ASTM A514/A514M Carbon Steel Plates
ASTM A514/A514M covers quenched-and-tempered alloy structural plates up to 150 mm. Grades are A, B, E, F, H, P, Q and S. Yield is 690 MPa to 65 mm and 620 MPa over 65 mm. There is no ASME SA-514 book in Section II. For Code QT vessel plate use SA-517. SHH STEEL supplies A514 mill-direct from China origin.
-
ASTM A514 Grade B Steel Plate | A514 Gr.B 100ksi QT Structural Plate
ASTM A514 Grade B / A514 Gr.B is quenched-and-tempered 100 ksi structural plate to 32 mm. Yield is 690 MPa and tensile is 760–895 MPa. SHH STEEL supplies A514GRB worldwide as a global steel mill sourcing partner.View More -
ASTM A514 Grade Q Steel Plate | A514 Gr.Q 100ksi QT Structural Plate supplier
ASTM A514 Grade Q / A514 Gr.Q is quenched-and-tempered 100 ksi structural plate. Yield is 690 MPa to 65 mm and 620 MPa over 65 mm. SHH STEEL supplies A514GRQ worldwide as a global steel mill sourcing partner.View More
ASTM A514/A514M Carbon Steel Plates
Structural Steel Plates
SHH STEEL, a top Structural Steel Plates exporter, produces and exports structural steel plates for buildings, bridges, and infrastructure. Our plates, such as ASTM A36, deliver exceptional strength and weldability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for construction steel plates and custom solutions for large-scale structural projects.
Structural Steel Plates
X