What is GB/T 3531-2014 09MnNiDR steel plate?
GB/T 3531 09MnNiDR Steel Plate is a low-carbon manganese-nickel, aluminium-killed plate for welded vessels in deep low-temperature service, ordered to GB/T 3531-2014. Carbon is held to 0.12 % maximum, nickel is 0.30–0.80 %, and the impact test is at -70°C.
GB/T 3531-2014, Steel plates for low temperature pressure vessels, was issued on 24 June 2014 as GB 3531-2014 and implemented on 1 April 2015, replacing GB 3531-2008. It was later converted to a recommended national standard, which is why it is cited as GB/T 3531-2014. It covers plates 5 mm to 120 mm thick for pressure vessels working from -196°C to below -20°C. The edition was withdrawn on 1 March 2024 and replaced by GB/T 713.3-2023, with the nickel grades moved to GB/T 713.4-2023.
The same designation continues in the 2023 book as GB/T 713.3 09MnNiDR. Order this page when the drawing or data sheet still names GB/T 3531-2014.
SHH STEEL produces and exports GB/T 3531-2014 09MnNiDR plate to the ordered edition, delivery condition, dimensions and extra tests written on the enquiry. This grade is listed in our GB/T 3531 range under Nuclear-Grade Steel Plates.
Material specification for GB/T 3531 09MnNiDR
The items below follow GB/T 3531-2014. Thickness, width, length and the inspection document are stated on the enquiry rather than listed here as stock or capacity ranges.
| Parameter | Detail |
|---|---|
| Standard | GB/T 3531-2014, Steel plates for low temperature pressure vessels (issued as GB 3531-2014; replaced GB 3531-2008) |
| Edition status | Withdrawn 1 March 2024. Replaced by GB/T 713.3-2023 for the low-alloy grades and GB/T 713.4-2023 for 08Ni3DR and 06Ni9DR. This page covers the 2014 edition only |
| Scope of the standard | Plates 5 mm to 120 mm thick for low-temperature pressure vessels from -196°C to below -20°C |
| Grades in the 2014 edition | 16MnDR, 15MnNiDR, 15MnNiNbDR, 09MnNiDR, 08Ni3DR, 06Ni9DR |
| Grade | 09MnNiDR |
| Delivery condition (Table 2) | Normalized, or normalized and tempered |
| Impact requirement | -70°C / 60 J for all tabulated thicknesses |
| Optional route for thick plate | Over 60 mm, normalizing followed by accelerated cooling and tempering by agreement |
| Thickness tabulated for this grade | 6–120 mm (standard limits in Table 2, not a stock range) |
| Steelmaking | Basic oxygen or electric furnace with secondary refining. Reduction ratio at least 3 from continuous-cast slab or ingot, at least 2 from electroslag remelted slab |
| Dimensions and tolerances | GB/T 709-2006, thickness tolerance Class B; Class C or tighter tolerances by agreement |
| Ultrasonic testing | Plate by plate for N or N+T plate over 20 mm and Q+T plate over 16 mm; method JB/T 4730.3, GB/T 2970 or GB/T 28297, class stated on the contract |
| Our supply | We produce and export 09MnNiDR plate to GB/T 3531-2014 with the dimensions, tests and inspection document written on the enquiry |
Chemical composition of GB/T 3531-2014 09MnNiDR
The heat analysis below is the 09MnNiDR row of GB/T 3531-2014 Table 1. The low carbon ceiling is the main reason the grade reaches -70°C toughness at modest strength.
| Element | Heat analysis, GB/T 3531-2014 Table 1 (wt. %) |
|---|---|
| Carbon (C) | ≤0.12 |
| Silicon (Si) | 0.15–0.50 |
| Manganese (Mn) | 1.20–1.60 |
| Nickel (Ni) | 0.30–0.80 |
| Niobium (Nb) | ≤0.04 |
| Total aluminium (Alt) | ≥0.020 |
| Phosphorus (P) | ≤0.020 |
| Sulfur (S) | ≤0.008 |
Notes to Table 1: Als may be determined instead of Alt, in which case Als shall be not less than 0.015 %; when Nb + V + Ti exceeds 0.015 %, aluminium is not an acceptance requirement. Nb, V and Ti may be added to improve properties, with Nb + V + Ti not more than 0.12 %, and the amounts added reported on the certificate. As residual elements, Cr and Cu are each limited to 0.25 % and Mo to 0.08 %, and Ni to 0.40 % where nickel is not a specified alloying element; the supplier need not analyse them when it guarantees compliance. Product analysis tolerances follow GB/T 222.
