GB/T 713.4 08Ni3DR Steel Plate | 08Ni3DR 3.5Ni -100°C Vessel Plate
What is GB/T 713.4 08Ni3DR Steel?
08Ni3DR is Chinese 3.5Ni vessel plate. Buyers search GB/T 713.4 08Ni3DR, 08Ni3DR 3.5Ni -100°C vessel plate, GB/T 3531 08Ni3DR, GB/T 24510 08Ni3DR and 3.5Ni steel. All of those names belong on this page.
Current product rules sit in GB/T 713.4-2023. That book replaces GB/T 24510-2017. The same commercial name also left GB/T 3531-2014 when nickel grades moved into Part 4. Do not look for 08Ni3DR in GB/T 713.3. That part stops at low-alloy grades such as 09MnNiDR.
Yield is 320 MPa at 6–60 mm. Tensile is 490–620 MPa. Delivery is normalized or normalized and tempered. Quenched and tempered is allowed when the buyer agrees. Impact is −100 °C, 60 J. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade.
Do not ship 06Ni9DR against 08Ni3DR. 06Ni9DR is 9Ni and −196 °C. Do not ship 09MnNiDR. That grade is 0.3–0.8% Ni. Do not ship 07Ni5DR or 06Ni7DR and call them 3.5Ni.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | GB/T 713.4 08Ni3DR | Confirmed |
| Product Specification | GB/T 713.4-2023 (replaces GB/T 24510-2017) | Applied |
| Older names | GB/T 3531 08Ni3DR, GB/T 24510 08Ni3DR | Confirmed |
| Service idea | 3.5Ni vessels, not lower than −100 °C | Confirmed |
| Steel type | 3.5% nickel low-temp vessel plate | Confirmed |
| Usual delivery | N or N+T; QT if agreed | Confirmed |
| Yield idea | 320 MPa at 6–60 mm | Confirmed |
| Tensile | 490–620 MPa at 6–60 mm | Confirmed |
| Impact | −100 °C / 60 J | Confirmed |
| Thickness range | 6–150 mm in Table 2 | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | Americas, Europe, Middle East, Africa, Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. ASME comparisons belong on ASME SA203, not as automatic substitutes.
Chemical Composition
GB/T 713.4 08Ni3DR Steel Plate | 08Ni3DR 3.5Ni -100°C Vessel Plate
Brief Description
GB/T 713.4 08Ni3DR is Chinese 3.5% nickel low-temperature vessel plate for service down to -100 °C. Yield is 320 MPa at 6–60 mm. Tensile is 490–620 MPa. SHH STEEL supplies 08Ni3DR worldwide as a global steel mill sourcing partner. FOB Shanghai / CIF Houston / Antwerp / Ulsan.
SEO Title
GB/T 713.4 08Ni3DR Steel Plate | 08Ni3DR 3.5Ni -100°C Vessel Plate – SHH STEEL
SEO Keywords
GB/T 713.4 08Ni3DR, 08Ni3DR, 3.5Ni steel plate, GB/T 3531 08Ni3DR, GB/T 24510 08Ni3DR, SA203 Gr.D, 12Ni14, SL3N, 08Ni3DR supplier
SEO Description
SHH STEEL supplies GB/T 713.4 08Ni3DR 3.5Ni -100°C vessel plate worldwide, 320 MPa yield, 490–620 MPa tensile. FOB Shanghai / CIF Houston / Antwerp / Ulsan. EN 10204 3.1/3.2. Contact now.
General Description
08Ni3DR is Chinese 3.5Ni vessel plate. Buyers search GB/T 713.4 08Ni3DR, 08Ni3DR 3.5Ni -100°C vessel plate, GB/T 3531 08Ni3DR, GB/T 24510 08Ni3DR and 3.5Ni steel. All of those names belong on this page.
Current product rules sit in GB/T 713.4-2023. That book replaces GB/T 24510-2017. The same commercial name also left GB/T 3531-2014 when nickel grades moved into Part 4. Do not look for 08Ni3DR in GB/T 713.3. That part stops at low-alloy grades such as 09MnNiDR.
Yield is 320 MPa at 6–60 mm. Tensile is 490–620 MPa. Delivery is normalized or normalized and tempered. Quenched and tempered is allowed when the buyer agrees. Impact is −100 °C, 60 J. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade.
