ASME SA662 Grade C Steel Plate | SA662 Gr.C Low Temp Vessel Plate
What is ASME SA662 Grade C Steel ?
ASME SA662 Grade C, also written ASME SA662 GR.C, is killed carbon-manganese-silicon steel plate under ASME SA-662/SA-662M. The specification is identical with ASTM A662/A662M. It covers three grades — Grade A, Grade B and Grade C — intended primarily for welded pressure vessels where improved low-temperature notch toughness is important. Grade C is the highest line in this book: 295 MPa yield and 485–620 MPa tensile. Plates of Grade C over 40 mm shall be normalized. Plates of Grade C 40 mm and under are normally supplied as-rolled unless the order names normalize or stress relief. SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this Grade. Plate is produced to ASME SA-662/SA-662M and shipped to buyers in the USA, Europe, Middle East and Southeast Asia.
Buyers write ASME SA662 Grade C, ASME SA662 GR.C, SA662 Gr.C, SA662GRC, SA-662 Grade C, SA 662 Gr C, A662 Grade C and ASTM A662 Gr.C. A purchase order that only says “SA662” is incomplete. A purchase order that writes “SA612 Grade C” is mixing this book with SA612, which has no Grade split. This page is not SA516 Gr.70. The tensile band looks close to Grade 70, but yield, carbon-manganese balance, toughness intent and the 40 mm normalize rule are not the same. It is not QT Ni-Cr-Mo like SA543. It is not HSLA like SA737. It is not heat-treated C-Mn-Si like SA738.
The steel shall be killed and shall conform to the fine austenitic grain size requirement of ASME SA-20 / ASTM A20. Current practice normally limits thickness to about 50 mm. Dual marking SA662 / A662 Grade C is available. Certificates can be EN 10204 3.1 or 3.2. Company scope: global steel mill sourcing partner – SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade | ASME SA662 Grade C | Confirmed |
| Product Specification | ASME SA-662/SA-662M | Applied |
| Companion Spec | ASTM A662 Grade C | Dual cert available |
| General Requirements | ASME SA-20 / ASTM A20 | Applied |
| Steel type | Killed C-Mn-Si, fine grain | Confirmed |
| Heat treatment | Normalize over 40 mm; as-rolled ≤40 mm unless ordered otherwise | Confirmed |
| Service idea | Moderate and lower temperature, improved toughness | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Markets | USA, Europe, Middle East, Southeast Asia | FOB / CIF as ordered |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in pressure vessel steel plates and carbon steel plates. It does not sit with ASME SA387 Cr-Mo alloy plate or ASTM A36 steel plate structural plate.
SA-20 still governs marking, testing location, retests, repair rules and supplementary requirements unless the product specification overrides them.
Chemical Composition
ASME SA662 Grade C / ASME SA662 GR.C uses the Grade C column. Manganese and silicon are the widest of the three grades.
Heat Analysis and Product Analysis — ASME SA662 Grade C (typical Table 1 limits)
| Element | Heat Analysis (%) | Product Analysis (%) |
|---|---|---|
| Carbon (C), max | 0.20 | 0.24 |
| Manganese (Mn) | 1.00 – 1.60 | 0.92 – 1.72 |
| Phosphorus (P), max | 0.025 | 0.025 |
| Sulfur (S), max | 0.025 | 0.025 |
| Silicon (Si) | 0.15 – 0.50 | 0.13 – 0.55 |
Grade A carbon heat is 0.14% max. Grade B carbon heat is 0.19% max and silicon heat is 0.15–0.40%. Do not ship Grade A or Grade B as Grade C because all three are C-Mn-Si. Vacuum carbon-deoxidized steel under S17 may replace part of the table when specified.
SHH STEEL reports heat analysis on every certificate and product analysis when SA-20 requires it. If a Houston, Rotterdam or Jebel Ali specification tightens phosphorus or sulfur, write that on the order.
Mechanical Properties
Grade C is the highest line in this book.
Tensile Requirements — ASME SA662 Grade C
| Property | Requirement |
|---|---|
| Yield strength, min | 295 MPa (43 ksi) |
| Tensile strength | 485 – 620 MPa (70 – 90 ksi) |
| Elongation in 200 mm, min | 18% |
| Elongation in 50 mm, min | 22% |
| Density | 7.85 g/cm³ |
| Hardness | Not a default substitute for tensile |
Grade A is 275 MPa yield and 400–540 MPa tensile. Grade B is 275 MPa yield and 450–585 MPa tensile. Do not stamp Grade B as Grade C because a coupon came in high. Do not treat Grade C as a free substitute for SA516 Gr.70 just because tensile overlaps. Yield is higher on Grade C (295 vs 260 MPa), carbon-manganese limits differ, and Grade C over 40 mm must be normalized.
