ASME SA302 Grade D Steel Plate | SA302 Gr.D Mn-Mo-Ni Vessel Plate - SHH STEEL

ASME SA302 Grade D Steel Plate | SA302 Gr.D Mn-Mo-Ni Vessel Plate

ASME SA302 Grade D is a manganese-molybdenum-nickel pressure-vessel plate under ASME SA-302/SA-302M. Yield 345 MPa, tensile 550–690 MPa, Ni 0.70–1.00%. SHH STEEL supplies SA302 Gr.D / A302 Gr.D as China mill-Direct Supply with 3.1 or 3.2 certificates.
Keywords
ASME SA302 Grade D, SA302 Gr.D, SA302 Gr D, SA302GRD, SA302 GR D, SA-302 Grade D, ASTM A302 Grade D, A302GRD, Mn-Mo-Ni vessel plate, ASME SA-302, SA302 Grade D supplier
Equivalent Grades
ASTM A302 Gr D / ASME SA302 Gr D / JIS G3119 SBV2 (near) / GB 15MnNiDR (near) / EN 10028-3 P355N (near) — Material Specification: ASME SA-302 / ASTM A302 — Delivery: Normalized (N) or Normalized + Tempered (N+T)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Elevated-Temperature and Vessel Service
Weldability
Heat Treatment
Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is ASME SA302 Grade D Steel?

As a professional China mill-Direct Supply and ASME pressure-vessel plate exporter, SHH STEEL supplies ASME SA302 Grade D Steel Plate produced to ASME SA-302/SA-302M.

On drawings, MTCs and RFQs this grade is written many ways: ASME SA302 Grade D, SA302 Gr.D, SA302 Gr D, SA302GRD, SA302 GR D, SA-302 Grade D, SA-302 Gr.D, ASTM A302 Grade D, A302 Gr.D, A302GRD, Mn-Mo-Ni vessel plate, manganese molybdenum nickel boiler plate and A/SA302 Grade D. All of these names refer to the same manganese-molybdenum-nickel alloy plate at the higher nickel band. ASME SA-302/SA-302M is the Boiler and Pressure Vessel Code companion to ASTM A302/A302M.

SA302 Gr.D is the highest-nickel grade in ASME SA-302. Grades A and B are Mn-Mo with no specified nickel. Grade C adds 0.40–0.70% Ni. Grade D raises nickel to 0.70–1.00% on heat analysis. Strength of Grade D matches Grade B and Grade C: minimum yield 345 MPa (50 ksi) and tensile 550–690 MPa (80–100 ksi). Molybdenum heat analysis is 0.45–0.60%.

The plate is intended for welded boilers and other pressure vessels under ASME Section VIII when the drawing names Grade D or requires the higher nickel band at Grade B strength. It is not a 3.5Ni low-temperature grade such as SA203 Gr.D/E, and it is not a Cr-Mo elevated-temperature grade such as ASME SA387 (SA-387). Compared with carbon vessel steels such as ASME SA516 (SA-516) and ASTM A516, Grade D adds both molybdenum and a higher nickel addition.

General requirements follow ASME SA-20. Steel is killed and produced to fine-grain practice. Plates 50 mm and under are normally supplied as-rolled unless normalizing or stress relieving is ordered. Plates over 50 mm shall be normalized.

SHH STEEL supplies SA302 Gr.D as true China mill-Direct Supply. Dual marking ASME SA302 Grade D / ASTM A302 Grade D is available for equipment built to ASME Section VIII. Certificates can be EN 10204 3.1 or EN 10204 3.2.

