GB/T 3531 Carbon Steel Plates
SHH STEEL offers GB/T 3531-compliant 15CrMoR low-alloy steel plates for low-temperature pressure vessels. GB/T 3531 specifies plates from 5-120mm thick for -196°C to -20°C service. Impact-tough, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GB/T 3531 06Ni9DR Steel Plate | 06Ni9DR -196°C Vessel Plate
GB/T 3531 06Ni9DR is 9 % nickel steel plate for cryogenic pressure vessels under GB/T 3531-2014. It is supplied quenched and tempered in 5–50 mm, with Charpy V-notch energy of 100 J minimum at -196°C and minimum yield of 560 MPa up to 30 mm. The grade moved to GB/T 713.4-2023 in the 2023 revision. SHH STEEL produces and exports 06Ni9DR plate to the 2014 edition when the project documents call for it.View More -
GB/T 3531 08Ni3DR Steel Plate | 08Ni3DR -100°C Vessel Plate
GB/T 3531 08Ni3DR is 3.5 % nickel steel plate for low-temperature pressure vessels under GB/T 3531-2014. It is supplied normalized, normalized and tempered, or quenched and tempered in 6–100 mm, with Charpy V-notch energy of 60 J minimum at -100°C. The grade moved to GB/T 713.4-2023 in the 2023 revision. SHH STEEL produces and exports 08Ni3DR plate to the 2014 edition when the project documents call for it.View More -
GB/T 3531 09MnNiDR Steel Plate | 09MnNiDR -70°C Vessel Plate
GB/T 3531 09MnNiDR is low-carbon manganese-nickel steel plate for low-temperature pressure vessels under GB/T 3531-2014. It is supplied normalized or normalized and tempered in 6–120 mm, with Charpy V-notch energy of 60 J minimum at -70°C, the lowest test temperature among the low-alloy grades of the 2014 edition. SHH STEEL produces and exports 09MnNiDR plate to the 2014 edition when the project documents call for it.View More -
GB/T 3531 15MnNiNbDR Steel Plate | 15MnNiNbDR -50°C Vessel Plate
GB/T 3531 15MnNiNbDR is niobium-microalloyed manganese-nickel steel plate for low-temperature pressure vessels under GB/T 3531-2014. It is the highest-strength low-alloy grade of the 2014 edition, supplied normalized or normalized and tempered in 10–60 mm, with Charpy V-notch energy of 60 J minimum at -50°C. SHH STEEL produces and exports 15MnNiNbDR plate to the 2014 edition when the project documents call for it.View More -
GB/T 3531 15MnNiDR Steel Plate | 15MnNiDR -45°C Vessel Plate
GB/T 3531 15MnNiDR is manganese-nickel steel plate for low-temperature pressure vessels under GB/T 3531-2014. It is supplied normalized or normalized and tempered in 6–60 mm, with Charpy V-notch energy of 60 J minimum at -45°C. The grade was dropped from the 2023 successor standard, so it is now ordered to the 2014 edition or to a project specification that names it. SHH STEEL produces and exports 15MnNiDR plate when the project documents call for it.View More -
GB/T 3531 16MnDR Steel Plate | 16MnDR -40°C Vessel Plate
GB/T 3531 16MnDR is carbon-manganese steel plate for low-temperature pressure vessels under GB/T 3531-2014, the 2014 edition of the Chinese low-temperature vessel plate standard. It is supplied normalized or normalized and tempered and is Charpy tested at -40°C for plate up to 60 mm and at -30°C for thicker plate up to 120 mm, with 47 J minimum. SHH STEEL produces and exports 16MnDR plate to the 2014 edition when the project documents call for it.View More
GB/T 3531 Carbon Steel Plates
Nuclear-Grade Steel Plates
SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.
Nuclear-Grade Steel Plates
ASME SA542/SA542M
ASME SA543/SA543M
ASME SA612/SA612M
ASME SA662/SA662M
ASME SA737/SA737M
ASME SA202/SA202M
ASTM A202/A202M
ASTM A1017/A1017M
SA-1017/SA-1017M
ASTM A662/A662M
ASME SA724/SA724M
ASME SA736/SA736M
ASME SA832/SA832M
ASME SA533/SA533M
ASTM A533
ASME SA508/SA508M
ASTM A508
ASME SA387/SA387M
ASTM A387/A387M
ASME SA-738/SA-738M
ASTM A738
ASME SA-203/SA-203M
ASTM A203
EN 10028-7
RCC-M M3307
JIS G3118
GB/T 3531
GOST 10859
X