JIS G3115 SPV490 Steel Plate | SPV490 QT Vessel Plate
What is JIS G3115 SPV490 Steel ?
SPV490 is the highest common strength step in JIS G3115. Buyers search JIS G3115 SPV490, SPV490 steel plate, SPV490 QT vessel plate, SPV490 equivalent and SPV490 supplier. The number is the yield idea: 490 MPa minimum. Tensile is 610–740 MPa. Delivery for this grade is quenched and tempered. That is why the title on this page is QT vessel plate, not a normalized carbon page.
This is not SPV450. SPV450 sits one step lower. This is not SPV410. This is not Q345R steel plate. This is not SA516 Grade 70. Quenched-and-tempered vessel plate is a different production route from normalized carbon plate.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplying JIS G3115 SPV490 to the USA, Europe, Middle East, Southeast Asia, Africa and South America.
Do not ship SPV450 steel plate against an SPV490 drawing. Do not ship SA537 Class 2 and call QT close unless both books are written and met. Dual marking is possible only when chemistry, tensile, impact and heat treatment all fit.
Company scope: global exporter SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | JIS G3115 SPV490 | Confirmed |
| Product specification | JIS G3115 | Applied |
| Steel type | High-strength pressure-vessel plate | Confirmed |
| Usual delivery | Quenched and tempered (QT) | Confirmed |
| Yield | 490 MPa min | Confirmed |
| Tensile | 610–740 MPa | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | USA, Europe, Middle East, SE Asia, Africa, South America | As ordered |
| Certification | EN 10204 3.1 or 3.2 / mill MTC | As ordered |
This plate sits in pressure vessel steel plates and JIS G3115. Heat-treated vessel comparisons also belong on ASTM A537 and ASME SA537.
Chemical Composition
Cast analysis follows JIS G3115. Product analysis is reported when the order names finished-plate chemistry. Google queries such as SPV490 chemical composition and JIS G3115 SPV490 chemistry should be answered from this table, not from an SPV355 table.
Cast Analysis and Product Analysis — JIS G3115 SPV490
| Element | Cast Analysis (%) | Product Analysis, when ordered (%) |
|---|---|---|
| Carbon (C), max | 0.18 | 0.20 |
| Silicon (Si) | 0.15 – 0.75 | 0.10 – 0.80 |
| Manganese (Mn), max | 1.60 | 1.70 |
| Phosphorus (P), max | 0.030 | 0.035 |
| Sulfur (S), max | 0.030 | 0.035 |
| Nickel (Ni), max | 0.60 | 0.65 |
| Chromium (Cr), max | 0.30 | 0.35 |
| Molybdenum (Mo), max | 0.20 | 0.23 |
| Copper (Cu), max | 0.30 | 0.35 |
Carbon stays limited because the strength comes from quenching and tempering, not from a high carbon melt. Residual nickel, chromium and molybdenum are controlled. This is still a carbon-manganese vessel plate family, not 2.25Cr-1Mo and not 9Ni. SHH STEEL reports heat analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.
Mechanical Properties
Buyers search SPV490 mechanical properties, SPV490 yield strength and SPV490 tensile strength. Values below are the usual JIS G3115 idea. Thickness columns on the mill certificate govern.
Tensile and Yield — JIS G3115 SPV490
| Item | Requirement |
|---|---|
| Yield min | 490 MPa |
| Tensile | 610 – 740 MPa |
| Elongation | typically 16–19% min, thickness dependent |
| Impact | as ordered, often 0 °C |
| Delivery | Quenched and tempered |
| Density | 7.85 g/cm³ |
Do not quote 490 MPa yield on a plate that was only normalized. SPV490 on this page is a QT grade. Do not treat 610–740 MPa tensile as permission to stamp SA537 Class 2 or Q460R steel plate without checking both books.