If the project compares other coded vessel plates, SHH STEEL places SA302 Gr.D next to ASME SA537 (SA-537), ASTM A537, ASME SA515 (SA-515) and ASTM A285.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade ASME SA302 Grade D / SA302 Gr.D / SA302GRD Confirmed
Product Specification ASME SA-302/SA-302M Applied
Companion Spec ASTM A302 Grade D / A302 Gr.D Dual cert available
General Requirements ASME SA-20 / ASTM A20 Applied
Code Context ASME Section VIII As specified
Product Form Pressure vessel / boiler plate Available
Alloy Type Manganese-molybdenum-nickel Confirmed
Delivery Condition As-rolled ≤50 mm; normalized >50 mm As specified
Typical Thickness 6 mm – 150 mm Heavier by enquiry
Width / Length Up to about 4600 mm wide / 12000 mm long Mill capability
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This product belongs to the Pressure Vessel Steel Plates family. It is a Mn-Mo-Ni coded vessel plate under ASME SA-302, not a structural Carbon Steel Plates grade.

Chemical Composition

SA302 Grade D chemistry under ASME SA-302/SA-302M is reported as heat analysis (ladle analysis) and, when specified, product analysis.

Heat Analysis (Ladle Analysis) — Grade D

Element Thickness / Basis Heat Analysis (%)
Carbon (C), max ≤ 25 mm (1 in.) 0.20
Carbon (C), max > 25 mm to 50 mm (1–2 in.) 0.23
Carbon (C), max > 50 mm (2 in.) 0.25
Manganese (Mn) All 1.15 – 1.50
Phosphorus (P), max All 0.025
Sulfur (S), max All 0.025
Silicon (Si) All 0.15 – 0.40
Molybdenum (Mo) All 0.45 – 0.60
Nickel (Ni) All 0.70 – 1.00

Product Analysis — Grade D

Element Thickness / Basis Product Analysis (%)
Manganese (Mn) All 1.07 – 1.62
Silicon (Si) All 0.13 – 0.45
Molybdenum (Mo) All 0.41 – 0.64
Nickel (Ni) All 0.67 – 1.03
C, P, S Product check per SA-20/SA-302 Per order

Grade D uses the same manganese and molybdenum bands as Grade B and Grade C. The difference is nickel: heat 0.70–1.00%, product 0.67–1.03%. Grade C stays at 0.40–0.70% Ni on heat analysis. Tighter residuals or carbon equivalent limits are supplementary requirements.

SHH STEEL reports ladle analysis on every certificate. Product analysis is added when ASME SA-20 product analysis or the vessel specification requires it. Nickel must fall in the Grade D band; a Grade C heat cannot be recertified as Grade D.

Mechanical Properties

Tensile Requirements — ASME SA302 Grade D per ASME SA-302/SA-302M

Property Requirement
Tensile strength 550 – 690 MPa (80 – 100 ksi)
Yield strength, min (0.2%) 345 MPa (50 ksi)
Elongation in 200 mm (8 in.), min 17%
Elongation in 50 mm (2 in.), min 20%

Strength and elongation of Grade D match Grade C. The extra nickel does not raise room-temperature strength above Grade B; it is specified for toughness and drawing compliance. Density is 7.85 g/cm³. Hardness after the agreed heat treatment is typically in the 160–200 HB range unless a special window is ordered.

Specimens are prepared under ASME SA-20. If simulated PWHT is specified, coupons are heat-treated to the vessel cycle before testing.

Material Comparison

Grade Alloy type Ni (heat) Yield min Tensile Typical use
SA302 Gr.A Mn-Mo Not specified 310 MPa 515–655 MPa Lower-strength Mn-Mo
SA302 Gr.B Mn-Mo Not specified 345 MPa 550–690 MPa Same strength, no Ni
SA302 Gr.C Mn-Mo-Ni 0.40–0.70% 345 MPa 550–690 MPa Same strength, lower Ni
SA302 Gr.D Mn-Mo-Ni 0.70–1.00% 345 MPa 550–690 MPa Highest-Ni SA-302 grade

Order SA302 Gr.D / SA302GRD when the ASME SA-302 drawing names Grade D or requires 0.70–1.00% nickel. If 0.40–0.70% Ni is enough, Grade C is the correct band. If nickel is not required, Grade B is the lower-alloy option at the same strength. Carbon QT options include ASME SA537 and ASTM A537. HSLA Steel Plates are not a coded substitute for ASME SA-302.