Density is 7.85 g/cm³. Notch toughness is the reason buyers pick this book. Write the temperature, energy, location and orientation. For plates over 40 mm, normalize is a specification requirement.
Material Comparison
| Grade | Route | Strength idea | Swap? |
|---|---|---|---|
| SA662 Grade A | Normalized C-Mn-Si | 275 / 400–540 | No |
| SA662 Grade B | C-Mn-Si low-temp | 275 / 450–585 | No |
| SA662 Gr.C | C-Mn-Si low-temp | 295 / 485–620 | This page |
| SA516 Gr.70 | C-Mn-Si vessel | 260 / 485–620 | No |
| ASME SA612 | High-strength C-Mn-Si | 345 yield | No |
| SA738 Grade A | Heat-treated C-Mn-Si | Different book | No |
| SA285 Gr.C | Low/intermediate carbon | Different table | No |
| SA299 Gr.A | C-Mn-Si vessel | Different table | No |
SA203 Gr.A, SA225 Gr.C and SA455 steel plate are also vessel plates. None of them is ASME SA662 GR.C.
Low-Temperature C-Mn-Si Vessel Service
ASME SA662 Grade C / ASME SA662 GR.C is selected when the vessel wants killed fine-grain C-Mn-Si with improved low-temperature notch toughness and the Grade C tensile band. Typical equipment is welded storage and process vessels written to SA-662 Grade C. Grades A, B and C comply substantially with ISO pressure vessel steels P9, P15 and P18 respectively. Allowable stress comes from ASME Section II Part D after the Code lists this Grade.
SHH STEEL supplies this plate to fabricators in the United States, Europe, the Middle East and Southeast Asia. It is not nickel low-temp plate like SA203 Gr.D or SA203 Gr.E. Those grades use nickel for toughness. SA662 Grade C uses carbon control, manganese, fine grain and, above 40 mm, normalize. It is not QT alloy like SA543. It is not SA302 Gr.B. Stainless inquiries belong on ASME SA240 or ASTM A240.
Do not assume every Grade C plate is as-rolled. Over 40 mm, normalize is mandatory. Under 40 mm, as-rolled is normal unless the drawing names normalize for toughness. Do not treat Grade C as SA516 Grade 70 stock with a different stamp.
Weldability
SA662 Gr.C is killed fine-grain C-Mn-Si at the Grade C tensile band. Welding is Code welding.
Qualify procedures to ASME Section IX. Use consumables written for 485–620 MPa tensile. A SA516 Gr.70 procedure may look close on paper. Review chemistry, normalize condition and impact temperature before copying it. Do not use a QT alloy procedure from SA543. Hydrogen control, preheat and PWHT follow the qualified procedure and the vessel specification.
Do not copy a SA387 Gr.12 Cl.2 procedure onto SA662 Grade C. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review, including packages prepared for US, EU or Middle East inspectors.
Heat Treatment
Plates of Grade C over 40 mm shall be normalized. Plates of Grade C 40 mm and under are normally supplied as-rolled. The purchaser may order normalize or stress relief, or both, on the thinner band. Grade A is different: every Grade A plate is normalized, including thin plate.
If the vessel will see PWHT, test coupons shall follow a simulated cycle when the order names it. This is not the SA543 QT route and not the SA537 Cl.1 heat-treated carbon route. Special heat treatment, extra simulation or third-party hold points add time. Plan about two months when those extras are on the order.
Delivery Condition
Usual delivery from SHH STEEL is ASME SA662 Grade C / ASME SA662 GR.C plate normalized above 40 mm, and as-rolled at 40 mm and under unless the order names normalize or stress relief.
The certificate lists ASME SA662 Grade C and, when dual certified, ASTM A662 Grade C; heat number; heat analysis; product analysis when ordered; tensile results to the Grade C table; heat-treatment statement; impact when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.
Surface is mill scale unless the order names shot blast, paint or machine allowance. Cutting, beveling and nest sizes belong on the purchase order.
