ASME SA285 Grade C Steel Plate | SA285 Gr.C Pressure Vessel Plate - SHH STEEL

ASME SA285 Grade C Steel Plate | SA285 Gr.C Pressure Vessel Plate

ASME SA285 Grade C is a low-to-intermediate tensile carbon vessel plate under ASME SA-285/SA-285M. Tensile 380–515 MPa, yield 205 MPa, max 50 mm. SHH STEEL supplies SA285 Gr.C / A285 Gr.C as China mill-Direct Supply with 3.1 or 3.2 certificates.
Keywords
ASME SA285 Grade C, SA285 Gr.C, SA285GRC, SA285 GR C, SA-285 Grade C, ASTM A285 Grade C, A285GRC, pressure vessel plate, ASME SA-285, SA285 Grade C supplier
Equivalent Grades:
ASTM A285 Gr C / ASME SA285 Gr C / JIS G3103 SB450 / GB Q245R / EN 10028-2 P265GH — Material Specification: ASME SA-285 / ASTM A285
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Intermediate and Lower Temperature Vessel Service
Weldability
Heat Treatment
Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA285 Grade C Steel?

ASME SA285 Grade C is the highest-strength grade in ASME SA-285/SA-285M. The specification covers carbon steel plates of low and intermediate tensile strength for fusion-welded pressure vessels. Grade C is the grade most buyers actually type into a search box. As Direct Mill Supply by SHH STEEL, the plate is produced to ASME SA-285/SA-285M.

The same plate is written SA285 Gr.C, SA285GRC, SA285 GR C, SA-285 Grade C, SA285 Grade C, ASME SA285 GR.C, ASME SA285GRC, ASTM A285 Grade C, A285 Gr.C, A285GRC and A/SA285 Grade C. They all mean Grade C. ASTM A285/A285M is the product companion.

Do not treat this page as ASME SA516 or ASTM A516. A516 is fine-grain, higher-quality vessel plate with a different tensile table and a different heat-treatment habit. Do not treat it as ASME SA515 either. SA515 is silicon-killed carbon plate for intermediate and higher temperature. ASME SA285 Grade C is the simpler, lower-to-intermediate tensile carbon vessel grade, usually supplied as-rolled, with a specification thickness ceiling of 50 mm (2 in.).

The steel follows ASME SA-20 general requirements. It may be rimmed, capped, semi-killed or killed as agreed. Fine austenitic grain practice is not the default the way it is on SA516. If the drawing wants killed steel, fine grain, or normalized delivery, that has to be written on the purchase order.

For Code work the plate is used under ASME Section VIII. Dual marking ASME SA285 Grade C / ASTM A285 Grade C is available. Certificates can be EN 10204 3.1 or EN 10204 3.2.

When a project is still choosing carbon vessel plate, a China mill Agent path through SHH STEEL puts SA285GRC next to ASME SA537, ASTM A537, ASME SA387 and ASTM A285, so the buyer can see whether Grade C is enough or whether the vessel actually needs A516 / SA516.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade ASME SA285 Grade C / SA285 Gr.C / SA285GRC Confirmed
Product Specification ASME SA-285/SA-285M Applied
Companion Spec ASTM A285 Grade C / A285GRC Dual cert available
General Requirements ASME SA-20 / ASTM A20 Applied
Code Context ASME Section VIII As specified
Product Form Pressure vessel plate Available
Typical Practice Rimmed, capped, semi-killed or killed as ordered Confirmed
Usual Delivery As-rolled Confirmed
Maximum Thickness 50 mm (2 in.) Per SA-285
Typical Supply 6 mm – 50 mm By mill enquiry
Width / Length Up to about 4000 mm / 12000 mm Mill capability
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate belongs to the Pressure Vessel Steel Plates family. It is not a structural HSLA Steel Plates substitute and not a Carbon Steel Plates structural grade such as A36.

Chemical Composition

Chemistry for ASME SA285 Grade C is reported as heat analysis and, when specified, product analysis under ASME SA-285/SA-285M. Carbon is the grade marker. Grade C allows more carbon than Grade A or Grade B.

