ASME SA841 Grade E Class 4 TMCP vessel plate, Gr.E Cl.4, YS 70 ksi, TS 84–104 ksi, max 40 mm, SHH STEEL

ASME SA841 Grade E Class 4 Steel Plate | SA841 Gr.E Cl.4 TMCP Vessel Plate

ASME SA841 Grade E Class 4 is TMCP vessel plate under ASME SA-841/SA-841M. Yield 485 MPa, tensile 580–715 MPa, max 40 mm. SHH STEEL supplies SA841 Gr.E Cl.4 mill-direct with 3.1 or 3.2 certificates.
Keywords:
ASME SA841 Grade E Class 4, SA841 Gr.E Cl.4, SA841GRE CL4, SA-841 Grade E Class 4, SA841 E4, TMCP vessel plate, SA841 Grade E Class 4 supplier
Equivalent Grades:
A841 Gr E / EN 10028-5 P500ML2-P550ML (near) / GB Q500CF-Q550CF — Material Specification: ASME SA-841 / ASTM A841 — Delivery: TMCP
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
TMCP Vessel Service
Weldability
Heat Treatment
Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA841 Grade E Class 4 Steel?

ASME SA841 Grade E Class 4 is one of the two Class lines assigned to Grade E in ASME SA-841/SA-841M. Grades A, B and C use Class 1 and Class 2. Grade D uses Class 3 only. Grade E uses Class 4 and Class 5. Class 4 is the lower of those two Grade E lines: 485 MPa yield and 580–715 MPa tensile. Maximum nominal thickness for Grade E is 40 mm. As Direct Mill Supply by SHH STEEL, the plate is produced to ASME SA-841/SA-841M by thermo-mechanical control process.

Buyers write the same product as SA841 Grade E Class 4, SA841 Gr.E Cl.4, SA841GRE CL4, SA-841 Grade E Class 4, SA841 E4 and SA 841 Gr E Cl 4. ASTM A841 Grade E Class 4 is the companion mill specification. A purchase order that only says “SA841 Grade E” is incomplete. Class 5 on the same Grade raises yield to 515 MPa. Those two plates do not interchange.

Do not read the Class number as a simple ladder across the whole specification. Class 3 on Grade D is 690 MPa yield. Class 4 on Grade E is 485 MPa yield. The Class number follows the Grade. It does not mean “stronger than Class 3.” This page is not [SA841 Grade D Class 3] chemistry with a different stamp. Grade E carbon is 0.07% maximum. Nickel max is 0.60%. Molybdenum max is 0.30%. That ladle is not Grade D.

This page is not SA537 Cl.2. SA537 Class 2 is heat-treated C-Mn-Si. SA841 Grade E Class 4 is TMCP. It is not SA517 Gr.B QT alloy. It is not SA533 Type B Class 1 QT Mn-Mo-Ni. It is not ASME SA516 and not ASME SA387.

Thickness is the second filter. Grade E stops at 40 mm. An 80 mm Class 4 inquiry cannot be rolled as SA841 Grade E. Dual marking SA841 / A841 Grade E Class 4 is available. Certificates can be EN 10204 3.1 or 3.2. Company scope: China steel Mill Agent-SHH STEEL.

Material Specification

ASME SA841 Grade E Class 4 Steel Plate | SA841 Gr.E Cl.4 TMCP Vessel Plate

Brief Description
ASME SA841 Grade E Class 4 is TMCP vessel plate under ASME SA-841/SA-841M. Yield 485 MPa, tensile 580–715 MPa, max 40 mm. SHH STEEL supplies SA841 Gr.E Cl.4 mill-direct with 3.1 or 3.2 certificates.