Dimensions
Usual supply range from SHH STEEL for SA662 Gr.C low temp vessel plate:
- Thickness: commonly 6 mm – 50 mm. Current practice normally limits this specification to about 50 mm. The 40 mm mark is the normalize trigger
- Width: 1500 mm – 4000 mm
- Length: 3000 mm – 12000 mm
- Cut-to-length shells, heads and nest sizes inside those limits
Structural sizes belong on EN 10025-2 or JIS G3106. Weathering plate belongs on EN 10025-5 or Corten A/B. Fine-grain structural belongs on EN 10025-3 or EN 10025-4. QT structural belongs on EN 10025-6.
Tolerances
Dimensional limits follow ASME SA-20. Thickness, width, length, flatness and camber are vessel-plate tolerances, not structural-plate tolerances from ASTM A36/A36M. UT to A435 / A577 / A578 is added when the order names it.
Repair welding of surface defects follows SA-20 rules unless the order forbids repair.
Supplementary Requirements
Most export ASME SA662 Grade C / ASME SA662 GR.C orders add extras. SHH STEEL does not assume them.
Charpy details. Temperature, energy, location and orientation. Improved low-temperature toughness is the reason this specification exists.
Simulated PWHT. Same-heat coupons follow the vessel cycle when named.
NDE. UT to A435 / A577 / A578.
Vacuum carbon deoxidation (S17). When specified.
Normalize on ≤40 mm plate. Optional unless written.
Third-party. EN 10204 3.2, with inspectors arranged for US, European or Middle East
Equivalent Material Grades
These names are project-comparison grades. They are not automatic substitutes.
| Designation | Standard / region | Notes |
|---|---|---|
| ASME SA662 Grade C / ASME SA662 GR.C | ASME SA-662/SA-662M | Code name on this page |
| ASTM A662 Grade C | ASTM A662/A662M | Companion US product spec |
| ISO P18 related | ISO vessel steels | Spec note vs Grade C |
| P355NH / P355NL / P460 related | EN 10028 | European comparison only |
| SPV355 / SPV410 related | JIS G3115 | Japanese vessel comparison |
| Q345R / Q370R related | GB/T 713 | Chinese vessel comparison |
| SA516 Gr.70 | SA-516 | Related carbon vessel, different yield and rules |
| ASME SA515 | SA-515 | Intermediate/higher temperature carbon |
| ASTM A516 | A516 family | Related carbon vessel family |
Applications
| Industry | Typical components |
|---|---|
| Low-temperature welded vessels | ASME SA662 Grade C shells and ASME SA662 GR.C heads |
| C-Mn-Si toughness equipment | SA662 Gr.C courses |
| Dual-certified export | SA662 / A662 Grade C plate from SHH STEEL |
| Fabrication | SA662 Gr.C cut to nest sizes |
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering inquiries belong on weathering steel plates. Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless.
Other vessel comparisons: SA203 Gr.B, SA302 Gr.C, A516 Grade 70, SA533 Type C Cl.2, SA517 Gr.P.
Global Delivery & Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN and JIS steel to the USA, Europe, Middle East and Southeast Asia. Origin is mill-direct, China origin. We do not treat SA662 Grade C as an Asia-only stock item. Inquiry packages are written for fabricators and EPC buyers in Houston, Rotterdam, Antwerp, Jebel Ali, Dammam, Singapore and surrounding ports.
Typical trade terms:
- FOB Shanghai
- CIF Houston
- CIF Rotterdam
- CIF Jebel Ali
- Other CIF / CFR ports on request (Los Angeles, New York, Hamburg, Genoa, Jeddah, Mundra, Ho Chi Minh)
Typical lead time for ASME SA662 Grade C / ASME SA662 GR.C:
- Ex-stock / ready plate: about 5–7 days after order confirmation, subject to actual warehouse size and cutting
- Mill rolling, standard delivery: about 45 days
- Special heat treatment, simulated PWHT, 3.2 hold or extra NDE: about 2 months
Documents travel with the cargo: mill certificate, packing list, commercial invoice, bill of lading, and EN 10204 3.1 or 3.2 as ordered. Third-party inspection can be arranged before loading for US, European or Middle East projects. Packing is seaworthy, with edge protection and marking in English as specified on the order.