Elevated-Temperature and Vessel Service

SA302 Grade D is specified for welded boilers and pressure vessels under ASME Section VIII when the higher nickel band is required at Grade B strength. Molybdenum and nickel in ASME SA-302/SA-302M support alloy vessel and boiler service. Allowable stress at temperature is taken from the applicable ASME Section II Part D table for SA-302 Grade D, not from a commercial datasheet.

Impact temperature, orientation and energy minimums are agreed on the order. They are not automatic on Grade D, but the higher nickel is often the reason Charpy testing is added. When the vessel specification sets Charpy values, SHH STEEL produces SA302 Gr.D Mn-Mo-Ni vessel plate with those sets and lists the results on the 3.1 or 3.2 certificate. Grade D is not a 3.5Ni cryogenic plate.

Weldability

SA302 Grade D under ASME SA-302 is a welded boiler and pressure-vessel plate. Mn-Mo-Ni steel is welded with low-hydrogen procedures qualified to ASME Section IX.

Consumables are selected to match molybdenum, the higher nickel band and the required joint toughness. Preheat depends on thickness, hydrogen control and restraint. When ASME Section VIII requires PWHT, the shop cycle is commonly in the 595–650°C range for this alloy family. If properties after that cycle are needed, simulated PWHT of mill coupons should be ordered before shipment.

SHH STEEL recommends a qualified WPS/PQR for each thickness break and can support procedure review through steel welding services. Do not assume an SA302 Grade C procedure is automatically valid for Grade D if nickel matching or impact requirements change.

Heat Treatment

Heat treatment of SA302 Grade D follows ASME SA-302/SA-302M:

  • Plates 50 mm (2 in.) and under are normally supplied in the as-rolled condition. They may be ordered normalized, stress relieved, or both.
  • Plates over 50 mm (2 in.) shall be normalized.

Normalizing is heating into the austenite range followed by air cooling. Stress relieving, when ordered, is a separate lower-temperature hold to reduce residual stress. Quench-and-temper practice used for SA533 / SA537 Class 2 must not be applied to Grade D unless the order is changed to a QT specification.

If the specification fixes a normalizing temperature band or holding time per thickness under ASME SA-20, SHH STEEL writes those parameters into the mill instruction and reports them on the certificate.

Delivery Condition

SHH STEEL delivers ASME SA302 Grade D / SA302 Gr.D as follows:

  • ≤ 50 mm: as-rolled as standard, or normalized / stress relieved when ordered
  • 50 mm: normalized as required by ASME SA-302

The certificate lists SA302 Gr.D and, when dual certified, A302 Gr.D; heat number; heat analysis; product analysis when ordered; tensile results; heat-treatment condition; agreed Charpy values; and supplementary tests. Plates are industrial vessel plate: heat-treated as required, then pickled or shot-blasted as agreed.

Decorative finishes such as 2B, BA or No.4 are not used. Surface condition is vessel-plate quality for welding, NDE and coating. Heat number and grade marking support ASME Section VIII traceability.

Certificates may be EN 10204 3.1 or EN 10204 3.2. Third-party stamps (BV, LR, DNV, TUV, SGS or the purchaser’s agency) are arranged when written on the order.

Dimensions

Typical supply range from SHH STEEL for SA302 Gr.D Mn-Mo-Ni vessel plate:

  • Thickness: 6 mm – 150 mm (heavier by mill enquiry)
  • Width: up to about 4600 mm
  • Length: up to about 12000 mm

Because heat treatment changes at 50 mm in ASME SA-302, the purchase order should state the ordered thickness and the required condition. Cut-to-length shells, heads and nest sizes are available.

Tolerances

Dimensional tolerances follow ASME SA-20 / ASTM A20 for pressure-vessel plates.

