JIS G3101

Product Showcase

JIS G3101 Carbon Steel Plates

SHH STEEL offers JIS G3101-compliant SS400 rolled steels for general structures. JIS G3101 specifies hot-rolled mild steel plates for welding, bolting, and riveting in buildings and ships. Cost-effective, certified quality, competitive prices, customizable. Trust SHH STEEL!

JIS G3101 SS540 Steel Plate | JIS G3101 Steel - SHH STEEL

JIS G3101 SS540 Steel Plate

JIS G3101 SS540 is a hot-rolled general structural steel. It is the highest-tensile JIS G 3101 grade. The name marks a 540 N/mm² tensile minimum, not yield. Table 3 gives 540 N/mm² minimum tensile strength. Yield is 400 N/mm² up to 16 mm and 390 N/mm² through 40 mm. Plate thickness is limited to 40 mm. Carbon is 0.30 % max and manganese is 1.60 % max. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
JIS G3101 SS490 Steel Plate | JIS G3101 Steel - SHH STEEL

JIS G3101 SS490 Steel Plate

JIS G3101 SS490 is a hot-rolled general structural steel. The name marks a 490 N/mm² tensile minimum, not yield. Table 3 gives a tensile range of 490–610 N/mm². Yield is 285 N/mm² up to 16 mm, then 275, 255 and 245 N/mm² in thicker bands, including over 100 mm. Carbon and manganese are not specified; phosphorus and sulfur are each 0.050 % maximum. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
JIS G3101 SS400 Steel Plate | JIS G3101 Steel - SHH STEEL

JIS G3101 SS400 Steel Plate

JIS G3101 SS400 is a hot-rolled general structural steel. The name marks a 400 N/mm² tensile minimum, not yield. Table 3 gives a tensile range of 400–510 N/mm². Yield is 245 N/mm² up to 16 mm, then 235, 215 and 205 N/mm² in thicker bands, including over 100 mm. Carbon and manganese are not specified; phosphorus and sulfur are each 0.050 % maximum. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
JIS G3101 SS330 Steel Plate | JIS G3101 Steel - SHH STEEL

JIS G3101 SS330 Steel Plate

JIS G3101 SS330 is a hot-rolled general structural steel. The name marks a 330 N/mm² tensile minimum, not yield. Table 3 gives a tensile range of 330–430 N/mm². Yield is 205 N/mm² up to 16 mm, then 195, 175 and 165 N/mm² in thicker bands, including over 100 mm. The grade covers plates, strip, flats and bars, not sections. Carbon and manganese are not specified. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
SHH STEEL Structural Steel Plates – Carbon and Alloy Steel

Structural Steel Plates

SHH STEEL, a top Structural Steel Plates exporter, produces and exports structural steel plates for buildings, bridges, and infrastructure. Our plates, such as ASTM A36, deliver exceptional strength and weldability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for construction steel plates and custom solutions for large-scale structural projects.

Structural Steel Plates