SEO Title
ASME SA841 Grade E Class 4 Steel Plate | SA841 Gr.E Cl.4 TMCP Vessel Plate – SHH STEEL

SEO Keywords
ASME SA841 Grade E Class 4, SA841 Gr.E Cl.4, SA841GRE CL4, SA-841 Grade E Class 4, SA841 E4, TMCP vessel plate, SA841 Grade E Class 4 supplier

SEO Description
SHH STEEL supplies ASME SA841 Grade E Class 4 / SA841 Gr.E Cl.4 TMCP vessel plate, 485 MPa yield, max 40 mm. China Mill Direct Exporter, EN 10204 3.1/3.2. Contact now.


General Description

ASME SA841 Grade E Class 4 is one of the two Class lines assigned to Grade E in ASME SA-841/SA-841M. Grades A, B and C use Class 1 and Class 2. Grade D uses Class 3 only. Grade E uses Class 4 and Class 5. Class 4 is the lower of those two Grade E lines: 485 MPa yield and 580–715 MPa tensile. Maximum nominal thickness for Grade E is 40 mm. As Direct Mill Supply by SHH STEEL, the plate is produced to ASME SA-841/SA-841M by thermo-mechanical control process.

Buyers write the same product as SA841 Grade E Class 4, SA841 Gr.E Cl.4, SA841GRE CL4, SA-841 Grade E Class 4, SA841 E4 and SA 841 Gr E Cl 4. ASTM A841 Grade E Class 4 is the companion mill specification. A purchase order that only says “SA841 Grade E” is incomplete. Class 5 on the same Grade raises yield to 515 MPa. Those two plates do not interchange.

Do not read the Class number as a simple ladder across the whole specification. Class 3 on Grade D is 690 MPa yield. Class 4 on Grade E is 485 MPa yield. The Class number follows the Grade. It does not mean “stronger than Class 3.” This page is not [SA841 Grade D Class 3] chemistry with a different stamp. Grade E carbon is 0.07% maximum. Nickel max is 0.60%. Molybdenum max is 0.30%. That ladle is not Grade D.

This page is not SA537 Cl.2. SA537 Class 2 is heat-treated C-Mn-Si. SA841 Grade E Class 4 is TMCP. It is not SA517 Gr.B QT alloy. It is not SA533 Type B Class 1 QT Mn-Mo-Ni. It is not ASME SA516 and not ASME SA387.

Thickness is the second filter. Grade E stops at 40 mm. An 80 mm Class 4 inquiry cannot be rolled as SA841 Grade E. Dual marking SA841 / A841 Grade E Class 4 is available. Certificates can be EN 10204 3.1 or 3.2. Company scope: China steel Mill Agent-SHH STEEL.


Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade / Class ASME SA841 Grade E Class 4 Confirmed
Product Specification ASME SA-841/SA-841M Applied
Companion Spec ASTM A841 Grade E Class 4 Dual cert available
General Requirements ASME SA-20 / ASTM A20 Applied
Process TMCP Confirmed
Grain practice Killed, fine austenitic grain Applied
Alloy idea Very low C, restricted S, limited Ni-Mo Confirmed
Intended use Welded pressure vessels As specified
Maximum Thickness 40 mm for Grade E Per SA-841
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in the pressure vessel steel plates family. It does not sit with carbon steel plates that have no TMCP Class 4 table, and it does not sit with structural steel plates or ASTM A36/A36M. If a buyer sends an HSLA cutting list from ASTM A572 and a vessel drawing on the same email, those are two different books.

SA-20 still governs marking, testing location, retests and repair rules. TMCP does not cancel SA-20. Two tension tests from each plate-as-rolled remain the specification habit unless the order tightens the plan.

Chemical Composition

ASME SA841 Grade E Class 4 uses Grade E chemistry. Class 4 and Class 5 share that table. The Class only changes the tensile line.

