SHH STEEL offers GB/T 700-compliant Q235 carbon structural steel plates. GB/T 700 specifies hot-rolled carbon steels for welded structures, general engineering, and construction. High strength, versatile, certified quality, competitive prices, customizable. Trust SHH STEEL!

GB/T 700 Q275D Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q275D Steel Plate

GB/T 700 Q275D is a carbon structural steel. The name marks a 275 N/mm² yield class and quality D. Table 2 gives tensile strength 410–540 N/mm² and a −20 °C Charpy value of 27 J. Carbon is 0.20 % maximum; phosphorus and sulfur are each 0.035 % maximum. Deoxidation is special killed steel. This quality is not an automatic substitute for Q275A, Q275B or Q275C. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q275C Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q275C Steel Plate

GB/T 700 Q275C is a carbon structural steel. The name marks a 275 N/mm² yield class and quality C. Table 2 gives tensile strength 410–540 N/mm² and a 0 °C Charpy value of 27 J. Carbon is 0.20 % maximum; phosphorus and sulfur are each 0.040 % maximum. Deoxidation is killed steel. This quality is not an automatic substitute for Q275A, Q275B or Q275D. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q275B Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q275B Steel Plate

GB/T 700 Q275B is a carbon structural steel. The name marks a 275 N/mm² yield class and quality B. Table 2 gives tensile strength 410–540 N/mm² and a +20 °C Charpy value of 27 J. Carbon is 0.21 % maximum at 40 mm or less and 0.22 % maximum over 40 mm. This quality is not an automatic substitute for Q275A, Q275C or Q275D. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q275A Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q275A Steel Plate

GB/T 700 Q275A is a carbon structural steel. The name marks a 275 N/mm² yield class and quality A. Table 2 gives tensile strength 410–540 N/mm². Yield is 275 N/mm² at 16 mm or less and decreases in the thicker bands, including over 100 mm. Quality A has no Charpy requirement and is not the same designation as Q275B, Q275C or Q275D. Carbon is 0.24 % maximum. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q235D Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q235D Steel Plate

GB/T 700 Q235D is a carbon structural steel. The name marks a 235 N/mm² yield class and quality D. Table 2 gives tensile strength 370–500 N/mm² and a −20 °C Charpy value of 27 J. Carbon is 0.17 % maximum; phosphorus and sulfur are each 0.035 % maximum. Deoxidation is special killed steel. This quality is not an automatic substitute for Q235A, Q235B or Q235C. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q235C Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q235C Steel Plate

GB/T 700 Q235C is a carbon structural steel. The name marks a 235 N/mm² yield class and quality C. Table 2 gives tensile strength 370–500 N/mm² and a 0 °C Charpy value of 27 J. Carbon is 0.17 % maximum; phosphorus and sulfur are each 0.040 % maximum. Deoxidation is killed steel. This quality is not an automatic substitute for Q235A, Q235B or Q235D. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q235B Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q235B Steel Plate

GB/T 700 Q235B is a carbon structural steel. The name marks a 235 N/mm² yield class and quality B. Table 2 gives tensile strength 370–500 N/mm² and a +20 °C Charpy value of 27 J. Carbon is 0.20 % maximum, or 0.22 % by agreement. This quality is not an automatic substitute for Q235A, Q235C or Q235D. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q235A Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q235A Steel Plate

GB/T 700 Q235A is a carbon structural steel. The name marks a 235 N/mm² yield class and quality A. Table 2 gives tensile strength 370–500 N/mm². Yield starts at 235 N/mm² at 16 mm or less and decreases in thicker bands. Quality A has no Charpy requirement and is not the same designation as Q235B, Q235C or Q235D. Carbon is 0.22 % maximum and sulfur is 0.050 % maximum. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q215B Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q215B Steel Plate

GB/T 700 Q215B is a carbon structural steel. The name marks a 215 N/mm² yield class and quality B. Table 2 gives tensile strength 335–450 N/mm² and a +20 °C Charpy value of 27 J. Quality A of the same strength class has no impact requirement. Sulfur is 0.045 % maximum. This quality is not an automatic substitute for Q215A. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q215A Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q215A Steel Plate

GB/T 700 Q215A is a carbon structural steel. The name marks a 215 N/mm² yield class and quality A. Table 2 gives tensile strength 335–450 N/mm². Quality A has no Charpy requirement; quality B of the same strength class is tested at +20 °C. Carbon is 0.15 % maximum and sulfur is 0.050 % maximum. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
GB/T 700 Q195 Steel Plate | GB/T 700 Steel - SHH STEEL

GB/T 700 Q195 Steel Plate

GB/T 700 Q195 is a carbon structural steel. The name marks a 195 N/mm² yield class, and Table 2 note a says that yield is for reference only. Tensile strength is 315–430 N/mm². Elongation is 33 % at 40 mm or less. No quality letter and no Charpy value are specified. Carbon is 0.12 % maximum. SHH STEEL produces and exports this steel plate to the ordered thickness, tests and documentation.
View More
SHH STEEL Structural Steel Plates – Carbon and Alloy Steel

Structural Steel Plates

SHH STEEL, a top Structural Steel Plates exporter, produces and exports structural steel plates for buildings, bridges, and infrastructure. Our plates, such as ASTM A36, deliver exceptional strength and weldability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Trust SHH STEEL for construction steel plates and custom solutions for large-scale structural projects.

Structural Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X