ASTM A789 UNS S32506 Duplex Stainless Steel Tube
What is ASTM A789 UNS S32506 Duplex Stainless Steel Tube
ASTM A789 / A789M covers seamless and welded ferritic/austenitic stainless steel tubing for general corrosion service with particular emphasis on stress corrosion cracking resistance. UNS S32506 is a tungsten-bearing duplex with heat limits of carbon ≤0.030%, chromium 24.0–26.0%, nickel 5.5–7.2%, molybdenum 3.0–3.5%, nitrogen 0.08–0.20%, and tungsten 0.05–0.30% in A789/A789M-24 Table 1. High Cr plus Mo and a W addition place it above basic 2205 on many chloride screens while the QUEUE still titles it Duplex rather than Super Duplex.
SHH STEEL can produce and supply ASTM A789 UNS S32506 duplex stainless steel tube as seamless and welded product (welded without filler metal) in the usual heat-exchanger and process OD × wall / BWG band, with EN 10204 3.1 mill test certificates. Dual A789/SA789 marking only when both standards are named on the order. Hub: A789/A789M.
Compare with A789 S32205, W-bearing A789 S31260, and super duplex A789 S32750 / A789 S32760. Plate: A240.
Chemical Composition of A789 S32506
Heat analysis must meet A789/A789M-24 Table 1. Product analysis follows A480/A480M annex tolerances when ordered.
| Element | Heat analysis, % |
|---|---|
| C | 0.030 max |
| Mn | 1.00 max |
| P | 0.040 max |
| S | 0.015 max |
| Si | 0.90 max |
| Ni | 5.5–7.2 |
| Cr | 24.0–26.0 |
| Mo | 3.0–3.5 |
| N | 0.08–0.20 |
| W | 0.05–0.30 |
Using the W-adjusted screening form Cr + 3.3(Mo + ½W) + 16N at mid-range (Cr 25, Mo 3.25, W 0.18, N 0.14) gives roughly PREN ≈ 38–39 — high standard duplex, approaching the lower super duplex band. Elongation floor in older Table 4 copies is only 18%, lower than most sister duplex grades.
Mechanical Properties of A789 S32506
Tensile and hardness floors come from older A789 Table 4 reprints; the public A789/A789M-24 sample did not include that table. Reconfirm on the PO edition.
| Property | Requirement (older A789 Table 4 copies) |
|---|---|
| Tensile strength, min | 90 ksi [620 MPa] |
| Yield strength (0.2% offset), min | 65 ksi [450 MPa] |
| Elongation in 2 in. or 50 mm, min | 18% |
| Hardness, max | 302 HBW / 32 HRC |
Note the 18% elongation minimum and 302 HBW / 32 HRC hardness cap in older copies — tighter ductility/hardness than typical 25%/290 HBW duplex entries. Fabrication procedures should respect that.
Seamless and Welded Tube
A789 Section 5 allows seamless or welded manufacture with no filler metal added. Seamless S32506 tube is typically hot-finished then cold-drawn to final OD and wall; welded tube is roll-formed from matching strip and autogenously welded, then usually cold-worked and re-annealed so the seam meets parent-metal heat treatment and mechanical floors.
Seamless lots take a flaring test (minimum 10% inside-diameter expansion); welded lots take a flange test plus a reverse flattening test on a specimen from each 1500 ft [450 m] of finished tubing. Tension and hardness sampling apply to both routes. SHH STEEL produces and supplies both seamless and welded A789 S32506 against the route named on the enquiry, with EN 10204 3.1 coverage of chemistry and mechanicals.
Dimensions and Tolerances
Average wall is the default under A789; specify minimum wall on the order when that is the design basis. Outside diameter and wall are ordered as tube sizes (metric or inch OD × wall / BWG). General dimensional requirements sit in Specification A1016/A1016M unless A789 states otherwise.
| Item | Typical enquiry practice for S32506 tube |
|---|---|
| Outside diameter | 12.7–76.2 mm common HX/process band; larger OD by agreement |
| Wall | Average wall default; minimum wall when named; BWG 10–20 class and metric equivalents |
| Length | Cut-to-length for exchanger bundles; mill random by agreement |
| Straightness / ovality | Per A1016/A1016M and any tighter project tolerance |
When converting a pipe schedule into tube wall, state clearly whether acceptance is average or minimum wall — the two are not interchangeable on the mill ticket. SHH STEEL confirms OD × wall, length, and finish before the heat is reserved.
Equivalent Grades
UNS S32506 is a less common commercial grade than 2205 or 2507; specify by UNS on every order.
| System | Designation (indicative) |
|---|---|
| UNS | S32506 |
| Family | Duplex (W-bearing) |
| ASTM tube | A789 / A789M S32506 |
| ASME | SA789 S32506 when Code stamping is required |
Dual A789/SA789 on request. Hub: A789/A789M.
Heat Treatment and Delivery Condition
A789/A789M-24 Table 2 lists UNS S32506 at 1870–2050 °F [1020–1120 °C] with rapid cooling in water or by other means (unless Table 2 states a different quench). Seamless tube may be quenched directly after hot forming while at or above the minimum solution temperature where the standard allows that alternate.
Rapid cooling limits time in the sigma-forming window (roughly 700–1000 °C). A789’s scope warns that these steels are susceptible to embrittlement if used for prolonged periods at elevated temperatures, including 475 °C (885 °F) ferrite embrittlement. SHH STEEL supplies S32506 solution-annealed and quenched per Table 2.