Do not ship 06Ni9DR against 08Ni3DR. 06Ni9DR is 9Ni and −196 °C. Do not ship 09MnNiDR. That grade is 0.3–0.8% Ni. Do not ship 07Ni5DR or 06Ni7DR and call them 3.5Ni.
Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | GB/T 713.4 08Ni3DR | Confirmed |
| Product Specification | GB/T 713.4-2023 (replaces GB/T 24510-2017) | Applied |
| Older names | GB/T 3531 08Ni3DR, GB/T 24510 08Ni3DR | Confirmed |
| Service idea | 3.5Ni vessels, not lower than −100 °C | Confirmed |
| Steel type | 3.5% nickel low-temp vessel plate | Confirmed |
| Usual delivery | N or N+T; QT if agreed | Confirmed |
| Yield idea | 320 MPa at 6–60 mm | Confirmed |
| Tensile | 490–620 MPa at 6–60 mm | Confirmed |
| Impact | −100 °C / 60 J | Confirmed |
| Thickness range | 6–150 mm in Table 2 | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | Americas, Europe, Middle East, Africa, Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates. ASME comparisons belong on ASME SA203, not as automatic substitutes.
Chemical Composition
Heat analysis follows GB/T 713.4 Table 1. Product analysis follows GB/T 713.1. Write both on the PO if the destination file needs finished-plate chemistry.
Heat Analysis and Product Analysis — GB/T 713.4 08Ni3DR
| Element | Heat Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.10 | 0.12 |
| Silicon (Si) | 0.15 – 0.35 | 0.13 – 0.40 |
| Manganese (Mn) | 0.30 – 0.80 | 0.25 – 0.85 |
| Phosphorus (P), max | 0.015 | 0.018 |
| Sulfur (S), max | 0.005 | 0.008 |
| Nickel (Ni) | 3.25 – 3.75 | 3.20 – 3.85 |
| Chromium (Cr), max | 0.25 | 0.30 |
| Copper (Cu), max | 0.35 | 0.40 |
| Molybdenum (Mo), max | 0.12 | 0.15 |
| Vanadium (V), max | 0.05 | 0.06 |
| Niobium (Nb), max | 0.08 | 0.10 |
| Acid-soluble aluminum (Alt), min | 0.015 | 0.010 |
| Cr + Mo + Cu, max | 0.50 | 0.55 |
Nickel is 3.25–3.75%. That is 3.5Ni, not 9Ni. For thickness greater than 100 mm, carbon upper limit may rise to 0.12% when the standard note applies. SHH STEEL reports heat analysis on every certificate and product analysis when the order names it.
Density is 7.85 g/cm³. Do not use the 7.89 g/cm³ figure from 9Ni plate.
Mechanical Properties
Tensile and Yield — GB/T 713.4 08Ni3DR
| Thickness (mm) | Yield min (MPa) | Tensile (MPa) |
|---|---|---|
| 6 – 60 | 320 | 490 – 620 |
| 60 – 100 | 300 | 480 – 610 |
| 100 – 150 | 290 | 470 – 600 |
| Density | 7.85 g/cm³ | 7.85 g/cm³ |
Elongation is 21% min. Impact is −100 °C, 60 J. Bend is 180°, D=3a. Tensile and impact specimens are transverse.
Do not quote 320 MPa yield on a 120 mm plate. Do not treat 490–620 MPa tensile as a free pass to stamp SA203 Gr.D without checking nickel, impact temperature and PWHT.
Material Comparison
| Grade | Book | Service idea | Swap? |
|---|---|---|---|
| GB/T 713.3 09MnNiDR | 0.3–0.8Ni, −70 °C | Different book | No |
| GB/T 713.4 08Ni3DR | 3.5Ni, −100 °C | This page | This page |
| GB/T 713.4 07Ni5DR | 5Ni | Different nickel | No |
| GB/T 713.4 06Ni7DR | 7Ni | Different nickel | No |
| GB/T 713.4 06Ni9DR | 9Ni, −196 °C | Different nickel | No |
| SA203 Gr.D | ASME 3.5Ni | Comparison only | No |
Equivalent Material Grades
Comparison names help a buyer search. They do not authorize substitution.
