ASTM A514 Grade M quenched and tempered 100 ksi structural steel plate, Ni-Mo-B alloy, max 2 in, SHH STEEL

ASTM A514 Grade M Steel Plate | A514 Gr.M 100ksi QT Structural Plate supplier

ASTM A514 Grade M / A514 Gr.M is a historical 100 ksi QT structural grade from earlier A514 tables, 50 mm max. Current Table 1 no longer lists Grade M. SHH STEEL still sources A514GRM when the old drawing names it.
Keywords
ASTM A514 Grade M, A514 Gr.M, A514GRM, A514-M, historical A514 Grade M, 100 ksi QT plate, Q690E, A514 Gr.M supplier
Equivalent Grades:
A514 Gr M / A517 Gr M / EN S690Q (near) / JIS — / GB Q690 — Material Specification: ASTM A514 / A514M — Delivery: Quenched + Tempered (QT); Mn-Cr-Ni-Mo-B; max 50 mm
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
100 ksi QT Structural Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Supply Capability
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is ASTM A514 Grade M Steel ?

ASTM A514 Grade M, also searched as A514 Gr.M, A514GRM, A514-M, A514M and 100 ksi QT plate, is a historical grade from earlier editions of ASTM A514/A514M. Older tables listed Grade M with a maximum thickness of 2 in / 50 mm. Current A514/A514M-18 / -22 Table 1 lists only A, B, E, F, H, P, Q and S. Grade M is not on that current table.

A purchase order that still writes Grade M is usually an old boom drawing, a spare-part list, or a mill spec that was never revised. SHH STEEL will not silently recertify it as current Grade H or Grade P. Current Grade H is a 50 mm nickel grade with chromium and vanadium. Current Grade P is a 150 mm nickel-chromium grade. Historical Grade M is a nickel-molybdenum-boron grade with no chromium window. Those heats are not the same steel.

There is no ASME SA-514 / SA-514M book in current Section II, Part A. Inquiries that write SA514 Gr.M are still talking about historical ASTM A514 Grade M. Code quenched-and-tempered vessel plate belongs on ASTM A517, not on an old A514 letter.

This page is not current Grade H. This page is not current Grade P. This page is not current Grade Q. This page is not current Grade F. This page is not A572 Gr.50. This page is not EN 10025-6 S690QL. This page is not GB/T 16270 Q690E.

On the old table, yield to 50 mm is 100 ksi / 690 MPa min and tensile is 110–130 ksi / 760–895 MPa. Elongation is 18% in 2 in. Hardness on plate to 20 mm is 235–293 HBW. Delivery is quenched and tempered. General requirements follow ASTM A6 / ASME SA-6.

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We source historical Grade M when the order writes that chemistry, print heat analysis and product analysis when ordered, record QT on the certificate, and ship plate to fabricators in the USA, Europe, Middle East, Southeast Asia, Africa and South America. If the drawing is 80 mm, we will not roll Grade M and call 100 ksi enough.

Related category pages: structural steel plates, ASTM A572 / A572M and EN 10025-6.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Historical book Earlier A514/A514M Grade M Confirmed on PO
Current Table 1 Not listed Stated on quote
Current 50 mm sister Grade H Offered only if PO allows
Current thick Ni sister Grade P / Grade Q Offered only if PO allows
Other search names A514GRM, A514-M, historical Grade M Covered
Steel type Killed QT Ni-Mo-B structural plate Confirmed
General requirements A6 / SA-6 Confirmed
Max thickness, old table 50 mm (2 in) Confirmed
Yield to 50 mm 690 MPa (100 ksi) min Confirmed
Product analysis A6 tolerances when ordered Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Certification EN 10204 3.1 or 3.2 / third-party As ordered

Current thick-plate sisters belong on Grade Q, Grade E and Grade P. QT vessel work belongs on ASTM A517 Grade P or ASTM A517 Grade Q, not on historical A514 Grade M.

Chemical Composition

Old-table Grade M is a nickel-molybdenum-boron grade with a low manganese window and no chromium requirement. Values below follow earlier A514 chemistry tables. Current Table 1 does not reprint this column.

