Product Showcase
ASME SA533/SA533M Carbon Steel Plates
SHH STEEL offers ASME SA533/SA533M-compliant quenched and tempered Mn-Mo and Mn-Mo-Ni alloy steel plates. SA533/SA533M specifies plates for welded pressure vessels in nuclear and high-temp applications. Tough, impact-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASME SA533 Type C Class 3 Steel Plate | SA533 Gr.C Cl.3 Mn-Mo-Ni Vessel Plate
ASME SA533 Type C Class 3 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Type C has the highest nickel band. Tensile 690–860 MPa, yield 570 MPa, max 65 mm. SHH STEEL supplies SA533 Type C Cl.3 / A533 Gr.C Cl.3 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type C Class 2 Steel Plate | SA533 Gr.C Cl.2 Mn-Mo-Ni Vessel Plate
ASME SA533 Type C Class 2 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Type C has the highest nickel band. Tensile 620–795 MPa, yield 485 MPa. SHH STEEL supplies SA533 Type C Cl.2 / A533 Gr.C Cl.2 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type D Class 1 Steel Plate | SA533 Gr.D Cl.1 Mn-Mo-Ni Vessel Plate
ASME SA533 Type D Class 1 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Type D has the lowest nickel band. Tensile 550–690 MPa, yield 345 MPa. SHH STEEL supplies SA533 Type D Cl.1 / A533 Gr.D Cl.1 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type D Class 3 Steel Plate | SA533 Gr.D Cl.3 Mn-Mo-Ni Vessel Plate
ASME SA533 Type D Class 3 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Type D has the lowest nickel band. Tensile 690–860 MPa, yield 570 MPa, max 65 mm. SHH STEEL supplies SA533 Type D Cl.3 / A533 Gr.D Cl.3 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type D Class 2 Steel Plate | SA533 Gr.D Cl.2 Mn-Mo-Ni Vessel Plate
ASME SA533 Type D Class 2 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Type D has the lowest nickel band. Tensile 620–795 MPa, yield 485 MPa. SHH STEEL supplies SA533 Type D Cl.2 / A533 Gr.D Cl.2 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type C Class 1 Steel Plate | SA533 Gr.C Cl.1 Mn-Mo-Ni Vessel Plate
ASME SA533 Type C Class 1 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Type C has the highest nickel band. Tensile 550–690 MPa, yield 345 MPa. SHH STEEL supplies SA533 Type C Cl.1 / A533 Gr.C Cl.1 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type B Class 3 Steel Plate | SA533 Gr.B Cl.3 Mn-Mo-Ni Vessel Plate
ASME SA533 Type B Class 3 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Tensile 690–860 MPa, yield 570 MPa, max 65 mm. SHH STEEL supplies SA533 Type B Cl.3 / A533 Gr.B Cl.3 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type B Class 2 Steel Plate | SA533 Gr.B Cl.2 Mn-Mo-Ni Vessel Plate
ASME SA533 Type B Class 2 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Tensile 620–795 MPa, yield 485 MPa. SHH STEEL supplies SA533 Type B Cl.2 / A533 Gr.B Cl.2 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type B Class 1 Steel Plate | SA533 Gr.B Cl.1 Mn-Mo-Ni Vessel Plate
ASME SA533 Type B Class 1 is quenched-and-tempered Mn-Mo-Ni vessel plate under ASME SA-533/SA-533M. Tensile 550–690 MPa, yield 345 MPa. SHH STEEL supplies SA533 Type B Cl.1 / A533 Gr.B Cl.1 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type A Class 3 Steel Plate | SA533 Gr.A Cl.3 Mn-Mo Vessel Plate
ASME SA533 Type A Class 3 is quenched-and-tempered Mn-Mo vessel plate under ASME SA-533/SA-533M. Tensile 690–860 MPa, yield 570 MPa, max 65 mm. SHH STEEL supplies SA533 Type A Cl.3 / A533 Gr.A Cl.3 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type A Class 2 Steel Plate | SA533 Gr.A Cl.2 Mn-Mo Vessel Plate
ASME SA533 Type A Class 2 is quenched-and-tempered Mn-Mo vessel plate under ASME SA-533/SA-533M. Tensile 620–795 MPa, yield 485 MPa. SHH STEEL supplies SA533 Type A Cl.2 / A533 Gr.A Cl.2 mill-direct with 3.1 or 3.2 certificates.View More -
ASME SA533 Type A Class 1 Steel Plate | SA533 Gr.A Cl.1 Mn-Mo-Ni Vessel Plate
ASME SA533 Type A Class 1 is quenched-and-tempered Mn-Mo vessel plate under ASME SA-533/SA-533M. Tensile 550–690 MPa, yield 345 MPa. SHH STEEL supplies SA533 Type A Cl.1 / A533 Gr.A Cl.1 mill-direct with 3.1 or 3.2 certificates.View More
ASME SA533/SA533M Carbon Steel Plates
Nuclear-Grade Steel Plates
SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.
Nuclear-Grade Steel Plates
ASME SA542/SA542M
ASME SA543/SA543M
ASME SA612/SA612M
ASME SA662/SA662M
ASME SA737/SA737M
ASME SA202/SA202M
ASTM A202/A202M
ASTM A1017/A1017M
SA-1017/SA-1017M
ASTM A662/A662M
ASME SA724/SA724M
ASME SA736/SA736M
ASME SA832/SA832M
ASME SA533/SA533M
ASTM A533
ASME SA508/SA508M
ASTM A508
ASME SA387/SA387M
ASTM A387/A387M
ASME SA-738/SA-738M
ASTM A738
ASME SA-203/SA-203M
ASTM A203
EN 10028-7
RCC-M M3307
JIS G3118
GB/T 3531
GOST 10859
X