Material Comparison
| Grade | Book | What buyers search | Swap? |
|---|---|---|---|
| SPV355 steel plate | JIS G3115 | SPV355 | No |
| SPV410 steel plate | JIS G3115 | SPV410 | No |
| SPV450 steel plate | JIS G3115 | SPV450 | No |
| JIS G3115 SPV490 | JIS G3115 | SPV490 steel plate | This page |
| SA537 Class 1 | A537 | A537CL1 | No |
| SA537 Class 2 | A537 | A537CL2 | No auto swap |
| Q460R steel plate | GB/T 713.2 | Q460R | No auto swap |
| SA516 Grade 70 | SA-516 | SA516 Gr.70 | No |
| Q345R steel plate | GB/T 713.2 | Q345R | No |
Equivalent Material Grades
Search habits mix SPV490 equivalent, JIS G3115 SPV490 equivalent and SPV490 vs A537 Class 2. Those names help a buyer find the right page. They do not authorize substitution.
| Designation | Standard / region | Notes |
|---|---|---|
| JIS G3115 SPV490 | JIS G3115 | Name on this page |
| SPV450 steel plate | JIS G3115 | Lower JIS step |
| SA537 Class 2 | A537 / SA-537 | Closest ASME QT talk grade |
| SA537 Class 3 | A537 | Higher class |
| Q460R steel plate | GB/T 713.2 | Chinese higher vessel |
| Q420R steel plate | GB/T 713.2 | Lower Chinese step |
| SA517 Grade Q | A517 | QT high-strength, different book |
| SA738 Grade B | SA-738 | Heat-treated vessel |
| SA516 Grade 70 | SA-516 | Normalized carbon |
QT Pressure-Vessel Service
Buyers pick SPV490 when a Japanese or export vessel file wants 490 MPa yield in the JIS G3115 family and the mill route is quench and temper. Search phrases such as SPV490 boiler plate, SPV490 pressure vessel plate and JIS G3115 SPV490 all point here.
It is not a substitute for 16MnDR steel plate. That grade is −40 °C low-temperature plate. It is not a substitute for 06Ni9DR steel plate. That grade is 9Ni. It is not Cr-Mo plate like 15CrMoR steel plate.
An ASME file that wants heat-treated carbon-manganese plate should name A537 / SA-537 on ASTM A537 and then write extras. Dual marking is possible only when both books are met.
SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.
Weldability
SPV490 is quenched-and-tempered vessel plate at 610–740 MPa tensile. Treat welding as production welding, and as Code welding when the equipment is a vessel.
Qualify to the applicable code. Consumables must match the SPV490 tensile band. A procedure written for SA516 Grade 70 is normalized carbon practice and is not automatically valid. A procedure written for SA537 Class 2 is a comparison only. Preheat follows thickness and hydrogen control. Heat input and interpass matter because QT plate can lose heat-affected-zone toughness if the procedure is sloppy. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL is quenched and tempered JIS G3115 SPV490. Buyers who search SPV490 QT or SPV490 heat treatment are asking for this route, not as-rolled plate and not a simple +N carbon route.
If the vessel will see PWHT, say so. Test coupons then follow a simulated cycle. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.
The certificate lists JIS G3115 SPV490; heat number; cast analysis; product analysis when ordered; tensile; QT; impact when ordered. Certificates may be mill MTC plus EN 10204 3.1 or EN 10204 3.2.
Dimensions
Usual supply range from SHH STEEL for SPV490 QT vessel plate:
- Thickness: commonly 8 mm – 100 mm, thicker by mill agreement
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
Lower JIS G3115 steps belong on SPV315 steel plate and SPV355 steel plate. Carbon vessel plate belongs on Q345R steel plate.
Tolerances
Dimensional limits follow JIS G3115 and the mill thickness table unless the order names JIS G3193 or another tolerance book. If the destination file was written to EN 10029 or SA-20, write that table on the purchase order. Do not apply ASTM A36 structural tolerances to a QT vessel plate without writing them.
Thickness minus tolerance should be named when the vessel calculation used minimum thickness after corrosion allowance. Flatness after quench and temper should be named when the plate will go to CNC cutting. QT plate can carry more residual shape than normalized carbon plate. Ask for flattening if the cutting bed needs it.
Supplementary Requirements
Charpy details. Temperature, energy, location and orientation.
Product analysis. Add this when the destination file wants finished-plate chemistry.
Simulated PWHT. When the equipment will be stress-relieved.
NDE. JIS or EN 10160 / ASTM A435 as named.
Through-thickness / Z-test. When written.
Third-party. EN 10204 3.2 when written.