Heat Analysis and Product Analysis — historical ASTM A514 Grade M

Element Heat Analysis (%) Product Analysis (%)
Carbon (C) 0.12 – 0.21 0.10 – 0.24
Manganese (Mn) 0.45 – 0.70 0.40 – 0.76
Phosphorus (P), max 0.035 0.040
Sulfur (S), max 0.035 0.040
Silicon (Si) 0.20 – 0.35 0.15 – 0.40
Nickel (Ni) 1.20 – 1.50 1.15 – 1.55
Molybdenum (Mo) 0.45 – 0.60 0.41 – 0.64
Boron (B) 0.001 – 0.005 0.0005 – 0.006

Current Grade H uses 0.30–0.70% Ni plus chromium and vanadium. Current Grade P uses 1.20–1.50% Ni plus 0.85–1.20% Cr and goes to 150 mm. Historical Grade M has the high nickel window of Grade P but no chromium column and stops at 50 mm. Do not stamp Grade M chemistry as Grade H or Grade P unless the purchase order allows the swap. If product analysis is on the purchase order, SHH STEEL prints both columns on the certificate. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search A514 Gr.M mechanical properties, A514GRM yield, A514 M 100 ksi and historical A514 Grade M tensile.

Tensile, Yield and Hardness — historical ASTM A514 Grade M

Thickness Yield min Tensile Elongation in 2 in, min Hardness
To 20 mm (¾ in) incl. 100 ksi / 690 MPa 110–130 ksi / 760–895 MPa 18% 235–293 HBW
Over 20 to 50 mm (2 in) 100 ksi / 690 MPa 110–130 ksi / 760–895 MPa 18% —

The old table did not give Grade M a 65–150 mm row. That row belongs only to current Grade Q, Grade E and Grade P. If the RFQ is 80 mm and the name is Grade M, the mill cannot certify historical A514 Grade M. Move that inquiry to current Grade P or Grade Q after the purchase order is revised.

A572 Gr.50 is 345 MPa yield. ASTM A36 steel plate is 250 MPa yield. Neither is A514.

Material Comparison

Grade Status Max thickness Alloy idea Swap?
A514 Grade M Historical 50 mm Ni-Mo-B This page
A514 Grade H Current Table 1 50 mm Ni-Cr-Mo-V-B No, unless PO allows
A514 Grade P Current Table 1 150 mm Ni-Cr-Mo-B No
A514 Grade Q Current Table 1 150 mm Ni-Cr-Mo-V No
A514 Grade F Current Table 1 65 mm Ni-Cr-Mo-V-Cu-B No
A514 Grade K Historical 50 mm Mn-Mo-B, no Ni No
EN 10025-6 S690QL Europe S690QL Comparison only
GB/T 16270 Q690E China Q690E Comparison only

Equivalent Material Grades

Historical Grade M has no official current twin. What buyers compare is the 690 MPa QT structural idea in the 50 mm nickel band.

In the United States the current official names are A, B, E, F, H, P, Q and S. Grade M is a search name from earlier books. Market shops still say T-1. T-1 is a product name, not the ASTM grade. ASTM A517 vessel grades are not A514. Do not dual-mark historical Grade M as A517 unless both books are fully met for that Code year.

In Europe the usual comparison is EN 10025-6 S690Q or EN 10025-6 S690QL. See EN 10025-6. Dual marking only when both books are met.

In China the nearest QT comparison is GB/T 16270 Q690D / Q690E. That book is high-yield quenched-and-tempered structural plate. Q690E adds a −40 °C impact table. GB/T 1591 Q690C / Q690D / Q690E is a different book and is not automatically QT A514. GB chemistry does not copy the historical Grade M nickel-molybdenum window. Dual marking only when both books are fully met. Do not treat Q345B or Q355B as A514.

