ASTM A789 UNS S83072 Super Duplex Stainless Steel Tube | ASTM A789 Stainless Steel - SHH STEEL

ASTM A789 UNS S83072 Super Duplex Stainless Steel Tube

ASTM A789 UNS S83072 super duplex stainless steel tube (Cr 28.5–30.5%, Mo 0.7–1.7%, W 3.0–4.0%, N 0.35–0.45%). SHH STEEL produces and supplies seamless and welded A789 S83072 with EN 10204 3.1 MTC. Not in SA-789 (2023) per GRADE_LIST; tensile table not verified in public excerpts used here.
Grade
UNS S83072
Standard
ASTM A789 / A789M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × wall / BWG in the HX and process band (e.g. 12.7–76.2 mm OD); other sizes by agreement; average wall default, minimum wall when specified
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A789 UNS S83072 Super Duplex Stainless Steel Tube

ASTM A789 / A789M covers seamless and welded ferritic/austenitic stainless steel tubing for general corrosion service with particular emphasis on stress corrosion cracking resistance. UNS S83072 is a high-tungsten super duplex with heat limits of carbon ≤0.030%, chromium 28.5–30.5%, nickel 6.0–8.0%, molybdenum 0.7–1.7%, nitrogen 0.35–0.45%, copper 0.5% max, and tungsten 3.0–4.0% in A789/A789M-24 Table 1. GRADE_LIST notes this UNS appears in A789-24 but not in ASME SA-789 (2023) — fine for this ASTM series, but confirm SA789 listing before dual-marking for Code work.

SHH STEEL can produce and supply ASTM A789 UNS S83072 super duplex stainless steel tube as seamless and welded product (welded without filler metal) in typical OD × wall / BWG sizes, with EN 10204 3.1 mill test certificates. Dual A789/SA789 marking only when both standards are named and SA789 actually lists the grade for your Code year. Hub: A789/A789M.

Compare with sister A789 S83071, high-W A789 S32808, and A789 S32760. Plate: A240.

Chemical Composition of A789 S83072

Heat analysis must meet A789/A789M-24 Table 1. Product analysis follows A480/A480M annex tolerances when ordered.

Element Heat analysis, %
C 0.030 max
Mn 0.50–1.50
P 0.030 max
S 0.030 max
Si 0.30 max
Ni 6.0–8.0
Cr 28.5–30.5
Mo 0.7–1.7
N 0.35–0.45
Cu 0.5 max
W 3.0–4.0

W-adjusted PREN = Cr + 3.3(Mo + ½W) + 16N at mid-range (Cr 29.5, Mo 1.2, W 3.5, N 0.40) is about PREN ≈ 47–48. Very high W (3.0–4.0%) with modest Mo is the signature, similar in spirit to S32808 but with higher N. Mechanicals not in older Table 4 reprints — see Mechanical Properties. Si max 0.30% is unusually low.

Mechanical Properties of A789 S83072

The public A789/A789M-24 sample did not include the tensile/hardness table, and older Table 4 reprints available to this writer also did not list UNS S83072. Mechanical property minima are therefore not verified here — obtain them from the A789 edition named on your purchase order or from a controlled mill datasheet before design acceptance. Chemistry (Table 1) and heat-treatment temperatures (Table 2) below remain from the -24 public sample.

Seamless and Welded Tube

A789 Section 5 allows seamless or welded manufacture with no filler metal added. Seamless S83072 tube is typically hot-finished then cold-drawn to final OD and wall; welded tube is roll-formed from matching strip and autogenously welded, then usually cold-worked and re-annealed so the seam meets parent-metal heat treatment and mechanical floors.

Seamless lots take a flaring test (minimum 10% inside-diameter expansion); welded lots take a flange test plus a reverse flattening test on a specimen from each 1500 ft [450 m] of finished tubing. Tension and hardness sampling apply to both routes. SHH STEEL produces and supplies both seamless and welded A789 S83072 against the route named on the enquiry, with EN 10204 3.1 coverage of chemistry and mechanicals.

Dimensions and Tolerances

Average wall is the default under A789; specify minimum wall on the order when that is the design basis. Outside diameter and wall are ordered as tube sizes (metric or inch OD × wall / BWG). General dimensional requirements sit in Specification A1016/A1016M unless A789 states otherwise.

Item Typical enquiry practice for S83072 tube
Outside diameter 12.7–76.2 mm common HX/process band; larger OD by agreement
Wall Average wall default; minimum wall when named; BWG 10–20 class and metric equivalents
Length Cut-to-length for exchanger bundles; mill random by agreement
Straightness / ovality Per A1016/A1016M and any tighter project tolerance

When converting a pipe schedule into tube wall, state clearly whether acceptance is average or minimum wall — the two are not interchangeable on the mill ticket. SHH STEEL confirms OD × wall, length, and finish before the heat is reserved.

Equivalent Grades

Specify by UNS S83072. Note: present in A789-24; not in ASME SA-789 (2023) per GRADE_LIST — verify before Code dual-mark requests.