If the buyer needs a dual ASTM A662 / ASME SA662 stamp for a Section VIII vessel in the United States, say so on the inquiry. If the buyer needs a PED / 3.2 file for Europe, say so on the inquiry. Do not assume a domestic Chinese certificate format will pass at destination.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). We supply ASTM / EN / JIS steel to the USA, Europe, the Middle East and Southeast Asia. On ASME SA662 Grade C / ASME SA662 GR.C that means mill pricing, dual SA662/A662 marking, Grade C chemistry reported, normalize when thickness requires it, tensile results at 295 MPa yield and 485–620 MPa tensile, 3.1 as standard and 3.2 when specified. Trade terms include FOB Shanghai and CIF Houston / Rotterdam / Jebel Ali.
We keep the Grade on the order. Grade C is not Grade A and is not Grade B. SA662 is not SA612. SA662 Grade C is not SA516 Grade 70. SA662 is not SA387 Gr.22 Cl.2. If the drawing is over 40 mm, we will not ship as-rolled Grade C and call it close.
Company scope: global steel mill sourcing partner – SHH STEEL.
FAQ
-
What names are used for ASME SA662 Grade C / ASME SA662 GR.C?
- Buyers write ASME SA662 Grade C, ASME SA662 GR.C, SA662 Gr.C, SA662GRC, SA-662 Grade C, A662 Grade C and ASTM A662 Gr.C. SHH STEEL prints the wording on the purchase order.
-
Is ASME SA662 Grade C the same as ASTM A662 Grade C?
- Chemistry and tensile limits match. ASME SA-662 is the Code version. ASTM A662 is the product spec. SHH STEEL dual-certifies both names when the vessel must be stamped in the United States or elsewhere.
-
What is the yield strength of SA662 Gr.C?
- 295 MPa minimum. Tensile is 485–620 MPa. Elongation is 18% in 200 mm and 22% in 50 mm.
-
Must ASME SA662 GR.C be normalized?
- Over 40 mm, yes. At 40 mm and under, as-rolled is normal unless the order names normalize or stress relief. Grade A is always normalized.
-
How is ASME SA662 Grade C different from Grade A and Grade B?
- Grade C carbon heat is 0.20% max, manganese heat is 1.00–1.60%, yield is 295 MPa and tensile is 485–620 MPa. Grade A and Grade B stay at 275 MPa yield with lower tensile bands.
-
How is SA662 Grade C different from SA516 Grade 70?
- Tensile bands look close. Grade C yield is 295 MPa versus 260 MPa on Grade 70. Chemistry, toughness intent and the 40 mm normalize rule also differ.
-
Can SHH STEEL ship ASME SA662 Grade C outside Asia?
- Yes. SHH STEEL is a global steel mill sourcing partner. We supply this plate to the USA, Europe, the Middle East and Southeast Asia on FOB Shanghai or CIF Houston / Rotterdam / Jebel Ali.
-
What is the delivery time for SA662 Gr.C?
- Ex-stock about 5–7 days. Standard mill rolling about 45 days. Special heat treatment, simulated PWHT or 3.2 inspection about 2 months.
-
Can welding of SA662 Grade C be qualified to ASME Section IX?
- Yes. Use a WPS written for this C-Mn-Si tensile band. The fabricator owns the procedure.
-
Can SHH STEEL issue EN 10204 3.2 for ASME SA662 Grade C?
- Yes. EN 10204 3.1 is standard. EN 10204 3.2 is arranged when written on the order.
Conclusion
ASME SA662 Grade C Steel Plate, also searched as ASME SA662 GR.C, is killed C-Mn-Si plate under ASME SA-662/SA-662M for moderate and lower temperature welded vessels, at 295 MPa yield and 485–620 MPa tensile. Whether the inquiry says ASME SA662 Grade C, ASME SA662 GR.C, SA662 Gr.C or A662 Grade C, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with Grade C chemistry, the correct heat-treatment route, and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies ASME SA662 Grade C / SA662 Gr.C Low Temp Vessel Plate to the USA, Europe, the Middle East and Southeast Asia for ASME Section VIII work that actually names this Grade. FOB Shanghai / CIF Houston / Rotterdam / Jebel Ali.
Contact SHH STEEL for mill rolling, stock inquiry, dual SA662/A662 marking, impact testing, 3.2 inspection or a quotation.
ASME SA662 Grade C Steel Plate, ASME SA662 GR.C, SA662 Gr.C, SA662GRC, SA-662 Grade C, A662 Grade C, low temp vessel plate, global steel mill sourcing partner SHH STEEL