ASTM A283/A283M Carbon Steel Plates
SHH STEEL offers ASTM A283/A283M-compliant Grade A/B/C/D carbon steel plates. ASTM A283/A283M specifies low to intermediate tensile strength riveted/bolted/welded structures for general applications. Reliable, affordable, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASTM A283 Grade B Steel Plate | A283 Gr.B Structural Steel Plate
ASTM A283 Grade B is a low-to-intermediate tensile carbon structural plate under ASTM A283/A283M. Tensile 345–450 MPa, yield 185 MPa. China mill Distributor SHH STEEL supplies A283 Gr.B / SA283 Gr.B with 3.1 or 3.2 certificates.View More -
ASTM A283 Grade A Steel Plate | A283 Gr.A Structural Steel Plate
ASTM A283 Grade B is a low-to-intermediate tensile carbon structural plate under ASTM A283/A283M. Tensile 345–450 MPa, yield 185 MPa. China mill Distributor SHH STEEL supplies A283 Gr.B / SA283 Gr.B with 3.1 or 3.2 certificates.View More -
ASTM A283 Grade D Steel Plate | A283 Gr.D Structural Steel Plate
ASTM A283 Grade D is the highest-strength grade in ASTM A283/A283M. Tensile 415–550 MPa, yield 230 MPa. Direct Mill Supply by SHH STEEL for A283 Gr.D / SA283 Gr.D with 3.1 or 3.2 certificates.View More -
ASTM A283 Grade C Steel Plate | A283 Gr.C Structural Steel Plate
ASTM A283 Grade C is a low-to-intermediate tensile carbon structural plate under ASTM A283/A283M. Tensile 380–515 MPa, yield 205 MPa. SHH STEEL supplies A283 Gr.C / SA283 Gr.C as China mill-Direct Supply with 3.1 or 3.2 certificates.View More
Structural Steel Plates
SHH STEEL, a top Structural Steel Plates exporter, produces and exports structural steel plates for buildings, bridges, and infrastructure. Our plates, such as ASTM A36, deliver exceptional strength and weldability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for construction steel plates and custom solutions for large-scale structural projects.