System Designation (indicative)
UNS S83072
Family Super duplex (high-W)
ASTM tube A789 / A789M S83072
ASME SA789 Not listed in SA-789 (2023) per workspace GRADE_LIST — confirm current Code year

Hub: A789/A789M.

Heat Treatment and Delivery Condition

A789/A789M-24 Table 2 lists UNS S83072 at 1830–2100 °F [1000–1150 °C]. Follow the quench stated in Table 2. Seamless tube may be quenched directly after hot forming while at or above the minimum solution temperature where that alternate is allowed.

Rapid cooling limits time in the sigma-forming window (roughly 700–1000 °C). A789’s scope warns that these steels are susceptible to embrittlement if used for prolonged periods at elevated temperatures, including 475 °C (885 °F) ferrite embrittlement. SHH STEEL supplies S83072 in the heat-treated condition required by Table 2.

Corrosion Resistance

S83072 targets high-PREN chloride service via Cr+W+N with only modest Mo. Mid-range W-adjusted PREN ≈47–48 is aggressive on paper — only if quench practice preserves the microstructure. Compare carefully with A789 S83071 (Mo-driven) and A789 S32808 (also high-W).

Applications of A789 S83072 Tube

Severe chloride tube duties that freeze S83072 by UNS under ASTM A789. For ASME Code dual-mark, confirm the grade exists in the SA789 edition you need. SHH STEEL produces and supplies A789 S83072 with verified mechanicals on the MTC even though older public Table 4 reprints omitted the row.

Weldability

Autogenous A789 welded tube must meet parent anneal and mechanicals without filler. Fabrication welds that use filler typically take matching or overalloyed duplex/super duplex consumables with controlled heat input and interpass temperature so ferrite–austenite balance stays qualified. Re-anneal after heavy hot work when required; keep bake and stress-relief cycles out of the sigma nose and the 400–500 °C embrittlement band unless a qualified procedure says otherwise.

Surface Finishes

Standard delivery is solution-annealed and pickled (or otherwise descaled) so the passive film can form uniformly. Bright-annealed or lightly polished OD/ID finishes are available by agreement when the exchanger or hygienic duty needs a smoother bore. Passivation after pickling or after fabrication welding is good practice in chloride service; remove carbon-steel tooling contamination before commissioning. SHH STEEL states the finish route on the quotation and on the MTC.

Inspection and Testing

Each A789 tube takes either a nondestructive electric test or a hydrostatic test. Mechanical sampling covers tension, hardness, and flaring for seamless or flange plus reverse flattening for welded, with full heat analysis on the mill test certificate. Product analysis and supplementary corrosion or ferrite tests are added when the purchase order asks for them. SHH STEEL issues EN 10204 3.1 as standard and arranges third-party inspection / 3.2 when the enquiry names an agency, with lot identity per A789 Notes 1 and 2.

Packaging and Shipping

Tube is typically packed in hexagonal bundles or plywood cases with end protectors and waterproof wrapping for ocean freight, with bundle tags repeating heat number, size, and standard. Cut-to-length exchanger tube may be boxed by length group; U-bends travel in purpose-built crates when ordered. SHH STEEL ships FOB, CFR, CIF, or EXW under the Incoterm on the order, with commercial invoice, packing list, and the EN 10204 3.1 or 3.2 certificate set.

Why Choose SHH STEEL

SHH STEEL produces and supplies ASTM A789 UNS S83072 — flagging the SA789 (2023) listing gap and the missing older Table 4 row — while coordinating high-W chemistry, anneal, testing, and EN 10204 3.1 documents to the PO. Production capability, not trader-only.

Supply Capability

SHH STEEL can produce and supply ASTM A789 UNS S83072 against the edition, size, and finish route named on your enquiry. The capability table below summarizes what we regularly quote, followed by the Stock / Available sizes map.

Item SHH STEEL capability for S83072
Standard ASTM A789 / A789M (dual SA789 marking on request)
Grade UNS S83072
Product form Seamless and welded (no filler metal); heat-treated
Size Typical HX/process OD × wall / BWG; other diameters by agreement
Wall Average wall default; minimum wall when specified
Length Cut-to-length; mill random; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension, hardness, flaring or flange + reverse flattening, hydro or NDE; full ladle chemistry on MTC
Documents EN 10204 3.1; third-party / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S83072 tube against a practical production-and-stock enquiry range rather than a frozen warehouse SKU list with published tonnages. Availability of any single line on a given week depends on mill drawing and inbound schedule — treat the table as a supply map for enquiry.

Item Typical stock / enquiry range for S83072
Outside diameter 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (other HX ODs on enquiry)
Wall / BWG BWG 10–20 class and metric min- or avg-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — confirm avg vs min wall
Length Cut lengths for exchanger bundles; straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, welded or seamless route, dual A789/SA789 marking — confirm before the heat is reserved

When you send an enquiry, include the ASTM edition if known, seamless or welded, OD × wall (avg or min), length, finish, test extras, and destination port. Sister grades such as A789 S83071, A789 S32808, and A789 S32760 can be quoted on the same enquiry when the project mixes duplex classes.