Applications
| Industry | Typical components |
|---|---|
| Japanese / export pressure vessels | JIS G3115 SPV490 shells |
| High-strength QT drums | SPV490 courses |
| Dual-certified export | SPV490 / SA537 Class 2 when both books fit |
| Comparison vs carbon | SPV490 next to SA516 Grade 70 |
Supply Capability
SHH STEEL sources JIS G3115 SPV490 from first-line Chinese mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron & Steel, Baosteel, Xinyu, Xingcheng, Yongjin, Tsingshan, TISCO (Taiyuan), Jiuquan (JISCO), Lianzhong, Zhangpu and Baoxin, plus other qualified mills when the size or quench-and-temper route requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual stock and rolling thickness for this family: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 32 mm, 36 mm, 40 mm, 50 mm, 60 mm, 80 mm, 100 mm, with thicker plate by mill agreement.
Processing available with the plate: CNC or flame cutting to drawing, bevel preparation, flattening after QT, and ultrasonic testing to the named class. Extra NDE is written on the order, not assumed.
Trade terms: FOB Shanghai is the usual main term. CIF to the buyer’s destination port can be quoted. Payment is TT, LC, or TT + LC, as agreed on the contract.
Destination ports and typical ocean time from Shanghai, subject to sailing and customs:
- US West Coast (Los Angeles / Long Beach / Oakland): about 14–18 days
- US Gulf (Houston / New Orleans): about 28–35 days
- Rotterdam / Antwerp: about 28–35 days
- Jebel Ali: about 18–25 days
- Singapore: about 7–12 days
- Other major ports in Mexico, South America, the Mediterranean, India, Africa, Japan and Korea: quoted case by case
Third-party inspection can be SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector the buyer names.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin. The commercial offer is not limited to one region.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time:
- Ex-stock: about 5–7 days when SPV490 is in yard
- Mill rolling, standard QT: about 45 days
- Simulated PWHT, 3.2 or extra NDE: about 2 months
Company scope: worldwide delivery SHH STEEL.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). On JIS G3115 SPV490 that means mill pricing from Wuyang, Angang, Baosteel and other first-line mills, heat analysis reported, product analysis when ordered, recorded quench and temper, tensile to 490 / 610–740 MPa, 3.1 as standard and 3.2 when specified.
We keep the grade on the order. SPV490 is not SPV450. SPV490 is not SA516 Grade 70. SPV490 is not Q345R steel plate. If the drawing says SPV450, we will not ship SPV490 and call 490 better without the buyer writing the new name.
Company scope: global exporter SHH STEEL.
FAQ
-
What is SPV490 steel plate?
- SPV490 is a JIS G3115 high-strength pressure-vessel plate with 490 MPa minimum yield and 610–740 MPa tensile. Delivery is quenched and tempered. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
What is the equivalent of SPV490?
- Related comparisons are SA-537 Class 2 and Q460R. Dual marking is possible only when both books are fully met.
-
How is SPV490 different from SPV450?
- SPV450 is the lower JIS G3115 step. SPV490 is 490 MPa yield. Do not swap them on the same drawing.
-
Is SPV490 quenched and tempered?
- Yes. On this page SPV490 is supplied QT. Do not assume a normalized carbon route.
-
Can SPV490 be welded?
- Yes, with a qualified high-strength vessel procedure. A SA-516 Grade 70 procedure is not automatically valid.
-
Can SHH STEEL ship SPV490 to the USA, Europe or the Middle East?
- Yes. SHH STEEL quotes FOB Shanghai and CIF to US West, US Gulf, Rotterdam, Jebel Ali, Singapore and other major ports.
-
What is the delivery time for SPV490?
- Ex-stock about 5–7 days when plate is in yard. Standard QT mill rolling about 45 days. Simulated PWHT or 3.2 inspection about 2 months.
-
Can SHH STEEL issue EN 10204 3.2 for SPV490?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged with SGS, TÜV, BV, ABS, CCS, DNV, NK or the inspector named on the order.
Conclusion
JIS G3115 SPV490 Steel Plate is Japanese quenched-and-tempered pressure-vessel plate at 490 MPa yield and 610–740 MPa tensile. Whether the inquiry says JIS G3115 SPV490, SPV490 steel plate or SPV490 QT Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with SPV490 chemistry, recorded QT, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies JIS G3115 SPV490 QT Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.
Contact SHH STEEL for mill rolling, stock inquiry, cutting, bevel, 3.2 inspection or a worldwide quotation.
JIS G3115 SPV490 Steel Plate, SPV490 QT vessel plate, SPV490 supplier, global exporter SHH STEEL