Product Showcase

ASTM A789/A789M Stainless Steel Products

SHH STEEL offers ASTM A789/A789M-compliant 304/316 stainless steel tubes. ASTM A789/A789M specifies seamless and welded duplex/super duplex stainless steel tubes for high-corrosion environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!

ASTM A789 UNS S32520 Super Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32520 Super Duplex Stainless Steel Tube

ASTM A789 UNS S32520 super duplex stainless steel tube (Cr 23.0–25.0%, Mo 3.0–5.0%, N 0.20–0.35%, Cu 0.50–3.00%). SHH STEEL produces and supplies seamless and welded A789 S32520 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S82441 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S82441 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S82441 lean duplex stainless steel tube / LDX 2404-type (Cr 23.0–25.0%, Ni 3.0–4.5%, Mo 1.00–2.00%, N 0.20–0.30%). SHH STEEL produces and supplies seamless and welded A789 S82441 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S82031 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S82031 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S82031 lean duplex stainless steel tube (Cr 19.0–22.0%, Ni 2.0–4.0%, Mo 0.60–1.40%, N 0.14–0.24%). SHH STEEL produces and supplies seamless and welded A789 S82031 with EN 10204 3.1 MTC. Tensile table not verified in public excerpts used here.
View More
ASTM A789 UNS S82011 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S82011 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S82011 lean duplex stainless steel tube (Cr 20.5–23.5%, Ni 1.00–2.00%, Mo 0.10–1.00%, N 0.15–0.27%). SHH STEEL produces and supplies seamless and welded A789 S82011 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32304 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32304 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S32304 lean duplex stainless steel tube / 2304 (Cr 21.5–24.5%, Ni 3.0–5.5%, Mo 0.05–0.60%). SHH STEEL produces and supplies seamless and welded A789 S32304 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32202 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32202 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S32202 lean duplex stainless steel tube (Cr 21.5–24.0%, Ni 1.00–2.80%, Mo 0.45 max, N 0.18–0.26%). SHH STEEL produces and supplies seamless and welded A789 S32202 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32101 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32101 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S32101 lean duplex stainless steel tube / LDX 2101 family (Cr 21.0–22.0%, Ni 1.35–1.70%, Mn 4.0–6.0%, N 0.20–0.25%). SHH STEEL produces and supplies seamless and welded A789 S32101 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32003 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32003 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S32003 lean duplex stainless steel tube (Cr 19.5–22.5%, Ni 3.0–4.0%, Mo 1.50–2.00%, N 0.14–0.20%). SHH STEEL produces and supplies seamless and welded A789 S32003 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32001 Lean Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32001 Lean Duplex Stainless Steel Tube

ASTM A789 UNS S32001 lean duplex stainless steel tube (Cr 19.5–21.5%, Ni 1.0–3.0%, Mn 4.00–6.00%, Mo 0.60 max). SHH STEEL produces and supplies seamless and welded A789 S32001 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32900 Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32900 Duplex Stainless Steel Tube

ASTM A789 UNS S32900 duplex stainless steel tube (Cr 23.0–28.0%, Ni 2.5–5.0%, Mo 1.00–2.00%, C 0.08 max; no N minimum). SHH STEEL produces and supplies seamless and welded A789 S32900 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32506 Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32506 Duplex Stainless Steel Tube

ASTM A789 UNS S32506 duplex stainless steel tube (Cr 24.0–26.0%, Mo 3.0–3.5%, W 0.05–0.30%). SHH STEEL produces and supplies seamless and welded A789 S32506 with EN 10204 3.1 MTC.
View More
ASTM A789 UNS S32205 Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S32205 Duplex Stainless Steel Tube

ASTM A789 UNS S32205 duplex stainless steel tube / 2205 (Cr 22.0–23.0%, Ni 4.5–6.5%, Mo 3.0–3.5%, N 0.14–0.20%). SHH STEEL produces and supplies seamless and welded A789 S32205 with EN 10204 3.1 MTC. Distinct from S31803.
View More

ASTM A789/A789M Stainless Steel Products

Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.