ASTM A514 Grade F quenched and tempered 100 ksi structural steel plate, Ni-Cr-Mo-Cu-V-B alloy, max 2.5 in, SHH STEEL

ASTM A514 Grade F Steel Plate | A514 Gr.F 100ksi QT Structural Plate supplier

ASTM A514 Grade F / A514 Gr.F is quenched-and-tempered 100 ksi structural plate to 65 mm. Yield is 690 MPa and tensile is 760–895 MPa. SHH STEEL supplies A514GRF worldwide as a global steel mill sourcing partner.
Keywords
ASTM A514 Grade F, A514 Gr.F, A514GRF, A514-F, T-1 plate Grade F, 100 ksi QT plate, A514 Gr.F supplier
Equivalent Grades:
A514 Gr F / A517 Gr F / EN 10025-6 S690QL1 (near) / JIS — / GB Q690E (near) — Material Specification: ASTM A514 / A514M — Delivery: Quenched + Tempered (QT); Mn-Ni-Cr-Mo; max 65 mm
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
100 ksi QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is ASTM A514 Grade F Steel?

ASTM A514 Grade F, also searched as A514 Gr.F, A514GRF, A514-F, A514F, T-1 Grade F and 100 ksi QT plate, is the nickel-bearing mid-thickness grade in ASTM A514/A514M. That book covers quenched-and-tempered alloy structural plates intended primarily for welded bridges and other structures. Maximum thickness for Grade F is 2½ in / 65 mm. General requirements follow ASTM A6 / ASME SA-6, not A20 / SA-20.

There is no ASME SA-514 / SA-514M book in current Section II, Part A. Inquiries that write SA514 Gr.F are still buying ASTM A514 Grade F. Code quenched-and-tempered vessel plate is ASTM A517 Grade F, not A514.

This page is not Grade B. Grade B stops at 32 mm and has no nickel window. This page is not Grade Q. Grade Q goes to 150 mm and uses 1.20–1.50% Ni. This page is not Grade E. Grade E goes to 150 mm with 1.40–2.00% Cr and no nickel requirement. This page is not A572 Gr.50. This page is not EN 10025-6 S690QL.

To 65 mm, yield is 100 ksi / 690 MPa min and tensile is 110–130 ksi / 760–895 MPa. Elongation is 18% in 2 in. Hardness on plate to 20 mm is 235–293 HBW. Grade F has no 90 ksi row because the grade itself stops at 65 mm. Delivery is quenched and tempered. Grade F chemistry carries nickel, chromium, molybdenum, vanadium, copper and boron.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We buy this grade from qualified Chinese mills, check Ni-Cr-Mo-V-Cu-B on the heat analysis, record QT on the certificate, and ship plate to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America. If the drawing is 80 mm, we will not roll Grade F and call 100 ksi enough.

Related category pages: structural steel plates, ASTM A572 / A572M and EN 10025-6.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Plate book ASTM A514/A514M Grade F Confirmed
ASME twin book None. No SA-514 in Section II Stated on MTC as A514
Other search names A514GRF, T-1 F, 100 ksi QT Covered
Steel type Killed QT Ni-Cr-Mo-V-Cu-B structural plate Confirmed
General requirements A6 / SA-6 Confirmed
Max thickness, Grade F 65 mm (2½ in) Confirmed
Yield to 65 mm 690 MPa (100 ksi) min Confirmed
Tensile to 65 mm 760–895 MPa (110–130 ksi) Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

Thicker A514 sisters belong on Grade Q, Grade E and Grade P. QT vessel sisters belong on ASTM A517 Grade F and ASME SA517 Grade F. European 690 MPa QT sisters belong on EN 10025-6 S690Q and EN 10025-6 S690QL.

Chemical Composition

Grade F is the Ni-Cu member of the mid-thickness A514 band. Heat analysis is the mill table. Product analysis, when ordered, follows A6 product-analysis tolerances.

Heat Analysis — ASTM A514 Grade F

Element Heat Analysis (%)
Carbon (C) 0.10 – 0.20
Manganese (Mn) 0.60 – 1.00
Phosphorus (P), max 0.030
Sulfur (S), max 0.030
Silicon (Si) 0.15 – 0.35
Nickel (Ni) 0.70 – 1.00
Chromium (Cr) 0.40 – 0.65
Molybdenum (Mo) 0.40 – 0.60
Vanadium (V) 0.03 – 0.08
Copper (Cu) 0.15 – 0.50
Boron (B) 0.0005 – 0.005

Grade Q uses more nickel (1.20–1.50%) and more chromium (1.00–1.50%). Grade B has no nickel and no copper window. Grade E has 1.40–2.00% Cr and no nickel requirement. Do not accept a B heat on a Grade F order. Do not accept an F heat on an 80 mm Q order. SHH STEEL prints heat analysis on every certificate. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search A514 Gr.F mechanical properties, A514GRF yield, A514 F 100 ksi and T-1 Grade F tensile.

