Product Showcase
GOST 14637 Carbon Steel Plates
SHH STEEL offers GOST 14637-compliant St3sp/St3ps carbon steel plates. GOST 14637 specifies hot-rolled heavy plates of ordinary-quality non-alloy steel, grades St0 to St5Gps, for welded and general structures. Durable, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GOST 14637 St5Gps Steel Plate | St5Gps Mn Semi-Killed Carbon Steel Plate
GOST 14637 St5Gps (Ст5Гпс) steel plate is a manganese semi-killed (Гпс) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this manganese semi-killed grade to the ordered 2024 requirements.View More -
GOST 14637 St5sp Steel Plate | St5sp Killed Carbon Steel Plate
GOST 14637 St5sp (Ст5сп) steel plate is a killed (sp) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this killed grade to the ordered 2024 requirements.View More -
GOST 14637 St5ps Steel Plate | St5ps Semi-Killed Carbon Steel Plate
GOST 14637 St5ps (Ст5пс) steel plate is a semi-killed (ps) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this semi-killed grade to the ordered 2024 requirements.View More -
GOST 14637 St4sp Steel Plate | St4sp Killed Carbon Steel Plate
GOST 14637 St4sp (Ст4сп) steel plate is a killed (sp) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this killed grade to the ordered 2024 requirements.View More -
GOST 14637 St4ps Steel Plate | St4ps Semi-Killed Carbon Steel Plate
GOST 14637 St4ps (Ст4пс) steel plate is a semi-killed (ps) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this semi-killed grade to the ordered 2024 requirements.View More -
GOST 14637 St3Gsp Steel Plate | St3Gsp Mn Killed Carbon Steel Plate
GOST 14637 St3Gsp (Ст3Гсп) steel plate is a manganese killed (Гсп) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this manganese killed grade to the ordered 2024 requirements.View More -
GOST 14637 St3Gps Steel Plate | St3Gps Mn Semi-Killed Carbon Steel Plate
GOST 14637 St3Gps (Ст3Гпс) steel plate is a manganese semi-killed (Гпс) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this manganese semi-killed grade to the ordered 2024 requirements.View More -
GOST 14637 St3sp Steel Plate | St3sp Killed Carbon Steel Plate
GOST 14637 St3sp (Ст3сп) steel plate is a killed (sp) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this killed grade to the ordered 2024 requirements.View More -
GOST 14637 St3ps Steel Plate | St3ps Semi-Killed Carbon Steel Plate
GOST 14637 St3ps (Ст3пс) steel plate is a semi-killed (ps) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this semi-killed grade to the ordered 2024 requirements.View More -
GOST 14637 St3kp Steel Plate | St3kp Rimmed Carbon Steel Plate
GOST 14637 St3kp (Ст3кп) steel plate is a rimmed (kp) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this rimmed grade to the ordered 2024 requirements.View More -
GOST 14637 St2sp Steel Plate | St2sp Killed Carbon Steel Plate
GOST 14637 St2sp (Ст2сп) steel plate is a killed (sp) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this killed grade to the ordered 2024 requirements.View More -
GOST 14637 St2ps Steel Plate | St2ps Semi-Killed Carbon Steel Plate
GOST 14637 St2ps (Ст2пс) steel plate is a semi-killed (ps) general-quality nonalloyed plate grade under GOST 14637-2024, Rolled plates from nonalloyed steel of general quality. Specifications. The 2024 edition is the current standard as of 12 November 2026: it was introduced as a national standard of the Russian Federation on 1 March 2025, with the right of early application, and it replaces GOST 14637-89. SHH STEEL produces and exports this semi-killed grade to the ordered 2024 requirements.View More
GOST 14637 Carbon Steel Plates
Structural Steel Plates
SHH STEEL, a top Structural Steel Plates exporter, produces and exports structural steel plates for buildings, bridges, and infrastructure. Our plates, such as ASTM A36, deliver exceptional strength and weldability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for construction steel plates and custom solutions for large-scale structural projects.
Structural Steel Plates
X