Heat Analysis — ASME SA841 Grade E

Element Heat Analysis (%)
Carbon (C), max 0.07
Manganese (Mn), t ≤ 40 mm 0.70 – 1.60
Phosphorus (P), max 0.015
Sulfur (S), max 0.005
Silicon (Si) 0.05 – 0.30
Copper (Cu), max 0.35
Nickel (Ni), max 0.60
Chromium (Cr), max 0.30
Molybdenum (Mo), max 0.30
Niobium (Nb), max 0.08
Vanadium (V), max 0.06

Product analysis follows SA-20 / A20 tolerances on those heat limits. Carbon at 0.07% maximum is lower than Grade A (0.20%), Grade B (0.15%), Grade C (0.10%) and Grade D (0.09%). Sulfur at 0.005% maximum is in the same tight band as Grade D. Nickel max is 0.60%, which is Grade B territory, not Grade D’s 1.0–5.0% band. A ladle at 2% nickel is Grade D chemistry, not Grade E.

There is no “over 40 mm” manganese line because Grade E is not permitted over 40 mm. If chromium and molybdenum sit in a SA387 Gr.11 Cl.2 or SA387 Gr.22 Cl.2 window, the plate belongs on the Cr-Mo page. If the process is QT Mn-Mo-Ni, look at SA533 Type B Class 2. If the ladle is carbon only, look at SA516 Gr.70 or SA515 Gr.70.

SHH STEEL reports heat analysis on every certificate, including nickel, molybdenum, phosphorus and sulfur, and adds product analysis when SA-20 requires it.

Mechanical Properties

Class 4 is the strength line on this page. Grade E only identifies the chemistry family.

Tensile Requirements — ASME SA841 Grade E Class 4

Property t ≤ 40 mm
Yield strength, min 485 MPa (70 ksi)
Tensile strength 580 – 715 MPa (84 – 104 ksi)
Elongation in 50 mm, min 20%
Density 7.85 g/cm³
Hardness Not a Table 3 default

There is no “over 40 mm” column. The specification marks thicker Class 4 on Grade E as not applicable. Do not quote 65 mm Class 2 numbers from Grades A–C onto this page. Grades A–C never use Class 4.

Class 5 on the same Grade E is 515 MPa yield and 605–745 MPa tensile. A Class 4 heat cannot be stamped Class 5 because the coupon came in high. Class 3 belongs to Grade D and sits at 690 MPa yield. Do not call Class 4 “the next step after Class 3” without reading the Grade letter.

Density is 7.85 g/cm³ for weight take-off. Hardness is not a mandatory SA-841 Table 3 value. Typical TMCP Class 4 plate sits around 170–220 HB. If a drawing writes a hardness cap, put that number on the order. SHH STEEL will then test and print it. Do not read Brinell as a substitute for the 485 MPa yield test.

Charpy is not a hidden default. Export tanks and winter shells almost always add an impact temperature. Write the temperature, energy, location and orientation. Simulated PWHT coupons are common because shops that buy Grade E still want a vessel cycle.

Do not treat 485 MPa yield as permission to substitute high strength low alloy plates, EN 10025-6 structural QT plate, or SA302 Gr.C. Those books have their own chemistry and Code listings.

Material Comparison

Grade Route Strength / thickness Swap?
SA841 Grade A/B/C Class 2 TMCP 415 MPa, to 100 mm No
SA841 Grade D Class 3 TMCP 690 MPa, 40 mm max No
SA841 Gr.E Cl.4 TMCP 485 MPa, 40 mm max This page
SA841 Grade E Class 5 TMCP 515 MPa, 40 mm max Same Grade, higher Class
SA841 Grade F Class 6 TMCP Different Grade No
SA537 Cl.2 Heat-treated C-Mn-Si Similar yield window, not TMCP Grade E No
SA517 Gr.A QT alloy Different family No
SA516 Gr.70 Fine-grain carbon No Class 4 TMCP No

SA299 Gr.B, SA225 Gr.D, SA455 and SA285 Gr.C are also vessel plates. None of them is Grade E Class 4.

The practical question is whether Grade E Class 4 can replace SA537 Class 2 or SA841 Class 2. Only if the drawing and the allowable-stress line name SA-841 Grade E Class 4. Similar yield is not a substitution rule. The 40 mm cap is also not optional.

