ASME SA841 Grade F Class 6 Steel Plate | SA841 Gr.F Cl.6 TMCP Vessel Plate
What is ASME SA841 Grade F Class 6 Steel?
ASME SA841 Grade F Class 6 is the lower Class line on Grade F in ASME SA-841/SA-841M. Grade F does not use Class 1 or Class 2. Those Classes belong to Grades A, B and C. Grade D uses Class 3. Grade E uses Class 4 and Class 5. Grade F uses Class 6 and Class 7. Class 6 is the lower Grade F line: 485 MPa yield and 565–705 MPa tensile. Maximum nominal thickness for Grade F is 40 mm. As Direct Mill Supply by SHH STEEL, the plate is produced to ASME SA-841/SA-841M by thermo-mechanical control process.
Buyers write the same product as SA841 Grade F Class 6, SA841 Gr.F Cl.6, SA841GRF CL6, SA-841 Grade F Class 6, SA841 F6 and SA 841 Gr F Cl 6. ASTM A841 Grade F Class 6 is the companion mill specification. A purchase order that only says “SA841 Grade F” is incomplete. Class 7 on the same Grade raises yield to 515 MPa. Those two plates do not interchange.
Do not read the Class number as a simple ladder. Class 6 yield is 485 MPa, the same yield number as Grade E Class 4, not a jump past Class 5. The Class follows the Grade. Grade F chemistry is not Grade E chemistry. Grade F carbon is 0.10% maximum. Manganese is 1.10–1.70%. Nickel max is 0.85%. Molybdenum max is 0.50%. Niobium and vanadium sit higher than on Grade E. That ladle is a different steel.
This page is not SA537 Cl.2. SA537 Class 2 is heat-treated C-Mn-Si. SA841 Grade F Class 6 is TMCP. It is not SA517 Gr.B QT alloy. It is not SA533 Type B Class 1 QT Mn-Mo-Ni. It is not ASME SA516 and not ASME SA387.
Thickness is the second filter. Grade F stops at 40 mm. An 80 mm Class 6 inquiry cannot be rolled as SA841 Grade F. Dual marking SA841 / A841 Grade F Class 6 is available. Certificates can be EN 10204 3.1 or 3.2. Company scope: China steel Mill Agent-SHH STEEL.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Grade / Class | ASME SA841 Grade F Class 6 | Confirmed |
| Product Specification | ASME SA-841/SA-841M | Applied |
| Companion Spec | ASTM A841 Grade F Class 6 | Dual cert available |
| General Requirements | ASME SA-20 / ASTM A20 | Applied |
| Process | TMCP | Confirmed |
| Grain practice | Killed, fine austenitic grain | Applied |
| Alloy idea | Low C, higher Mn-Ni-Mo-Nb-V than Grade E | Confirmed |
| Intended use | Welded pressure vessels | As specified |
| Maximum Thickness | 40 mm for Grade F | Per SA-841 |
| Certification | EN 10204 3.1 or 3.2 / third-party | As ordered |
This plate sits in the pressure vessel steel plates family. It does not sit with carbon steel plates that have no TMCP Class 6 table, and it does not sit with structural steel plates or ASTM A36/A36M. If a buyer sends an HSLA cutting list from ASTM A572 and a vessel drawing on the same email, those are two different books.
SA-20 still governs marking, testing location, retests and repair rules. TMCP does not cancel SA-20. Two tension tests from each plate-as-rolled remain the specification habit unless the order tightens the plan.
Chemical Composition
ASME SA841 Grade F Class 6 uses Grade F chemistry. Class 6 and Class 7 share that table. The Class only changes the tensile line.