| Designation | Standard / region | Notes |
|---|---|---|
| GB/T 713.4 08Ni3DR | GB/T 713.4-2023 | Name on this page |
| GB/T 24510-2017 08Ni3DR | Replaced book | Same commercial name |
| GB/T 3531-2014 08Ni3DR | Old low-temp book | Moved into 713.4 |
| SA203 Gr.D | SA-203 | 3.5Ni comparison |
| SA203 Gr.E | SA-203 | 3.5Ni, higher strength |
| SA203 Gr.F | SA-203 | 3.5Ni QT |
| 12Ni14 | EN 10028-4 / ISO 9328-4 | Closest EN 3.5Ni |
| SL3N255 / SL3N275 / SL3N440 | JIS G3127 | Japanese 3.5Ni family |
| 06Ni9DR | GB/T 713.4 | 9Ni sister |
| 07Ni5DR | GB/T 713.4 | 5Ni sister |
| 09MnNiDR | GB/T 713.3 | Low-Ni sister |
| ASTM A36 steel plate | A36 | Structural, not nickel |
−100 °C 3.5Ni Pressure-Vessel Service
Buyers pick 08Ni3DR for ethylene-related equipment, low-temperature separators and other vessels that name Chinese 3.5Ni plate. It is not LNG inner-tank 9Ni plate. If the minimum design temperature is −196 °C, the drawing should name 06Ni9DR, SA353 or SA553.
It is not an ASME Section VIII plate by default. An ASME 3.5Ni file should name SA203 Gr.D, SA203 Gr.E or SA203 Gr.F and then write the extras. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia. Stainless inquiries belong on ASME SA240 or ASTM A240.
Weldability
08Ni3DR is 3.5Ni vessel plate. Treat welding as Code welding when the equipment is a vessel.
Qualify to the applicable code. ASME dual-name work uses ASME Section IX. Consumables must match 3.5Ni practice, not a 9Ni 06Ni9DR procedure and not a 09MnNiDR procedure. Preheat follows thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is normalized or normalized-and-tempered GB/T 713.4 08Ni3DR. Quenched and tempered is available when the order agrees. That is different from 06Ni9DR, which is QT by default.
If the vessel will see PWHT, say so. Test coupons then follow a simulated cycle. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists GB/T 713.4 08Ni3DR; heat number; heat analysis; product analysis when ordered; tensile to the correct thickness column; N, N+T or QT; impact at −100 °C. Certificates may be EN 10204 3.1 or EN 10204 3.2. UT to NB/T 47013.3 Class I is the GB default.
Dimensions
Usual supply range from SHH STEEL for 08Ni3DR 3.5Ni -100°C vessel plate:
- Thickness: commonly 6 mm – 150 mm
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
- Cut-to-length plates and nest sizes inside those limits
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering plate belongs on EN 10025-5 or Corten A/B. TMCP fine-grain structural belongs on EN 10025-4. QT structural belongs on EN 10025-6. Ordinary structural belongs on EN 10025-2 or JIS G3106.
Tolerances
Dimensional limits follow GB/T 713.1 and the mill rolling standard named on the order. Do not apply ASTM A36/A36M structural tolerances to a 3.5Ni vessel plate without writing them. UT to NB/T 47013.3 Class I is the GB default. EN 10160 or ASTM A435 / A578 may be added when the order names it.
Supplementary Requirements
Most export 08Ni3DR orders add extras. SHH STEEL does not assume them.
Charpy details. −100 °C, energy, location and orientation.
Product analysis. Add this when the destination file wants finished-plate chemistry.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. UT Class I unless a tighter class is written.
Z-direction. Z15 / Z25 / Z35 when the drawing names it.
HIC / NACE / SSC. Only when written.
Third-party. EN 10204 3.2, with inspectors arranged for US, Mexican, European, Middle East, Japanese or Korean documentation packages.
Applications
| Industry | Typical components |
|---|---|
| −100 °C 3.5Ni vessels | GB/T 713.4 08Ni3DR shells |
| Ethylene and cold-region tanks | 08Ni3DR courses |
| Separators and drums | 08Ni3DR plate from SHH STEEL |
| Dual-certified export | 08Ni3DR / SA203 Gr.D when chemistry fits |
Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless. Other vessel comparisons: SA203 Gr.B, SA302 Gr.B, A516 Grade 70, SA533 Type C Cl.1, SA517 Gr.P, SA738 Gr.C.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to:
- North America: USA, Mexico
- South America: Argentina, Peru and other South American ports
- Central America: El Salvador
- Europe: Spain, Netherlands, Germany and surrounding ports
- Middle East: UAE, Saudi Arabia and nearby Gulf ports
- Africa: South Africa
- South / Southeast Asia: India, Thailand, Singapore, Vietnam, Philippines
- East Asia: Japan, Korea
Typical trade terms on this grade: FOB Shanghai, CIF Houston, CIF Antwerp, CIF Ulsan, plus Rotterdam, Jebel Ali, Singapore, Busan, Barcelona, Yokohama, Manzanillo, Callao and Mumbai.