Heat Analysis — ASME SA285 Grade C / SA285 Gr.C

Element Heat Analysis (%)
Carbon (C), max 0.28
Manganese (Mn), max 0.90
Phosphorus (P), max 0.025
Sulfur (S), max 0.025

Product Analysis — SA285GRC / A285 Grade C

Element Product Analysis (%)
Carbon (C), max 0.31
Manganese (Mn), max 0.98
Phosphorus (P), max 0.025
Sulfur (S), max 0.025

Silicon is not mandated in the base SA-285 Grade C table the way it is in SA515. Copper 0.20–0.35% can be specified when atmospheric corrosion resistance is wanted. If the drawing requires killed steel, a silicon or aluminum minimum belongs on the mill order, not as an assumption.

A Grade B heat cannot be recertified as Grade C if carbon or tensile results sit outside the Grade C table. If the drawing says ASME SA285 Grade C or ASME SA285GRC, the ladle and the tensile test must sit in Grade C. SHH STEEL reports heat analysis on every certificate and adds product analysis when ASME SA-20 or the vessel specification requires it.

Mechanical Properties

Tensile Requirements — ASME SA285 Grade C per ASME SA-285/SA-285M

Property Requirement
Tensile strength 380 – 515 MPa (55 – 75 ksi)
Yield strength, min 205 MPa (30 ksi)
Elongation in 200 mm (8 in.), min 23%
Elongation in 50 mm (2 in.), min 27%

That tensile window is why Grade C is the commercial grade in this specification. Grade A is 310–450 MPa. Grade B is 345–485 MPa. Grade C is 380–515 MPa. If the drawing says SA285 Gr.C, do not ship Grade B and hope the numbers overlap.

Density is 7.85 g/cm³. Hardness is not a default requirement in SA-285. A special HBW window is supplementary.

Charpy impact is not a default line in SA-285 the way it is in SA516. If the vessel needs a stated test temperature and energy, that is a supplementary requirement. Write it on the purchase order.

Specimens follow ASME SA-20. Simulated PWHT of coupons is added when the shop will stress-relieve or otherwise heat-treat the vessel after welding.

Material Comparison

Grade Strength class Max thickness Notes
ASME SA285 Gr.C / ASTM A285 Gr.C 380–515 MPa 50 mm This page
ASME SA285 Gr.B / ASTM A285 Gr.B 345–485 MPa 50 mm Lower tensile
ASME SA285 Gr.A / ASTM A285 Gr.A 310–450 MPa 50 mm Lowest tensile
ASME SA516 Gr.60 / ASTM A516 Gr.60 415–550 MPa Thicker capability Fine-grain PV plate
ASME SA515 Gr.60 / ASTM A515 Gr.60 415–550 MPa Thicker capability High-temp silicon-killed
ASTM A36 Structural Structural spec Not a vessel spec

Order ASME SA285 Grade C when the drawing names Grade C and thickness is 50 mm or less. If the vessel needs fine-grain practice, guaranteed impact, or plate thicker than 50 mm, move the conversation to SA516 / A516. SHH STEEL does not swap SA285GRC for A516 Gr.70 without a written revision.

Intermediate and Lower Temperature Vessel Service

ASME SA285 Grade C is selected for fusion-welded tanks, drums and low-to-moderate pressure equipment that do not need the toughness package of SA516. Allowable stress for Code work comes from ASME Section II Part D for SA-285 Grade C, not from a mill flyer.

Typical use is shop tanks, air receivers, low-pressure process drums and utility vessels. It is not a cryogenic nickel grade, not a QT 690 MPa grade, and not a creep-focused Cr-Mo grade.

Weldability

SA285GRC is a plain carbon vessel plate. Welding is straightforward compared with SA517 QT alloy plate, but it is still Code welding.

Procedures for Code work are qualified to ASME Section IX. Low-hydrogen consumables such as E7018 (AWS A5.1) are the usual shop choice for 90% joint efficiency work. Preheat depends on thickness, restraint and hydrogen. Grade C carbon is high enough that a thick, restrained joint should not be started cold and wet.

PWHT follows the vessel specification and ASME Section VIII, not a mill default. Simulated PWHT of mill coupons should be on the purchase order when the shop cycle is known.

Do not copy an SA517 or SA387 procedure onto ASME SA285 Grade C. Procedure review can go through steel welding services. The fabricator owns the qualified WPS.