Heat Analysis — ASME SA841 Grade F
| Element | Heat Analysis (%) |
|---|---|
| Carbon (C), max | 0.10 |
| Manganese (Mn), t ≤ 40 mm | 1.10 – 1.70 |
| Phosphorus (P), max | 0.020 |
| Sulfur (S), max | 0.008 |
| Silicon (Si) | 0.10 – 0.45 |
| Copper (Cu), max | 0.40 |
| Nickel (Ni), max | 0.85 |
| Chromium (Cr), max | 0.30 |
| Molybdenum (Mo), max | 0.50 |
| Niobium (Nb), max | 0.10 |
| Vanadium (V), max | 0.09 |
Product analysis follows SA-20 / A20 tolerances on those heat limits. Compared with Grade E, Grade F raises manganese, nickel, molybdenum, niobium and vanadium. Carbon is 0.10% maximum versus 0.07% on Grade E. Sulfur is 0.008% maximum versus 0.005% on Grade E. A Grade E ladle cannot be stamped Grade F. A Grade D ladle with 1.0–5.0% nickel cannot be stamped Grade F either.
There is no “over 40 mm” manganese line because Grade F is not permitted over 40 mm. If chromium and molybdenum sit in a SA387 Gr.11 Cl.2 or SA387 Gr.22 Cl.2 window, the plate belongs on the Cr-Mo page. If the process is QT Mn-Mo-Ni, look at SA533 Type B Class 2. If the ladle is carbon only, look at SA516 Gr.70 or SA515 Gr.70.
SHH STEEL reports heat analysis on every certificate, including nickel, molybdenum, niobium and vanadium, and adds product analysis when SA-20 requires it.
Mechanical Properties
Class 6 is the strength line on this page. Grade F only identifies the chemistry family.
Tensile Requirements — ASME SA841 Grade F Class 6
| Property | t ≤ 40 mm |
|---|---|
| Yield strength, min | 485 MPa (70 ksi) |
| Tensile strength | 565 – 705 MPa (82 – 102 ksi) |
| Elongation in 50 mm, min | 20% |
| Density | 7.85 g/cm³ |
| Hardness | Not a Table 3 default |
There is no “over 40 mm” column. The specification marks thicker Class 6 on Grade F as not applicable. Do not quote 65 mm Class 2 numbers from Grades A–C onto this page. Grades A–C never use Class 6.
Class 7 on the same Grade F is 515 MPa yield and 590–730 MPa tensile. A Class 6 heat cannot be stamped Class 7 because the coupon came in high. Grade E Class 4 also uses 485 MPa yield, but the tensile band and the chemistry are not the same. Do not ship Grade E and call it Grade F.
Density is 7.85 g/cm³ for weight take-off. Hardness is not a mandatory SA-841 Table 3 value. Typical TMCP Class 6 plate sits around 170–220 HB. If a drawing writes a hardness cap, put that number on the order. SHH STEEL will then test and print it. Do not read Brinell as a substitute for the 485 MPa yield test.
Charpy is not a hidden default. Export tanks and winter shells almost always add an impact temperature. Write the temperature, energy, location and orientation. Simulated PWHT coupons are common because shops that buy Grade F still want a vessel cycle.
Do not treat 485 MPa yield as permission to substitute high strength low alloy plates, EN 10025-6 structural QT plate, or SA302 Gr.C. Those books have their own chemistry and Code listings.
Material Comparison
| Grade | Route | Strength / thickness | Swap? |
|---|---|---|---|
| SA841 Grade A/B/C Class 2 | TMCP | 415 MPa, to 100 mm | No |
| SA841 Grade D Class 3 | TMCP | 690 MPa, 40 mm max | No |
| SA841 Grade E Class 4 | TMCP | 485 MPa, different chemistry | No |
| SA841 Gr.F Cl.6 | TMCP | 485 MPa, 40 mm max | This page |
| SA841 Grade F Class 7 | TMCP | 515 MPa, same Grade | Same Grade, higher Class |
| SA537 Cl.2 | Heat-treated C-Mn-Si | Similar yield window, not TMCP Grade F | No |
| SA517 Gr.A | QT alloy | Different family | No |
| SA516 Gr.70 | Fine-grain carbon | No Class 6 TMCP | No |
SA299 Gr.B, SA225 Gr.D, SA455 and SA285 Gr.C are also vessel plates. None of them is Grade F Class 6.
The practical question is whether Grade F Class 6 can replace Grade E Class 4 or SA537 Class 2. Only if the drawing names SA-841 Grade F Class 6. Same yield number is not a substitution rule. The chemistry and the 40 mm cap still have to match.