Corrosion Resistance
S32506 is selected when chloride SCC resistance and a Mo+W crevice margin above A789 S32205 are needed without a full super duplex PREN ≥40 mandate. Mid-range W-adjusted PREN ≈38–39 supports that positioning.
It is not automatically interchangeable with A789 S32750 or A789 S32760 on seawater crevice datasheets. Use heat-certificate chemistry and project limits.
Applications of A789 S32506 Tube
Chemical-process and chloride-bearing heat-exchanger tube, selected oil-and-gas utility circuits, and projects that freeze S32506 by UNS. Lower elongation floor versus 2205 may affect severe forming — confirm with the fabricator.
SHH STEEL produces and supplies A789 S32506 for enquiry sizes and can quote A789 S32750 when PREN ≥40 is mandatory.
Weldability
Autogenous A789 welded tube must meet parent anneal and mechanicals without filler. Fabrication welds that use filler typically take matching or overalloyed duplex/super duplex consumables with controlled heat input and interpass temperature so ferrite–austenite balance stays qualified. Re-anneal after heavy hot work when required; keep bake and stress-relief cycles out of the sigma nose and the 400–500 °C embrittlement band unless a qualified procedure says otherwise.
Surface Finishes
Standard delivery is solution-annealed and pickled (or otherwise descaled) so the passive film can form uniformly. Bright-annealed or lightly polished OD/ID finishes are available by agreement when the exchanger or hygienic duty needs a smoother bore. Passivation after pickling or after fabrication welding is good practice in chloride service; remove carbon-steel tooling contamination before commissioning. SHH STEEL states the finish route on the quotation and on the MTC.
Inspection and Testing
Each A789 tube takes either a nondestructive electric test or a hydrostatic test. Mechanical sampling covers tension, hardness, and flaring for seamless or flange plus reverse flattening for welded, with full heat analysis on the mill test certificate. Product analysis and supplementary corrosion or ferrite tests are added when the purchase order asks for them. SHH STEEL issues EN 10204 3.1 as standard and arranges third-party inspection / 3.2 when the enquiry names an agency, with lot identity per A789 Notes 1 and 2.
Packaging and Shipping
Tube is typically packed in hexagonal bundles or plywood cases with end protectors and waterproof wrapping for ocean freight, with bundle tags repeating heat number, size, and standard. Cut-to-length exchanger tube may be boxed by length group; U-bends travel in purpose-built crates when ordered. SHH STEEL ships FOB, CFR, CIF, or EXW under the Incoterm on the order, with commercial invoice, packing list, and the EN 10204 3.1 or 3.2 certificate set.
Why Choose SHH STEEL
SHH STEEL produces and supplies ASTM A789 UNS S32506 duplex tube — coordinating W-bearing chemistry, tube making, anneal, test, and EN 10204 3.1 documents to the PO. Production capability, not trader-only.
We flag the 18% elongation / 302 HBW floors from older Table 4 copies so buyers and fabricators are not surprised versus 2205 practice.
Supply Capability
SHH STEEL can produce and supply ASTM A789 UNS S32506 against the edition, size, and finish route named on your enquiry. The capability table below summarizes what we regularly quote, followed by the Stock / Available sizes map.
| Item | SHH STEEL capability for S32506 |
|---|---|
| Standard | ASTM A789 / A789M (dual SA789 marking on request) |
| Grade | UNS S32506 |
| Product form | Seamless and welded (no filler metal); heat-treated |
| Size | Typical HX/process OD × wall / BWG; other diameters by agreement |
| Wall | Average wall default; minimum wall when specified |
| Length | Cut-to-length; mill random; U-bends on enquiry |
| Finish | Annealed and pickled; bright annealed or light polish by agreement |
| Testing | Tension, hardness, flaring or flange + reverse flattening, hydro or NDE; full ladle chemistry on MTC |
| Documents | EN 10204 3.1; third-party / 3.2 on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes
SHH STEEL quotes S32506 tube against a practical production-and-stock enquiry range rather than a frozen warehouse SKU list with published tonnages. Availability of any single line on a given week depends on mill drawing and inbound schedule — treat the table as a supply map for enquiry.
| Item | Typical stock / enquiry range for S32506 |
|---|---|
| Outside diameter | 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (other HX ODs on enquiry) |
| Wall / BWG | BWG 10–20 class and metric min- or avg-wall equivalents; lighter and heavier walls by agreement |
| Common OD × wall examples | 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — confirm avg vs min wall |
| Length | Cut lengths for exchanger bundles; straight random lengths on enquiry |
| Special | Non-standard OD/wall, bright anneal, welded or seamless route, dual A789/SA789 marking — confirm before the heat is reserved |
When you send an enquiry, include the ASTM edition if known, seamless or welded, OD × wall (avg or min), length, finish, test extras, and destination port. Sister grades such as A789 S32205, A789 S31260, and A789 S32750 can be quoted on the same enquiry when the project mixes duplex classes.
FAQ
Conclusion
ASTM A789 UNS S32506 is a duplex stainless steel tube grade under the A789 seamless-and-welded duplex tubing specification. SHH STEEL produces and supplies seamless and welded S32506 to the A789 anneal and test regime with EN 10204 3.1 documentation. For sizes, dual marking, or grade comparisons, contact admin@steelspecs.com.