TMCP Vessel Service

ASME SA841 Grade E Class 4 is used when the vessel wants a low-carbon TMCP Grade with 485 MPa yield and the wall stays inside 40 mm. Designers pick Grade E when they want tighter carbon and sulfur than Grades A–C, without jumping to Grade D’s 690 MPa Class 3 line and 1.0–5.0% nickel.

Allowable stress comes from ASME Section II Part D after the Code lists this Grade and Class. Do not copy a SA537 Cl.2 allowable and apply it here. Do not copy a Grade B Class 2 allowable either. The chemistry and the thickness cap are not the same.

Typical components are process shells, heads and courses written specifically to SA-841 Grade E Class 4. It is not cryogenic 3.5Ni plate like SA203 Gr.D or SA203 Gr.E. Grade E nickel is a limited TMCP addition, not a nickel-steel designation. Stainless work belongs on ASME SA240/SA240M, ASTM A240/A240M or stainless steel sheets and plates.

The TMCP temperature cap still applies. Except for Grade G, forming and PWHT stay at or below 650 °C, and only when clause 6.1 and any simulated coupons are satisfied. Do not run a 900 °C normalize on Grade E and expect Class 4 yield to remain.

Weldability

SA841 Gr.E Cl.4 is killed, fine-grain TMCP plate with very low carbon. Welding is still Code welding.

Qualify procedures to ASME Section IX. Use low-hydrogen consumables. Carbon at 0.07% maximum and sulfur at 0.005% maximum help HAZ toughness. Nickel up to 0.60% and molybdenum up to 0.30% still belong in the carbon-equivalent calculation. Do not use a Grade A worksheet.

Preheat depends on thickness, restraint, hydrogen and the qualified WPS. After welding, many shops want PWHT. That cycle must stay inside the TMCP window and must be proven on mill coupons when the vessel specification already knows the hold.

Do not copy a SA387 Gr.12 Cl.2 Cr-Mo procedure or a SA533 Type A Class 1 QT procedure onto Grade E Class 4 without review. The fabricator owns the WPS. SHH STEEL supplies the plate and the test data.

Heat Treatment

The steel shall be killed and shall meet fine austenitic grain practice under ASME SA-20. Plates shall be produced by TMCP. Slab reheating, reduction schedule, finish temperature and accelerated cooling are the mill tools. There is no mandatory furnace normalize and no mandatory quench and temper in the specified condition.

If the vessel will be warm formed or post-weld heat-treated, the test coupons must follow that cycle. A coupon tested as-rolled does not prove a 620 °C shell hold. Ask for simulated PWHT when the vessel specification already knows the temperature and time.

This is not the normalize route used for SA516 Gr.60. It is not the QT route used for SA537 Cl.1 or SA517 Gr.E. SHH STEEL prints TMCP and Class 4 on the certificate so the inspector does not treat the plate as ordinary as-rolled carbon.

Delivery Condition

Usual delivery is TMCP Grade E Class 4 plate, 8 mm to 40 mm.

The mill test certificate lists ASME SA841 Grade E Class 4 and, when dual certified, ASTM A841 Grade E Class 4; heat number; heat analysis including Ni, Mo, P and S; product analysis when ordered; tensile results to the Class 4 table; TMCP statement; impact results when ordered; simulated PWHT results when ordered; and UT when ordered. Surface is vessel-plate quality. Shot blast and shop primer are available.

Certificates may be EN 10204 3.1 or EN 10204 3.2. Third-party surveyors can witness rolling, cooling and testing when the order names the agency.

Dimensions

Usual supply range from SHH STEEL for SA841 Gr.E Cl.4 TMCP vessel plate:

  • Thickness: 8 mm – 40 mm. That 40 mm ceiling is the Grade E rule in SA-841, not a mill preference
  • Width: 1500 mm – 4000 mm, subject to the Grade E rolling schedule
  • Length: 3000 mm – 12000 mm
  • Cut-to-length shells, dish-head blanks and nest sizes inside those limits

A 45 mm inquiry is outside Grade E. Do not “see if the mill can roll it” and still stamp SA841 Grade E Class 4. Grades A, B and C go to 100 mm, but they do not carry Class 4.