Thickness, width, length, flatness and camber are vessel-plate tolerances, not strip tolerances. Restricted thickness or extra-flatness can be accepted when the vessel drawing requires it. Ultrasonic testing to A435 or A578 is added when specified. Cutting to finished sizes is available through steel cutting services.

Supplementary Requirements

ASME Section VIII specifications for higher-nickel vessel plate often add tests beyond the base SA-302 Grade D table. SHH STEEL treats the following as supplementary requirements.

Simulated PWHT. Coupons from the same heat and thickness receive the vessel PWHT cycle. Tensile and Charpy tests are run on those coupons.

Nondestructive examination. UT to A435, A577 or A578 with purchaser acceptance levels. Edge MT/PT after cutting if required.

Impact testing. Test temperature, specimen size, orientation and minimum average/single values as written on the RFQ.

Special hardness. HBW or HV window after the agreed heat treatment or after simulated PWHT.

Restricted chemistry. Tighter C, P, S, residuals or carbon equivalent on heat and product analysis per ASME SA-302 / SA-20. Nickel must remain inside the Grade D band.

HIC testing. NACE TM0284 with purchaser solution and CLR/CTR/CSR limits. Not automatic on SA302 Gr.D.

NACE / sour-service notes. Review against NACE MR0175 / ISO 15156 or MR0103 only when the datasheet cites the clause.

Z-direction testing. ASTM A770 or purchaser Z15/Z25/Z35 for thick nozzles and restrained joints.

Third-party witnessing. Witness of heat treatment, mechanical tests, UT and documents. Output can be EN 10204 3.2.

Supplementary tests go through steel testing service and appear line by line on the certificate. Items not on the purchase order are not assumed.

Equivalent Material Grades

Designation Standard / Region Notes
ASME SA302 Grade D / SA302 Gr.D / SA302GRD ASME SA-302/SA-302M Code name on this page
ASTM A302 Grade D / A302 Gr.D / A302GRD ASTM A302/A302M Companion material spec
Mn-Mo-Ni vessel plate Commercial Alloy-content search name
GB/T 713 related Ni-Mo vessel GB Project-specific comparison
EN 10028 related Mn-Mo-Ni vessel EN Project-specific comparison
JIS related Mo-Ni boiler plate JIS Project-specific dual cert

For ASME stamping, the purchase order should say ASME SA302 Grade D to ASME SA-302/SA-302M, or dual SA302 / A302 Grade D. Nearby carbon vessel grades include ASME SA516, ASTM A516, ASME SA515 and ASTM A285.

Applications

ASME SA302 Grade D / SA302 Gr.D is selected for ASME Section VIII boilers and vessels that need the higher nickel band at 345 MPa yield. Typical applications of ASME SA302 Grade D Steel Plate include:

Industry / Sector Typical Components (with keywords)
Boilers & Steam Drums SA302 Gr.D boiler plate and SA302GRD Mn-Mo-Ni vessel plate
ASME Section VIII Vessels ASME SA302 Grade D shells, heads and welded pressure parts
Oil, Gas & Petrochemical SA-302 Grade D reactors, separators and process vessels
Energy & Power SA302 Grade D heat-exchange shells and power-plant vessels
Dual-Certified Export Jobs SA302 / A302 Gr.D plate to ASME SA-302 and ASTM A302
Heavy Vessel Fabrication SA302 Gr D plate cut to nest sizes

SHH STEEL supplies SA302 Gr.D with full heat traceability. Related industry pages include petrochemical industry and energy industry. Supporting services include steel cutting services, steel welding services, steel testing service and worldwide shipping service.