Designation Country / region Standard Notes
A514 Gr.M / A514GRM USA Earlier A514 Historical name on this page
A514 Grade H USA Current A514 Current 50 mm Ni sister
A514 Grade P USA Current A514 Current 150 mm Ni-Cr
A514 Grade Q USA Current A514 Current 150 mm Ni-Cr-V
A514 Grade K USA Earlier A514 Historical 50 mm, no Ni
EN 10025-6 S690Q Europe EN 10025-6 690 MPa QT comparison
EN 10025-6 S690QL Europe EN 10025-6 −40 °C QT comparison
GB/T 16270 Q690E China GB/T 16270 QT structural comparison
GB/T 16270 Q690D China GB/T 16270 QT comparison, milder impact
GB/T 1591 Q690E China GB/T 1591 HSLA book, not auto A514
A572 Gr.50 USA A572 345 MPa HSLA, not QT

100 ksi QT Structural Service

Buyers pick A514 Gr.M when an old boom, trailer frame, mining attachment or spare-part list still prints Grade M. Search phrases such as A514GRM, A514 Grade M, A514-M and historical A514 Grade M all point here.

SHH STEEL will ask two questions before rolling: does the file need the historical Ni-Mo-B heat, or can it move to current Grade H or Grade P? We will not invent a current Table 1 stamp that says Grade M. We will not ship 80 mm plate as Grade M. We will not treat Grade M as a vessel grade.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia when the legacy file still names it.

Weldability

Historical A514 Grade M is killed QT alloy structural plate at 690 MPa yield with 1.20–1.50% nickel and no chromium window. Treat welding as production welding. Heat input, preheat and interpass have to stay inside a written WPS.

Qualify to the applicable structural code. Consumables must match a 100 ksi QT family. A procedure written for current Grade H may not cover the higher nickel. A procedure written for A572 Gr.50 is 345 MPa HSLA, not A514. Do not overheat the plate and then call it still Grade M. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL for A514 Gr.M is quenched and tempered.

A514 does not supply Grade M as-rolled or normalized only. If the mill skipped quench and temper, the plate cannot be certified as historical A514 Grade M.

If the job wants Charpy, write the temperature and joules. A514 does not automatically include impact. Extra 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists ASTM A514 Grade M as a historical grade when that is what the order writes; heat number; heat analysis and product analysis when ordered; tensile to the 50 mm table; QT delivery. Certificates may be EN 10204 3.1 or EN 10204 3.2. The quote will also state that current Table 1 does not list Grade M.

Dimensions

Usual supply range from SHH STEEL for historical A514 Gr.M 100 ksi QT structural plate:

  • Thickness: commonly 6 mm – 50 mm (old-table max 2 in)
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Do not order Grade M for 80 mm or 100 mm. Those thicknesses belong to current Grade P or Grade Q after the purchase order is revised. Browse more sizes on the products index.

Tolerances

Dimensional limits for historical ASTM A514 Grade M follow ASTM A6 / ASME SA-6 unless the purchase order names another table. Do not apply pressure-vessel A20 extras unless the order writes them.

Typical thickness tolerance idea for A514 Gr.M (A6 / SA-6 reference)

Nominal thickness (mm) Usual minus (mm) Usual plus (mm)
6 – 16 −0.4 +0.8
16 – 25 −0.5 +0.9
25 – 40 −0.6 +1.0
40 – 50 −0.8 +1.2

Width on 1500–4000 mm plate is commonly held to about ±20–25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm or ±25 mm by mill practice. Flatness follows A6 / SA-6 unless a tighter class is written. SHH STEEL will not assume a zero-minus extra on A514GRM unless the order says so.

Supplementary Requirements

Historical Grade M already defines chemistry, QT and the 100 ksi table inside 50 mm. Extra items still have to be written on the purchase order.

Book year. Write the old A514 edition if the file depends on that table.

Historical name. Write ASTM A514 Grade M. State on the quote that current Table 1 does not list Grade M.

Thickness check. Confirm the ordered thickness is ≤ 50 mm before the heat is planned as Grade M.

Product analysis. Write it if the file needs the second chemistry column, especially Ni, Mo and B.

Charpy details. Write temperature, joules, location and orientation.

Through-thickness / Z-test. Name Z15, Z25 or Z35 when needed.

NDE. A6 ultrasonic extras as named.

Hardness. The book already gives 235–293 HBW on plate to 20 mm.

Identification and stamping. Heat number, A514 Grade M, thickness and mill logo.

Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS, CCS, DNV or the inspector named.