Mechanical properties of GB/T 3531-2014 09MnNiDR
Table 2 of GB/T 3531-2014 tabulates 09MnNiDR in four bands up to 120 mm. Strength is lower than for 16MnDR, but elongation is higher and the impact requirement is -70°C / 60 J in every band.
| Nominal thickness (mm) | Tensile strength Rm (MPa) | Yield strength ReL, min (MPa) | Elongation A, min (%) | Charpy V test temperature | KV2, min (J) | 180° bend, b = 2a |
|---|---|---|---|---|---|---|
| 6–16 | 440–570 | 300 | 23 | -70°C | 60 | D = 2a |
| >16–36 | 430–560 | 280 | 23 | -70°C | 60 | D = 2a |
| >36–60 | 430–560 | 270 | 23 | -70°C | 60 | D = 2a |
| >60–120 | 420–550 | 260 | 23 | -70°C | 60 | D = 2a |
Charpy V-notch energy is the mean of three specimens. One single value may fall below the Table 2 figure, but not below 70 % of it. Plates under 12 mm are tested with sub-size specimens: 10 × 7.5 × 55 mm for plate over 8 mm and under 12 mm, with results not less than 75 % of the Table 2 value, and 10 × 5 × 55 mm for 6–8 mm plate, with results not less than 50 %. Plate thinner than 6 mm is not impact tested. Higher impact energy than Table 2 may be agreed and written on the contract. Yield is ReL; where yielding is not distinct, Rp0.2 is measured instead. In the bend column, a is the specimen thickness and D the mandrel diameter; the bend test may be waived when the supplier guarantees it.
Delivery conditions for GB/T 3531 09MnNiDR
Table 2 lists 09MnNiDR as normalized, or normalized and tempered. With the purchaser’s agreement, plate thicker than 60 mm may be supplied normalized, accelerated cooled and tempered. State the condition on the order, and request simulated PWHT testing if the vessel will be stress relieved.
Welding and thermal cutting
The low carbon content gives 09MnNiDR good weldability. The weld metal and heat-affected zone must still reach -70°C toughness, so consumables and heat input are chosen by the qualified procedure with impact tests at the required temperature.
Preheat, interpass temperature and post-weld heat treatment are set by the procedure qualification, the thickness and the vessel code.
Dimensions, tolerances and inspection
Dimensions, shape and permitted deviations follow GB/T 709-2006. Thickness tolerance is Class B unless the purchaser asks for Class C, and tighter tolerances may be agreed. Plates are invoiced on theoretical weight, calculated from the mean of the maximum and minimum permitted thickness.
Cracks, blisters, scabs, folds and inclusions are not permitted on the surface. They may be removed by dressing, provided the dressed depth does not exceed half the thickness tolerance and the minimum permitted thickness is kept. Dressed areas must be smooth.
Acceptance is by batch: one grade, one heat, one thickness and one heat-treatment condition, not more than 30 t per batch; a single plate heavier than 30 t is its own batch. Each batch receives one tensile test, one bend test and a set of three Charpy specimens; chemical analysis is one per heat. Ultrasonic testing is plate by plate for normalized or normalized-and-tempered plate thicker than 20 mm.
Applications and specification limits
We produce and export 09MnNiDR for low-temperature vessels designed around a -70°C impact class, such as ethylene and propane process equipment, deethanizer and demethanizer duty, carbon dioxide service and refrigerated storage. Some designers also use it for -40°C vessels where extra toughness margin over 16MnDR is wanted. The allowable minimum design temperature is set by the vessel code and the impact test.
Edition note. This page is the GB/T 3531-2014 product. Its 2023 successor coverage is GB/T 713.3 09MnNiDR, with revised chemistry and mechanical tables; the 2023 book also limits its scope to service not below -70°C. The 2014 and 2023 books are not the same specification, and a certificate to one edition is not an automatic substitute for an order written to the other.
GB/T 3531-2014 is a low-temperature pressure vessel plate standard. On its own it does not impose nuclear-class requirements; where a nuclear or other special code applies, its supplementary requirements must be written on the order.
Compare GB/T 3531 09MnNiDR with other low-temperature plates
The comparison below places 09MnNiDR against the 2014 low-alloy grades, its 2023 successor and the 3.5 % nickel grade used below -70°C. These grades are related, not interchangeable.
| Material | Type | Delivery | Key requirement | Substitution limit |
|---|---|---|---|---|
| GB/T 3531 09MnNiDR (this plate) | Low-C Mn-Ni | N or N+T | ReL 300 MPa min at 6–16 mm; -70°C / 60 J; to 120 mm | 2014 edition only |
| GB/T 3531 16MnDR | C-Mn | N or N+T | ReL 315 MPa min at 6–16 mm; -40°C / 47 J to 60 mm | Not for -70°C service |
| GB/T 3531 15MnNiDR | Mn-Ni | N or N+T | -45°C / 60 J; to 60 mm | Higher test temperature |
| GB/T 3531 08Ni3DR | 3.5 % Ni | N, N+T or Q+T | -100°C / 60 J | Deeper cold; nickel steel |
| GB/T 713.3 09MnNiDR | Low-C Mn-Ni (2023 edition) | N or N+T | 2023 tables; see that page | Successor coverage, not the same specification |
| GB/T 713.3 11MnNiMoDR | 2023 Mn-Ni-Mo grade | See that page | 2023 tables | New 2023 grade, not in GB/T 3531-2014 |
Equivalent and related grades by country
The grades below are near equivalents by impact class and chemistry family, not certified equivalents. Check chemistry, strength bands and impact rules against the project specification.
