SHH STEEL offers ASTM A203-compliant Grade D/E/F nickel-alloy steel plates. ASTM A203 specifies plates for welded pressure vessels designed for low-temperature service. Excellent ductility, certified quality, competitive prices, customizable. Trust SHH STEEL!

ASTM A203 Grade F Steel Plate | A203 Gr.F QT Nickel Steel Plate - SHH STEEL

ASTM A203 Grade F Steel Plate | A203 Gr.F QT Nickel Steel Plate

ASTM A203 Grade F is a 3.5% nickel quenched-and-tempered pressure vessel plate. Yield 380 MPa (≤50 mm) or 345 MPa (>50 mm). SHH STEEL supplies A203 Gr.F / SA203 Gr.F as China mill-Direct Supply with 3.1 or 3.2 certificates.
View More
ASTM A203 Grade E Steel Plate | A203 Gr.E 3.5Ni Pressure Vessel Plate - SHH STEEL

ASTM A203 Grade E Steel Plate | A203 Gr.E 3.5Ni Pressure Vessel Plate

ASTM A203 Grade E is a 3.5% nickel alloy steel plate for welded pressure vessels. Yield 275 MPa, tensile 485–620 MPa. SHH STEEL supplies A203 Gr.E / SA203 Gr.E as China mill-Direct Supply with 3.1 or 3.2 certificates.
View More
ASTM A203 Grade D Steel Plate | A203 Gr.D 3.5Ni Low Temperature Plate - SHH STEEL

ASTM A203 Grade D Steel Plate | A203 Gr.D 3.5Ni Low Temperature Plate

ASTM A203 Grade D is a 3.5% nickel alloy steel plate for welded low-temperature pressure vessels. Yield 255 MPa, tensile 450–585 MPa. SHH STEEL supplies A203 Gr.D / SA203 Gr.D as China mill-Direct Supply with 3.1 or 3.2 certificates.
View More
ASTM A203 Grade B Steel Plate | A203 Gr.B 2.25Ni Pressure Vessel Plate - SHH STEEL

ASTM A203 Grade B Steel Plate | A203 Gr.B 2.25Ni Pressure Vessel Plate

ASTM A203 Grade B is a 2.25% nickel alloy steel plate for welded pressure vessels. Yield 275 MPa, tensile 485–620 MPa. SHH STEEL supplies A203 Gr.B / SA203 Gr.B as China mill-Direct Supply with mill pricing and full MTCs.
View More
ASTM A203 Grade A Steel Plate | A203 Gr.A Nickel Pressure Vessel Plate - SHH STEEL

ASTM A203 Grade A Steel Plate | A203 Gr.A Nickel Pressure Vessel Plate

ASTM A203 Grade A is a 2.25% nickel alloy steel plate for welded low-temperature pressure vessels. Tensile 450–585 MPa, yield 255 MPa. SHH STEEL supplies A203 Gr.A / SA203 Gr.A as China mill-Direct Supply with mill pricing and full MTCs.
View More

Nuclear-Grade Steel Plates

SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.