FAQ

What are the tensile requirements for A789 S83072?
They are not verified in this article. The public A789/A789M-24 sample excerpt did not include the tensile/hardness table, and older publicly circulated Table 4 reprints also did not list UNS S83072. Obtain tensile, yield, elongation, and hardness minima from the A789 edition named on your purchase order or from a controlled mill datasheet before design acceptance. Chemistry and heat-treatment temperatures on this page remain from the -24 Table 1 and Table 2 sample.
Is S83072 in ASME SA789?
Workspace GRADE_LIST notes S83072 is in ASTM A789-24 but not in ASME SA-789 (2023). That is acceptable for this ASTM-led series, but dual A789/SA789 marking for Code work should wait until you confirm the grade appears in the SA789 edition required by your project. SHH STEEL will not invent a Code listing.
What heat treatment does S83072 need?
A789/A789M-24 Table 2 lists 1830–2100 °F [1000–1150 °C] with rapid cooling in water or equivalent. High W and N make sigma control critical. A789 warns about embrittlement after prolonged elevated-temperature use, including 475 °C ferrite embrittlement. Always reconfirm numeric limits against the A789 edition named on your purchase order before design, forming, or corrosion acceptance.
How does S83072 compare with S83071?
S83071 uses Mo 3.0–4.0% without W; S83072 uses Mo 0.7–1.7% with W 3.0–4.0% and higher N (0.35–0.45%). Both can screen near PREN mid-to-high 40s by different chemistries. Match the named UNS and PREN form on the purchase order.
Why are tensile values missing on this page?
The -24 public sample lacked Table 4, and older Table 4 PDF reprints consulted for this series did not include a row for S83072. Numbers are not invented. Request the edition-named Table 4 values or mill datasheet with your enquiry; SHH STEEL will report verified mechanicals on the EN 10204 3.1 certificate.
Is ASTM A789 the same as ASME SA789 for S83072?
No. ASTM A789 / A789M is the ASTM International product specification for seamless and welded duplex stainless tubing; ASME SA789 is the separate Boiler and Pressure Vessel Code Book adoption of that grade text. Chemistry and mechanical floors align closely for a given referenced edition, but they remain two independent documents. Dual-mark A789/SA789 tube only when the purchase order asks for both names on the stencil and the mill test certificate.
Does A789 S83072 cover seamless and welded tube?
Yes. Section 5 of ASTM A789 states that tubes shall be made by the seamless or welded process with no filler metal added. Seamless product takes a flaring test with at least 10% inside-diameter expansion; welded product takes a flange test and a reverse flattening test every 1500 ft [450 m]. Both routes are solution-annealed and quenched per Table 2. SHH STEEL produces and supplies both routes for S83072 when named on the enquiry.
Can SHH STEEL produce S83072 tube, or only trade it?
SHH STEEL can produce and supply ASTM A789 UNS S83072 as seamless and welded tube in the usual heat-exchanger and process OD × wall band, documented on EN 10204 3.1 certificates. Melting chemistry, tube making, solution annealing, mechanical and hydro or NDE testing, and export packing are coordinated to the purchase order — production capability, not a trader-only offer.
Is S83072 suitable for continuous high-temperature service?
Generally no for prolonged elevated-temperature duty. Duplex grades including S83072 are susceptible to 475 °C (885 °F) embrittlement from spinodal decomposition in ferrite and to sigma-phase formation at higher temperatures if held too long. A789's own scope highlights embrittlement risk for prolonged elevated-temperature use; select a different alloy family when creep or continuous high-temperature strength is the design driver.
Which tests are mandatory on A789 S83072 tube?
Tension and hardness tests are required on a lot basis, and each tube must take either a hydrostatic test or a nondestructive electric test. Seamless tube also takes a flaring test; welded tube takes a flange test plus reverse flattening. Heat analysis appears on the mill certificate; product analysis and supplementary corrosion or ferrite tests are ordered extras. Lot definitions follow A789 Notes 1 and 2.
What sizes of S83072 tube can SHH STEEL supply?
Typical enquiry sizes for heat-exchanger and process duty run from about 12.7 mm to 76.2 mm outside diameter with BWG 10–20 class walls or metric average- or minimum-wall equivalents, supplied cut-to-length or as mill random lengths, seamless or welded. Non-standard diameters and heavier or lighter walls are quoted by agreement. See the Stock / Available sizes block and list OD × wall on the enquiry.
How should S83072 tube be marked and certified?
Stencil and MTC should carry ASTM A789 / A789M, UNS S83072, size, heat number, and the seamless or welded route. EN 10204 3.1 is the usual certificate; 3.2 with third-party attendance is available on request. Add SA789 to the marking only when the purchase order requires the ASME Code adoption alongside ASTM.

Conclusion

ASTM A789 UNS S83072 is covered here as super duplex stainless steel tube under the A789 seamless-and-welded duplex tubing specification. SHH STEEL produces and supplies seamless and welded S83072 to the A789 heat-treatment and test regime with EN 10204 3.1 documentation. For sizes, dual marking, or grade comparisons, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X