| Country / region | Standard | Grade | Similarity and key differences | Caveat |
|---|---|---|---|---|
| China | GB/T 3531-2014 | 09MnNiDR | This product | — |
| China | GB/T 713.3-2023 | GB/T 713.3 09MnNiDR | Same designation in the successor book with revised tables | Different edition; not automatic |
| Europe | EN 10028-4 | EN 10028-4 11MnNi5-3 | Low-carbon Mn-Ni plate for low-temperature vessels | Different nickel window and impact temperature |
| Europe | EN 10028-4 | EN 10028-4 13MnNi6-3 | Mn-Ni plate for low-temperature vessels | Higher carbon and manganese |
| United States | ASTM A203 | ASTM A203 Grade A | 2.25 % Ni plate used for similar cold service | Much higher nickel; different chemistry route |
| Japan | JIS G3127 | JIS G3127 SL2N255 | 2.5 % Ni low-temperature plate | Nickel steel, not Mn-Ni |
Why choose SHH STEEL for GB/T 3531 09MnNiDR
- SHH STEEL produces and exports GB/T 3531-2014 09MnNiDR plate as a producer, exporter and mill agent
- We quote to the edition written on your order and keep GB/T 3531-2014 values separate from GB/T 713.3 or GB/T 713.4 values
- We confirm whether thick 09MnNiDR may use the accelerated-cooling route before quoting
- We review impact temperature, ultrasonic class and any simulated PWHT before quoting, not after rolling
- We match the inspection document to what the purchase order requires
How to enquire for GB/T 3531 09MnNiDR plate
| Item | What to specify |
|---|---|
| Standard and grade | GB/T 3531-2014 09MnNiDR; state the edition year rather than only GB/T 3531 |
| Delivery condition | Normalized, or normalized and tempered; over 60 mm, normalized + accelerated cooling + tempered if agreed; state if simulated PWHT is required |
| Dimensions | Thickness, width and length; we confirm production and export feasibility against the enquiry |
| Impact testing | Table 2 temperature and energy, or a higher agreed energy; state specimen orientation if the project specifies it |
| Ultrasonic testing | JB/T 4730.3, GB/T 2970 or GB/T 28297, with the acceptance class |
| Supplementary tests | Simulated post-weld heat treatment, through-thickness or product analysis only when written on the order |
| Documentation | Inspection document type required by the project, for example EN 10204 3.1 or 3.2 |
| Other editions | If GB/T 713.3-2023 or GB/T 713.4-2023 must also be met, say so on the enquiry; we review both editions before quoting |
FAQ
-
What impact temperature does GB/T 3531-2014 09MnNiDR meet?
- Table 2 requires 60 J minimum at -70°C for every tabulated thickness from 6 mm to 120 mm.
-
What is the yield strength of 09MnNiDR?
- Minimum ReL is 300 MPa at 6–16 mm, 280 MPa over 16–36 mm, 270 MPa over 36–60 mm and 260 MPa over 60–120 mm.
-
Can thick 09MnNiDR be accelerated cooled?
- Yes, with the purchaser's agreement. Plate over 60 mm may be supplied normalized, accelerated cooled and tempered under GB/T 3531-2014.
-
How does this page differ from the GB/T 713.3 09MnNiDR page?
- This page is the 2014 edition. The 2023 book revised the chemistry and mechanical tables. Order the edition your design documents name.
-
What should a quotation enquiry include?
- GB/T 3531-2014, grade 09MnNiDR, delivery condition, thickness by width by length, quantity, impact and ultrasonic requirements, any simulated PWHT, and the inspection document.
Request a quotation
Contact SHH STEEL for a quotation for GB/T 3531-2014 09MnNiDR low-temperature pressure vessel plate. Please include your required quantity, plate thickness, width and length, delivery destination and preferred delivery schedule so we can review your production and export requirements.
State the delivery condition, the Charpy test temperature and energy if they differ from Table 2, the ultrasonic testing standard and class, any simulated post-weld heat treatment, and the inspection document required by the project.
If you are considering 16MnDR, 08Ni3DR or the GB/T 713.3-2023 version of 09MnNiDR, send the design temperature and project specification. We will review the differences rather than assume the grades or editions are interchangeable.
For a detailed quotation, email your material specification, quantity and delivery requirements to our team.
Contact: admin@steelspecs.com