Typical lead time for GB/T 713.4 08Ni3DR:
- Ex-stock: about 5–7 days
- Mill rolling, standard N or N+T: about 45 days
- QT, simulated PWHT, 3.2 or extra NDE: about 2 months
Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading. Packing is seaworthy, with edge protection and marking in English as specified on the order.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / ASME / EN / DIN / JIS / GB steel to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia. On GB/T 713.4 08Ni3DR that means mill pricing, 08Ni3DR chemistry reported as heat analysis and as product analysis when ordered, recorded N, N+T or QT, tensile results to the correct thickness column, −100 °C impact, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. 08Ni3DR is not 06Ni9DR. 08Ni3DR is not 07Ni5DR. 08Ni3DR is not 09MnNiDR. 08Ni3DR is not SA203 Gr.D unless both books are met. If the drawing says 9Ni, we will not ship 3.5Ni and call nickel close.
Company scope: global steel mill sourcing partner – SHH STEEL.
FAQ
-
What is 08Ni3DR steel plate?
- 08Ni3DR is a GB/T 713.4 3.5% nickel low-temperature pressure-vessel plate. Yield is 320 MPa at 6–60 mm and tensile is 490–620 MPa. Impact is −100 °C / 60 J. Delivery is N or N+T, or QT when agreed. SHH STEEL supplies this plate as a global steel mill sourcing partner.
-
Does GB/T 713.4 replace GB/T 24510 and GB/T 3531 for 08Ni3DR?
- Yes. GB/T 713.4-2023 replaces GB/T 24510-2017. The same name also left GB/T 3531-2014.
-
What is the equivalent of 08Ni3DR?
- Related comparisons are SA203 Grade D / E / F, EN 12Ni14 and JIS SL3N255 / SL3N275 / SL3N440. Dual marking is possible only when both books are fully met.
-
How is 08Ni3DR different from 06Ni9DR?
- 08Ni3DR is 3.5Ni and −100 °C. 06Ni9DR is 9Ni and −196 °C.
-
How is 08Ni3DR different from 09MnNiDR?
- 09MnNiDR is GB/T 713.3 with 0.30–0.80% Ni and −70 °C. 08Ni3DR is GB/T 713.4 with 3.25–3.75% Ni and −100 °C.
-
Can SHH STEEL ship 08Ni3DR to the USA, Europe or Korea?
- Yes. SHH STEEL has supplied plates to the USA, Mexico, Europe, Korea, Japan, the Middle East, Southeast Asia, India, South Africa and South America.
-
What is the delivery time for 08Ni3DR?
- Ex-stock about 5–7 days. Standard N or N+T mill rolling about 45 days. QT, simulated PWHT or 3.2 inspection about 2 months.
Conclusion
GB/T 713.4 08Ni3DR Steel Plate is Chinese 3.5% nickel low-temperature pressure-vessel plate at the 320 MPa yield step, 490–620 MPa tensile at 6–60 mm, N or N+T delivery, for service down to −100 °C. Whether the inquiry says GB/T 713.4 08Ni3DR, GB/T 3531 08Ni3DR, GB/T 24510 08Ni3DR or 08Ni3DR 3.5Ni -100°C Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 08Ni3DR chemistry, heat and product analysis when ordered, recorded N, N+T or QT, −100 °C impact, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies GB/T 713.4 08Ni3DR 3.5Ni -100°C Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade. FOB Shanghai / CIF Houston / Antwerp / Ulsan.
Contact SHH STEEL for mill rolling, stock inquiry, N or N+T, QT, 3.2 inspection or a quotation.
GB/T 713.4 08Ni3DR Steel Plate, 08Ni3DR 3.5Ni -100°C vessel plate, SA203 Gr.D, 12Ni14, SL3N, 08Ni3DR supplier, global steel mill sourcing partner SHH STEEL