60 days. Simulated heat treatment or 3.2 inspection about 2 months.

Conclusion

EN 10028-4 X7Ni9 Steel Plate is European 9Ni cryogenic pressure-vessel plate, steel number 1.5663, at the 490 MPa yield class and 640–840 MPa tensile after QT, with Charpy at −196 °C when ordered. Whether the inquiry says EN 10028-4 X7Ni9, 1.5663, X7Ni9 9Ni -196°C Vessel Plate or X7Ni9 supplier, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with X7Ni9 chemistry, recorded QT, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10028-4 X7Ni9 9Ni -196°C Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

EN 10028-4 X7Ni9 Steel Plate, X7Ni9 9Ni -196°C vessel plate, 1.5663, X7Ni9 supplier, global exporter SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X