Heat Treatment

Standard delivery of ASME SA285 Grade C is as-rolled.

Normalizing, stress relieving or annealing is supplementary. If the drawing says “normalized SA285 Gr.C”, that cycle is ordered and recorded. Do not assume every SA285GRC plate left the mill normalized.

Holding practice follows mill procedure and ASME SA-20 when a heat treatment is specified. SHH STEEL reports the actual delivery condition on the MTC.

Delivery Condition

Usual delivery is as-rolled pressure-vessel plate. Normalized or stress-relieved plate is supplied when specified.

The certificate lists ASME SA285 Grade C and, when dual certified, ASTM A285 Grade C; heat number; heat analysis; product analysis when ordered; tensile results; heat-treatment condition; and supplementary tests.

Surface is vessel-plate quality. Shot blasting and shop primer are available.

Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for SA285 Gr.C pressure vessel plate:

  • Thickness: 6 mm – 50 mm (Grade C maximum in ASME SA-285 is 50 mm)
  • Width: up to about 4000 mm
  • Length: up to about 12000 mm

If the inquiry is 60 mm, SA-285 is the wrong specification. Cut-to-length shells and nest sizes are available inside 50 mm.

Tolerances

Dimensional limits follow ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances.

Ultrasonic testing to A435 or A578 is added when specified. Finished sizes go through steel cutting services.

Supplementary Requirements

Most export ASME SA285 Grade C orders add tests beyond the base tensile table. SHH STEEL does not assume these extras.

Killed steel / fine grain. Base SA-285 does not force killed, fine-grain practice. If the vessel specification wants it, write it.

Heat treatment. Normalize or stress relieve as specified. Simulated PWHT of coupons when the shop cycle is known.

Charpy impact. Temperature, energy, specimen orientation and location as agreed. Not a default in SA-285.

NDE. UT to A435 / A577 / A578; edge MT/PT after cutting.

Hardness survey. Surface HBW when the datasheet sets a window.

Restricted chemistry. Tighter P, S, copper addition, or residuals per SA-20.

HIC / NACE. Only when TM0284 or MR0175 / ISO 15156 is cited. Grade C is not automatically sour-service plate.

Z-direction. A770 or Z15/Z25/Z35 when the joint is strained.

Third-party. Witness of rolling, testing and documents. Output can be EN 10204 3.2.

These tests run through steel testing service. If an item is not on the purchase order, it is not assumed.

Equivalent Material Grades

These names are used for project comparison. They are not automatic substitutes.

Designation Standard Region / notes
ASME SA285 Grade C / SA285 Gr.C / SA285GRC ASME SA-285/SA-285M Code name on this page
ASTM A285 Grade C / A285 Gr.C / A285GRC ASTM A285/A285M Companion spec
EN 10028-2 P265GH EN 10028-2 Closest common EU carbon PV comparison
EN 10028-2 P235GH EN 10028-2 Lower strength than Grade C
DIN 17155 HII DIN 17155 (historical) Old German boiler plate comparison
DIN 17155 19Mn6 related DIN 17155 Higher-Mn historical comparison
ISO 9328 P265GH related ISO 9328 ISO PV comparison
JIS G3118 SGV410 / SGV450 JIS G3118 Japanese intermediate-temp PV comparison
JIS G3103 SB410 JIS G3103 Japanese boiler plate comparison
GB/T 713 Q245R GB/T 713 Chinese boiler/vessel comparison, confirm tensile
GB 6654 20R (historical) GB 6654 Older Chinese PV comparison
ASME SA516 Gr.60 ASME SA-516 Fine-grain upgrade, not a substitute

For stamping, write ASME SA285 Grade C or dual SA285 / A285 Grade C. Nearby vessel pages: ASME SA516, ASTM A516, ASME SA537, ASTM A537.

Applications

ASME SA285 Grade C / SA285 Gr.C is selected when a Section VIII or equivalent vessel needs intermediate-tensile carbon plate inside 50 mm.