Structural lengths belong on EN 10025-2 or JIS G3106. Weathering plate belongs on EN 10025-5 or Corten A/B. Fine-grain structural belongs on EN 10025-3 or EN 10025-4. QT structural belongs on EN 10025-6.

Tolerances

Dimensional limits follow ASME SA-20. Thickness tolerance, width, length, flatness and camber are vessel-plate rules.

TMCP plate can move during accelerated cooling. Flatness should be written if the head shop is tight. Ultrasonic testing to A435, A577 or A578 is common on Grade E plate. Extra-flatness and edge-camber limits are negotiated items, not assumed extras.

Supplementary Requirements

Most export ASME SA841 Grade E Class 4 orders add extras. The specification does not assume them.

Charpy V-notch. Temperature, absorbed energy, specimen location and orientation.

Simulated PWHT and warm forming. Same-heat coupons follow the vessel cycle. Tensile and impact are then run on those coupons.

NDE. UT to A435 / A577 / A578. Edge MT or PT after cutting when the shop wants it.

Restricted P, S and CEV. Table 1 is already tight on sulfur. Some projects go tighter on phosphorus and carbon equivalent.

Through-thickness / Z testing. When lamellar tearing is a design concern.

Third-party inspection. EN 10204 3.2, with the agency named on the order.

If an item is not written, it is not tested and it is not printed as if it were.

Equivalent Material Grades

There is no one-to-one dual stamp outside ASTM A841. The names below are project comparisons. Chemistry, TMCP route, 40 mm cap and impact temperature still have to match the purchase order.

Designation Standard Notes
ASME SA841 Grade E Class 4 / SA841 Gr.E Cl.4 ASME SA-841/SA-841M Code name on this page
ASTM A841 Grade E Class 4 ASTM A841/A841M Companion spec; dual mark available
SA841 Grade E Class 5 SA-841 Same Grade, 515 MPa Class
EN 10028-5 P460M / P460ML EN Closest TMCP vessel comparison for this yield window
EN 10028-6 P500Q related EN QT comparison, not TMCP Grade E
JIS G3115 SPV450 / SPV490 JIS Pressure-vessel comparison; confirm process and impact
JIS G3124 related JIS Confirm TMCP and 40 mm cap
GB/T 19189 07MnNiMoDR related GB Chinese TMCP / QT vessel comparison; confirm route
GB 713 Q370R / Q420R related GB Strength talk only
DIN EN 10028-5 P460M DIN / EN Current German path is EN, not old DIN 17155
DIN 17102 TStE 460 / 500 related DIN (historical) Do not stamp as SA841
ASME SA537 Class 2 SA-537 Heat-treated, not TMCP
ASTM A537 Cl.2 A537 Same caution

DIN 17100, ASTM A516, ASME SA515 and ASTM A285 are not Grade E Class 4. SHH STEEL will dual-certify SA841 / A841. EN, JIS or GB dual marking is only when the mill heat meets both books and the order says so.

Applications

Industry Typical components
Pressure vessels ASME SA841 Grade E Class 4 shells and SA841 Gr.E Cl.4 heads to 40 mm
Process equipment SA-841 Gr.E Cl.4 TMCP courses
Dual-certified export SA841 / A841 Grade E Class 4 plate
Fabrication SA841 Gr.E Cl.4 cut to nest sizes inside 40 mm

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering inquiries belong on weathering steel plates. Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless.

Other vessel comparisons: SA203 Gr.B, SA302 Gr.C, A516 Gr.70, SA533 Type C Class 2, SA517 Gr.P.

Why Choose SHH STEEL

SHH STEEL works as a China Mill Direct Exporter for plates to ASME SA-841/SA-841M. On ASME SA841 Grade E Class 4 that means mill pricing, dual SA841/A841 marking, Grade E chemistry with carbon at 0.07% max and sulfur at 0.005% max, recorded TMCP delivery, Class 4 tensile results at 485 MPa yield and 580–715 MPa tensile, the 40 mm ceiling respected, 3.1 as standard and 3.2 when specified.