TMCP Vessel Service
ASME SA841 Grade F Class 6 is used when the vessel wants Grade F residuals and the Class 6 tensile table, with the wall inside 40 mm. Designers pick Grade F when they want more manganese, nickel, molybdenum and microalloy than Grade E, without jumping to Grade D Class 3.
Allowable stress comes from ASME Section II Part D after the Code lists this Grade and Class. Do not copy a SA537 Cl.2 allowable and apply it here. Do not copy a Grade E Class 4 allowable onto a Grade F drawing.
Typical components are process shells, heads and courses written specifically to SA-841 Grade F Class 6. It is not cryogenic 3.5Ni plate like SA203 Gr.D or SA203 Gr.E. Grade F nickel is a limited TMCP addition, not a nickel-steel designation. Stainless work belongs on ASME SA240/SA240M, ASTM A240/A240M or stainless steel sheets and plates.
The TMCP temperature cap still applies. Except for Grade G, forming and PWHT stay at or below 650 °C, and only when clause 6.1 and any simulated coupons are satisfied. Do not run a 900 °C normalize on Grade F and expect Class 6 yield to remain.
Weldability
SA841 Gr.F Cl.6 is killed, fine-grain TMCP plate. Welding is Code welding.
Qualify procedures to ASME Section IX. Use low-hydrogen consumables. Carbon at 0.10% maximum is still lean, but manganese, nickel, molybdenum, niobium and vanadium all sit higher than Grade E. Calculate carbon equivalent from the actual ladle. Do not use a Grade A or Grade E worksheet.
Preheat depends on thickness, restraint, hydrogen and the qualified WPS. After welding, many shops want PWHT. That cycle must stay inside the TMCP window and must be proven on mill coupons when the vessel specification already knows the hold.
Do not copy a SA387 Gr.12 Cl.2 Cr-Mo procedure or a SA533 Type A Class 1 QT procedure onto Grade F Class 6 without review. The fabricator owns the WPS. SHH STEEL supplies the plate and the test data.
Heat Treatment
The steel shall be killed and shall meet fine austenitic grain practice under ASME SA-20. Plates shall be produced by TMCP. Slab reheating, reduction schedule, finish temperature and accelerated cooling are the mill tools. There is no mandatory furnace normalize and no mandatory quench and temper in the specified condition.
If the vessel will be warm formed or post-weld heat-treated, the test coupons must follow that cycle. A coupon tested as-rolled does not prove a 620 °C shell hold. Ask for simulated PWHT when the vessel specification already knows the temperature and time.
This is not the normalize route used for SA516 Gr.60. It is not the QT route used for SA537 Cl.1 or SA517 Gr.F. SHH STEEL prints TMCP and Class 6 on the certificate so the inspector does not treat the plate as ordinary as-rolled carbon.
Delivery Condition
Usual delivery is TMCP Grade F Class 6 plate, 8 mm to 40 mm.
The mill test certificate lists ASME SA841 Grade F Class 6 and, when dual certified, ASTM A841 Grade F Class 6; heat number; heat analysis including Ni, Mo, Nb and V; product analysis when ordered; tensile results to the Class 6 table; TMCP statement; impact results when ordered; simulated PWHT results when ordered; and UT when ordered. Surface is vessel-plate quality. Shot blast and shop primer are available.
Certificates may be EN 10204 3.1 or EN 10204 3.2. Third-party surveyors can witness rolling, cooling and testing when the order names the agency.
Dimensions
Usual supply range from SHH STEEL for SA841 Gr.F Cl.6 TMCP vessel plate:
- Thickness: 8 mm – 40 mm. That 40 mm ceiling is the Grade F rule in SA-841, not a mill preference
- Width: 1500 mm – 4000 mm, subject to the Grade F rolling schedule
- Length: 3000 mm – 12000 mm
- Cut-to-length shells, dish-head blanks and nest sizes inside those limits
A 45 mm inquiry is outside Grade F. Do not “see if the mill can roll it” and still stamp SA841 Grade F Class 6. Grades A, B and C go to 100 mm, but they do not carry Class 6.