Industry Typical components
Pressure vessels ASME SA285 Grade C shells and SA285GRC heads
Petrochemical SA-285 Grade C low-to-moderate pressure drums
Energy and utility ASME SA285 Grade C air receivers and shop tanks
Storage SA285 Gr.C welded tanks
Dual-certified export SA285 / A285 Gr.C plate
Fabrication SA285GRC cut to nest sizes

Related pages: petrochemical industry, energy industry, steel cutting services, steel welding services, steel testing service, worldwide shipping service.

Why Choose SHH STEEL

SHH STEEL works as a China Mill Direct Exporter for plates to ASME SA-285/SA-285M. On ASME SA285 Grade C that means mill pricing, dual SA285/A285 marking, heat and product analysis, as-rolled or specified heat treatment, 3.1 as standard and 3.2 when specified, and the extra tests a vessel shop actually writes on the PO.

We also keep the order on the right grade. Grade C is not Grade B. Grade C is not SA516 Gr.70. Grade C is not A36. If the thickness is 60 mm, we will say so before anyone tries to buy SA285. If the drawing wants fine-grain impact-tested plate, we will point the inquiry to SA516 instead of forcing SA285GRC.

Export packing goes through worldwide shipping service. Company scope: China steel Mill Agent-SHH STEEL.

FAQ

What names are used for ASME SA285 Grade C?
Buyers write SA285 Gr.C, SA285GRC, SA285 GR C, SA-285 Grade C, ASME SA285 GR.C, ASME SA285GRC, ASTM A285 Grade C and A285GRC. They all mean Grade C in ASME SA-285/SA-285M. SHH STEEL prints the wording on the purchase order.
Is ASME SA285 Grade C the same as ASTM A285 Grade C?
Chemistry and tensile limits match. ASME SA-285 is the Code version used with ASME Section VIII. ASTM A285 is the product spec. As China mill-Direct Supply, SHH STEEL dual-certifies SA285 Gr.C / A285 Gr.C when the vessel must be stamped.
What is the tensile strength of SA285 Gr.C?
380–515 MPa. Yield is 205 MPa minimum. Elongation is 23% in 200 mm and 27% in 50 mm, per ASME SA-285.
Why specify Grade C instead of Grade B?
Grade C is the higher tensile grade in SA-285. Grade B is 345–485 MPa. Follow the grade on the drawing.
Is SA285GRC the same as SA516 Gr.60 or A36?
No. SA516 Gr.60 is fine-grain pressure-vessel plate with a different tensile table and impact habit. A36 is structural. ASME SA285 Grade C is a low-to-intermediate tensile carbon vessel plate under SA-285 and SA-20.
What is the maximum thickness for ASME SA285 Grade C?
50 mm (2 in.) in ASME SA-285. Thicker carbon vessel plate usually moves to SA516 / A516.
Is heat treatment mandatory for SA285 Gr.C?
No. Standard delivery is as-rolled. Normalize or stress relieve only when specified.
Can welding of SA285 Gr.C be qualified to ASME Section IX?
Yes. It is a fusion-welded vessel plate. E7018-type low-hydrogen procedures are common. The fabricator owns the WPS.
Can SHH STEEL issue EN 10204 3.2 on ASME SA285 Grade C?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 or another third-party witness is arranged when it is written on the order.
What is the density of SA285 Gr.C plate?
7.85 g/cm³. SHH STEEL uses this value for shipping-weight estimates on ASME SA-285 plate

Conclusion

ASME SA285 Grade C Steel Plate is the highest-strength carbon grade in ASME SA-285/SA-285M for low- and intermediate-tensile pressure vessels. Whether the inquiry says SA285 Gr.C, SA285GRC, ASME SA285 GR.C, ASME SA285GRC or A285 Grade C, SHH STEEL supplies plate with heat and product analysis, as-rolled or specified heat treatment, agreed extras, and EN 10204 3.1 or 3.2 certification.

As a China mill Distributor, SHH STEEL provides ASME SA285 Grade C / SA285 Gr.C Pressure Vessel Plate for ASME Section VIII fabrication.

Contact SHH STEEL for mill rolling, dual SA285/A285 marking, 3.2 inspection or a quotation.

ASME SA285 Grade C Steel Plate, SA285 Gr.C, SA285GRC, ASME SA285GRC, ASTM A285 Grade C, pressure vessel plate, SA285 Grade C supplier, Direct Mill Supply by SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *