ASME SA841 Grade C Class 1 TMCP vessel plate, Gr.C Cl.1, C ≤0.10%, YS 50 ksi, SHH STEEL

ASME SA841 Grade C Class 1 Steel Plate | SA841 Gr.C Cl.1 TMCP Vessel Plate

ASME SA841 Grade C Class 1 is TMCP pressure-vessel plate under ASME SA-841/SA-841M. Grade C is the low-carbon titanium Grade. Yield 345 MPa, tensile 485–620 MPa to 65 mm. SHH STEEL supplies SA841 Gr.C Cl.1 mill-direct with 3.1 or 3.2 certificates.
Keywords:
ASME SA841 Grade C Class 1, SA841 Gr.C Cl.1, SA841GRC CL1, SA-841 Grade C Class 1, SA841 C1, TMCP vessel plate, SA841 Grade C Class 1 supplier
Equivalent Grades:
A841 Gr C / EN 10028-5 P460ML1-ML2 (near) / GB Q460CF — Material Specification: ASME SA-841 / ASTM A841 — Delivery: TMCP
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
TMCP Vessel Service
Weldability
Heat Treatment
Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA841 Grade C Class 1 Steel?

ASME SA841 Grade C Class 1 is the low-carbon, titanium-treated Grade in ASME SA-841/SA-841M at the Class 1 strength window. The plate is made by thermo-mechanical control process. Grade C carbon is capped at 0.10%. Class 1 is the 345 MPa yield line shared with Grades A and B. As Direct Mill Supply by SHH STEEL, the plate is produced to ASME SA-841/SA-841M.

The same plate is written SA841 Grade C Class 1, SA841 Gr.C Cl.1, SA841GRC CL1, SA-841 Grade C Class 1, SA841 C1 and SA 841 Gr C Cl 1. ASTM A841 Grade C Class 1 is the companion product spec. A purchase order that only says “SA841 Grade C” is incomplete. Class 2 on Grade C is 415 MPa yield. Those two plates do not interchange.

This page is not SA537 Cl.1. SA537 Class 1 is heat-treated C-Mn-Si. SA841 Grade C Class 1 is TMCP. It is not ASME SA516 carbon plate and not ASME SA387 Cr-Mo plate. Maximum nominal thickness for Grade C is 100 mm. Dual marking SA841 / A841 Grade C Class 1 is available. Certificates can be EN 10204 3.1 or 3.2. Company scope: China steel Mill Agent-SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade / Class ASME SA841 Grade C Class 1 Confirmed
Product Specification ASME SA-841/SA-841M Applied
Companion Spec ASTM A841 Grade C Class 1 Dual cert available
General Requirements ASME SA-20 / ASTM A20 Applied
Process TMCP Confirmed
Grain practice Killed, fine austenitic grain Applied
Intended use Welded pressure vessels As specified
Maximum Thickness 100 mm for Grade C Per SA-841
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in the pressure vessel steel plates family. It is not carbon steel plates without a TMCP Class table, not structural steel plates, and not ASTM A36/A36M.

Chemical Composition

Class 1 does not get a private chemistry table. ASME SA841 Grade C Class 1 uses Grade C chemistry. The Grade C marker is low carbon plus titanium.

Heat Analysis — ASME SA841 Grade C

Element Heat Analysis (%)
Carbon (C), max 0.10
Manganese (Mn), t ≤ 40 mm 0.70 – 1.60
Manganese (Mn), t > 40 mm 1.00 – 1.60
Phosphorus (P), max 0.030
Sulfur (S), max 0.015
Silicon (Si) 0.15 – 0.50
Copper (Cu), max 0.35
Nickel (Ni), max 0.25
Chromium (Cr), max 0.25
Molybdenum (Mo), max 0.08
Niobium (Nb), max 0.06
Vanadium (V), max 0.06
Titanium (Ti) 0.006 – 0.02

Product analysis follows SA-20 / A20 tolerances on the Grade C heat limits. Grade A carbon max is 0.20%. Grade B carbon max is 0.15% with higher nickel and molybdenum. Grade C is the low-carbon titanium route. A Grade A ladle cannot be stamped Grade C. Sulfur on Grade C is tighter (0.015% max) than Grade A (0.030%).

If chromium and molybdenum sit in a SA387 Gr.11 Cl.1 or SA387 Gr.22 Cl.1 window, the plate belongs on the Cr-Mo page. If the process is QT Mn-Mo, look at SA533 Type A Class 1. SHH STEEL reports heat analysis on every certificate, including titanium, and adds product analysis when SA-20 requires it.

Mechanical Properties

Class 1 is the strength line. Grade C only tells the chemistry family.

Tensile Requirements — ASME SA841 Class 1 (Grades A, B, C)

Property t ≤ 65 mm t > 65 mm
Yield strength, min 345 MPa (50 ksi) 310 MPa (45 ksi)
Tensile strength 485 – 620 MPa (70 – 90 ksi) 450 – 585 MPa (65 – 85 ksi)
Elongation in 50 mm, min 22% 22%
Elongation in 200 mm, min 18% 18%
Density 7.85 g/cm³ 7.85 g/cm³
Hardness Not a Table 3 default Not a Table 3 default

Class 2 on Grade C is 415 MPa yield and 550–690 MPa tensile through 65 mm. A Class 1 heat cannot be stamped Class 2. Typical TMCP Class 1 hardness is about 140–190 HB. Print hardness only when the order sets a limit. Density 7.85 g/cm³ is used for weight take-off.

Charpy is not a hidden default. Write the impact temperature when the vessel specification needs it. Do not treat 345 MPa yield as a reason to substitute ASTM A36 steel plate, ASTM A572 or high strength low alloy plates.

Material Comparison

Grade Route Chemistry idea Swap?
SA841 Grade A Class 1 TMCP C 0.20 max No
SA841 Grade B Class 1 TMCP C 0.15 max, higher Ni/Mo No
SA841 Gr.C Cl.1 TMCP C 0.10 max + Ti This page
SA841 Grade C Class 2 TMCP Same Grade, higher Class No
SA537 Cl.1 Heat-treated C-Mn-Si Not TMCP No
SA516 Gr.70 Fine-grain carbon No TMCP Class table No
SA515 Gr.70 Si-killed carbon No TMCP No
SA533 Type A Class 1 QT Mn-Mo Different family No

Nearby vessel pages: SA299 Gr.A, SA225 Gr.C, SA455, SA285 Gr.C.

TMCP Vessel Service

ASME SA841 Grade C Class 1 is selected when the vessel wants TMCP Class 1 strength and the lower carbon / titanium Grade C chemistry. Designers pick Grade C when weldability and lower carbon matter more than Grade B nickel. Allowable stress comes from ASME Section II Part D for SA-841 Grade C Class 1.

Typical use is welded tanks, process shells and other equipment written to SA-841 Grade C Class 1. It is not nickel low-temp plate like SA203 Gr.A or SA203 Gr.D. It is not QT alloy like SA517 Gr.A. Stainless inquiries belong on ASME SA240/SA240M, ASTM A240/A240M or stainless steel sheets and plates.

Warm forming and PWHT must stay inside the TMCP limit, normally not above 650 °C, with simulated coupons when the vessel cycle is known. Do not form this plate like as-rolled SA285 Gr.A.

Weldability

SA841 Gr.C Cl.1 is killed, fine-grain TMCP plate with the lowest carbon cap among Grades A–C. Welding is still Code welding.

Procedures are qualified to ASME Section IX. Low-hydrogen practice is the usual shop choice. Carbon at 0.10% maximum and sulfur at 0.015% maximum help HAZ toughness. Titanium is part of the Grade C grain-control package. Calculate carbon equivalent from the actual ladle, including manganese on the thick side of the table.

Preheat depends on thickness, restraint, hydrogen and the WPS. After welding, many shops want PWHT. That stay inside the 650 °C TMCP ceiling unless simulated testing supports the cycle.

Do not copy a SA387 Gr.12 Cl.1 procedure or a SA533 Type B Class 1 QT procedure onto Grade C Class 1 without review. The fabricator owns the WPS.

Heat Treatment

The steel shall be killed and shall meet fine austenitic grain practice under ASME SA-20. Plates shall be produced by TMCP. There is no separate mandatory normalize or quench-and-temper in the specified condition.

If the vessel will see warm forming or PWHT, test coupons shall follow a simulated cycle. This is not the normalize route used for SA516 Gr.60 and not the QT route used for SA537 Cl.2. SHH STEEL reports TMCP as the delivery process on the MTC.

Delivery Condition

Usual delivery is TMCP Grade C Class 1 plate.

The certificate lists ASME SA841 Grade C Class 1 and, when dual certified, ASTM A841 Grade C Class 1; heat number; heat analysis including Ti; product analysis when ordered; tensile results to the Class 1 table; TMCP statement; Charpy results when ordered; and supplementary tests. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for SA841 Gr.C Cl.1 TMCP vessel plate:

  • Thickness: 8 mm – 100 mm (Grade C maximum in SA-841)
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm
  • Cut-to-length shells and nest sizes inside those limits

If the inquiry is 120 mm, Grade C cannot be used under this specification. Structural sizes belong on EN 10025-2 or JIS G3106. Weathering plate belongs on EN 10025-5 or Corten A/B. Fine-grain structural belongs on EN 10025-3 or EN 10025-4. QT structural belongs on EN 10025-6.

Tolerances

Dimensional limits follow ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances. UT to A435 / A577 / A578 is commonly added on thicker TMCP plate.

Supplementary Requirements

Most export ASME SA841 Grade C Class 1 orders add extras. SHH STEEL does not assume them.

Charpy details. Temperature, energy, location and orientation.

Simulated PWHT / warm forming. Same-heat coupons follow the vessel cycle.

NDE. UT to A435 / A577 / A578.

Restricted P, S / CEV. When specified.