Applications

Industry Typical components
Legacy crane and boom A514 Gr.M / A514GRM mid-thickness inserts
Old trailer drawings Grade M frames from SHH STEEL
Replacement parts Historical 50 mm nickel 100 ksi QT
Current alternative Move to Grade H or Grade P if the PO allows
Comparison vs Q690E A514GRM next to GB/T 16270 Q690E
Comparison vs S690 A514GRM next to EN 10025-6 S690QL

Historical A514 Grade M is the plate for a file that still wants 100 ksi QT structural plate inside 50 mm with the old Ni-Mo-B chemistry. It is the wrong plate for 150 mm chords. That work is current Grade P or Grade Q. It is the wrong plate for a pressure vessel that names SA-517. That work sits on ASTM A517. It is the wrong plate for ordinary carbon frames. That work sits on ASTM A36 steel plate or structural steel plates.

Supply Capability

SHH STEEL sources historical ASTM A514 Grade M from first-line Chinese mills when the order writes that chemistry, and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or QT route requires it.

Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.

Usual stock and rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 40 mm, 45 mm, 50 mm.

Processing: CNC or flame cutting, bevel, flattening, UT to the named class.

Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.

Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.

Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical lead time: ex-stock 5–7 days; standard rolling / QT about 45–60 days; 3.2 inspection about 2 months. Historical grades can take the longer mill window because the heat is not a daily current-table program.

Why Choose SHH STEEL

Experience on this grade is simple: say it is historical, keep the 50 mm cap, print product analysis when ordered, and do not pretend current Table 1 still lists Grade M. SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) will either roll the old Ni-Mo-B chemistry or offer current Grade H / Grade P when the purchase order allows the move.

We keep the book on the order. A514GRM is not current Grade H just because both stop at 50 mm. A514 Grade M is not Grade P at 80 mm. A514 Grade M is not ASTM A517 Grade P. A514 Grade M is not GB/T 16270 Q690E unless both books are met. If the drawing says 100 mm A514, we will move the inquiry to current Grade P or Grade Q instead of forcing Grade M.

FAQ

What is A514 Grade M steel plate?
ASTM A514 Grade M, also searched as A514 Gr.M, A514GRM and A514-M, is a historical 100 ksi QT structural grade from earlier A514 tables. Maximum thickness is 50 mm. Chemistry is Ni-Mo-B with no chromium window. Current A514/A514M Table 1 no longer lists Grade M. SHH STEEL still sources it when the old drawing names it.
Is Grade M still in the current ASTM book?
No. Current Table 1 lists A, B, E, F, H, P, Q and S only.
Can SHH STEEL replace Grade M with Grade H or Grade P?
Only if the purchase order allows it. Grade H is the current 50 mm nickel sister with chromium. Grade P is the current 150 mm Ni-Cr sister. Neither copies Grade M chemistry automatically.
What is the Chinese equivalent of A514 Grade M?
The nearest QT comparison is GB/T 16270 Q690D or Q690E. It is a strength comparison, not an automatic plate substitute. GB/T 1591 Q690E is a different book.
Is there ASME SA-514 Grade M?
No. There is no SA-514 book in current Section II.
What is the maximum thickness for A514 Grade M?
50 mm on the old table. Thicker plate must move to a current grade such as Grade P or Grade Q.

Conclusion

ASTM A514 Grade M Steel Plate is a historical 100 ksi QT structural grade from earlier A514 tables, limited to 50 mm, with 690 MPa yield and 760–895 MPa tensile. Current A514/A514M Table 1 does not list Grade M. Whether the inquiry says ASTM A514 Grade M, A514 Gr.M, A514GRM, A514-M or historical A514 Grade M, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) will confirm the old Ni-Mo-B chemistry, print heat and product analysis as ordered, record QT delivery, and issue EN 10204 3.1 or 3.2.

SHH STEEL supplies historical ASTM A514 Grade M / A514 Gr.M 100ksi QT Structural Plate for replacement and legacy files that still name this grade and stay inside 50 mm.

Contact SHH STEEL for mill rolling, a current-grade alternative, cutting, bevel, 3.2 inspection or a worldwide quotation.

ASTM A514 Grade M Steel Plate, A514 Gr.M, A514GRM, historical A514 Grade M, 100 ksi QT plate, A514 Gr.M supplier, SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X