Structural lengths belong on EN 10025-2 or JIS G3106. Weathering plate belongs on EN 10025-5 or Corten A/B. Fine-grain structural belongs on EN 10025-3 or EN 10025-4. QT structural belongs on EN 10025-6.
Tolerances
Dimensional limits follow ASME SA-20. Thickness tolerance, width, length, flatness and camber are vessel-plate rules.
TMCP plate can move during accelerated cooling. Flatness should be written if the head shop is tight. Ultrasonic testing to A435, A577 or A578 is common on Grade F plate. Extra-flatness and edge-camber limits are negotiated items, not assumed extras.
Supplementary Requirements
Most export ASME SA841 Grade F Class 6 orders add extras. The specification does not assume them.
Charpy V-notch. Temperature, absorbed energy, specimen location and orientation.
Simulated PWHT and warm forming. Same-heat coupons follow the vessel cycle. Tensile and impact are then run on those coupons.
NDE. UT to A435 / A577 / A578. Edge MT or PT after cutting when the shop wants it.
Restricted P, S and CEV. When specified.
Through-thickness / Z testing. When lamellar tearing is a design concern.
Third-party inspection. EN 10204 3.2, with the agency named on the order.
If an item is not written, it is not tested and it is not printed as if it were.
Equivalent Material Grades
There is no one-to-one dual stamp outside ASTM A841. The names below are project comparisons. Chemistry, TMCP route, 40 mm cap and impact temperature still have to match the purchase order.
| Designation | Standard | Notes |
|---|---|---|
| ASME SA841 Grade F Class 6 / SA841 Gr.F Cl.6 | ASME SA-841/SA-841M | Code name on this page |
| ASTM A841 Grade F Class 6 | ASTM A841/A841M | Companion spec; dual mark available |
| SA841 Grade F Class 7 | SA-841 | Same Grade, 515 MPa Class |
| EN 10028-5 P460M / P460ML | EN | Closest common TMCP vessel comparison |
| EN 10028-6 P500Q related | EN | QT comparison, not TMCP Grade F |
| JIS G3115 SPV450 / SPV490 | JIS | Pressure-vessel comparison; confirm process and impact |
| JIS G3124 related | JIS | Confirm TMCP and 40 mm cap |
| GB/T 19189 07MnNiMoDR / 07MnNiMoVDR related | GB | Chinese TMCP / QT vessel comparison; confirm route |
| GB 713 Q370R / Q420R related | GB | Strength talk only |
| DIN EN 10028-5 P460M | DIN / EN | Current German path is EN, not old DIN 17155 |
| DIN 17102 TStE 460 / 500 related | DIN (historical) | Do not stamp as SA841 |
| ASME SA537 Class 2 | SA-537 | Heat-treated, not TMCP |
| ASTM A537 Cl.2 | A537 | Same caution |
DIN 17100, ASTM A516, ASME SA515 and ASTM A285 are not Grade F Class 6. SHH STEEL will dual-certify SA841 / A841. EN, JIS or GB dual marking is only when the mill heat meets both books and the order says so.
Applications
| Industry | Typical components |
|---|---|
| Pressure vessels | ASME SA841 Grade F Class 6 shells and SA841 Gr.F Cl.6 heads to 40 mm |
| Process equipment | SA-841 Gr.F Cl.6 TMCP courses |
| Dual-certified export | SA841 / A841 Grade F Class 6 plate |
| Fabrication | SA841 Gr.F Cl.6 cut to nest sizes inside 40 mm |
Ship plate inquiries belong on shipbuilding steel plates or BV Rules. Weathering inquiries belong on weathering steel plates. Stainless inquiries belong on stainless steel products, JIS G4305 or AISI stainless.
Other vessel comparisons: SA203 Gr.B, SA302 Gr.C, A516 Gr.70, SA533 Type C Class 2, SA517 Gr.P.