We keep Grade and Class on the order. Grade E Class 4 is not Grade E Class 5. Grade E is not Grade D and is not Grade C. SA841 is not SA516 Gr.55. SA841 is not SA387 Gr.91 Cl.2. SA841 Gr.E Cl.4 is not SA533 Type C Class 1. If the drawing names 80 mm at this Grade, we will say Grade E cannot be used. If it names Class 5, we will not ship Class 4 and call it close. If the shop plans a 900 °C form, we will say TMCP is the wrong process before the slab is booked.

Company scope: China steel Mill Agent-SHH STEEL.

FAQ

What names are used for ASME SA841 Grade E Class 4?
Buyers write SA841 Grade E Class 4, SA841 Gr.E Cl.4, SA841GRE CL4, SA-841 Grade E Class 4, SA841 E4 and SA 841 Gr E Cl 4. SHH STEEL prints the wording on the purchase order.
Is ASME SA841 Grade E Class 4 the same as ASTM A841 Grade E Class 4?
Chemistry and tensile limits match. ASME SA-841 is the Code version. ASTM A841 is the product spec. As China mill-Direct Supply, SHH STEEL dual-certifies both names when the vessel must be stamped.
What is the yield strength of SA841 Gr.E Cl.4?
485 MPa minimum. Tensile is 580–715 MPa. Elongation is 20% in 50 mm. Those numbers apply only through 40 mm.
Is Class 4 stronger than Class 3?
Not in this specification. Class 3 is Grade D at 690 MPa yield. Class 4 is Grade E at 485 MPa yield. Read Grade and Class together.
How is Grade E different from Grade D and Grade C?
Grade E carbon is 0.07% max and sulfur is 0.005% max. Nickel max is 0.60%. Grade D nickel is 1.0–5.0% and Class 3 yield is 690 MPa. Grade C carbon is 0.10% with titanium and goes to 100 mm in Class 1 or Class 2.
What is the closest EN, JIS, GB or DIN grade?
EN 10028-5 P460M / P460ML is the usual TMCP comparison for this yield window. JIS G3115 SPV450 / SPV490 and GB/T 19189 related vessel steels are project comparisons. Old DIN names are historical. None of them is an automatic dual stamp.
Is SA841 Grade E Class 4 the same as SA537 Class 2?
No. The yield window can look similar. SA537 Class 2 is heat-treated. SA841 Grade E Class 4 is TMCP and stops at 40 mm.
Can the plate be hot formed like normalized carbon plate?
Not without a planned cycle. Forming and PWHT are normally held at or below 650 °C, with simulated coupons when required.
Can welding be qualified to ASME Section IX?
Yes. Use a low-hydrogen WPS written for TMCP vessel plate at Class 4 strength. The fabricator owns the procedure.

Conclusion

ASME SA841 Grade E Class 4 Steel Plate is TMCP pressure-vessel plate under ASME SA-841/SA-841M, limited to 40 mm, with 485 MPa yield and 580–715 MPa tensile. Whether the inquiry says SA841 Grade E Class 4, SA841 Gr.E Cl.4, SA841GRE CL4 or SA-841 Grade E Class 4, SHH STEEL supplies plate with Grade E chemistry, recorded TMCP delivery, Class 4 tensile results, and EN 10204 3.1 or 3.2 certification.

As a China mill Distributor, SHH STEEL provides ASME SA841 Grade E Class 4 / SA841 Gr.E Cl.4 TMCP Vessel Plate for ASME Section VIII work that actually names this Grade and Class.

Contact SHH STEEL for mill rolling, dual SA841/A841 marking, simulated PWHT testing, 3.2 inspection or a quotation.

ASME SA841 Grade E Class 4 Steel Plate, SA841 Gr.E Cl.4, SA841GRE CL4, SA-841 Grade E Class 4, TMCP vessel plate, Direct Mill Supply by SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X