Tensile, Yield and Hardness — ASTM A514 Grade F

Thickness Yield min Tensile Elongation in 2 in, min Hardness
To 20 mm (¾ in) incl. 100 ksi / 690 MPa 110–130 ksi / 760–895 MPa 18% 235–293 HBW
Over 20 to 65 mm (2½ in) 100 ksi / 690 MPa 110–130 ksi / 760–895 MPa 18% —

Grade F does not have a 65–150 mm row. That row belongs to Grade Q, Grade E and Grade P, where yield already drops to 90 ksi / 620 MPa. If the RFQ is 80 mm and the name is Grade F, the mill cannot certify A514 Grade F.

A572 Gr.50 is 345 MPa yield. ASTM A36 steel plate is 250 MPa yield. Neither is A514.

Material Comparison

Grade Book Max thickness Alloy idea Swap?
ASTM A514 Grade F A514 65 mm Ni-Cr-Mo-V-Cu-B This page
A514 Grade Q A514 150 mm Ni-Cr-Mo-V No
A514 Grade B A514 32 mm Cr-Mo-V-Ti-B No
A514 Grade E A514 150 mm 1.4–2.0Cr-Mo-Ti-B No
A514 Grade H A514 50 mm Ni-Cr-Mo-V-B No
A514 Grade S A514 65 mm Mn-Mo-Nb-B No
ASTM A517 Grade F A517 Vessel QT A517 Gr.F No
EN 10025-6 S690QL EN 10025-6 S690QL Comparison only

Equivalent Material Grades

There is no official one-to-one worldwide swap for A514 Gr.F. What buyers compare is the 690 MPa QT structural idea in the 65 mm band.

In the United States the official plate name is ASTM A514 Grade F. Market shops still say T-1. T-1 is a product name, not the ASTM grade. ASTM A517 Grade F is the vessel QT cousin under A20. Do not dual-mark A514 as A517 unless both books are fully met.

In Europe the usual comparison is EN 10025-6 S690Q or EN 10025-6 S690QL. See EN 10025-6. Dual marking only when both books are met.

In China there is no daily GB/T 1591 twin that copies Grade F chemistry. Q690 market plate is a strength comparison, not an automatic A514 Gr.F certificate.

Designation Country / region Standard Notes
A514 Gr.F / A514GRF / T-1 F USA A514 Name on this page
A514 Grade Q USA A514 150 mm Ni-Cr-Mo-V
A514 Grade B / E / H / S USA A514 Sister grades, different limits
ASTM A517 Grade F USA A517 Vessel QT, A20
EN 10025-6 S690Q Europe EN 10025-6 690 MPa QT comparison
EN 10025-6 S690QL Europe EN 10025-6 −40 °C QT comparison
A572 Gr.50 USA A572 345 MPa HSLA, not QT

100 ksi QT Structural Service

Buyers pick A514 Gr.F when a boom, trailer frame or mining attachment wants 100 ksi yield, nickel-bearing chemistry, and the plate stays inside 65 mm. Search phrases such as A514GRF, A514 Grade F, A514-F, T-1 Grade F and 100 ksi QT plate all point here.

It is the wrong plate for 80 mm or 150 mm chords. That work is Grade Q or Grade E. It is the wrong plate for a Section VIII vessel that names SA-517. That work is ASTM A517 Grade F. It is the wrong plate for a 345 MPa frame that names A572 Gr.50.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

A514 Grade F is killed QT alloy structural plate at 690 MPa yield with nickel and copper. Treat welding as production welding. Heat input, preheat and interpass have to stay inside a written WPS.

Qualify to the applicable structural code. Consumables must match a 100 ksi QT family. A procedure written for Grade B may not cover the nickel-copper window. A procedure written for A572 Gr.50 is 345 MPa HSLA, not A514. Do not overheat the plate and then call it still Grade F. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for A514 Gr.F is quenched and tempered.

A514 does not supply Grade F as-rolled or normalized only. If the mill skipped quench and temper, the plate cannot be certified A514 Grade F.

If the job wants Charpy, write the temperature and joules. A514 does not automatically include impact. Extra 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists ASTM A514 Grade F; heat number; heat analysis including Ni, Cr, Mo, V, Cu and B; tensile to the 65 mm table; QT delivery. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for A514 Gr.F 100 ksi QT structural plate:

  • Thickness: commonly 6 mm – 65 mm (Grade F max 2½ in)
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Do not order Grade F for 80 mm or 100 mm. Those thicknesses belong to Grade Q, Grade E or Grade P. Grade B stops at 32 mm. Browse more sizes on the products index.