Why Choose SHH STEEL
SHH STEEL works as a China Mill Direct Exporter for plates to ASME SA-841/SA-841M. On ASME SA841 Grade F Class 6 that means mill pricing, dual SA841/A841 marking, Grade F chemistry with manganese in the 1.10–1.70% band and molybdenum to 0.50%, recorded TMCP delivery, Class 6 tensile results at 485 MPa yield and 565–705 MPa tensile, the 40 mm ceiling respected, 3.1 as standard and 3.2 when specified.
We keep Grade and Class on the order. Grade F Class 6 is not Grade F Class 7. Grade F is not Grade E and is not Grade D. SA841 is not SA516 Gr.55. SA841 is not SA387 Gr.91 Cl.2. SA841 Gr.F Cl.6 is not SA533 Type C Class 1. If the drawing names 80 mm at this Grade, we will say Grade F cannot be used. If it names Class 7, we will not ship Class 6 and call it close. If the shop plans a 900 °C form, we will say TMCP is the wrong process before the slab is booked.
Company scope: China steel Mill Agent-SHH STEEL.
FAQ
-
What names are used for ASME SA841 Grade F Class 6?
- Buyers write SA841 Grade F Class 6, SA841 Gr.F Cl.6, SA841GRF CL6, SA-841 Grade F Class 6, SA841 F6 and SA 841 Gr F Cl 6. SHH STEEL prints the wording on the purchase order.
-
Is ASME SA841 Grade F Class 6 the same as ASTM A841 Grade F Class 6?
- Chemistry and tensile limits match. ASME SA-841 is the Code version. ASTM A841 is the product spec. As China mill-Direct Supply, SHH STEEL dual-certifies both names when the vessel must be stamped.
-
What is the yield strength of SA841 Gr.F Cl.6?
- 485 MPa minimum. Tensile is 565–705 MPa. Elongation is 20% in 50 mm. Those numbers apply only through 40 mm.
-
How is Class 6 different from Class 7 on Grade F?
- Same Grade F chemistry. Class 6 is 485 MPa yield and 565–705 MPa tensile. Class 7 is 515 MPa yield and 590–730 MPa tensile. Follow the Class on the drawing.
-
How is Grade F different from Grade E?
- Grade F has higher manganese, nickel, molybdenum, niobium and vanadium. Carbon max is 0.10% versus 0.07% on Grade E. Same 40 mm cap. Do not swap the ladles.
-
What is the closest EN, JIS, GB or DIN grade of SA841 Grade F Class 6?
- EN 10028-5 P460M / P460ML is the usual TMCP comparison for this yield window. JIS G3115 SPV450 / SPV490 and GB/T 19189 related vessel steels are project comparisons. Old DIN names are historical. None of them is an automatic dual stamp.
-
Is SA841 Grade F Class 6 the same as SA537 Class 2?
- No. The yield window can look similar. SA537 Class 2 is heat-treated. SA841 Grade F Class 6 is TMCP and stops at 40 mm.
-
Can the plate be hot formed like normalized carbon plate?
- Not without a planned cycle. Forming and PWHT are normally held at or below 650 °C, with simulated coupons when required.
Conclusion
ASME SA841 Grade F Class 6 Steel Plate is TMCP pressure-vessel plate under ASME SA-841/SA-841M, limited to 40 mm, with 485 MPa yield and 565–705 MPa tensile. Whether the inquiry says SA841 Grade F Class 6, SA841 Gr.F Cl.6, SA841GRF CL6 or SA-841 Grade F Class 6, SHH STEEL supplies plate with Grade F chemistry, recorded TMCP delivery, Class 6 tensile results, and EN 10204 3.1 or 3.2 certification.
As a China mill Distributor, SHH STEEL provides ASME SA841 Grade F Class 6 / SA841 Gr.F Cl.6 TMCP Vessel Plate for ASME Section VIII work that actually names this Grade and Class.
Contact SHH STEEL for mill rolling, dual SA841/A841 marking, simulated PWHT testing, 3.2 inspection or a quotation.
ASME SA841 Grade F Class 6 Steel Plate, SA841 Gr.F Cl.6, SA841GRF CL6, SA-841 Grade F Class 6, TMCP vessel plate, Direct Mill Supply by SHH STEEL