Why Choose SHH STEEL

SHH STEEL is a China mill-Direct Supply for plates to ASME SA-302/SA-302M. For SA302 Grade D we offer:

  • China mill-Direct Supply pricing on SA302 Gr.D / A302 Gr.D
  • Dual ASME SA302 / ASTM A302 marking
  • Heat analysis and product analysis per ASME SA-20 / SA-302, including the 0.70–1.00% Ni band
  • EN 10204 3.1 standard; EN 10204 3.2 or nominated third-party inspection on request
  • As-rolled or normalized delivery per thickness rule
  • Supplementary PWHT simulation, UT, HIC, NACE review and Z-direction testing
  • Cutting to shell and head nest sizes
  • Technical support to separate Grade D from A/B/C and from SA516 / SA387 / SA537
  • Export packing through worldwide shipping service

For company scope and other vessel grades, visit China steel Mill Agent-SHH STEEL.

FAQ

What other names are used for ASME SA302 Grade D?
Buyers also write SA302 Gr.D, SA302GRD, SA-302 Grade D, ASTM A302 Grade D, A302GRD and Mn-Mo-Ni vessel plate. They all mean the higher-nickel Grade D plate in ASME SA-302/SA-302M. SHH STEEL prints the exact name required on the purchase order.
Is SA302 Grade D the same as A302 Grade D?
They are companion specifications. ASME SA-302 is the Code version used with ASME Section VIII; ASTM A302 is the ASTM product spec. Chemistry and tensile limits match. SHH STEEL dual-certifies when the vessel must be Code-stamped.
What is the nickel content of SA302 Gr.D?
Heat analysis is 0.70–1.00% Ni and product analysis is 0.67–1.03% Ni under ASME SA-302. That is the higher nickel band. Grade C uses 0.40–0.70% Ni on heat analysis.
What is the difference between SA302 Grade C and Grade D?
Strength is the same (345 MPa yield, 550–690 MPa tensile, 17%/20% elongation). Grade C nickel is 0.40–0.70%; Grade D nickel is 0.70–1.00%. Order the nickel band written on the ASME drawing. SHH STEEL does not recertify a Grade C heat as Grade D.
What is the difference between SA302 Grade B and Grade D?
Strength is the same. Grade B has no specified nickel. Grade D adds 0.70–1.00% Ni and has higher elongation minima (17%/20% versus 15%/18%).
Must SA302 Grade D be normalized?
Plates over 50 mm shall be normalized per ASME SA-302. Plates 50 mm and under are normally as-rolled unless the purchaser orders normalizing or stress relieving.
Can welding be qualified to ASME Section IX?
Yes. SA302 Gr.D is a welded boiler and vessel plate. Procedures should be qualified to ASME Section IX with low-hydrogen consumables matched to the higher-nickel Mn-Mo-Ni chemistry. The fabricator owns the qualified WPS.
Can SHH STEEL issue EN 10204 3.2?
Yes. EN 10204 3.1 is standard. EN 10204 3.2 or another third-party witness is arranged when it is written on the order.
What is the density of SA302 Gr.D?
7.85 g/cm³. SHH STEEL uses this value for shipping-weight estimates on ASME SA-302 plate.

Conclusion

ASME SA302 Grade D Steel Plate is the higher-nickel manganese-molybdenum-nickel, 345 MPa yield vessel grade in ASME SA-302/SA-302M. Whether the inquiry says SA302 Gr.D, SA302GRD, SA-302 Grade D or Mn-Mo-Ni vessel plate, SHH STEEL supplies plate with heat and product analysis in the 0.70–1.00% Ni band, thickness-correct heat treatment, optional supplementary tests, and EN 10204 3.1 or 3.2 certification.

As a professional China mill-Direct Supply, SHH STEEL provides ASME SA302 Grade D / SA302 Gr.D Mn-Mo-Ni Vessel Plate with full traceability for ASME Section VIII fabrication.

Contact SHH STEEL today for stock, nickel analysis, dual SA302/A302 marking to ASME SA-302, 3.2 inspection or a quotation.

ASME SA302 Grade D Steel Plate, SA302 Gr.D, SA302GRD, SA-302 Grade D, ASME SA-302, ASTM A302 Grade D, Mn-Mo-Ni vessel plate, SA302 Grade D supplier, China mill-Direct Supply

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X