Third-party. EN 10204 3.2.

Equivalent Material Grades

Designation Standard Notes
ASME SA841 Grade C Class 1 / SA841 Gr.C Cl.1 ASME SA-841/SA-841M Code name on this page
ASTM A841 Grade C Class 1 ASTM A841/A841M Companion spec
SA841 Grade C Class 2 SA-841 Same Grade, higher Class
EN 10028-5 P355M / P355ML related EN Project comparison only
ASME SA537 Class 1 SA-537 Heat-treated, not TMCP
ASTM A537 Cl.1 A537 Same caution

DIN 17100, ASTM A516, ASME SA515 and ASTM A285 are not SA841 Grade C Class 1.

Applications

Industry Typical components
Pressure vessels ASME SA841 Grade C Class 1 shells and SA841 Gr.C Cl.1 heads
Storage tanks SA-841 Gr.C Cl.1 TMCP courses
Process equipment ASME SA841 Grade C Class 1 TMCP vessel plate
Dual-certified export SA841 / A841 Grade C Class 1 plate
Fabrication SA841 Gr.C Cl.1 cut to nest sizes

Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering inquiries belong on weathering steel plates. Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless.

Other vessel comparisons: SA203 Gr.B, SA302 Gr.A, A516 Gr.70, SA533 Type D Class 1.

Why Choose SHH STEEL

SHH STEEL works as a China Mill Direct Exporter for plates to ASME SA-841/SA-841M. On ASME SA841 Grade C Class 1 that means mill pricing, dual SA841/A841 marking, Grade C chemistry with carbon at 0.10% max and titanium in the specified band, recorded TMCP delivery, Class 1 tensile results at 345 MPa yield, 3.1 as standard and 3.2 when specified.

We keep Grade and Class on the order. Grade C Class 1 is not Grade C Class 2 and is not Grade A Class 1. SA841 is not SA516 Gr.55. SA841 is not SA387 Gr.91 Cl.2. SA841 Gr.C Cl.1 is not SA533 Type C Class 1. If the drawing names heat-treated carbon, we point the inquiry to SA537. If it names Grade A, we will not ship Grade C and call lower carbon an upgrade.

Company scope: China steel Mill Agent-SHH STEEL.

FAQ

What names are used for ASME SA841 Grade C Class 1?
Buyers write SA841 Grade C Class 1, SA841 Gr.C Cl.1, SA841GRC CL1, SA-841 Grade C Class 1, SA841 C1 and SA 841 Gr C Cl 1. SHH STEEL prints the wording on the purchase order.
Is ASME SA841 Grade C Class 1 the same as ASTM A841 Grade C Class 1?
Chemistry and tensile limits match. ASME SA-841 is the Code version. ASTM A841 is the product spec. As China mill-Direct Supply, SHH STEEL dual-certifies both names when the vessel must be stamped.
What is the yield strength of SA841 Gr.C Cl.1?
345 MPa minimum through 65 mm. Over 65 mm the Class 1 yield drops to 310 MPa. Tensile is 485–620 MPa through 65 mm.
How is Grade C different from Grade A and Grade B?
Grade C carbon is 0.10% max and titanium is specified at 0.006–0.02%. Sulfur max is 0.015%. Grade A carbon is 0.20% max. Grade B carbon is 0.15% max with higher nickel and molybdenum. Class 1 is the same tensile table on all three.
: Is SA841 Grade C Class 1 the same as SA537 Class 1?
No. The numbers sit in a similar window. SA537 Class 1 is heat-treated. SA841 Grade C Class 1 is TMCP.
What is the maximum thickness?
100 mm for Grade C. D, E and F stop at 40 mm.
Can the plate be hot formed like normalized carbon plate?
Not without a planned cycle. Forming and PWHT are normally held at or below 650 °C, with simulated coupons when required.
Can welding be qualified to ASME Section IX?
es. Use a low-hydrogen WPS written for TMCP vessel plate. The fabricator owns the procedure.

Conclusion

ASME SA841 Grade C Class 1 Steel Plate is TMCP pressure-vessel plate under ASME SA-841/SA-841M, using low-carbon titanium Grade C chemistry and the Class 1 tensile table. Whether the inquiry says SA841 Grade C Class 1, SA841 Gr.C Cl.1, SA841GRC CL1 or SA-841 Grade C Class 1, SHH STEEL supplies plate with recorded TMCP delivery, Class 1 tensile results, and EN 10204 3.1 or 3.2 certification.

As a China mill Distributor, SHH STEEL provides ASME SA841 Grade C Class 1 / SA841 Gr.C Cl.1 TMCP Vessel Plate for ASME Section VIII work.

Contact SHH STEEL for mill rolling, dual SA841/A841 marking, 3.2 inspection or a quotation.

ASME SA841 Grade C Class 1 Steel Plate, SA841 Gr.C Cl.1, SA841GRC CL1, SA-841 Grade C Class 1, TMCP vessel plate, Direct Mill Supply by SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X