Tolerances

Dimensional limits for ASTM A514 Grade F follow ASTM A6 / ASME SA-6 unless the purchase order names another table.

Typical thickness tolerance idea for A514 Gr.F (A6 / SA-6 reference)

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
6 – 16 −0.4 +0.8
16 – 25 −0.5 +0.9
25 – 40 −0.6 +1.0
40 – 65 −0.8 +1.2

Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows A6 / SA-6 unless a tighter class is written. SHH STEEL will not assume a zero-minus extra on A514GRF unless the order says so.

Supplementary Requirements

A514 Grade F already defines chemistry, QT and the 100 ksi table inside 65 mm. Extra items still have to be written on the purchase order.

Book name. Write ASTM A514 Grade F. If the inquiry said SA514, state on the PO that the mill will certify A514.

Thickness check. Confirm the ordered thickness is ≤ 65 mm before the heat is planned as Grade F.

Charpy details. Write temperature, joules, location and orientation.

Product analysis. Especially C, Ni, Cr, Mo, V, Cu, B, P and S.

Through-thickness / Z-test. Name Z15, Z25 or Z35 when needed.

NDE. A6 ultrasonic extras as named.

Hardness. The book already gives 235–293 HBW on plate to 20 mm.

Identification and stamping. Heat number, A514 Grade F, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named.

Applications

Industry Typical components
Crane and boom A514 Gr.F / A514GRF mid-thickness chords
Trailers and chassis Grade F frames from SHH STEEL
Mining attachments 100 ksi QT brackets to 65 mm
Comparison vs Grade Q A514GRF next to A514 Grade Q
Comparison vs S690 A514GRF next to EN 10025-6 S690QL
Not for Code vessels Use ASTM A517 Grade F instead

A514 Grade F is the plate for a file that wants 100 ksi QT structural plate inside 65 mm with nickel-copper chemistry. It is the wrong plate for 150 mm chords. That work is Grade Q or Grade E. It is the wrong plate for a pressure vessel that names SA-517. That work sits on ASTM A517 Grade F. It is the wrong plate for ordinary carbon frames. That work sits on ASTM A36 steel plate or structural steel plates.

Supply Capability

SHH STEEL sources ASTM A514 Grade F from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or QT route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 50 mm, 60 mm, 65 mm.

Processing: CNC or flame cutting, bevel, flattening, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard rolling / QT about 45–60 days; 3.2 inspection about 2 months.

Why Choose SHH STEEL

Experience on this grade is simple: print A514 Grade F, keep the 65 mm cap, keep Ni-Cu on the certificate, and do not invent SA-514. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) prices A514GRF from first-line mills, reports Ni-Cr-Mo-V-Cu-B chemistry, records the 100 ksi table, and issues 3.1 as standard or 3.2 when specified.

We keep the book on the order. A514GRF is not Grade Q at 80 mm. A514 Grade F is not Grade B just because both say 100 ksi. A514 Grade F is not ASTM A517 Grade F. If the drawing says 100 mm A514, we will move the inquiry to Grade Q or Grade E instead of forcing Grade F.

FAQ

What is A514 Grade F steel plate?
ASTM A514 Grade F, also searched as A514 Gr.F, A514GRF, A514-F and T-1 Grade F, is quenched-and-tempered alloy structural plate limited to 65 mm. Yield is 690 MPa and tensile is 760–895 MPa. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
Is there an ASME SA-514 Grade F?
No. Current Section II, Part A does not contain SA-514. The plate book is ASTM A514/A514M. Code QT vessel plate is SA-517.
What is the maximum thickness for A514GRF?
65 mm (2½ in). Thicker plate must be Grade Q, Grade E or Grade P.
How is Grade F different from Grade Q?
Grade F stops at 65 mm and uses 0.70–1.00% Ni plus copper. Grade Q goes to 150 mm with 1.20–1.50% Ni and no copper requirement.
How is A514GRF different from A517 Grade F?
A514 is structural QT under A6. A517 is pressure-vessel QT under A20. Do not swap them.

Conclusion

ASTM A514 Grade F Steel Plate is quenched-and-tempered 100 ksi structural plate limited to 65 mm, with 690 MPa yield and 760–895 MPa tensile. Whether the inquiry says ASTM A514 Grade F, A514 Gr.F, A514GRF, A514-F, T-1 Grade F or SA514 Gr.F, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with Grade F chemistry, the 65 mm A514 table, recorded QT delivery, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies ASTM A514 Grade F / A514 Gr.F 100ksi QT Structural Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade and stays inside 65 mm.

Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.

ASTM A514 Grade F Steel Plate, A514 Gr.F, A514GRF, T-1 Grade F, 100 ksi QT plate, A514 Gr.F supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X