Product Showcase
ASTM A533 Carbon Steel Plates
SHH STEEL offers ASTM A533-compliant Mn-Mo and Mn-Mo-Ni alloy steel plates. ASTM A533 specifies quenched and tempered plates for welded pressure vessels, ideal for nuclear reactors and high-strength needs. Reliable, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASTM A533 Type E Class 3 Steel Plate | A533 Gr.E Cl.3 Mn-Mo-Ni Vessel Plate
ASTM A533 Type E Class 3 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type E carries 0.60–1.00 % nickel. Class 3 requires 100 to 125 ksi [690 to 860 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type E Class 2 Steel Plate | A533 Gr.E Cl.2 Mn-Mo-Ni Vessel Plate
ASTM A533 Type E Class 2 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type E carries 0.60–1.00 % nickel. Class 2 requires 90 to 115 ksi [620 to 795 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type E Class 1 Steel Plate | A533 Gr.E Cl.1 Mn-Mo-Ni Vessel Plate
ASTM A533 Type E Class 1 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type E carries 0.60–1.00 % nickel. Class 1 requires 80 to 100 ksi [550 to 690 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type D Class 3 Steel Plate | A533 Gr.D Cl.3 Mn-Mo-Ni Vessel Plate
ASTM A533 Type D Class 3 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type D carries 0.20–0.40 % nickel. Class 3 requires 100 to 125 ksi [690 to 860 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type D Class 2 Steel Plate | A533 Gr.D Cl.2 Mn-Mo-Ni Vessel Plate
ASTM A533 Type D Class 2 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type D carries 0.20–0.40 % nickel. Class 2 requires 90 to 115 ksi [620 to 795 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type D Class 1 Steel Plate | A533 Gr.D Cl.1 Mn-Mo-Ni Vessel Plate
ASTM A533 Type D Class 1 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type D carries 0.20–0.40 % nickel. Class 1 requires 80 to 100 ksi [550 to 690 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type C Class 3 Steel Plate | A533 Gr.C Cl.3 Mn-Mo-Ni Vessel Plate
ASTM A533 Type C Class 3 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type C carries 0.70–1.00 % nickel. Class 3 requires 100 to 125 ksi [690 to 860 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type C Class 2 Steel Plate | A533 Gr.C Cl.2 Mn-Mo-Ni Vessel Plate
ASTM A533 Type C Class 2 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type C carries 0.70–1.00 % nickel. Class 2 requires 90 to 115 ksi [620 to 795 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type C Class 1 Steel Plate | A533 Gr.C Cl.1 Mn-Mo-Ni Vessel Plate
ASTM A533 Type C Class 1 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type C carries 0.70–1.00 % nickel. Class 1 requires 80 to 100 ksi [550 to 690 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type B Class 3 Steel Plate | A533 Gr.B Cl.3 Mn-Mo-Ni Vessel Plate
ASTM A533 Type B Class 3 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type B carries 0.40–0.70 % nickel. Class 3 requires 100 to 125 ksi [690 to 860 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type B Class 2 Steel Plate | A533 Gr.B Cl.2 Mn-Mo-Ni Vessel Plate
ASTM A533 Type B Class 2 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type B carries 0.40–0.70 % nickel. Class 2 requires 90 to 115 ksi [620 to 795 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More -
ASTM A533 Type B Class 1 Steel Plate | A533 Gr.B Cl.1 Mn-Mo-Ni Vessel Plate
ASTM A533 Type B Class 1 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type B carries 0.40–0.70 % nickel. Class 1 requires 80 to 100 ksi [550 to 690 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.View More
ASTM A533 Carbon Steel Plates
Nuclear-Grade Steel Plates
SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.
Nuclear-Grade Steel Plates
ASME SA542/SA542M
ASME SA543/SA543M
ASME SA612/SA612M
ASME SA662/SA662M
ASME SA737/SA737M
ASME SA202/SA202M
ASTM A202/A202M
ASTM A1017/A1017M
SA-1017/SA-1017M
ASTM A662/A662M
ASME SA724/SA724M
ASME SA736/SA736M
ASME SA832/SA832M
ASME SA533/SA533M
ASTM A533
ASME SA508/SA508M
ASTM A508
ASME SA387/SA387M
ASTM A387/A387M
ASME SA-738/SA-738M
ASTM A738
ASME SA-203/SA-203M
ASTM A203
EN 10028-7
RCC-M M3307
JIS G3118
GB/T 3531
GOST 10859
X